Wissenschaftliche Artikel der BAM
Filtern
Dokumenttyp
Referierte Publikation
- nein (5) (entfernen)
Schlagworte
- Termites (2)
- Acidobacteria (1)
- Biofilm (1)
- Biofouling (1)
- Coptotermes (1)
- Core microbiome (1)
- Fluorides (1)
- Hi-Tension (1)
- Holzschutzmittel (1)
- Hylotrupes bajulus, Anobium punctatum, natural durability, tropical wood, native wood. (1)
Organisationseinheit der BAM
- 4.1 Biologische Materialschädigung und Referenzorganismen (5) (entfernen)
Microbiologically influenced corrosion (MIC) is a crucial issue for industry and infrastructure. Biofilms are known to form on different kinds of surfaces such as metal, concrete, and medical equipment. However, in some cases the effect of microorganisms on the material can be negative for the consistency and integrity of the material. Thus, to overcome the issues raised by MIC on a system, different physical, chemical, and biological strategies have been considered; all having their own advantages, limitations, and sometimes even unwanted disadvantages. Among all the methods, biocide treatments and antifouling coatings are more common for controlling MIC, though they face some challenges. They lack specificity for MIC microorganisms, leading to cross-resistance and requiring higher concentrations. Moreover, they pose environmental risks and harm non-target organisms. Hence, the demand for eco-friendly, long-term solutions is increasing as regulations tighten. Recently, attentions have been directed to the application of nanomaterials to mitigate or control MIC due to their significant antimicrobial efficiency and their potential for lower environmental risk compared to the conventional biocides or coatings. Use of nanomaterials to inhibit MIC is very new and there is a lack of literature review on this topic. To address this issue, we present a review of the nanomaterials examined as a biocide or in a form of a coating on a surface to mitigate MIC. This review will help consolidate the existing knowledge and research on the use of nanomaterials for MIC mitigation. It will further contribute to a better understanding of the potential applications and challenges associated with using nanomaterials for MIC prevention and control.
Microbial communities in the immediate environment of socialized invertebrates can help to suppress pathogens, in part by synthesizing bioactive natural products. Here we characterized the core microbiomes of three termite species (genus Coptotermes) and their nest material to gain more insight into the diversity of termite-associated bacteria.
Sampling a healthy termite colony over time implicated a consolidated and highly stable microbiome, pointing toward the fact that beneficial bacterial phyla play a major role in termite fitness. In contrast, there was a significant shift in the composition of the core microbiome in one nest during a fungal infection, affecting the abundance of wellcharacterized Streptomyces species (phylum Actinobacteria) as well as less-studied bacterial phyla such as Acidobacteria. High-throughput cultivation in microplates was implemented to isolate and identify these less-studied bacterial phylogenetic group.
Amplicon sequencing confirmed that our method maintained the bacterial diversity of the environmental samples, enabling the isolation of novel Acidobacteriaceae and expanding the list of cultivated species to include two strains that may define new species within the genera Terracidiphilus and Acidobacterium.
Fluorides are well-known as wood preservatives. One of the limitations of fluoride-based wood preservatives is their high leachability. Alternative to current fluoride salts such as NaF used in wood protection are low water-soluble fluorides. However, impregnation of low water-soluble fluorides into wood poses a challenge. To address this challenge, low water-soluble fluorides like calcium fluoride (CaF2) and magnesium fluoride (MgF2) were synthesized as nanoparticles via the fluorolytic sol−gel synthesis and then impregnated into wood specimens. In this study, the toxicity of nano metal fluorides was assessed by termite mortality, mass loss and visual analysis of treated specimens after eight weeks of exposure to termites, Coptotermes formosanus. Nano metal fluorides with sol concentrations of 0.5 M and higher were found to be effective against termites resulting in 100% termite mortality and significantly inhibited termite feeding. Among the formulations tested, the least damage was found for specimens treated with combinations of CaF2 and MgF2 with an average mass loss less than 1% and visual rating of “1”. These results demonstrate the efficacy of low water-soluble nano metal fluorides to protect wood from termite attack.
Aim of study: In this study, natural durability of some domestic and foreign wood species against Hylotrupes bajulus and Anobium punctatum larvae were tested on laboratory scale
Area of study: This study was conducted at Department of Forest Products Engineering in Duzce University, Turkey and Federal Institute for Materials Research and Testing (BAM), Germany.
Material and Methods: Scotch pine (Pinus sylvestris), fir (Abies nordmanniana), spruce (Picea orientalis), cedar (Cedrus libani), poplar (Populus tremula) and beech (Fagus orientalis) woods were used to test H. bajulus larvae (EN 46-1). Alder (Alnus glutinosa), oak (Quercus cerris), poplar (Populus tremula), beech (Fagus orientalis), maple (Acer carpinifolium), ash (Fraxinus angustifolia), teak (Tectona grandis), ayous (Triplochiton scleroxylon), movingui (Distemonanthus benthamianus), dahoma (Piptadeniastrum africanum), iroko (Chlorophora excelsa), bubinga (Guibourtia tessmannii) and sapele (Entandrophragma cylindiricum) woods were used for A. punctatum larvae (EN 49-1). At the end of the experiment, the mortality rates of the larvae were determined and the size and weights of the surviving larvae were measured.
Main results: F. orientalis and C. libani were found to be the most resistant wood species against H. bajulus larvae while A. nordmanniana was the least resistant. All tropical wood species and oak and maple from domestic wood species showed 100% mortality rate therefore found to be the most resistant against A. punctatum larvae. The most vulnerable wood species was found to be alder with a 35% mortality.
Research highlights: while F. orientalis, C. libani, and P. tremula were found the most resistance wood species against H. bajulus, P. sylvestris and A. nordmanniana were determined as most vulnerable. All tropical wood species and two domestic species (Q. cerris and A. carpinifolium) showed the highest mortality rate as 100%. The least durable domestic wood was determined as alder.