Wissenschaftliche Artikel der BAM
Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (2095)
- Beitrag zu einem Tagungsband (388)
- Forschungsbericht (19)
- Beitrag zu einem Sammelband (10)
- Buchkapitel (9)
- Sonstiges (7)
- Tagungsband (Herausgeberschaft für den kompletten Band) (2)
- Corrigendum (2)
- Dissertation (1)
- Zeitschriftenheft (Herausgeberschaft für das komplette Heft) (1)
Sprache
- Englisch (2297)
- Deutsch (233)
- Mehrsprachig (3)
- Portugiesisch (1)
Schlagworte
- Additive manufacturing (69)
- Fluorescence (56)
- Nanoparticles (48)
- Concrete (46)
- SAXS (46)
- Ultrasound (38)
- Corrosion (37)
- MALDI-TOF MS (37)
- Quantum yield (36)
- Non-destructive testing (34)
Organisationseinheit der BAM
- 8 Zerstörungsfreie Prüfung (451)
- 6 Materialchemie (448)
- 1 Analytische Chemie; Referenzmaterialien (358)
- 7 Bauwerkssicherheit (232)
- 5 Werkstofftechnik (218)
- 9 Komponentensicherheit (216)
- 4 Material und Umwelt (198)
- 6.3 Strukturanalytik (172)
- 8.5 Röntgenbildgebung (139)
- 6.1 Oberflächen- und Dünnschichtanalyse (102)
- 8.2 Zerstörungsfreie Prüfmethoden für das Bauwesen (101)
- 5.1 Mikrostruktur Design und Degradation (79)
- 9.3 Schweißtechnische Fertigungsverfahren (79)
- 1.2 Biophotonik (73)
- 6.6 Physik und chemische Analytik der Polymere (72)
- 9.4 Integrität von Schweißverbindungen (70)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (68)
- 8.4 Akustische und elektromagnetische Verfahren (67)
- 6.2 Material- und Oberflächentechnologien (63)
- 1.1 Anorganische Spurenanalytik (61)
- 7.4 Baustofftechnologie (61)
- 3 Gefahrgutumschließungen; Energiespeicher (57)
- 6.5 Synthese und Streuverfahren nanostrukturierter Materialien (57)
- 8.3 Thermografische Verfahren (57)
- 1.4 Prozessanalytik (56)
- 4.1 Biologische Materialschädigung und Referenzorganismen (56)
- 1.7 Organische Spuren- und Lebensmittelanalytik (55)
- 6.0 Abteilungsleitung und andere (51)
- 8.0 Abteilungsleitung und andere (50)
- 8.6 Faseroptische Sensorik (50)
- 1.5 Proteinanalytik (49)
- 1.8 Umweltanalytik (43)
- 5.2 Metallische Hochtemperaturwerkstoffe (42)
- 4.3 Schadstofftransfer und Umwelttechnologien (41)
- 7.2 Ingenieurbau (40)
- 5.4 Multimateriale Fertigungsprozesse (39)
- 1.9 Chemische und optische Sensorik (38)
- 9.0 Abteilungsleitung und andere (35)
- 9.2 Versuchsanlagen und Prüftechnik (32)
- 4.2 Material-Mikrobiom Wechselwirkungen (31)
- 2 Prozess- und Anlagensicherheit (29)
- 4.0 Abteilungsleitung und andere (29)
- 5.3 Polymere Verbundwerkstoffe (29)
- 4.5 Kunst- und Kulturgutanalyse (28)
- 5.5 Materialmodellierung (27)
- 5.6 Glas (27)
- S Qualitätsinfrastruktur (27)
- 2.1 Sicherheit von Energieträgern (26)
- 7.6 Korrosion und Korrosionsschutz (26)
- 4.4 Thermochemische Reststoffbehandlung und Wertstoffrückgewinnung (24)
- 9.5 Tribologie und Verschleißschutz (23)
- 9.6 Additive Fertigung metallischer Komponenten (23)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (22)
- VP Vizepräsident (22)
- VP.1 eScience (22)
- 7.1 Baustoffe (21)
- 1.3 Instrumentelle Analytik (19)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (17)
- 5.0 Abteilungsleitung und andere (17)
- 1.6 Anorganische Referenzmaterialien (16)
- S.2 Digitalisierung der Qualitätsinfrastruktur (16)
- 7.7 Modellierung und Simulation (15)
- 1.0 Abteilungsleitung und andere (13)
- 7.0 Abteilungsleitung und andere (13)
- P Präsident (11)
- 3.2 Gefahrguttanks und Unfallmechanik (10)
- 3.5 Sicherheit von Gasspeichern (10)
- P.0 Präsident und andere (10)
- 6.7 Materialsynthese und Design (9)
- 7.3 Brandingenieurwesen (9)
- 3.4 Sicherheit von Lagerbehältern (8)
- 6.4 Materialinformatik (8)
- 3.6 Elektrochemische Energiematerialien (7)
- S.3 Ökodesign und Energieverbrauchskennzeichnung (7)
- 3.0 Abteilungsleitung und andere (5)
- S.1 Qualität im Prüfwesen (5)
- 4.6 Molekulare und angewandte Entomologie (3)
- 2.0 Abteilungsleitung und andere (2)
- 2.2 Prozesssimulation (2)
- 2.3 Einstufung von Gefahrstoffen und -gütern (1)
- 2.5 Konformitätsbewertung Explosivstoffe/Pyrotechnik (1)
- 3.3 Sicherheit von Transportbehältern (1)
- KM Kommunikation, Marketing (1)
- PST Präsidiale Stabsstelle (1)
- VP.2 Informationstechnik (1)
Paper des Monats
- ja (72)
We present a systematic study on the effect of surface ligands on the luminescence properties and colloidal stability of β-NaYF4:Yb3+,Er3+ upconversion nanoparticles (UCNPs), comparing nine different surface coatings to render these UCNPs water-dispersible and bioconjugatable. A prerequisite for this study was a large-scale synthetic method that yields ~2 g per batch of monodisperse oleate-capped UCNPs providing identical core particles. These ~23 nm sized UCNPs display an upconversion quantum yield of ~0.35% when dispersed in cyclohexane and excited with a power density of 150 W cm-2, underlining their high quality. A comparison of the colloidal stability and luminescence properties of these UCNPs, subsequently surface modified with ligand exchange or encapsulation protocols, revealed that the ratio of the green (545 nm) and red (658 nm) emission bands determined at a constant excitation power density clearly depends on the surface chemistry. Modifications relying on the deposition of additional (amphiphilic) layer coatings, where the initial oleate coating is retained, show reduced non-radiative quenching by water as compared to UCNPs that are rendered water-dispersible via ligand exchange. Moreover, we could demonstrate that the brightness of the upconversion luminescence of the UCNPs is strongly affected by the type of surface modification, i.e., ligand exchange or encapsulation, yet hardly by the chemical nature of the ligand.
Polyglycerol (PG) coated polypropylene (PP) films were synthesized in a two-step approach that involved plasma bromination and subsequently grafting hyperbranched polyglycerols with very few amino functionalities. The influence of different molecular weights and density of reactive linkers were investigated for the grafted PGs. Longer bromination times and higher amounts of linkers on the surface afforded long-term stability. The protein adsorption and bacteria attachment of the PP-PG films were studied. Their extremely low amine content proved to be beneficial for preventing bacteria attachment.
In- and quasielastic neutron scattering is employed to investigate both the vibrational density of states and the molecular dynamics of two homologous discotic liquid crystals (DLC) with different length of the alkyl side chain based on a triphenylene derivate. For both compounds characteristic low frequency excess contributions to the vibrational density of states are found. Therefore it is concluded that these liquid crystals show a glass-like behaviour. Elastic scans further show that in these materials a rich molecular dynamics takes place.
This paper reflects recent progress in the field of fluorescent polymer optical fiber sensors (F-POF) for partial discharge (PD) detection in high voltage (HV) cable accessories using optical-only PD detection by coincidence single photon counting. In experiments with artificial PD sources these sensors show the ability to detect optical emissions from picocoulomb-level PDs in a real-scale model of a translucent high voltage cable accessory. False positives (caused by detector noise) are efficiently suppressedwhile maintaining sufficient sensitivity,even when the sensor is located in an unfavorable position.
This report is the result of a comprehensive study on the available CMs which come potentially in question for the reliable analysis of the number based size distribution of a nanomaterial according to the EC recommendation for a definition of nanomaterial. Based on the performance criteria already established in NanoDefine the potential CMs are evaluated according to studies available in the literature as well as following the expertise of the NanoDefine consortium partners. The specific advantages and disadvantages of each method with respect to its applicability to the scope of NanoDefine are particularly highlighted. An CM evaluation table is produced so that the mostly suited CMs with respect to the EC definition can be grouped and recommended to the corresponding NanoDefine work packages for further specific development (improvement and adaption), or for direct validation and standardisation, respectively. The actual evaluation report including the recommended CMs will be revised and, if necessary, eventually updated at the mid time of the project. The update will be jointly discussed in the NanoDefine consortium on the basis of the results of testing the methods on the NanoDefine real world materials.
Recommendations on a Revision of the EC Definition of Nanomaterial Based on Analytical Possibilities
(2015)
In October 2011 the European Commission (EC) published a "Recommendation on the definition of nanomaterial" (2011/696/EU), to promote consistency in the interpretation of the term "nanomaterial" for legislative and policy purposes in the EU. The EC NM Definition includes a commitment to its review in the light of experience and of scientific and technological developments. This review is ongoing in 2015 and as a contribution to the review the Joint Research Centre of the European Commission (JRC) has already developed a series of three scientific-technical reports with the title: “Towards a review of the EC Recommendation for a definition of the term nanomaterial” which provides to the EC policy services science-based options on how the definition could be revised or supported with additional guidance.
The overarching nature and wide scope of the EC NM Definition, as it does not exclude a priori any particulate material regardless the state, form and size, creates many analytical challenges in its imple-mentation for all stakeholders, including enterprises and regulators.
The NanoDefine project has as core objective to support the implementation of the EC NM Definition. In this report key aspects of the EC NM Definition are addressed, with the goal to improve the implement-ability of the EC NM Definition. These aspects are presented and discussed based on the results of two years of research performed within the framework of the project. As a result this report assesses how well the requirements of the EC NM Definition can be fulfilled with currently available analytical possi-bilities. It presents recommendations and options on a revision of the EC NM Definition to improve the implementability of the definition based on currently available analytical possibilities, according to the state of the art of mid-2015.
Of the technical issues considered in this report, the following seem to deserve the most attention in terms of clarification of the definition and/or provision of additional implementation guidance:
The term ‘external dimension’.
A clear definition of 'External dimension' should be included in the text of the EC NM definition and more precise guidance on what is considered as an external dimension and how to properly character-ise it should be provided.
The ‘number based particle size distribution‘.
The EC NM Definition uses a threshold related to the number based size distribution of particles. Yet most of the easily available techniques provide a mass-, volume- or scattered light intensity-based size distribution which needs to be converted into a number based distribution to be used for regulatory pur-poses. A specific guidance on the conditions under which these methods can be used to identify a na-nomaterial by employing appropriate quantity or metrics conversion should be provided.
The ‘polydispersity‘ and ‘upper size limit‘
Polydispersity is a challenge for the measurement of particle size distribution for the EC NM definition, specifically for materials with high polydispersity index and broad size distribution especially when the volume or mass of the fraction containing particles below 100 nm is very small. Therefore a dedicated guidance should be provided that allows applying an upper size limit in measurements and particle statistics.
Selective Electron Beam Melting (SEBM) is a promising powder bed Additive Manufacturing technique for near-net-shape manufacture of high-value titanium components. However without post-manufacture HIPing the fatigue life of SEBM parts is currently dominated by the presence of porosity. In this study, the size, volume fraction, and spatial distribution of the pores in model samples have been characterised in 3D, using X-ray Computed Tomography, and correlated to the process variables. The average volume fraction of the pores (b0.2%) was measured to be lower than that usually observed in competing processes, such as selective laser melting, but a strong relationship was found with the differentbeamstrategies used to contour ,and infill by hatching, a part section. The majority of pores were found to be small spherical gas pores, concentrated in the infill hatched region; this was attributed to the lower energy density and less focused beam used in the infill strategy allowing less opportunity for gas bubbles to escape the melt pool. Overall, increasing the energy density or focus of the beam was found to correlate strongly to a reduction in the level of gas porosity. Rarer irregular shaped pores were mostly located in the contour region and have been attributed to a lack of fusion between powder particles.
Sicherheitsrelevante und zyklisch hoch belastete Bauteile erfordern zur Vermeidung von kostenintensiven Ausfällen besonders stabile Prozessparameter. Bereits sehr kleine Randzonenfehler können unter zyklischer Bauteilbelastung zu Risswachstum und letztendlich zum Bauteilversagen führen. Die frühzeitige Erkennung von Randzonenfehler in Hochleistungsbauteilen wie z.B. Zahnräder, Ritzelwellen und Kurbelwellen erfordert daher eine leistungsfähige zerstörungsfreie Oberflächenrissprüfung, die es ermöglicht in den hochbeanspruchten Funktionsflächen auch Härterisse, Schleifrisse oder Zundereinschlüsse zu detektieren.
Hierzu sind in den letzten Jahren einige neue, innovative Oberflächenprüfverfahren wie die laserangeregte Thermografie und die Streuflussprüfung mit hochauflösenden GMR-Sensoren oder magnetooptischen Verfahren entwickelt worden. Zusätzlich zur hohen Empfindlichkeit zeichnen sich diese innovativen Verfahren durch einen schnellen und teils auch berührungslosen Einsatz aus. Da die noch relativ neu-en Verfahren naturgemäß noch nicht normativ verankert sind, wurden auch bereits erste Validierungen durchgeführt. Um die Leistungsfähigkeit der Verfahren eingehend zu untersuchen, erfolgten Testreihen an verschiedenen Testkörpern in Bezug auf Ortsauflösung, Empfindlichkeit, Automatisierung und Bewertung der Messsig-nale.
Neben den neuen Verfahren und ihren ersten Schritten hin zur Validierung kamen als Referenz auch die „klassischen“ Verfahren der Magnetpulver- und Wirbelstromprüfung zum Einsatz, deren Leistungsfähigkeit durch angepasste Sondenentwicklung auch für sehr kleine Oberflächendefekte nochmals unter Beweis gestellt wurde. Zusätzlich wurde an einigen Testkörpern eine hochauflösende CT durchgeführt. Die Ergebnisse dieses Vergleiches werden vorgestellt und Möglichkeiten sowie Grenzen der einzelnen Verfahren herausgearbeitet.
Absorption effects in total reflection X-ray fluorescence (TXRF) analysis are important to consider, especially if external calibration is to be applied. With a color X-ray camera (CXC), that enables spatially and energy resolved XRF analysis, the absorption of the primary beam was directly visualized for mL-droplets and an array of pL-droplets printed on a Si-wafer with drop-on-demand technology. As expected, deposits that are hit by the primary beam first shade subsequent droplets, leading to a diminished XRF signal. This shading effect was quantified with enhanced precision making use of sub-pixel analysis that improves the spatial resolution of the camera. The measured absorption was compared to simulated results using three different model calculations. It was found they match very well (average deviation < 10%). Thus errors in quantification due to absorption effects can be accounted for in a more accurate manner.
The reaction of iron chlorides with an alkaline reagent is one of the most prominent methods for the synthesis of iron oxide nanoparticles. We studied the particle formation mechanism using triethanolamine as reactant and stabilizing agent. In situ fast-X-ray absorption near edge spectroscopy and small-angle X-ray scattering provide information on the oxidation state and the structural information at the same time. In situ data were complemented by ex situ transmission electron microscopy, wide-angle X-ray scattering and Raman analysis of the formed nanoparticles. The formation of maghemite nanoparticles (γ-Fe2O3) from ferric and ferrous chloride was investigated. Prior to the formation of these nanoparticles, the formation and conversion of intermediate phases (akaganeite, iron(II, III) hydroxides) was observed which undergoes a morphological and structural collapse. The thus formed small magnetite nanoparticles (Fe3O4) grow further and convert to maghemite with increasing reaction time.
The color X-ray camera SLcam® is a full-field, single photon detector providing scanning-free, energy and spatially resolved X-ray imaging. Spatial resolution is achieved with the use of polycapillary optics guiding X-ray photons from small regions on a sample to distinct energy dispersive pixels on a charged-coupled device detector. Applying sub-pixel resolution, signals from individual capillary channels can be distinguished. Therefore, the SLcam® spatial resolution, which is normally limited to the pixel size of the charge-coupled device, can be improved to the size of individual polycapillary channels. In this work a new approach to a sub-pixel resolution algorithm comprising photon events also from the pixel centers is proposed. The details of the employed numerical method and several sub-pixel resolution examples are presented and discussed.
Effect of fluorescent staining on size measurements of polymeric nanoparticles using DLS and SAXS
(2015)
The influence of fluorescence on nanoparticle size measurements using dynamic light scattering (DLS) and small angle X-ray scattering (SAXS) was investigated. For this purpose, two series of 100 nm-sized polymer nanoparticles stained with different concentrations of the fluorescent dyes DY555 and DY680 were prepared, absorbing/emitting at around 560 nm/590 nm and 695 nm/715 nm, respectively. SAXS measurements of these particle series and a corresponding blank control (without dye) revealed similar sizes of all particles within an uncertainty of 1 nm. DLS measurements carried out at three different laboratories using four different DLS instruments and two different laser wavelengths, i.e., 532 nm and 633 nm, revealed also no significant changes in size (intensity-weighted harmonic mean diameter, ZAverage) and size distribution (polydispersity index, PI) within and between the two dye-stained particle series and the blank sample. Nevertheless, a significant decrease of the detected correlation coefficients was observed with increasing dye concentration, due to the increased absorption of the incident light and thus, less coherent light scattering. This effect was wavelength dependent, i.e. only measurable for the dye-stained particles that absorb at the laser wavelength used for the DLS measurements.
This paper describes the production and characteristics of the nanoparticle test materials prepared for common use in the collaborative research project NanoChOp (Chemical and optical characterization of nanomaterials in biological systems), in casu suspensions of silica nanoparticles and CdSe/CdS/ZnS quantum dots (QDs). This paper is the first to illustrate how to assess whether nanoparticle test materials meet the requirements of a "reference material" (ISO Guide 30, 2015) or rather those of the recently defined category of "representative test material (RTM)" (ISO/TS 16195, 2013). The NanoChOp test materials were investigated with small-angle X-ray scattering (SAXS), dynamic light scattering (DLS), and centrifugal liquid sedimentation (CLS) to establish whether they complied with the required monomodal particle size distribution. The presence of impurities, aggregates, agglomerates, and viable microorganisms in the suspensions was investigated with DLS, CLS, optical and electron microscopy and via plating on nutrient agar. Suitability of surface functionalization was investigated with attenuated total reflection Fourier transform infrared spectrometry (ATR-FTIR) and via the capacity of the nanoparticles to be fluorescently labeled or to bind antibodies. Between-unit homogeneity and stability were investigated in terms of particle size and zeta potential. This paper shows that only based on the outcome of a detailed characterization process one can raise the status of a test material to RTM or reference material, and how this status depends on its intended use.
In order to assess the anisotropy-related uncertainties of relatively determined photoluminescence quantum yields (ΦPL) of molecular emitters and luminescent nanomaterials, we compared ΦPL values measured without and with polarizers using magic angle conditions and studied systematically the dependence of the detected emission intensity on the polarizer settings for samples of varying anisotropy. This includes a dispersion of a spherical quantum dot (QD) with an ideally isotropic emission, a solution of a common small organic dye in a fluid solvent as well as dispersions of elongated quantum dot rods (QDR) with an anisotropic luminescence and a small organic dye in a rigid polymeric matrix, as ideally anisotropic emitter. Our results show that for instruments lacking polarizers, anisotropy-related measurement uncertainties of relative photoluminescence quantum yields can amount to more than 40%, with the size of these systematic errors depending on the difference in emission anisotropy between the sample and the standard.
Melt flow and dripping of the pyrolysing polymer melt can be both a benefit and a detriment during a fire. In several small-scale fire tests addressing the ignition of a defined specimen with a small ignition source, well-adjusted melt flow and dripping are usually beneficial to pass the test. The presence of flame retardants often changes the melt viscosity crucially. The influence of certain flame retardants on the dripping behaviour of four commercial polymers, poly(butylene terephthalate) (PBT), polypropylene (PP), polypropylene modified with ethylene-propylene rubber (PP-EP) and polyamide 6 (PA 6), is analysed based on an experimental monitoring of the mass loss due to melt dripping, drop size and drop temperature as a function of the furnace temperature applied to a rod-shaped specimen. Investigating the thermal transition (DSC), thermal and thermo-oxidative decomposition, as well as the viscosity of the polymer and collected drops completes the investigation. Different mechanisms of the flame retardants are associated with their influence on the dripping behaviour in the UL 94 test. Reduction in decomposition temperature and changed viscosity play a major role. A flow limit in flame-retarded PBT, enhanced decomposition of flame-retarded PP and PP-EP and the promotion of dripping in PA 6 are the salient features discussed.
In this work, sample losses of silver nanoparticles (Ag NPs) in asymmetrical flow field-flow fractionation (AF4) have been systematically investigated with the main focus on instrumental conditions like focusing and cross-flow parameters as well as sample concentration and buffer composition. Special attention was drawn to the AF4 membrane. For monitoring possible silver depositions on the membrane, imaging laser ablation coupled to inductively coupled plasma mass spectrometry (LA-ICP-MS) was used. Our results show that the sample residue on the membrane was below 0.6% of the total injected amount and therefore could be almost completely avoided at low sample concentrations and optimized conditions. By investigation of the AF4 flows using inductively coupled plasma mass spectrometry (ICP-MS), we found the recovery rate in the detector flow under optimized conditions to be nearly 90%, while the cross-flow, slot-outlet flow and purge flow showed negligible amounts of under 0.5%. The analysis of an aqueous ionic Ag standard solution resulted in recovery rates of over 6% and the ionic Ag content in the sample was found to be nearly 8%. Therefore, we were able to indicate the ionic Ag content as the most important source of sample loss in this study.
A user-friendly open-source Monte Carlo regression package (McSAS) is presented, which structures the analysis of small-angle scattering (SAS) using uncorrelated shape-similar particles (or scattering contributions). The underdetermined problem is solvable, provided that sufficient external information is available. Based on this, the user picks a scatterer contribution model (or 'shape') from a comprehensive library and defines variation intervals of its model parameters. A multitude of scattering contribution models are included, including prolate and oblate nanoparticles, core-shell objects, several polymer models, and a model for densely packed spheres. Most importantly, the form-free Monte Carlo nature of McSAS means it is not necessary to provide further restrictions on the mathematical form of the parameter distribution; without prior knowledge, McSAS is able to extract complex multimodal or odd-shaped parameter distributions from SAS data. When provided with data on an absolute scale with reasonable uncertainty estimates, the software outputs model parameter distributions in absolute volume fraction, and provides the modes of the distribution (e.g. mean, variance etc.). In addition to facilitating the evaluation of (series of) SAS curves, McSAS also helps in assessing the significance of the results through the addition of uncertainty estimates to the result. The McSAS software can be integrated as part of an automated reduction and analysis procedure in laboratory instruments or at synchrotron beamlines.
Bottom ash from municipal solid waste incineration (MSWI) consists of eiemental metals in considerable amounts. The fine fraction < 4 mm additionally contains chemically bound metals (oxides, carbonates, Silicates). Separation prospects with techniques as in ore processing (flotation, density separation, bioleaching, hydrothermal solution) are discussed. During alteration after wet extraction mineral material with hydraulic properties form coatings on almost all particles of the bottom ash and complicate separation procedures. ln addition bottom ash from MSWI is a heterogeneaus material. For sufficient enrichment different concerted treatment steps seemed to be essential associated with an uncertainty of economic viability. The utilisation of metal compounds present in bottom ash as secondary raw material depends on the energy- and resource-efficiency of the enrichment processes. Therefore energy and material flow considerations are presented.
N-Hydroxysuccinimide (NHS) esters are the most important activated esters used in many different bioconjugation techniques, such as protein labelling by fluorescent dyes and enzymes, surface activation of chromatographic supports, microbeads, nanoparticles, and microarray slides, and also in the chemical synthesis of peptides. Usually, reactions with NHS esters are very reliable and of high yield, however, the compounds are sensitive to air moisture and water traces in solvents. Therefore, the quantification of NHS would be a very helpful approach to identify reagent impurities or degradation of stored NHS esters. No robust and sensitive method for the detection of NHS (or the more hydrophilic sulfo-NHS) has been reported yet. Here, a chromatographic method based on HILIC conditions and UV detection is presented, reaching a detection limit of about 1 mg L-1, which should be sensitive enough for most of the applications mentioned above. Exemplarily, the hydrolytic degradation of a biotin-NHS ester and a purity check of a fluorescent dye NHS ester are shown. An important advantage of this approach is its universality, since not the structurally variable ester compound is monitored, but the constant degradation product NHS or sulfo-NHS, which avoids the necessity to optimize the separation conditions and facilitates calibration considerably.
Solgel prepared ternary FeF3–MgF2 materials have become promising heterogeneous catalysts due to their porosity and surface Lewis/Brønsted acidity (bi-acidity). Despite the good catalytic performance, nanoscopic characterisations of this type of material are still missing and the key factors controlling the surface properties have not yet been identified, impeding both a better understanding and further development of ternary fluoride catalysts. In this study, we characterised the interaction between the bi-acidic component (FeF3) and the matrix (MgF2) on the nano-scale. For the first time, the formation pathway of FeF3–MgF2 was profiled and the template effect of MgF2 during the synthesis process was discovered. Based on these new insights two novel materials, FeF3–CaF2 and FeF3–SrF2, were established, revealing that with decreasing the atomic numbers (from Sr to Mg), the ternary fluorides exhibited increasing surface acidity and surface area but decreasing pore size. These systematic changes gave rise to a panel of catalysts with tuneable surface and bulk properties either by changing the matrix alkaline earth metal fluoride or by adjusting their ratios to Fe or both. The template effect of the alkaline earth metal fluoride matrix was identified as the most probable key factor determining the surface properties and further influencing the catalytic performance in ternary fluoride based catalysts, and paves the way to targeted design of next-generation catalysts with tunable properties.
Die Blitzthermografie weist eine Reihe von Vorteilen gegenüber anderen Verfahren der aktiven Thermografie auf und hat daher eine relativ große Verbreitung in Forschung und Industrie gefunden. Ein wesentlicher Nachteil ist jedoch die begrenzte Energie, die pro Blitz genutzt werden kann. Es stellt sich die Frage, ob sich durch mehrere kurz hintereinander ausgeführte Blitze eine Verbesserung des Energieeintrags erreichen lässt. Zur experimentellen Untersuchung dieser Frage wurde ein Versuchsstand mit vier Blitzlampen so umgerüstet, dass die Blitzlampen zeitgleich oder nacheinander mit einer regelbaren Verzögerung ausgelöst werden können („Multiblitz“). Als Probekörper dienten Platten aus CFK, an deren Rückseite Flachbodenbohrungen (FBB) eingebracht worden waren. Betrachtet wurde jedoch nur der absolute Temperaturhub am ungestörten Material. Die Experimente zeigen relativ geringe Effekte im Prozentbereich, wie sie auch gemäß einer quantitativen Abschätzung zu erwarten sind. Interessanterweise vergrößerte sich der Einfluss der Multiblitzanregung auf die Energieeinkopplung deutlich bei einem etwas vergrößerten Abstand zwischen Blitzlampen und untersuchter Oberfläche. Die Ursache für diesen Effekt ist derzeit unklar, vermutet werden eine Temperaturabhängigkeit und/oder eine Abstandsabhängigkeit des Wärmübergangskoeffizienten im Konvektionsterm.
Aktive Thermografieverfahren werden immer häufiger zur zerstörungsfreien Prüfung von Faserverbundwerkstoffen eingesetzt, da diese völlig berührungslos arbeiten und sowohl zur Prüfung großflächiger Strukturen als auch von großen Stückzahlen kleinerer Komponenten in der Fertigung eingesetzt werden können. Dieser Beitrag beschäftigt sich mit Untersuchungen an typischen Defekten und Inhomogenitäten, die bereits während der Fertigung von CFK Bauteilen entstehen oder unbeabsichtigt mit eingebaut werden. Systematische Untersuchungen wurden mit Blitzthermografie in Reflexions- und Transmissionskonfiguration und mit Computertomographie (CT) durchgeführt. Die CT wurde dabei als Referenzverfahren genutzt, da dieses Verfahren auch kleinere Defekte mit relativ hoher Ortsauflösung und unabhängig von der Tiefe darstellen kann.
Im Rahmen des INS-Projekts „Durchführung von Ringversuchen zur Normung und Standardisierung der aktiven Thermografie mit Blitzlichtanregung“ wurden Ringversuche durchgeführt, die die Zuverlässigkeit, Vergleichbarkeit und Effektivität der Blitzthermografie für unterschiedliche Prüfprobleme nachweisen sollten. Weiterhin sollten diese Untersuchungen als Methodenvalidierungsstudie die Richtigkeit und Präzision der Blitzthermografie nachweisen und Vergleichsinformationen unterschiedlicher Geräteausstattungen liefern. Im Normausschuss NA 062-08-27 AA „Visuelle und thermografische Prüfung“ des DIN werden die Ergebnisse die Erarbeitung eines Normentwurfs zur Blitzthermografie unterstützen. In diesem Beitrag werden die Ringversuche beschrieben und ausgewählte Ergebnisse präsentiert.
Forderungen nach höherer Geschwindigkeit und die Komplexität der Fragen geben der analytischen Chemie neue Impulse. So nutzt die Prozessanalytik gepulste Ramanspektrometer, die Elemente Arsen und Quecksilber dominieren die Forschung in der Speziesanalytik, und die Omics-Techniken entwickeln sich zu Multi-Omics-Ansätzen. Ambiente MS-Techniken benötigen keine aufwendige Probenvorbereitung, multidimensionale Trenntechniken werden verstärkt in der Routine eingesetzt, und Chip-basierte Trennungen fallen durch Schnelligkeit auf. Molekülspektroskopie und Massenspektrometrie dominieren die bildgebenden Verfahren, und die Lateralauflösung der ToF-Sekundärionenmassenspektrometrie hat sich bei Oberflächenuntersuchungen verbessert.
Rekonstruktion des Bestandsplans im Zuge der Nachrechnung der Brücke über die Leine bei Schwarmstedt
(2016)
Der aktuell im Rahmen der Nachrechnungsrichtlinie geforderte Nachweis von Tragfähigkeit, Gebrauchstauglichkeit und Ermüdung der Brückenbauwerke im Bestand der Länder und des Bundes stellt eine enorme Herausforderung dar. Insbesondere bei unvollständigen oder fehlenden Bestandsplänen der Bauwerke sind Maßnahmen erforderlich, um die erforderlichen Informationen zu beschaffen. Ein wirkungsvolles Instrument können hierfür die zerstörungsfreien Prüfverfahren des Bauwesens sein. In dem präsentierten Forschungsprojekt erfolgte die Rekonstruktion eines Bestandsplanes direkt auf die Anforderungen des mit der Nachrechnung beauftragten Ingenieurbüros. Darüber hinaus wurde der Entwurf eines Leitfadens erstellt, der im Falle von unvollständigen oder fehlenden Bestandsplänen die Grundlagen für die Beauftragung und Durchführung der Nachrechnung schafft.
Modeling the lifetime reduction due to the superposition of TMF and HCF loadings in cast iron alloys
(2016)
The superposition of small amplitude, high frequency loading cycles (HCF) to slow, large amplitude loading cycles (TMF) can significantly reduce the fatigue life. In this work, the combined TMF+HCF loading has been experimentally investigated for a cast iron alloy. In particular, the influence of the HCF frequency of the HCF amplitude and of the location of the superposed HCF cycles has been assessed. It was observed that the HCF frequency has a limited impact on the TMF fatigue life. On the other side, the HCF-strain amplitude has a highly non-linear influence on the TMF fatigue life. A simple estimate for the fatigue life reduction due to the superposed HCF cycles has been derived from fracture mechanics considerations. It is assumed that the number of propagation cycles up to failure can be neglected after a threshold for the HCF loading has been reached. The model contains only two adjustable parameters and can be combined with any TMF life prediction model. The model predictions are compared with the test results for a large range of TMF+HCF loading conditions.
For non-destructive testing (NDT) appropriate reference blocks are required in order to verify and calibrate a testing procedure. At BAM a special electric discharge machining (EDM) system has been developed which is able to manufacture artificial defects having a width down to 30 μm.
Especially in the case of austenitic materials conventional EDM leads to a transformation of austenite to martensite. The martensite transformation causes a higher sensitivity of electromagnetic NDT methods (e. g. eddy current testing) at the artificial defects compared to natural defects of same size. The EDM system developed at BAM uses very low energy to avoid this material transformation. A side effect of the low-energy EDM is a lower surface roughness compared to conventional EDM. The artificial defects manufactured at BAM are measured optically and delivered with a certificate. A comparison of artificial defects shows the influence of material transformation on NDT and how differently the quality of the artificial defects can be.
In 2011, the German Association of Engineers (VDI) started working on a set of guidelines dealing with the improvement of resource efficiency. These guidelines represent a framework that defines resource efficiency and outlines proposals for the producing industry. A special guideline for small and medium-sized enterprises (SMEs) is included as well as guidelines on methodologies for evaluating resource use indicators, such as the cumulative raw material demand of products and production systems. The work on resource use indicators is still in progress. The evaluation of raw materials expenditure will include water, soil and land use. The model will include the availability of raw materials (criticality). Improving resource efficiency at the end-of-life stage is illustrated in this paper by the example of materials recovery from waste, here from residues out of municipal solid waste incineration (MSWI). With mechanical treatment valuable materials like ferrous and non-ferrous metals and secondary construction material can be extracted from MSWI bottom ash. The potential contribution on the resource efficiency is discussed.
We report on the development of ultra-small core-shell silver nanoparticles synthesized by an up-scaled modification of the polyol process. It is foreseen to use these thoroughly characterized particles as reference material to compare the catalytic and biological properties of functionalized silver nanoparticles. Small-angle X-ray scattering (SAXS) analysis reveal a narrow size distribution of the silver cores with a mean radius of RC = 3.0 nm and a distribution width of 0.6 nm. Dynamic light scattering (DLS) provides a hydrodynamic radius of RH = 10.0 nm and a PDI of 0.09. The particles’ surface is covered with poly(acrylic acid) (PAA) forming a shell with a thickness of 7.0 nm, which provides colloidal stability lasting for more than six months at ambient conditions. The PAA can be easily exchanged by biomolecules to modify the surface functionality. Replacements of PAA with glutathione (GSH) and bovine serum albumin (BSA) have been performed as examples. We demonstrate that the particles effectively catalyze the reduction of 4-nitrophenol to 4-aminophenol with sodium borohydride. With PAA as stabilizer, the catalytic activity of 436 ± 24 L g⁻¹ s⁻¹ is the highest reported in literature for silver nanoparticles. GSH and BSA passivate the surface substantially resulting in a catalytic activity of 77.6 ± 0.9 and 3.47 ± 0.50 L g⁻¹ s⁻¹, respectively.
Healable materials could play an important role in reducing the environmental footprint of our
modern technological society through extending the life cycles of consumer products and constructions. However, as most healing processes are carried out by heat alone, the ability to heal damage generally kills the parent material’s thermal and mechanical properties. Here we
present a dynamic covalent polymer network whose thermal healing ability can be switched ‘on’ and ‘off’ on demand by light, thereby providing local control over repair while retaining the advantageous macroscopic properties of static polymer networks. We employ a photoswitchable furan-based crosslinker, which reacts with short and mobile maleimidesubstituted poly(lauryl methacrylate) chains forming strong covalent bonds while simultaneously allowing the reversible, spatiotemporally resolved control over thermally induced de- and re-crosslinking. We reason that our system can be adapted to more complex materials and has the potential to impact applications in responsive coatings, photolithography and microfabrication.
The mechanism of nanotriangle formation in multivesicular vesicles (MMV) is investigated by using time-dependent SAXS measurements in combination with UV−vis spectroscopy, light, and transmission electron microscopy. In the first time period 6.5 nm sized spherical gold nanoparticles are formed inside of the vesicles, which build up soft nanoparticle aggregates. In situ SAXS experiments show a linear increase of the volume and molar mass of nanotriangles in the second time period. The volume growth rate of the triangles is 16.1 nm3/min, and the growth rate in the vertical direction is only 0.02 nm/min. Therefore, flat nanotriangles with a thickness of 7 nm and a diameter of 23 nm are formed. This process can be described by a diffusionlimited Ostwald ripening growth mechanism. TEM micrographs visualize soft coral-like structures with thin nanoplatelets at the periphery of the aggregates, which disaggregate in the third time period into nanotriangles and spherical particles. The 16 times faster growth of nanotriangles in the lateral than that in the vertical direction is related to the adsorption of symmetry breaking components, i.e., AOT and the polyampholyte PalPhBisCarb, on the {111} facets of the gold nanoplatelets in combination with confinement effects of the vesicular template phase.
Compact nuclear magnetic resonance (NMR) instruments make NMR spectroscopy and relaxometry accessible in industrial and harsh environments for reaction and process control. An increasing number of applications are reported. To build an interdisciplinary bridge between “process control” and “compact NMR”,we give a short overviewon current developments in the field of process Engineering such as modern process design, integrated processes, intensified processes along with requirements to process control, model based control, or soft sensing. Finally, robust field integration of NMR systems into processes environments, facing explosion protection or Integration into process control systems, are briefly discussed.
Process monitoring of an intensified continuous production unit with compact NMR spectroscopy
(2016)
Monitoring chemical reactions is the key to chemical process control. Today, mainly optical online methods are applied. NMR spectroscopy has a high potential for direct loop process control. Compact NMR instruments based on permanent magnets are robust and relatively inexpensive analyzers, which feature advantages like low cost, low maintenance, ease of use, and cryogen-free operation. Instruments for online NMR measurements equipped with a flow-through cell, possessing a good signal-to-noise-ratio, sufficient robustness, and meeting the requirements for integration into industrial plants (i.e., explosion safety and fully automated data analysis) are cur-rently not available off the rack. Recently, promising benchtop NMR instruments with acceptable performance came to market and process integrated sensors developed on basis of such laboratory instruments are on their way.
A great number of Central Asian wall paintings, archeological materials, architectural fragments, and textiles, as well as painting fragments on silk and paper, make up the so called Turfan Collection at the Asian Art Museum in Berlin. The largest part of the collection comes from the Kucha region, a very important cultural center in the third to ninth centuries. Between 1902 and 1914, four German expeditions traveled along the northern Silk Road. During these expeditions, wall paintings were detached from their original settings in Buddhist cave complexes. This paper reports a technical study of a wall painting, existing in eight fragments, from the Buddhist cave no. 40 (Ritterhöhle). Its original painted surface is soot blackened and largely illegible. Grünwedel, leader of the first and third expeditions, described the almost complete destruction of the rediscovered temple complex and evidence of fire damage. The aim of this case study is to identify the materials used for the wall paintings. Furthermore, soot deposits as well as materials from conservation interventions were of interest. Non-invasive analyses were preferred but a limited number of samples were taken to provide more precise information on the painting technique. By employing optical and scanning electron microscopy, energy dispersive X-ray spectroscopy, micro X-ray fluorescence spectroscopy, X-ray diffraction analysis, and Raman spectroscopy, a layer sequence of earthen render, a ground layer made of gypsum, and a paint layer containing a variety of inorganic pigments were identified.
Applications of fibre reinforced plastic (FRP) composites in modern industries are increasing due to their considerable advantages such as light weight and excellent mechanical properties. Accordingly, importance of operational safety of modern structures made of advanced composites by ensuring the material quality has led to increasing demands for development of non-destructive evaluation (NDE) systems. In the context of a European project entitled “Validated Inspection Techniques for Composites in Energy Applications” (VITCEA), the aim is to develop and validate traceable procedures for novel NDE techniques with contrasting damage detection capabilities in energy related applications such as wind and marine turbine blades, nacelles, oil and gas flexible risers. Accordingly, VITCEA focuses on optimization of ultrasonic tests (UTs) for quantitative defect detection and quality characterization of FRP structures. In this context, the present study describes the ultrasound field in heterogeneous composite materials. The theoretical predictions are compared with simulation results obtained from CIVA a software package dedicated to NDT simulations based on the asymptotic ray theory.
Ein wesentliches Grundbedürfnis ist die Sicherheit, d. h. die Gewissheit, in einer sicheren Umgebung zu leben und zu arbeiten. Die existenzielle Sicherheit ist eine notwendige Voraussetzung zur Befriedigung aller weiteren notwendigen Bedürfnisse. Auch die Technik ist ohne Sicherheit nicht denkbar. Trotz aller Bemühungen kommt es aber immer wieder zu Unfällen, aus welchen Gründen auch immer. Eine Strategie, Unfälle zu verhindern bzw. deren Eintrittswahrscheinlichkeit zu minimieren ist es, zwischen einem Objekt mit einem hohen Gefährdungspotenzial und seiner Nachbarschaft, Barrieren zu errichten, z. B. durch eine schützende Isolierung, Sicherheitsabstände oder durch eine Erdüberdeckung. Die erdgedeckte Verlegung von Pipelines ist Stand der Technik. Über die Überdeckungshöhen scheint es jedoch verschiedene Auffassungen zu geben. Im folgenden Beitrag werden dazu einige Beispiele vorgestellt.
Abstract Investigations on metal halide systems carried out by Knudsen effusion mass spectrometry in the period 1990-2014 are reviewed in the present paper.163 original papers were published focused on metal halides showing still considerable activity in this area. The fundamentals of the Knudsen effusion mass spectrometry method and thermodynamic background of the investigation are briefly reported. Data to the system studied, temperature ranges, Knudsen cell materials, vapor species identified in the equilibrium vapors and the thermodynamic properties obtained in the study are presented. The important issues of metal halide vaporization studies are briefly discussed and commented. The studies of the vaporization of metal halogens by Knudsen effusion mass spectrometry aimed firstly atthe determination of gaseous complexes species in the vapor and determination of its thermodynamic data like sublimation enthalpy etc. and secondly at the determination of negative ions formation and various ion-molecule equilibria reactions of metal halide systems. Many of the studied materials have a crucial role for modern technologies, for example metal halide lamps, hot corrosion caused by halide salts, phosphorus recovery technologies or gas assisted separation of lanthanides. The investigation of such systems gives information on mechanisms of vaporization, volatility of the systems under various conditions (temperature, pressure etc.), reactivity, thermal stability, resistance etc. that could be further applied for various calculations and to predict the behavior of various components under various technological aspects.
Rising importance of composite lightweight structures in aircraft and automobile industries increases the demand on reliable non-destructive testing methods for these structures. Air-coupled ultrasonic testing emerged to suit these requirements as it does not require any liquid coupling medium. In conventional air-coupled ultrasonic transducers, matching layers are used in order to decrease the impedance mismatch between transducer and air. Matching layers can be omitted by using ferroelectrets, which are charged cellular polymers having ferroelectric and piezoelectric properties. Especially a low Young’s modulus, low density and low sound velocity of cellular polypropylene (cPP) are properties being required for well-matched air-coupled ultrasonic transducers.
In our contribution we show recent enhancements of cPP transducers resulting in focused sound fields and thus improved lateral sensitivity. The influence of different transmitter apertures was evaluated using measurements of the emitted sound field. Further we show a transmission of a test specimen of carbon-fiber-reinforced plastic (CFRP) containing artificial damages. Results of focused transducers were compared to planar ferroelectret transducers, as well as to conventional air-coupled transducers.
An unusually fast and effective synthesis procedure for a host guest system consisting of a metal organic framework (MOF) and a polyoxometalate (POM) is described. The material was synthesised mechanochemically and the evolution of the structure was monitored ex and in situ using synchrotron X-ray diffraction (XRD).
Here we present the fabrication of a solid-core microstructured polymer optical fiber (mPOF) made of polycarbonate (PC), and report the first experimental demonstration of a fiber Bragg grating (FBG) written in a PC optical fiber. The PC used in this work has a glass transition temperature of 145°C. We also characterize the mPOF optically and mechanically, and further test the sensitivity of the PC FBG to strain and temperature. We demonstrate that the PC FBG can bear temperatures as high as 125°C without malfunctioning. In contrast, polymethyl methacrylate-based FBG technology is generally limited to temperatures below 90°C.
Advances in scanning electron microscopy (SEM) enable the high-resolution imaging of single nanoparticles (NPs) with sizes well below 10 nm. The SEM analysis in transmission mode (T-SEM) of NPs on thin film supports has many benefits when compared to the analysis of NPs on bulk substrates. The enhanced material (mass – thickness) contrast of the T-SEM imaging mode is well suited for in-depth and, particularly valuable, to very accurate, traceable, lateral dimensional measurements of NPs. Compared to samples prepared on bulk substrates, T-SEM with energy dispersive X-ray spectroscopy (EDS) achieves a drastically improved spatial resolution of the emitted X-rays. The poor signal-to-noise ratio of the X-ray spectra emitted by a single nanoparticle (NP) can be improved by the use of high-sensitivity (high collection solid angle) silicon drift (SDD), energy-dispersive X-ray spectrometers (EDS). The EDS spectral imaging of a single NP with a spatial resolution below 10 nm has become possible. This is demonstrated by means of various examples of nanostructures. Advanced data processing of T-SEM/EDS results sets the stage for the automated classification of NPs by feature analysis. This method combines the detection of morphological structures of interest by image processing of T-SEM micrographs with the chemical classification by EDS.
This review article comprises of three parts. Firstly, reports of brake manufacturers on the beneficial impact of solid lubricants for pad formulations are surveyed. Secondly, since tribofilms were identified to play a crucial role in friction stabilization and wear reduction, the knowledge about tribofilm structures formed during automotive braking was reviewed comprehensively. Finally, a model for simulating the sliding behavior of tribofilms is suggested and a review on modelling efforts with different model structures related to real tribofilms will be presented. Although the variety of friction composites involved in commercial brake systems is very broad, striking similarities were observed in respect to tribofilm nanostructures. Thus a generalization of the tribofilm nanostructure is suggested and prerequisites for smooth sliding performance and minimal wear rates have been identified. A minimum of 13 vol.% of soft inclusions embedded in an iron oxide based tribofilm is crucial for obtaining the desired properties. As long as the solid lubricants or their reaction products are softer than magnetite, the main constituent of the tribofilm, the model predicts smooth sliding and a minimum of wear.
Mit dem KorroPad Verfahren ist es dem Anwender möglich den Zustand der Passivschicht nichtrostender Stähle auf sehr einfache und schnelle Weise einschätzen zu können. Das Verfahren eignet sich dazu, den Grad der Passivität in Abhängigkeit der Umgebungsbedingungen und der Zeit nachzuvollziehen. Dies ermöglicht dem Anwender und Verarbeiter von nichtrostenden Stählen, die Lagerungsbedingungen und –zeiten einer frisch bearbeiteten Stahloberfläche zu ermitteln, welche für die Ausbildung einer stabilen Passivschicht notwendig sind, bevor diese risikoarm eingesetzt werden kann. Wie die hier dargestellten Beispiele und auch weitere zahlreiche praktische Anwendungen gezeigt haben, eignet sich das KorroPad ebenfalls für die Identifikation kritischer Prozessparameter bei der Verarbeitung nichtrostender Stähle. Mit dem Verfahren lassen sich viele prozessbedingte Einflussfaktoren auf die Oberflächengüte wie auch auf den Werkstoff charakterisieren. Aufgrund der schnellen und einfachen Auswertung der Prüfergebnisse können positive wie auch negative Veränderungen hinsichtlich der Passivschichtstabilität zügig erkannt werden. Dies ermöglicht es dem Anwender schnell zu reagieren, um kritische Einflüsse zu korrigieren und um eine Optimierung von Inhouse-Prozessen durchzuführen. Weitere Einsatzgebiete sind im Bereich der Wareneingangs- und/oder Warenausgangskontrolle denkbar, überall wo es um die Frage der Passivschichtstabilität einer nichtrostenden Stahloberfläche geht.
The preparation and characterization of poly(ionic liquid)s (PILs) bearing a polystyrene backbone via reversible addition fragmentation chain transfer (RAFT) polymerization and their photolithographic patterning on silicon wafers is reported. The controlled radical polymerization of the styrenic ionic liquid (IL) monomers ([BVBIM]X, X = Cl− or Tf2N−) by RAFT polymerization is investigated in detail. We provide a general synthetic tool to access this class of PILs with controlled molecular weight and relatively narrow molecular weight distribution (2000 g mol−1 ≤ Mn ≤ 10 000 g mol−1 with dispersities between 1.4 and 1.3 for p([BVBIM]Cl); 2100 g mol−1 ≤ MP ≤ 14 000 g mol−1 for p([BVBIM]Tf2N)). More importantly, we provide an in-depth characterization of the PILs and demonstrate a detailed mass spectrometric analysis via matrix-assisted laser desorption ionization (MALDI) as well as – for the first time for PILs – electrospray ionization mass spectrometry (ESI-MS). Importantly, p([BVBIM]Cl) and p([DMVBIM]Tf2N) were photochemically patterned on silicon wafers. Therefore, a RAFT agent carrying a photoactive group based on ortho-quinodimethane chemistry – more precisely photoenol chemistry – was photochemically linked for subsequent controlled radical polymerization of [BVBIM]Cl and [DMVBIM]Tf2N. The successful spatially-resolved photografting is evidenced by surface-sensitive characterization methods such as X-ray photoelectron spectroscopy (XPS) and time-of-flight secondary ion mass spectrometry (ToF-SIMS). The presented method allows for the functionalization of diverse surfaces with poly(ionic liquid)s.
Multiple anthropogenic stressors cause worldwide amphibian declines. Among several poorly investigated causes is global pollution of aquatic ecosystems with endocrine disrupting compounds (EDCs). These substances interfere with the endocrine system and can affect the sexual development of vertebrates including amphibians. We test the susceptibility to an environmentally relevant contraceptive, the artificial estrogen 17α-ethinylestradiol (EE2), simultaneously in three deeply divergent systematic anuran families, a model-species, Xenopus laevis (Pipidae), and two non-models, Hyla arborea (Hylidae) and Bufo viridis (Bufonidae). Our new approach combines synchronized tadpole exposure to three EE2-concentrations (50, 500, 5,000 ng/L) in a flow-through-system and pioneers genetic and histological sexing of metamorphs in non-model anurans for EDC-studies. This novel methodology reveals striking quantitative differences in genetic-male-to-phenotypic-female sex reversal in non-model vs. model species. Our findings qualify molecular sexing in EDC-analyses as requirement to identify sex reversals and state-of-the-art approaches as mandatory to detect speciesspecific vulnerabilities to EDCs in amphibians.
Wedemonstrate that a single-layer graphene replicates the shape ofDNAorigami nanostructures very well. It can be employed as a protective layer for the enhancement of structural stability of DNA origami nanostructures. Using the AFM based manipulation, we show that the normal force required to damage graphene encapsulated DNA origami nanostructures is over an order of magnitude greater
than for the unprotected ones. In addition, we show that graphene encapsulation offers protection to the DNA origami nanostructures against prolonged exposure to deionized water, and multiple immersions. Through these results we demonstrate that graphene encapsulated DNA origami nanostructures are strong enough to sustain various solution phase processing, lithography and
transfer steps, thus extending the limits of DNA-mediated bottom-up fabrication.
DNA origami nanostructures are a versatile tool to arrange metal nanostructures and other chemical entities with nanometer precision. In this way gold nanoparticle dimers with defined distance can be constructed, which can be exploited as novel substrates for surface enhanced Raman scattering (SERS). We have optimized the size, composition and arrangement of Au/Ag nanoparticles to create intense SERS hot spots, with Raman enhancement up to 10^10, which is sufficient to detect single molecules by Raman scattering. This is demonstrated using single dye molecules (TAMRA and Cy3) placed into the center of the nanoparticle dimers. In conjunction with the DNA origami nanostructures novel SERS substrates are created, which can in the future be applied to the SERS analysis of more complex biomolecular targets, whose position and conformation within the SERS hot spot can be precisely controlled.
Background: Biocidal products can be sources of active substances in surface waters caused by weathering of treated articles. Marketing and use of biocidal products can be limited according to the European Biocidal Products Regulation if unacceptable risks to the environment are expected. Leaching of active substances from treated articles was observed in field experiments to obtain information on leaching processes and investigate the suitability of a proposed test method.
Results: Leaching under weathering conditions proceeds discontinuously and tends to decrease with duration of exposure. It mainly depends on the availability of water, but is also controlled by transport processes within the materials and stability of the observed substances. Runoff amount proved to be a suitable basis to compare results from different experiments. Concentrations of substances are higher in runoff collected from vertical surfaces compared to horizontal ones, whereas the leached amounts per surface area are higher from horizontal surfaces. Gaps in mass balances indicate that additional processes such as degradation and evaporation may be relevant to the fate of active substances in treated articles. Leached amounts of substances were considerably higher when the materials were exposed to intermittent water contact under laboratory conditions as compared to weathering of vertically exposed surfaces.
Conclusions: Experiences from the field experiments were used to define parameters of a procedure that is now provided to fulfil requirements of the Biocidal Products Regulation. The experiments confirmed that the amount of water which is in contact with exposed surfaces is the crucial parameter determining leaching of substances.
Selecting a welding process for a given application is crucial with respect to the sustainability of part manufacturing. Unfortunately, since welding processes are evaluated by a number of criteria, preferences for one or the other process can be contradictory. However, the prevalent procedure of weight assignment for each criterion is subjective and does not provide information about the entire solution space. From the perspective of a decision maker it is important to be able to assess the entire set of possible weightings and answer the question which welding process is optimal for which set of weights. This issue is investigated by means of a weight space partitioning approach. Two welding processes are considered with respect to three criteria that reflect their economic and environmental performance. In order to find the most sustainable welding process the underlying weight space partition is evaluated.
Polysarcosine (M-n = 3650-20 000 g mol(-1), D similar to 1.1) was synthesized from the air and moisture stable N-phenoxycarbonyl-N-methylglycine. Polymerization was achieved by in situ transformation of the urethane precursor into the corresponding N-methylglycine-N-carboxyanhydride, when in the presence of a non-nucleophilic tertiary amine base and a primary amine initiator.
In this paper, we identify the strategic motives of German manufacturing companies in the electrical engineering and machinery industry to be involved in standards development organizations. First, we present the general motives for the formation of strategic alliances and relate them to specific standardization motives. Then, we identify pursuing specific company interests, solving technical problems, knowledge seeking, influencing regulation, and facilitating market access as motives to standardize by means of factor analysis. In a second step, we test hypotheses on the relationship between the importance of strategic motives and firm level variables, e.g. R&D intensity, innovation activities, and firm size. The results reveal that firms in electric engineering and machinery have a particularly strong interest in ensuring industry-friendly design of regulations, which can be achieved by standards. Moreover, the results confirm that small firms also from these two sectors are active in standardization alliances to access knowledge from other involved stakeholders.
Characterization of multiphase metal matrix composites by means of CT and neutron diffraction
(2016)
The present study examines the relationship between the microstructure of multiphase metal matrix composites and their damage mechanisms. The matrix AlSi12CuMgNi was combined with 15% vol. Al₂O₃ (short fibers), and with 7% vol. Al₂O₃ + 15% vol. SiC (short fibers and whiskers, respectively). The experimental approach encompasses 3D microstructure characterization by means of computed tomography of samples (a) as-cast, (b) after heat treatment, and (c) after compression tests at room temperature. The volume fraction of different phases, their distribution, their orientation, and the presence of defects and damage are studied.
The influence of the addition of SiC particles on mechanical properties of composite was investigated. Phase-specific load partition analysis for samples with fiber plane parallel to load was performed by using neutron diffraction (ND) during in-situ compression. ND results show damage in the Si phase, while Al₂O₃ short fibers carry load without damage until failure. The computed tomography observations confirm the load partition analysis.
Column percolation tests may be suitable for prediction of chemical leaching from soil and soil materials. However, compared with batch leaching tests, they are time-consuming. It is therefore important to investigate ways to shorten the tests without affecting the quality of results. In this study, we evaluate the feasibility of decreasing testing time by increasing flow rate and decreasing equilibration time compared to the conditions specified in ISO/TS 21268-3, with equilibration periods of 48 h and flow rate of 12 mL/h. We tested three equilibration periods (0, 12–16, and 48 h) and two flow rates (12 and 36 mL/h)on four different soils and compared the inorganic constituent releases. For soils A and D, we observed similar values for all conditions except for the 0 h–36 mL/h case. For soil B, we observed no appreciable differences between the tested conditions, while for soil C there were no consistent trends probably due to the difference in ongoing oxidation reactions between soil samples. These results suggest that column percolation tests can be shortened from 20 to 30 days to 7–9 days by decreasing the equilibration time to 12–16 h and increasing the flow rate to 36 mL/h for inorganic substances.
Multifunctional composite nanoprobes consisting of iron oxide nanoparticles linked to silver and gold nanoparticles, Ag–Magnetite and Au–Magnetite, respectively, were introduced by endocytic uptake into cultured fibroblast cells. The cells containing the non-toxic nanoprobes were shown to be displaceable in an external magnetic field and can be manipulated in microfluidic channels. The distribution of the composite nanostructures that are contained in the endosomal system is discussed on the basis of surfaceenhanced Raman scattering (SERS) mapping, quantitative laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) micromapping, and cryo soft X-ray tomography (cryo soft-XRT). Cryo soft-XRT of intact, vitrified cells reveals that the composite nanoprobes form intra-endosomal aggregates. The nanoprobes provide SERS signals from the biomolecular composition of their surface in the endosomal environment. The SERS data indicate the high stability of the nanoprobes and of their plasmonic properties in the harsh environment of endosomes and lysosomes. The spectra point at the molecular composition at the surface of the Ag–Magnetite and Au–Magnetite nanostructures that is very similar to that of other Composite structures, but different from the composition of pure silver and gold SERS nanoprobes used for intracellular investigations. As shown by the LA-ICP-MS data, the uptake efficiency of the magnetite composites is approximately two to three times higher than that of the pure gold and silver nanoparticles.
Safety assessment of nanoparticles (NPs) requires techniques that are suitable to quantify tissue and cellular uptake of NPs. The most commonly applied techniques for this purpose are based on inductively coupled plasma mass spectrometry (ICP-MS). Here we apply and compare three different ICP-MS methods to investigate the cellular uptake of TiO2 (diameter 7 or 20 nm, respectively) and Ag (diameter 50 or 75 nm, respectively) NPs into differentiated mouse neuroblastoma cells (Neuro-2a cells). Cells were incubated with different amounts of the NPs. Thereafter they were either directly analyzed by laser ablation ICP-MS (LA-ICP-MS) or were lysed and lysates were analyzed by ICP-MS and by single particle ICP-MS (SP-ICP-MS).
A new cocrystal of pyrazinamide with oxalic acid was prepared mechanochemically and characterized by PXRD, Raman spectroscopy, solid-state NMR spectroscopy, DTA-TG, and SEM. Based on powder X-ray diffraction data the structure was solved. The formation pathway of the reaction was studied in situ using combined synchrotron PXRD and Raman spectroscopy. Using oxalic acid dihydrate the initially neat grinding turned into a rapid self-accelerated liquid-assisted grinding process by the release of crystallization water. Under these conditions, the cocrystal was formed directly within two minutes.
The International Dangerous Goods Regulations prescribe the immersion under water method (“bubble test”) as standard method for the leakproofness test of dangerous goods packagings. But this test procedure acts as a test method for leak localisation, not for quantitative leakage rates measurement. Additionally, the sensitivity in detecting leaks of small diameters is restricted, depending on the test liquid and the test pressure. The bubble test is not suitable for a comparison with quantitative limit leakage rates based on realistic transport conditions. This is especially important when estimating the risk of the formation of an explosive atmosphere during the intercontinental carriage of dangerous goods packagings in freight containers. To compare measured leakage rates with limit leakage rates, a quantitative leak testing procedure is required. Therefore a new approach for dangerous goods packagings is implemented: The pressure technique by accumulation using Helium as a tracer gas. This work presents the test equipment necessary for the quantitative measurement of Helium leakage rates through closures of different kinds of dangerous goods packagings. The essential steps to achieve good repeatable results are: A controlled Helium filling process to reach a defined test pressure in the test sample, a sufficient homogenisation of the Helium-air-mixture inside the test sample and the ensuring of a constant pressure level of the test sample during the test. The Helium loss rate of the accumulation chamber has to be measured separately to receive a correction factor for the measured leakage rates. Different constructional measures are introduced to prevent a disturbing influence of the Helium leakage rate of the filling valves on the measurement results. Methods to estimate the disturbing effect of Helium permeation through permeable parts of the test sample are also presented. As a supporting method for the experimental investigations the Helium sniffer test can be applied. This practical application-oriented advice can enable other users to establish a pressure technique by accumulation for their own technical field.
In respect of modern approaches in material sciences and highly increased
requirements on materials on safety relevant components, quality management
and non-destructive testing reclaims a steadily increased meaning. The
destructive meaning of measuring the degree of purity is defined in DIN EN 10247
through metallurgical investigations, especially microsections.
For and comparable, but non-destructive testing due ultrasonic testing, the material
the SEP 1927 is a well-defined industry standard. A novel and alternative way
of reference block construction was focused by this work. The proposed amendments,
regarding the manufacturing and machining, are less time and cost consuming.
Verified by measurements the presented reference block fits the same acoustical
characteristics and the requirements of the guideline.
Determination of the elastic behavior of silicon nanowires within a scanning electron microscope
(2016)
Three-point bending tests were performed on double-anchored, <110> silicon nanowire samples inside a scanning electron microscope (SEM) via a micromanipulator equipped with a piezo-resistive force sensor. Representing the upper and lower boundaries achievable in a consistent manner, silicon nanowires with widths of 35 nm and 74 nm and a height of 168 nm were fabricated. The nanowires were obtained monolithically along with their 10-m-tall supports through a top-down fabrication approach involving a series of etching processes. Hence, no interface compliance was introduced between supports and nanowires. Exact nanowire dimensions and cross-sectional features were determined by transmission electron microscopy (TEM) following sample preparation through focused ion beam (FIB) machining. Conducting the experiments inside an SEM chamber further raised the opportunity of the direct observation of any deviation from ideal loading conditions such as twisting, which was taken into consideration in simulations. Measured force-displacement behavior was observed to exhibit close resemblance to simulation results obtained by finite element modeling, when the bulk value of 169 GPa was taken as the modulus of elasticity for <110> silicon. Hence, test results show neither any size effect nor evidence of residual stresses for the considered nanoscale objects. The increased effect of the native oxide with reduced nanowire dimensions was captured as well. Thus this very simple in-situ testing method was found to be an alternative to elaborate AFM measurements on geometrically formidable nanostructures. The results demonstrate the applicability of the developed fabrication approach to the incorporation of silicon nanowires in functional micromechanical devices.
The optical properties of semiconductor nanocrystals (SC NCs) are largely controlled by their size and surface chemistry, i.e., the chemical composition and thickness of inorganic passivation shells and the chemical nature and number of surface ligands as well as the strength of their bonds to surface atoms.
The latter is particularly important for CdTe NCs, which – together with alloyed CdₓHg₁₋ₓTe – are the only SC NCs that can be prepared in water in high quality without the need for an additional inorganic passivation shell. Aiming at a better understanding of the role of stabilizing ligands for the control of the application-relevant fluorescence features of SC NCs, we assessed the influence of two of the most commonly used monodentate thiol ligands, thioglycolic acid (TGA) and mercaptopropionic acid (MPA),
on the colloidal stability, photoluminescence (PL) quantum yield (QY), and PL decay behavior of a set of CdTe NC colloids. As an indirect measure for the strength of the coordinative bond of the ligands to SC NC surface atoms, the influence of the pH (pD) and the concentration on the PL properties of these colloids was examined in water and D₂O and compared to the results from previous dilution studies with a set of thiol-capped Cd₁₋ₓHgₓTe SC NCs in D₂O. As a prerequisite for these studies, the number of surface ligands was determined photometrically at different steps of purification after SC NC synthesis with Ellman’s test.
Our results demonstrate ligand control of the pH-dependent PL of these SC NCs, with MPA-stabilized CdTe NCs being less prone to luminescence quenching than TGA-capped ones. For both types of CdTe colloids, ligand desorption is more pronounced in H₂O compared to D₂O, underlining also the role of hydrogen bonding and solvent molecules.
This article reports a comprehensive investigation of the average and local structure of La5.6WO12-δ, which has excellent mixed proton, electron and oxide ion conduction suitable for device applications. Synchrotron X-ray and neutron powder diffraction show that a cubic fluorite supercell describes the average structure, with highly disordered lanthanum and oxide positions. On average, the tungsten sites are sixfold coordinated and a trace [3.7 (1.3)%] of anti-site disorder is detected. In addition to sharp Bragg reflections, strong diffuse neutron scattering is observed, which hints at short-range order. Plausible local configurations are considered and it is shown that the defect chemistry implies a simple 'chemical exchange' interaction that favours ordered WO6 octahedra. The local model is confirmed by synchrotron X-ray pair distribution function analysis and EXAFS experiments performed at the La K and W L-3 edges. It is shown that ordered domains of similar to 3.5 nm are found, implying that mixed conduction in La5.6WO12-δ is associated with a defective glassy-like anion sublattice. The origins of this ground state are proposed to lie in the nonbipartite nature of the face-centred cubic lattice and the pairwise interactions which link the orientation of neighbouring octahedral WO6 sites. This 'function through frustration' could provide a means of designing new mixed conductors.
In this study, a new reliable, economic, and environmentally-friendly one-step synthesis is established to obtain carbon nanodots (CNDs) with well-defined and reproducible photoluminescence (PL) properties via the microwave-assisted hydrothermal treatment of starch and Tris-acetate-EDTA (TAE) buffer as carbon sources. Three kinds of CNDs are prepared using different sets of above mentioned starting materials. The as-synthesized CNDs: C-CND (starch only), N-CND 1 (starch in TAE) and N-CND 2 (TAE only) exhibit highly homogenous PL and are ready to use without need for further purification.
The CNDs are stable over a long period of time (>1 year) either in solution or as freeze-dried powder. Depending on starting material, CNDs with PL quantum yield (PLQY) ranging from less than 1% up to 28% are obtained. The influence of the precursor concentration, reaction time and type of additives on the optical properties (UV-Vis absorption, PL emission spectrum and PLQY) is carefully investigated, providing insight into the chemical processes that occur during CND formation. Remarkably, upon freeze-drying the initially brown CND-solution turns into a non-fluorescent white/slightly Brown powder which recovers PL in aqueous solution and can potentially be applied as fluorescent marker in bio-imaging, as a reduction agent or as a photocatalyst.
A combined experimental numerical approach is applied to determine the transformation induced plasticity (TRIP)-parameter K for different strength low-alloy steels of grade S355J2+N and S960QL as well as the super martensitic filler CN13-4-IG containing 13 wt% chromium and 4 wt% nickel. The thermo-physical analyses were conducted using a Gleeble® 3500 facility. The thermal histories of the specimens to be tested were extracted from corresponding simulations of a real gas metal arc weldment. In contrast to common TRIP-experiments which are based on complex specimens a simple flat specimen was utilized together with an engineering evaluation method. The evaluation method was validated with literature values for the TRIP-parameter. It could be shown that the proposed approach enables a correct description of the TRIP behavior.
The corrosion resistance of martensitic stainless steels (MSS) depends strongly on the chemical composition and the applied heat treatment. Both determines the distribution of the alloying elements in the microstructure and the resulting material properties. The addition of nitrogen is known to be beneficial for the pitting corrosion resistance of stainless steels. In case of MSS this effect is not only connected to nitrogen itself because nitrogen can be used to substitute carbon which also influences the result of the heat treatment process. This paper shows the effect of nitrogen on the corrosion resistance in relation to the hardening process of MSS. Therefore the effects of austenitization duration, austenitization temperature and cooling rate on microstructure, hardness and corrosion resistance were studied on the MSS X30CrMoN15 1 and X50CrMoV15. The effect of different cooling rates was studied in the range of > 100 K/s down to 1 K/s using the jominy end quench test. The changes in corrosion resistance were detected with electrochemical potentiodynamic reactivation (EPR) and by the determination of critical pitting potentials. Besides this experimental approach thermodynamic calculations with the software thermocalc will be presented and used for the interpretation of the effect of nitrogen on the corrosion resistance of MSS.
The canister for the permanent storage of spent nuclear fuel used by SKB in Sweden consists of a cast iron insert surrounded by a five centimetre thick shell of copper. It is a safety critical component and in order to secure long-term structural integrity non-destructive methods are used to inspect 100% of the volume of each canister, before it is disposed of in the repository. One of the critical components that requires inspection is a sealing weld, joining the copper tube and the lid. The friction stir weld is inspected using an ultrasonic phased array system. The area of the weld is inspected with several inspection channels with different angles and varying coverage. To make sure that no defects that might occur in the weld are overseen, the reliability of the inspection must be quantified. The reliability of NDT is usually quantified with the probability of detection curves. The influence of the parameters that might influence the POD of the flaws in the weld is investigated analysing the experimental results, as well as with a help of a numerical simulation of the inspection.
Reliability analysis of the ultrasonic inspection system for the inspection of hollow railway axles
(2016)
Axles are safety critical train components that are subjected to significant cyclic loading during operation. If the crack is initiated in the axle, cyclic loading will lead to crack propagation. To maintain structural integrity, axles must be periodically inspected for fatigue cracks in the material. Deutsche Bahn uses mechanized ultrasonic inspection system to inspect hollow railway axles. The inspections are performed from the bore surface, using several conventional transducers with different incident angles, inspecting the axle along the entire length. As with the every safety critical system, the reliability of these inspections must be determined with regard to their flaw detection capabilities. Traditionally this is done according to the relevant standards for railway vehicles. To investigate the capability of the NDT system more thoroughly, we want to evaluate the capability of the inspection system to detect flaws by means of probability of detection (POD) curves. It will be shown that other parameters, beside the size of the crack, for example crack position in the axle, influence the detection of the crack. The influence of these parameters was evaluated using ultrasonic simulation. The evaluation served as an input for the manufacturing of the flaws in the real scale axle. Once these axles are inspected and the data evaluated, using data from both measurement and simulation, we will express the POD of the crack as function of influencing parameters using the multiparameter POD model.
Novel air-coupled ultrasonic transducer combining the thermoacoustic with the piezoelectric effect
(2016)
In recent years, there has been an increasing industrial demand for one-sided inspection of various structures by means of air-coupled ultrasonic technique. Lightweight structures based on carbon-fibre-reinforced polymers may have very complex shapes, making air-coupled transmission difficult or even impossible. The inspection of concrete structures is another example where one-sided inspection is required.
To address these challenges a new type of transducer for air-coupled pulse-echo inspection was developed, which unites two principles: thermoacoustic emission and piezoelectric reception. The thermoacoustic emitter is a titanium electrode with a thickness of several tens of nanometer. This electrode was deposited onto charged cellular polypropylene, which serves as a piezoelectric receiver. The thermoacoustic transmission is based on a transformation of the thermal energy of an electrically heated electrode into the acoustic energy of an ultrasonic wave. Thermoacoustic emitters provide resonance-free behaviour and thus extremely broadband pulses. Charged cellular polypropylene is piezoelectric due to the polarization of its cells and it is well matched to air, with a Young modulus in the order of magnitude of MPa. In this contribution we present some pulse-echo measurements with the first prototypes of the combined thermoacoustic-piezoelectric transducer.
Sub-aerial biofilms (SAB) are ubiquitous, self-sufficient microbial ecosystems found on mineral surfaces at all altitudes and latitudes. SABs, which are the principal causes of weathering on exposed terrestrial surfaces, are characterized by patchy growth dominated by associations of algae, cyanobacteria, fungi and heterotrophic bacteria. A recently developed in vitro system to study colonization of rocks exposed to air included two key SAB participants - the rock-inhabiting ascomycete Knufia petricola (CBS 123872) and the phototrophic cyanobacterium Nostoc punctiforme ATCC29133. Both partners are genetically tractable and we used them here to study weathering of granite, K-feldspar and plagioclase. Small fragments of the various rocks or minerals (1–6 mm) were packed into flow-through columns and incubated with 0.1% glucose and 10 μM thiamine-hydrochloride (90 μL min−1) to compare weathering with and without biofilms. Dissolution of the minerals was followed by: (i) analysing the degradation products in the effluent from the columns via Inductively Coupled Plasma Spectroscopy and (ii) by studying polished sections of the incubated mineral fragments/grains using scanning electron microscopy, transmission electron microscopy and energy dispersive X-ray analyses. K. petricola/N. punctiforme stimulated release of Ca, Na, Mg and Mn. Analyses of the polished sections confirmed depletion of Ca, Na and K near the surface of the fragments. The abrupt decrease in Ca concentration observed in peripheral areas of plagioclase fragments favored a dissolution-reprecipitation mechanism. Percolation columns in combination with a model biofilm can thus be used to study weathering in closed systems. Columns can easily be filled with different minerals and biofilms, the effluent as well as grains can be collected after long-term exposure under axenic conditions and easily analyzed.
Biological erosion is a key process for the recycling of carbonate and the formation of calcareous sediments in the oceans. Experimental studies showed that bioerosion is subject to distinct temporal variability, but previous long-term studies were restricted to tropical waters. Here, we present results from a 14-year bioerosion experiment that was carried out along the rocky limestone coast of the island of Rhodes, Greece, in the Eastern Mediterranean Sea, in order to monitor the pace at which bioerosion affects carbonate substrate and the sequence of colonisation by bioeroding organisms. Internal macrobioerosion was visualised and quantified by micro-computed tomography and computer-algorithm-based segmentation procedures. Analysis of internal macrobioerosion traces revealed a dominance of bioeroding sponges producing eight types of characteristic Entobia cavity networks, which were matched to five different clionaid sponges by spicule identification in extracted tissue. The morphology of the entobians strongly varied depending on the species of the producing sponge, its ontogenetic stage, available space, and competition by other bioeroders. An early community developed during the first 5 years of exposure with initially very low macrobioerosion rates and was followed by an intermediate stage when sponges formed large and more diverse entobians and bioerosion rates in-creased. After 14 years, 30 % of the block volumes were occupied by boring sponges, yielding maximum bioerosion rates of 900 g m.
Bei der Power-to-Gas-Technologie wird überschüssiger Strom aus erneuerbaren Ener-gien durch Elektrolyse von Wasser in Wasserstoff umgewandelt. Dieser Wasserstoff kann als „chemischer Energiespeicher“ dienen und rückverstromt werden oder aber in das Erdgasnetz eingespeist werden. Die BAM hat die Auswirkungen von Wasserstoffzu-sätzen zum Erdgas im Hinblick auf den Explosionsschutz untersucht und sicherheitstechnische Kenngrößen für Erdgas-Wasserstoff-Gemische bestimmt.
Von besonderem Interesse waren dabei die Explosionsgrenzen, die Sauerstoffgrenzkonzentration, die maximalen Explosionsdrücke, die KG-Werte und die Normspaltweiten. Für die Messungen sind zwei Modellgase eingesetzt worden, reines Methan und ein Modell-Erdgas mit Anteilen höherer Kohlenwasserstoffe. Sie repräsentieren die Bandbreite der in Deutschland eingesetzten Erdgase.
Die Untersuchungen ergaben, dass bei einem Zusatz von bis zu 10 Mol-% Wasserstoff keine der untersuchten Kenngrößen signifikant beeinflusst wird. Die Gemische haben nur geringfügig erweiterte Explosionsbereiche und bleiben, wie die reinen Erdgase, in der Explosionsgruppe IIA. Auch die maximalen Explosionsdrücke und die zeitlichen Druckanstiege bei den Gasexplosionen werden nur wenig beeinflusst.
The successful mechanochemical syntheses of three cadmium phenylphosphonates indicates that mechanochemistry is ideally suited for synthesizing metal phosphonates. With this powerful synthesis tool it is possible to synthesize rapidly and efficiently both known and novel phosphonates. The Crystal structures of the two new compounds, and, were solved from PXRD data. They contain monodeprotonated phenylphosphonate and neutral phenylphosphonic acid ligands. The synthesis pathways of all three compounds were investigated in situ. A diffusion mechanism is corroborated by our findings.
Intermediates could be detected and identified. The kinetically favored product (3) could always be detected during the syntheses. The thermodynamic stability of the compounds and the stoichiometric ratio of the starting materials are the two directing factors for the synthesis of the final products.
The folding of single-stranded telomeric DNA into guanine (G) quadruplexes is a conformational change that plays a major role in sensing and drug targeting. The telomeric DNA can be placed on DNA origami nanostructures to make the folding process extremely selective for K+ ions even in the presence of high Na+ concentrations. Here, we demonstrate that the K+-selective G-quadruplex formation is reversible when using a cryptand to remove K+ from the G-quadruplex. We present a full characterization of the reversible switching between single-stranded telomeric DNA and G-quadruplex structures using Förster resonance energy transfer (FRET) between the dyes fluorescein (FAM) and cyanine3 (Cy3). When attached to the DNA origami platform, the G-quadruplex switch can be incorporated into more complex photonic networks, which is demonstrated for a three-color and a four-color FRET cascade from FAM over Cy3 and Cy5 to IRDye700 with G-quadruplex-Cy3 acting as a switchable transmitter.
Emerging infectious diseases (EIDs) have contributed significantly to the current biodiversity crisis, leading to widespread epidemics and population loss. Owing to genetic variation in pathogen virulence, a complete understanding of species decline requires the accurate identification and characterization of EIDs. We explore this issue in the Western honeybee, where increasing mortality of populations in the Northern Hemisphere has caused major concern. Specifically, we investigate the importance of genetic identity of the main suspect in mortality, deformed wing virus (DWV), in driving honeybee loss. Using laboratory experiments and a systematic field survey, we demonstrate that an emerging DWV genotype (DWV-B) is more virulent than the established DWV genotype (DWV-A) and is widespread in the landscape. Furthermore, we show in a simple model that colonies infected with DWV-B collapse sooner than colonies infected with DWV-A. We also identify potential for rapid DWV evolution by revealing extensive genome-wide recombination in vivo. The emergence of DWV-B in naive honeybee populations, including via recombination with DWV-A, could be of significant ecological and economic importance. Our findings emphasize that knowledge of pathogen genetic identity and diversity is critical to understanding drivers of species decline.
Currently established and projected regulatory frameworks require the classification of materials (whether nano or non-nano) as specified by respective definitions, most of which are based on the size of the constituent particles. This brings up the question if currently available techniques for particle size determination are capable of reliably classifying materials that potentially fall under these definitions.
In this study, a wide variety of characterisation techniques, including counting, fractionating, and spectroscopic techniques, has been applied to the same set of materials under harmonised conditions.
The selected materials comprised well-defined Quality control materials (spherical, monodisperse) as well as industrial materials of complex shapes and considerable polydispersity. As a result, each technique could be evaluated with respect to the determination of the number-weighted median size. Recommendations on the most appropriate and efficient use of techniques for different types of material are given.
Self-assembling biomolecules provide attractive templates for the preparation of metallic nanostructures. However, the intuitive transfer of the “outer shape” of the assembled macromolecules to the final metallic particle depends on the intermolecular forces among the biomolecules which compete with interactions between template molecules and the metal during metallization. The shape of the bio-template may thus be more dynamic than generally assumed. Here, we have studied the metallization of phospholipid nanodiscs which are discoidal particles of ~10 nm diameter containing a lipid bilayer ~5 nm thick. Using negatively charged lipids, electrostatic adsorption of amine-coated Au nanoparticles was achieved and followed by electroless gold deposition. Whereas Au nanoparticle adsorption preserves the shape of the bio-template, metallization proceeds via invasion of Au into the hydrophobic core of the nanodisc. Thereby, the lipidic phase induces a lateral growth that increases the diameter but not the original thickness of the template. Infrared spectroscopy reveals lipid expansion and suggests the existence of internal gaps in the metallized nanodiscs, which is confirmed by surface-enhanced Raman scattering from the encapsulated lipids. Interference of metallic growth with non-covalent interactions can thus become itself a shape-determining factor in the metallization of particularly soft and structurally anisotropic biomaterials.
A combined analysis of EXAFS and Raman spectra is applied for the study of
InxGa1-xN alloys with 0.3<x<0.5. Alloying causes relaxation of the selection rules resulting in
Raman spectra that resemble the vibrational density of states. On the other hand, theoretical
simulation of the Raman spectra using the Equation of Motion routine of FEFF8 provides the
vibrational component of the Debye-Waller factor (DWF). The static disorder component of
the DWFs was obtained by fitting the Ga and In K-edge EXAFS spectra. The analysis revealed
that the nearest neighbor distances of the 1st and 2nd shell deviate from the values predicted by
the law of Vegard and the virtual crystal approximation. The static disorder in the first nearest
neighboring shell (In-N and Ga-N) is null whereas in the cation-cation neighboring shells the
static component is generally smaller than the vibrational.
We describe a fast and effective synthesis for molecular metal phosphonates. Isomorphic compounds [M(II)(HO₃PPh)₂(H₂O₃PPh)₂(H₂O)₂] (M = Mn (1), Co (2), Ni (3); Ph = C₆H₅) were obtained by grinding. The complexes are mononuclear compounds containing neutral and monodeprotonated phenylphosphonic acid and water as ligands. The crystal structures were determined using powder X-ray diffraction (PXRD) data and validated by extended X-ray absorption fine structure (EXAFS) data. Combined synchrotron XRD measurements and Raman spectroscopy were conducted for investigating the reactions in situ. Based on these data, the intermediates were characterized and the formation mechanism was derived.
Titanium dioxide (TiO₂) nanoparticles (NPs) are one of the main sources of the nanoparticulate matter to which humans are directly exposed and several studies have demonstrated their potential toxic effects. The in vivo detailed spatial distribution of TiO₂ NPs is investigated herein for the first time, using a 2D chemical imaging analysis based on confocal Raman spectroscopy. The invertebrate nematode C. elegans was employed as a prototypical model of living organisms. Rod, bipyramidal and quasispherical engineered TiO₂ NPs with different primary particle sizes and agglomeration states were prepared, characterized and then administered to nematodes. Exploiting the typical fingerprint of TiO₂ in the Raman spectrum, we monitored the biodistribution of NPs inside the worm using a non-invasive, label-free method. The high spatial resolution chemical imaging and the specificity of the Raman technique in the localization of TiO₂ NPs helped in the design of behavioral C. elegans studies aimed at elucidating the relationship among the size, shape, and agglomeration state of NPs and their ability to induce specific toxic effects. Rod-shaped NPs were the most toxic, greatly impairing pharyngeal function, reproduction and larval growth; this indicates that the rod shape, more than the bipyramidal and spherical shapes, enables NPs to interact with biological systems. These findings indicate that this Raman-nematode combined approach represents a step forward in the field of detection of NPs in living organisms, and being rapid and inexpensive enough, it can be applied as the first screening for the ability of NPs to biodistribute and exert toxicological properties in vivo.
Currently at Deutsche Bahn (DB) ultrasonic inspections in maintenance procedures for wheelset axles with a bore hole are, to the greatest possible extent, carried out using automated ultrasonic inspection system. Although the acceptance levels are in accordance with DIN 27201 part 7, the testing results have shown in recent years that in the case of true indications, the effective defect sizes were far below the level of acceptance. Due to this experience it can be assumed that the automated ultrasonic inspection systems are testing substantially more sensitively than required. This increased sensitivity leads to an increase in false indications, generally resulting in the unnecessary demounting of wheelsets. In Research cooperation between Federal Institute for Materials Research and Testing (BAM) and DB the effective flaw detection sensitivity of existing automated ultrasonic inspection system will be determined and the true/false indication ratio optimised. Through systematic investigations with the Probability of Detection method on the existing automated ultrasonic inspection system the results could be directly applied to the optimisation of existing ultrasonic inspections of wheelset axles with a bore hole in maintenance procedures and the level of reliability can be considerably increased.
The sliding behaviors of two simplified tribofilms with amorphous structure consisting either of SiO₂ molecules or C atoms were simulated by molecular dynamics modeling. The objective was to identify mechanisms explaining the experimentally observed lubricating properties of the two amorphous films. The impacts of layer thickness, normal pressure, temperature and different substrate materials were studied systematically, while the sliding velocity was kept constant at 30 m/s. While the layer thickness was not critical, all the other parameters showed special effects under certain conditions. Normal pressure impeded void formation and could even eliminate voids if applied at high temperature. Stick-slip sliding was changed to smooth sliding at high temperature due to void healing. Considering the carbon film, high friction forces and shearing of the entire film was observed with diamond substrates, whereas interface sliding at low friction forces and an amorphous layer of iron mixed with carbon was observed if the supporting substrates consisted of α-Fe. Both films show a decrease of friction forces and smooth sliding behavior at elevated temperature, corresponding well to the tribological behavior of and advanced nanocomposite sliding against a steel disc under severe stressing conditions when high flash temperatures can be expected.
Maintenance and renewal costs of a typical railway, track and substructure represents 50–60% of the total costs of such infrastructure over its entire service life. Innovations in track and substructure are therefore fundamental to achieve a significant
impact on the overall cost reduction for the railways. Therefore new solutions for track improvements that are effective and that can minimize the interruption of traffic are needed. Moreover, failures of railway embankments happened recently in different regions of the world. Such events, such as the one happened in UK in February 2013 (http://www.bbc.co.uk/news/uk-england-south-yorkshire-21441070), are showing the importance of monitoring track and infrastructure coupled with the use of numerical models for the localization of the critical areas and the design of appropriate countermeasures. Indeed embankment failures, landslides and uneven settlements and similar events are becoming much more common than in the past due to climate changes, and this requires the infrastructure managers to look from a different perspective infrastructure maintenance issues. What was previously consider as “extreme” is now “common” and thus actions need to be taken to be ready when such events will happen. The aim is to mitigate their effects on the infrastructure and to minimize disruptions to train services and reduce maintenance costs to restore the normal service conditions. If this mental change happens, then the need for solutions and techniques for global asset monitoring and ground stabilization will probably increase. Among the others, geotextiles and geogrids for soil reinforcement used in combination with condition monitoring techniques have the potential for minimizing catastrophic events, whilst at the same time providing a good balance among costs and benefits (i.e. sustainability).
The paper describe a case study where the use of multifunctional geotextiles, able to provide both strengthening and monitoring functions, has been tested along a railroad near the city of Chemnitz (Germany). The results are here reported to show the potential use and the innovative aspect of this solution.
The maximum magnetisation (saturation magnetisation) obtainable for iron oxide nanoparticles can be increased by doping the nanocrystals with non-magnetic elements such as zinc. Herein, we closely study how only slightly different synthesis approaches towards such doped nanoparticles strongly influence the resulting sub-nano/atomic structure. We compare two co-precipitation approaches, where we only vary the base (NaOH versus NH3), and a thermal decomposition route. These methods are the most commonly applied ones for synthesising doped iron oxide nanoparticles. The measurable magnetisation change upon zinc doping is about the same for all systems. However, the sub-nano structure, which we studied with Mössbauer and X-ray absorption near edge spectroscopy, differs tremendously. We found evidence that a much more complex picture has to be drawn regarding what happens upon Zn doping compared to what textbooks tell us about the mechanism. Our work demonstrates that it is crucial to study the obtained structures very precisely when “playing” with the atomic order in iron oxide nanocrystals.
Biofilm formation on materials leads to high costs in industrial processes, as well as in medical applications. This fact has stimulated interest in the development of new materials with improved surfaces to reduce bacterial colonization. Standardized tests relying on statistical evidence are indispensable to evaluate the quality and safety of these new materials. We describe here a flow chamber system for biofilm cultivation under controlled conditions with a total capacity for testing up to 32 samples in parallel. In order to quantify the surface colonization, bacterial cells were DAPI (4‘,6-diamidino-2-phenylindole)-stained and examined with epifluorescence microscopy. More than 100 images of each sample were automatically taken and the surface coverage was estimated using the free open source software g’mic, followed by a precise statistical evaluation. Overview images of all gathered pictures were generated to dissect the colonization characteristics of the selected model organism Escherichia coli W3310 on different materials (glass and implant steel). With our approach, differences in bacterial colonization on different materials can be quantified in a statistically validated manner. This reliable test procedure will support the design of improved materials for medical, industrial, and environmental (subaquatic or subaerial) applications.
With increased usage of highly demanded, modern materials on safety
relevant parts (e.g. railway wheel sets, generator shafts, turbine disks, medical
implants, etc.) comprehensive analyses regarding the quality of the material are
requested. This gives a focus to non-destructive methods using ultrasound immersion
tank testing for classifying the degree of purity. Two autonomous standards,
ASTM E588 and SEP 1927, have been established for the definition, execution and
evaluation for this high resolution ultrasonic measurements on steel products.
The propagation of ultrasonic waves and the resulting sound field are strongly
dependent on the acoustical properties of the inspected material and the geometry
of probes and specimen. The definition of the measurement setup and the evaluation
methods appear to differ significantly in the given standards. ASTM E588 and
SEP 1927 prescribe the requirement for surface roughness and probe selection, are
using threshold based methods for cleanliness detection, but differ in computation
for the degree of purity. This has been the motivation for a comparison between
both standards with the main focus on amplitude depth dependency and overall spatial
resolution taking the influence of different material characteristics, geometry of
the specimen and sound fields into account.
A performance comparison between the use of non-focusing and focusing probes
respective to the threshold based detection will be presented in this contribution. In
addition, the usage of complex reconstruction algorithms (e.g. SAFT, echo tomography)
is compared with the traditional approaches of inclusion detection and
estimation of the degree of purity
Grating interferometric set-ups have been established in the last decade. They are promising candidates to obtain enhanced image contrast from weakly absorbing micro and nano structures. They are based on X-ray refraction and near-field diffraction using the Talbot effect.
At the expense of taking multiple images, Talbot-Lau grating interferometry allows separating the absorption, refraction, and scattering contributions by analysing the disturbances of a phase grating interference pattern. Contrary to other refraction enhanced methods, this technique can be applied using conventional X-ray tubes (divergent, polychromatic source). This makes it attractive to solve typical non-destructive testing problems.
We investigated the efficiency of phase gratings, i.e. the visibility (the amplitude of oscillations) upon variation of propagation distance and phase grating rotation around an axis parallel to the grid lines. This grating rotation changes the grating shape (i.e. the distributions of phase shifts). This can yield higher visibilities than derived from rectangular shapes.
Our study includes experimental results obtained from synchrotron radiation, as well as simulations for monochromatic radiation. The advantages of Talbot-Lau interferometry are demonstrated at the example of glass capillaries.
A high-performance fiber Bragg grating-based (FBG) sensor device has been developed for the detection of small magnetic fields. Based on a smart multilayer jacket around the fibre over the physical length of the FBG, magnetic fields generated by rotating machine parts, power generators or power cable can be easily detected, analysed and evaluated. Consequently, this innovative, on-line and non-contact inspection method results in an increase in quality and reliability of high-performing machine parts, devices and cables. The basic physical principle is based on a magnetostrictive multilayer system that strains the high-resolution FBG element in presence of magnetic fields. Subsequently, a fixed relationship between induced magnetic field and wavelength change of the FBG element describes the characteristic sensitivity curve. Intensive tests regarding characterisation of this magnetic field FBG sensor have been carried out and its performance has been evaluated.
Maintenance, repair and overhaul of components are of increasing interest for parts of high complexity and expensive manufacturing costs. In this paper a production process for laser metal deposition is presented, and used to repair a gas turbine burner of Inconel 718. Different parameters for defined track geometries were determined to attain a near net shape deposition with consistent build-up rate for changing wall thicknesses over the manufacturing process. Spot diameter, powder feed rate, welding velocity and laser power were changed as main parameters for a different track size. An optimal overlap rate for a constant layer height was used to calculate the best track size for a fitting layer width similar to the part dimension. Deviations in width and height over the whole build-up process were detected and customized build-up strategies for the 3D sequences were designed. The results show the possibility of a near net shape repair by using different track geometries with laser metal deposition.
Mechanochemical reactions often result in 100% yields of single products, making purifying procedures obsolete. Mechanochemistry is also a sustainable and eco-friendly method. The ever increasing interest in this method is contrasted by a lack in mechanistic understanding of the mechanochemical reactivity and selectivity. Recent in situ investigations provided direct insight into formation pathways. However, the currently available theories do not predict temperature T as an influential factor. Here, we report the first determination of an apparent activation energy for a mechanochemical reaction. In a temperaturedependent in situ study the cocrystallisation of ibuprofen and nicotinamide was investigated as a model system. These experiments provide a pivotal step towards a comprehensive understanding of milling reaction mechanisms.
High-power laser beam welding became new stimuli within the last 10 years due to the availability of a new generation of high brightness multi kilowatt solid state lasers. In the welding research new approaches have been developed to establish reliable and praxis oriented welding processes meeting the demands of modern industrial applications during this time. The paper focuses on some of the current scientific and technological aspects in this research field like hybrid laser arc welding, simulation techniques, utilization of electromagnetic fields or reduced pressure environment for laser beam welding processes, which contributed to the further development of this technology or will play a crucial role in its further industrial implementation.
Since decades the evaluation of flaw indications on radiographs from welds or castings are based on well accepted reference film catalogues from organizations like IIW (weldments), ASTM (castings) or DGZfP (D5 recommendation on heavy steel castings). Today, the transformation of classical film radiography to the digital world is in full progress. Some ASTM standards do not permit the evaluation of digital radiographs in reference to film catalogues. Therefore, these reference film catalogues have to be converted into the digital age too. BAM is supporting this transition by high definition film scanning. The result is a corresponding reference image catalogue. The different standard organizations selected different ways to distribute the digital data. ASTM used high definition film scanning at 10 μm pixel size and distribution of a huge amount of high-res data via DVD. The user sub-samples these high-res data during catalogue import to the resolution of his system. The comparison is done by synchronized image viewing on the computer work station. IIW recently decided to distribute their ISO 5817 reference images installed on tablets, which are used for image viewing too. The tablet image has to be compared with the digital image on the system monitor. DGZfP transformed their D5 reference radiographs into a PDF for monitor viewing. This is the simplest and cheapest solution, but still allows the full usage of the catalogue in the digital era. The status of ongoing work in progress will be discussed.
Analyzing the reliability of non-destructive tests using the modular modell - a practical approach
(2016)
Non-destructive testing is an important tool to guarantee the safety of railway traffic.
The infrastructure with tracks, switches and sleepers is regularly tested, the
locomotives and wagons with their wheels, bogies and axles as well. Many years of experience and some events lead in Germany to a good practice in testing the railway components. Now, European authorities are drafting a system of common requirements and standards for the European Railway Market. The German practice combines an intensive training of the NDT-personnel including sufficient time for practical exercises with organizational measures of the companies, responsible for rolling stock and infrastructure. Through the example of UT-testing of railway axles it will be shown, how training and organizational measures influence the reliability of such testing.
The usefulness and purpose of evaluating nondestructive testing (NDT) systems and their capabilities has changed in the last decade. The conventional method of simply applying a familiar statistical algorithm to say whether the system is usable for the tasks is history.
Nowadays, multiple parameter methods which describe the probabilities of detection (POD) of different systems or real defects need new characteristics and a broader variety of statistical models to describe the true system behaviour. The appraisal of the NDT system involves diverse departments within a company (engineering, NDT-operators, and statisticians), but is, at the same time, more needed and requested than in the past. In this article, an approach is discussed in which professionals from different fields worked well together, accomplishing cost-intensive metallographic studies in correlation with well-understood physical behaviour of NDT-methods as well as deep-discussed mathematical methods to create a holistic evaluation of the technical reliability for a specific radiographic testing (RT) equipment. The first part of the publication will show the comparison between metallographic grinding and the RT indications. An essential innovation over past evaluation methods was the use of a multi-scale smoothing algorithm, which describes physical parameters, which were not used in evaluation like the POD in this way in the past.
In the second part the statistical requirements for the POD take the focus. It can often be hard to make significant statements; especially in the case where only a small amount of data is available. The combination of data and the use of knowledge from simulations are essential. One possible solution will be shown for the RT evaluation. The methodology is used for evaluating the digital RT system for the inspection of electron-beam welds, which was method considered to seal the Finnish copper canisters for the final deposit of spent nuclear fuel.
Ultrasonic phased array is, currently, the technology which is being applied as the solution to a lot of inspection problems. The perceived benefits are seen to be worth the outlay on equipment and specialised personnel. Yet, there is a source of knowledge, freely available, which can also deliver immediate benefits, through more reliable inspection results, and consequently increased client confidence, but which is largely ignored by the greater part of the NDT community. This talk will review the latest Human Factors knowledge and provide practical illustrations of how companies can use it to improve their competitive edge.
The General Guidance in the Swedish regulations state that the safety assessment for a final repository for spent nuclear fuel should be 1 million years after closure. SKB developed the KBS-3 method, according to which the spent nuclear fuel is protected by three barriers. It is encapsulated in canisters with a diameter of 1 metre and a length of 5 metres. The canister consists of a cast iron insert surrounded by a 5 centimetre thick shell of copper. The canisters are disposed in the bedrock at a depth of about 500 meters surrounded by bentonite clay. In order to assess the safety over this extremely long period, an extensive quality control programme is applied to the canisters before deposit. In this programme, the use of
non-destructive testing (NDT) is vital. The safety assessment of the canister in turn places high demands on the coverage, detectability, and reliability of the applied NDT inspections of the canister parts, i.e. cast iron insert, copper base, tube and lid, and the copper friction stir welds (FSW). This paper presents the extensive full-scale inspection development programme that runs at the Canister Laboratory in Oskarshamn (Sweden). In order to fulfil the high demands, phased array ultrasonic inspection techniques are developed using practical trials aided by ultrasonic modelling. The techniques apply, for example, different frequencies, inspection angles, focus depths, and both longitudinal and shear waves. Increased inspection reliability of the FSW is achieved by applying digital X-ray technique using a 9 MeV linear accelerator and a line detector. To complete the coverage, complementary surface inspections methods, i.e. eddy current array, magnetic flux sensor techniques and magnetic particle inspection, are applied. The canister safety assessment was the driving force to include reliability studies during the NDT development. Initially, the technical reliability was considered, resulting in development of advanced POD models (probability of detection). In combination with human factors studies, these models were implemented as tools in the development of the NDT techniques. Human factors studies were also applied to improve the inspection procedures to be more user-friendly enabling reliable inspections.
The properties of the encapsulant are critical to the long-term performance of photovoltaic (PV) modules under the influence of sunlight including UV, elevated temperature, humidity and diffusion of oxygen. Encapsulation process represents a bout 40% of the whole PV module cost. The introduction of new non-EVA encapsulant material type "Low-Cost, High-Performance" should provide a solution to outdoor yellowing degradation problems. The emerging encapsulant materials exhibit a good compatibility with emerging PV solar cells for long term durability. This new generation of encapsulant materials has the advantage to improve e the PV module performances and long term durability for specific climate like desert regions. This scientific contribution presents an overview of the different encapsulant materials currently on the market, the general requirements of the emerging encapsulant materials and characterizations techniques for degradation, diagnostic and reliability lifetime estimation in the framework of Algerian renewable energy strategy.
Molybdenum disulfide (MoS₂) is a well-known solid lubricant for tribosystems running in vacuum or dry gases. Problems arise due to its sensitivity to humidity, which is a drawback for its application under ambient conditions. However, by using a physical vapor deposition (PVD) process, deposition parameters can be optimized not only to gain a coatings structure with favorable frictional properties but also to minimize the sensitivity to attack by water molecules. Therefore, an improved tribological behavior even under moist conditions can be achieved. MoS₂coatings are also candidates for being applied at cryogenic temperatures. They already have proven their suitability, e.g., for sliding support elements between superconducting magnets of the nuclear fusion-experiment Wendelstein 7-X. However, these coatings were exclusively produced for this particular application and the utilization for more common tribosystems may be precluded due to cost considerations. In view of a wider range of applications, pure and Cr containing PVD-MoS₂ coatings with an optimized structure were tested under varying environments including hydrogen gas and cryogenic temperatures. Results of the most promising variant are presented in this paper.
Distickstoffmonoxid (N2O, Lachgas) und Helium (He) sind gängige Prüfgase für Dichtheitsprüfungen. Die einfachste Leckgeometrie stellt ein ideal zylindrisches Rohr dar. Es wurden Glaskapillaren verschiedener Abmessungen mit Lachgas und Helium durchströmt. Der Überdruck am Kapillareingang lag zwischen 100 mbar und 400 mbar. Es handelte sich um vier annähernd zylindrische Glaskapillaren mit den mittleren Durchmessern: Kapillare 1: ca. 102 μm; Kapillare 2: ca. 71 μm; Kapillare 3B: ca. 49 μm; Kapillare 4: ca. 53 μm. Zudem wurde eine nichtzylindrische Kapillare geprüft (Kapillare 3A). Die Kapillaren 1, 2 und 3B wurden mit beiden Prüfgasen getestet. Kapillare 3A wurde nur mit Lachgas durchströmt, Kapillare 4 nur mit Helium. Für die Messung der Leckageraten kam das Überdruckverfahren mit Ansammlung (Verfahren B3 nach DIN EN 1779: 1999-10) zum Einsatz. Als Detektor für Lachgas diente der Lachgasdetektor Maihak Unor 6 N, für Helium der Leckdetektor T-Guard der Firma Inficon.
Es wurden verschiedene Theorieansätze verglichen. Beim Theorieansatz Ib erfolgte die Umrechnung der Lachgas-Messwerte auf die Helium-Messwerte und umgekehrt anhand der Druck-, Temperatur- und Gasartabhängigkeit der Leckagerate für laminar-viskose Gasströmung (DIN EN 1779: 1999-10; DGZfP-Richtlinie DP2: 2009-12). Beim Theorieansatz II wurde die Berechnung der Leckagerate für die laminar-viskose Rohrströmung unter der Annahme einer ideal zylindrischen Kapillare durchgeführt. Zusätzlich wurde mit „ANSYS Fluent“ eine CFD-Simulation vorgenommen. Bei Kapillare 3A wurde eine Serienschaltung der Strömungsleitwerte von Rohr und Düse angesetzt. Bei Anwendung des Ansatzes Ib werden bei Umrechnung der Helium-Messwerte auf Lachgas die Lachgas-Messwerte überschätzt. Umgekehrt werden bei der Umrechnung der Lachgas-Messwerte auf Helium die Helium-Messwerte unterschätzt. Bei Analyse der Einlauflängen der Rohrdurchströmung ist festzustellen, dass diese für Lachgas stets größer als für Helium sind. Bei Lachgas liegt daher für einige Messwerte noch keine ausgebildete laminare Rohrströmung vor. Einlaufeffekte können somit nicht vernachlässigt werden. Als Fazit ergibt sich, dass bei Verwendung von Helium als Prüfgas und Umrechnung der Helium-Messwerte auf Lachgas die Lachgas-Leckageraten sicherheitstechnisch konservativ abgeschätzt werden.
The crystal structures and syntheses of four different copper(II) phenylphosphonates, the monophenylphosphonates α-, β-, and γ-Cu(O3PC6H5)·H2O (α-CuPhPmH (1) β-CuPhPmH (2) and γ-CuPhPmH (3)), and the diphosphonate Cu(HO3PC6H5)2·H2O (CuPhP2mH (4)), are presented. The compounds were synthesized from solution at room temperature, at elevated temperature, under hydrothermal conditions, and mechanochemical conditions. The structures of α-CuPhPmH (1) and CuPhP2mH (4) were solved from powder X-ray diffraction data. The structure of β-CuPhPmH (2) was solved by single crystal X-ray analysis. The structures were validated by extended X-ray absorption fine structure (EXAFS) and DTA analyses. Disorder of the crystal structure was elucidated by electron diffraction. The relationship between the compounds and their reaction pathways were investigated by in situ synchrotron measurements.
Today’s efforts for lightweight design result in a growing application of high-strength structural steels from 960 MPa. In welded structures of these steels increased demands regarding component safety and a high elastic ratio should be considered. Hence, the prevention of an evolution of high weld-induced tensile residual stresses is required. Recent studies showed that component related restraint conditions of welds are able to elevate welding induced stresses to critical values, depending on material characteristics, the welding process and parameters. This work involves multi-axial welding loads as a consequence of the superposition of local residual stresses, global reaction stresses and moments, varying the welding parameters under different restraint conditions. The global welding loads are measured via GMA-weld tests in a special testing facility and via a DIC(Digital Image Correlation)-system in a slot weld. Local transverse residual stresses were analysed by means of X-ray diffraction. The application of a less amount of weld runs due to a modified welding parameters and welds seam configurations revealed as a beneficial approach to reduce welding loads in high-strength steels.