Wissenschaftliche Artikel der BAM
Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (2054) (entfernen)
Sprache
- Englisch (2011)
- Deutsch (40)
- Mehrsprachig (2)
- Portugiesisch (1)
Schlagworte
- Additive manufacturing (64)
- Fluorescence (55)
- SAXS (46)
- Nanoparticles (44)
- Concrete (37)
- MALDI-TOF MS (36)
- Quantum yield (36)
- Corrosion (35)
- Mechanochemistry (29)
- Polylactide (28)
Organisationseinheit der BAM
- 6 Materialchemie (428)
- 1 Analytische Chemie; Referenzmaterialien (352)
- 8 Zerstörungsfreie Prüfung (314)
- 9 Komponentensicherheit (202)
- 5 Werkstofftechnik (196)
- 7 Bauwerkssicherheit (181)
- 4 Material und Umwelt (178)
- 6.3 Strukturanalytik (164)
- 8.5 Röntgenbildgebung (119)
- 6.1 Oberflächen- und Dünnschichtanalyse (97)
Paper des Monats
- ja (68)
The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a plate thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a highspeed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a great influence on the melt pool dynamics and the mixing of the elements of the filler wire. The highspeed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets.
One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds.
The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned during welding in 1G- and 2Gpositions.
Different techniques such as laser power ramp-down, abrupt switch-off of the laser power and change of the magnification of the laser spot diameter and defocusing of the laser beam relative to the workpiece were tested to remove the laser energy from the process. It could be shown that a high defocusing of the optic system above 40 mm with a resulting beam diameter > 2.9 mm in a short overlap length of approx.
20 mm leads to the formation of a cup-shaped weld seam, which is preferred for avoidance of cracks and pores in the end crater. A laser optics with motor-driven lens system was used for the welding experiments to defocuse the laser beam without changing the position of the arc.
Ancient papyri are a written heritage of culture that flourished more than 3000 years ago in Egypt. One of the most significant collections in the world is housed in the Egyptian Museum and Papyrus Collection in Berlin, from where the samples for our investigation come. The papyrologists, curators and conservators of such collections search intensely for the analytical detail that would allow ancient papyri to be distinguished from modern fabrications, in order to detect possible forgeries, assess papyrus deterioration state, and improve the design of storage conditions and conservation methods. This has become the aim of our investigation. The samples were studied by a number of methods, including spectroscopic (FTIR, fluorescent-FS, Raman) diffractional (XRD) and chromatographic (size exclusion chromatography-SEC), selected in order to determine degradation parameters: overall oxidation of lignocellulosic material, degree of polymerization and crystallinity of cellulose. The results were correlated with those obtained from carefully selected model samples including modern papyri and paper of different composition aged at elevated temperature in humid air. The methods were classified in the order SEC > FS > FTIR > XRD, based on their effectiveness in discriminating the state of papyri degradation. However, the most trustworthy evaluation of the age of papyri samples should rely on several methods.