Wissenschaftliche Artikel der BAM
Filtern
Erscheinungsjahr
- 2017 (128) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (105)
- Beitrag zu einem Tagungsband (15)
- Beitrag zu einem Sammelband (3)
- Sonstiges (2)
- Forschungsbericht (2)
- Buchkapitel (1)
Sprache
- Englisch (128) (entfernen)
Schlagworte
- SAXS (5)
- Online NMR Spectroscopy (4)
- Small-angle X-ray scattering (4)
- CONSENS (3)
- Corrosion (3)
- DNA (3)
- Fatigue strength (3)
- Femtosecond laser (3)
- Fracture mechanics (3)
- Ground vibration (3)
Reliable nanomaterial classification of powders using the volume-specific surface area method
(2017)
The volume-specific surface area (VSSA) of a particulate material is one of two apparently very different metrics recommended by the European Commission for a definition of "nanomaterial" for regulatory purposes: specifically, the VSSA metric may classify nanomaterials and non-nanomaterials differently than the median size in number metrics, depending on the chemical composition, size, polydispersity, shape, porosity, and aggregation of the particles in the powder.
Here we evaluate the extent of agreement between classification by electron microscopy (EM) and classification by VSSA on a large set of diverse particulate substances that represent all the anticipated challenges except mixtures of different substances. EM and VSSA are determined in multiple labs to assess also the level of reproducibility. Based on the results obtained on highly characterized benchmark materials from the
NanoDefine EU FP7 project, we derive a tiered screening strategy for the purpose of implementing the definition of nanomaterials. We finally apply the Screening strategy to further industrial materials, which were classified correctly and left only borderline cases for EM.
On platelet-shaped nanomaterials, VSSA is essential to prevent false-negative classification by EM. On porous materials, approaches involving extended Adsorption isotherms prevent false positive classification by VSSA. We find no false negatives by VSSA, neither in Tier 1 nor in Tier 2, despite real-world industrial polydispersity and diverse composition, shape, and coatings. The VSSA screening strategy is recommended for inclusion in a technical guidance for the implementation of the definition.
Halophilic bacteria use a variety of osmoregulatory methods, such as the accumulation of one or more compatible solutes. The wide diversity of compounds that can act as compatible solute complicates the task of understanding the different strategies that halophilic bacteria use to cope with salt. This is specially challenging when attempting to go beyond the pathway that produces a certain compatible solute towards an understanding of how the metabolic network as a whole addresses the problem. Metabolic reconstruction based on genomic data together with Flux Balance Analysis (FBA) is a promising tool to gain insight into this problem. However, as more of these reconstructions become available, it becomes clear that processes predicted by genome annotation may not reflect the processes that are active in vivo. As a case in point, E. coli is unable to grow aerobically on citrate in spite of having all the necessary genes to do it. It has also been shown that the realization of this genetic potential into an actual capability to metabolize citrate is an extremely unlikely event under normal evolutionary conditions. Moreover, many marine bacteria seem to have the same pathways to metabolize glucose but each species uses a different one. In this work, a metabolic network inferred from genomic annotation of the halophilic bacterium Halomonas elongata and proteomic profiling experiments are used as a starting point to motivate targeted experiments in order to find out some of the defining features of the osmoregulatory strategies of this bacterium. This new information is then used to refine the network in order to describe the actual capabilities of H. elongata, rather than its genetic potential.
Experimental and phase field studies of age hardening response of a high purity Al‐4Cu‐1Li‐0.25Mn‐alloy (mass %) during isothermal aging are conducted. In the experiments, two hardening phases are identified: the tetragonal θ′ (Al₂Cu) phase and the hexagonal T1 (Al₂CuLi) phase. Both are plate shaped and of nm size. They are analyzed with respect to the development of their size, number density and volume fraction during aging by applying different analysis techniques in TEM in combination with quantitative microstructural analysis. 3D phase‐field simulations of formation and growth of θ′ phase are performed in which the full interfacial, chemical and elastic energy contributions are taken into account. 2D simulations of T1 phase are also investigated using multi‐component diffusion without elasticity. This is a first step toward a complex phase‐field study of T1 phase in the ternary alloy. The comparison between experimental and simulated data shows similar trends. The still unsaturated volume fraction indicates that the precipitates are in the growth stage and that the coarsening/ripening stage has not yet been reached.
Welding is the most important joining technology. In the steel construction
industry, e.g. production of windmill sections, welding accounts for a
main part of the manufacturing costs and resource consumption. Moreover, social
issues attached to welding involve working in dangerous environments. This aspect
has unfortunately been neglected so far, in light of a predominant focus on economics
combined with a lack of suitable assessment methods. In this chapter,
exemplary welding processes are presented that reduce the environmental and
social impacts of thick metal plate welding. Social and environmental Life Cycle
Assessments for a thick metal plate joint are conducted for the purpose of
expressing and analysing the social and environmental impacts of welding.
Furthermore, it is shown that state-of-the-art technologies like Gas Metal Arc
Welding with modified spray arcs and Laser Arc-Hybrid Welding serve to increase
social and environmental performance in contrast to common technologies, and
therefore offer great potential for sustainable manufacturing.
We report on a study in which plasmid DNA in water was irradiated with 30 keV electrons generated by a scanning electron microscope and passed through a 100 nm thick Si3N4 membrane. The corresponding Monte Carlo simulations suggest that the kinetic energy spectrum of the electrons throughout the water is dominated by low energy electrons (<100 eV). The DNA radiation damage, single-strand breaks (SSB) and double-strand breaks (DSB), was determined by electrophoresis. The median lethal dose of D1/2 = 1.7 ± 0.3 Gy was found to be much smaller compared to partially or fully hydrated DNA irradiated under vacuum conditions. The ratio of DSB to SSB was found to be (1:12) as compared to 1:88) found for hydrated DNA. Our method enables quantitative measurements of radiation damage to biomolecules (DNA, proteins) in solutions under varying conditions (pH, salinity, cosolutes) for an electron energy range which is difficult to probe by standard methods.
We propose the use of alternating pulse wavelengths in a direct-detection coherent optical time domain reflectometry (C-OTDR) setup not only to measure strain and temperature changes but also to determine the correct algebraic sign of the change. The sign information is essential for the intended use in distributed mode shape analysis of civil engineering structures. Correlating relative backscatter signal shifts in the temporal/signal domain allows for measuring with correct magnitude and sign. This novel approach is simulated, experimentally implemented and demonstrated for temperature change measurement at a spatial resolution of 1 m.
Residual stresses and distortions in welded I-girders for steel construction are relevant when evaluating the stability of steel beams and column members. The application of high strength steels allows smaller wall thicknesses compared to conventional steels. Therefore, the risk of buckling has to be considered carefully. Due to the lack of knowledge concerning the residual stresses present after welding in high strength steel components conservative assumptions of their level and distribution is typically applied. In this study I-girders made of steels showing strengths of 355 MPa and 690 MPa were welded with varying heat input. Due to the dimension of the I-girders and the complex geometry the accessibility for residual stress measurement using X-ray diffraction was limited. Therefore, saw cutting accompanied by strain gauge measurement has been used to produce smaller sections appropriate to apply X-ray diffraction. The stress relaxation measured by strain gauges has been added to residual stresses determined by X-ray diffraction to obtain the original stress level and distribution before sectioning. The combination of both techniques can produce robust residual stress values. From practical point of view afford for strain gauge application can be limited to a number of measuring positions solely to record the global amount of stress relaxation. X-ray diffraction can be applied after sectioning to determine the residual stresses with sufficient spatial resolution.
A phosphaphenanthrene and triazinetrione group containing flame retardant (TAD) is combined with organically modified montmorillonite (OMMT) in epoxy resin thermosets (EP) to improve the performance of the flame-retardant system. When only 1 wt% OMMT/4 wt% TAD is introduced into the EP, the limited oxygen index (LOI) rises from 26% to 36.9% and a V-0 rating is achieved in a UL 94 test. The decomposition and pyrolysis products in the gas phase and condensed phase were characterized using thermogravimetry-Fourier transform infrared spectroscopy (TG-FTIR). The influence on the decomposition of EP, such as the increase in char yield, is limited with the incorporation of OMMT; a large amount of the phosphorus is released into the gas phase. The flame-retardant effect evaluation based on cone calorimeter data testified that OMMT improves the protective-barrier effect of the fire residue of OMMT/TAD/EP on the macroscopic scale, while TAD mainly causes flame inhibition. The fire residues showed a corresponding macroscopic appearance (digital photo) and microstructure (scanning electron microscope [SEM] results). The protective barrier effect of OMMT and the flame-inhibition effect of TAD combined to exert a superior flame-retardant effect, resulting in sufficient flame-retardant performance of OMMT/TAD/EP