Kerntechnische Entsorgung
Filtern
Dokumenttyp
- Vortrag (117)
- Beitrag zu einem Tagungsband (71)
- Posterpräsentation (28)
- Zeitschriftenartikel (21)
- Buchkapitel (7)
- Monografie (1)
- Beitrag zu einem Sammelband (1)
- Amtliche Bekanntmachung (1)
- Forschungsbericht (1)
Sprache
- Englisch (248) (entfernen)
Schlagworte
- Ageing (27)
- Drop test (17)
- Metal seal (17)
- Transport (17)
- Ring Compression Test (16)
- Spent Nuclear Fuel (16)
- Ageing Management (15)
- IAEA (15)
- Cladding Embrittlement (14)
- Compression set (13)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (248) (entfernen)
Paper des Monats
- ja (2)
Eingeladener Vortrag
- nein (117)
The safety demonstration of heavy weight type B transport packages used for storing spent nuclear fuel (SNF) or radioactive waste is ensured by a combination of physical testing and numerical calculations. While experiments are performed in accordance with the IAEA regulations for selected drop scenarios, Finite-Element-Method (FEM) simulations are used to predict the most damaging case and to investigate additional drop positions.
BAM as competent authority in Germany has performed different investigations of a welding seam for a typical large transport package made of A508 forged steel, where the bottom plate is welded to the cylindrical shell. The package has a mass of approx. 120 t. Results of physical drop tests with a full-scale model and accompanying preliminary FEM simulations are presented to determine the decisive stresses in the welding seam. A drop test only represents one set of a package and test parameters. A further parameter analysis is considered to account for allowable variations of packaging properties (e.g. resulting from the manufacturing process) and, based on IAEA requirements, the temperature dependence of the material behaviour. The results of the stress analyses from the drop test and the simulation form the basis and provide the input parameters for a fracture mechanics analysis. In addition to the IAEA specifications, further standards are taken into account for an in-depth investigation, see R6, BS 7910 and API 579-1/ASME FFS1.
All the above-mentioned standards require a manufacturer-specific defect analysis with respect to size and position. Both result from the welding process and the following heat treatment regime. The maximum defect sizes are ensured with non-destructive test methods (such as ultrasonic or particle methods) as integral part of the manufacturing process of the welding seam. Another important parameter in the welding process is the residual stress (secondary stress). The combination of the primary and secondary stress determines the total stress in the welding seam. The most damaging case of the welding seam is determined and evaluated with help of the above-mentioned standards and taking into account the IAEA requirements with respect to defect sizes, material properties, primary and residual stress, yield strength etc.
Component and material investigations on metal seals for high level radioactive waste containers
(2018)
In Germany casks for interim storage of spent nuclear fuel and high level radioactive waste are equipped with Helicoflex® metal seals as main sealing barrier of the double lid system. The long-term behaviour of those seals is investigated at Bundesanstalt für Materialforschung und –prüfung (BAM) in order to evaluate the safety function of the containment at different temperatures over storage periods of 40 years or more in case extended interim storage becomes necessary.
Long-term investigations have been done for ageing times of up to 8.5 years at temperatures ranging from room temperature to 150 °C. It was found that the seal force and useable resilience decrease over time, which is mainly caused by creep deformation of the aluminium (or silver) outer jacket of the seals. This effect becomes stronger with increasing temperature.
The ageing processes of the seal material and the overall seal behaviour is under investigation in order to derive analytical descriptions for the long-term seal performance. Thus, standardized tests on the basic seal materials, with focus on aluminium, and additional investigations on the seals as a component are conducted. The current investigations include compression and tension creep measurements as well as tensile testing. Furthermore, ageing of seal segments provides information on the development of the contact area width, jacket thickness and microstructural changes in dependence of time and temperature. The obtained data are used for the development of material models and an analytical approach to describe and predict the time and temperature dependent sealing behaviour in the long-term.
In Germany spent nuclear fuel (SNF) and high level radioactive waste (HLW) are stored in interim storage containers with double lid systems. Those lids are equipped with metal seals (e.g. Helicoflex®) that ensure the safe enclosure of the inventory. Being licensed for up to 40 years of interim storage the evaluation of the long-term behavior of the seals is necessary, taking into account storage conditions, decay heat and possible mechanical loads.
In Germany, spent nuclear fuel and high active waste from reprocessing is stored in transport and storage containers with double lid systems that are equipped with metal seals completing the primary sealing barrier. The tasks of the Bundesanstalt für Materialforschung und -prüfung (BAM) within the interim storage licensing procedures ruled by the German Atomic Energy Act include the long-term safety evaluation of the container design regarding the permanently safe enclosure of the inventory. In order to generate a knowledge base for the safety evaluation, research regarding the long-term behavior of the critical components is performed. So far, the containers are licensed for an interim storage period of 40 years. However, due to significant delays in establishing a final repository, the required time span for interim storage is expected to increase significantly. Thus, a widespread investigation program is run to gain systematic data on the long-term behavior of the seals and to develop prediction models.
Long-term seal investigations consider the development of their restoring seal force, their useable resilience and their achievable leakage rate caused by aging at temperatures ranging from room temperature up to 150 °C. This year, the total time span of the tests reaches 10 years. Furthermore, seal segments are aged at the selected temperatures for up to 300 days. From these segments additional information on the sealing behavior, changes of the seal contact and the material behavior is gained.
This contribution deals with the current results of the long-term seal investigations at BAM. Furthermore, insights of the more in-depth component and material investigations of the metal seals with focus on the seal contact development are discussed and the ongoing work aiming for an analytical description of the thermo-mechanical aging effects on metal seals are presented.
The Bundesanstalt für Materialforschung und –prüfung (BAM) runs an investigation program on the long-term behavior of multi-component metal seals. Such seals are used in a wide area of applications including transport and storage casks for spent nuclear fuel and high level radioactive waste. The seal function is mainly based on the compression of the inner helical spring, which generates the necessary seal force to keep the sealing surfaces in close contact. This in turn leads to a plastic deformation of the outer jacket of the seal, comprised of highly ductile aluminum or silver that adapts to the sealing surfaces of cask body and bolted lid, thus providing high level leak tightness. In Germany, those casks are licensed for interim storage periods of up to 40 years or more if extended interim storage would become necessary before a final repository is available. Thus, the sealing performance has to be evaluated, including factors like elevated temperature due to decay heat or mechanical loads due to transport under normal as well as accident conditions. Long-term investigations at BAM have been running over the last nine years to identify and evaluate the seal performance by measuring the remaining seal force, the useable resilience and the leakage rate after various time intervals at temperatures ranging from room temperature up to 150 °C. It was found that the seal force and useable resilience decrease with time and temperature, caused by creep deformation of the outer jacket. In order to obtain an analytical description for the seal behavior and to achieve more information on the material behavior under application conditions a comprehensive investigation program with focus on aluminum as outer jacket material was launched. The program includes material investigations such as compression and tension creep tests with representative basic materials. An additional test setup allows for the continuous measurement of the remaining seal force at temperatures of up to 150 °C. Furthermore, seal segments are compressed and stored in heating chambers, thus producing segments at different stages of the aging process. The segments are investigated regarding the development of the contact area width, jacket thickness and microstructural changes. This data will be used to develop material models and an analytical description of the time and temperature dependent long-term sealing behavior. This paper explains the current status of gained test results and modelling approaches and closes with an outlook to the future project plans.
In Germany spent nuclear fuel and high level radioactive waste is stored in interim storage containers with double lid systems. Those lids are equipped with metal seals (e.g. Helicoflex®) that ensure the safe enclosure of the inventory. The used metal seals consist of three components as can be seen in the cross-sectional view in Figure 1. The innermost part is a helical spring that is surrounded by an inner jacket made of stainless steel. The outer jacket that is made of a softer material which in case of assembly in the aforementioned storage containers is silver or aluminum (i.e. Al 99.5). During application the seal is compressed and due to the restoring force of the helical spring, the outer jacket is plastically deformed and adapts to the sealing surface. Hence, leakage paths are closed and the sealing function is generated. In Germany the above-mentioned containers are licensed for up to 40 years of interim storage, which in case extended storage becomes necessary before a final repository is available will have to be extended to even longer periods. Therefore, the evaluation of the long-term behavior of the seals is necessary, taking into account storage conditions, decay heat and possible mechanical loads as well.
At Bundesanstalt für Materialforschung und –prüfung (BAM) long-term investigations are being conducted in which seals are assembled in test flanges and aged at temperatures ranging from room temperature to 150°C for accelerated aging. The aged seals are tested semi-annually (after the first 6 months in which the seals are tested more frequently) regarding the sealing performance, the remaining seal force, and the useable resilience upon decompression. Results of these investigations have been published over the past years (e.g. Grelle, Wolff, Probst, Jaunich, & Völzke, 2017; Völzke, Wolff, Probst, Nagelschmidt, & Schulz, 2014). It was found that the seal force and the useable resilience decrease with time and temperature, which is in agreement with the result of other studies (Sassoulas et al., 2006; Wataru et al., 2016) as well. Geometry change of the outer jacket has been identified as the main reason for this seal behavior. At the prevailing operating temperatures and stresses the aluminum is subjected to creep deformation leading to a thinning of the outer jacket. Since the seal groove depth remains unchanged the helical spring expands, which in turn leads to a decrease of the generated spring and seal force.
Although the main reason for the change of seal parameters over time and temperature is known, a detailed characterization of the seal behavior and a reliable prediction of the parameter development for aging times that exceed the experimental time frame have not been possible, yet.
For deeper understanding of the aging processes, an Investigation program, which is covered in this contribution, is conducted at Bundesanstalt für Materialforschung und –prüfung (BAM) that focusses on the behavior of the aluminum jacket and its influence on the long-term sealing performance. The program investigates properties of material samples as well as the behavior of the seal as a component.
Original sheet material of the same aluminum that is used for manufacturing of the seals is investigated in compression creep tests. For this, a DMA (dynamic mechanical analysis) machine is employed (here used for static tests) that allows for a measurement of the specimens deformation under forces of up to 500 N. The advantage of this method is that the original material can be tested in the same shape as used for the seals which is 0.5 mm thick sheet material. For investigation of tensile creep standard specimens are used, that were machined from surrogate material of the same composition and annealing condition.
Furthermore, aluminum seals that are cut into smaller segments are assembled in flanges and placed in heating chambers at temperatures ranging from 23°C to 150°C. After different periods of time from 3 days to 300 days the segments are taken out of the flanges and are investigated, thus giving information on different states of aging. Measurements of the development of the seal contact width and the aluminum jacket thickness are done with an optical microscope. Further investigations on the segments will include metallography and hardness measurements.
From the detailed material and component behavior including the results of the long-term seal force and useable resilience investigations a better understanding of the overall seal behavior can be gained. The aim is to contribute to the development of material models and analytical approaches for the prediction of the sealing behavior in dependence of time and temperature.
In Germany, spent nuclear fuel and high active waste from reprocessing is stored in transport and storage containers with double lid systems that are equipped with metal seals completing the primary sealing barrier. The tasks of the Bundesanstalt für Materialforschung und -prüfung (BAM) within the interim storage licensing procedures ruled by the German Atomic Energy Act include the long-term safety evaluation of the container design regarding the permanently safe enclosure of the inventory. In order to generate a knowledge base for the safety evaluation, research regarding the long-term behavior of the critical components is performed. So far, the containers are licensed for an interim storage period of 40 years. However, due to significant delays in establishing a final repository, the required time span for interim storage is expected to increase significantly. Thus, a widespread investigation program is run to gain systematic data on the long-term behavior of the seals and to develop prediction models.
Long-term seal investigations consider the development of their restoring seal force, their useable resilience and their achievable leakage rate caused by aging at temperatures ranging from room temperature up to 150 °C. This year, the total time span of the tests reaches 10 years. Furthermore, seal segments are aged at the selected temperatures for up to 300 days. From these segments additional information on the sealing behavior, changes of the seal contact and the material behavior is gained.
This contribution deals with the current results of the long-term seal investigations at BAM. Furthermore, insights of the more in-depth component and material investigations of the metal seals with focus on the seal contact development are discussed and the ongoing work aiming for an analytical description of the thermo-mechanical aging effects on metal seals are presented.
The Bundesanstalt für Materialforschung und –Prüfung (BAM) runs an investigation program on the long-term behavior of multi-component metal seals. Such seals are used in a wide area of applications including transport and storage casks for spent nuclear fuel and high level radioactive waste.
The seal function is mainly based on the compression of the inner helical spring, which generates the necessary seal force to keep the sealing surfaces in close contact. This in turn leads to a plastic deformation of the outer jacket of the seal, comprised of highly ductile aluminum or silver that adapts to the sealing surfaces of cask body and bolted lid, thus providing high Level leak tightness. In Germany, those casks are licensed for Interim storage periods of up to 40 years or more if extended Interim storage would become necessary before a final repository is available. Thus, the sealing performance has to be evaluated, including factors like elevated temperature due to decay heat or mechanical loads due to transport under normal as well as accident conditions. Long-term investigations at BAM have been running over the last nine years to identify and evaluate the seal performance by measuring the remaining seal force, the useable resilience and the leakage rate after various time intervals at temperatures ranging from room temperature up
to 150 °C. It was found that the seal force and useable resilience decrease with time and temperature, caused by creep deformation of the outer jacket. In order to obtain an analytical description for the seal behavior and to achieve more information on the material behavior under application conditions a comprehensive investigation program with Focus on aluminum as outer jacket material was launched. The program includes material investigations such as compression and tension creep tests with representative basic materials. An additional test setup allows for the continuous measurement of the remaining seal force at temperatures of up to 150 °C. Furthermore, seal segments are compressed and stored in heating chambers, thus producing segments at different stages of the aging process. The segments are investigated regarding the development of the contact area width, jacket thickness and microstructural changes. This data will be used to develop material models and an analytical description of the time and temperature dependent long-term sealing behavior. This paper explains the current status of gained test results and modelling approaches and closes with an outlook to the future Project plans.
Component and material investigations on metal seals for high level radioactive waste containers
(2018)
Long-term investigations performed at BAM look to extend the state of knowledge on safety-related components of interim storage containers. Metal seals act as the primary sealing barrier in the bolted double lid closure system of the containers. The behaviour of metal seals has been investigated for ageing times up to 8.5 years and for various temperatures. The main cause for reduction in useable resilience overtime was due to creep deformation of the outer jacket of the seal.
Component and material investigations on metal seals for high level radioactive waste containers
(2018)
In Germany casks for interim storage of spent nuclear fuel and high level radioactive waste are equipped with Helicoflex® metal seals as main sealing barrier of the double lid system. The long-term behaviour of those seals is investigated at Bundesanstalt für Materialforschung und –prüfung (BAM) in order to evaluate the safety function of the containment at different temperatures over storage periods of 40 years or more in case extended interim storage becomes necessary.
Long-term investigations have been done for ageing times of up to 8.5 years at temperatures ranging from room temperature to 150 °C. It was found that the seal force and useable resilience decrease over time, which is mainly caused by creep deformation of the aluminium (or silver) outer jacket of the seals. This effect becomes stronger with increasing temperature.
The ageing processes of the seal material and the overall seal behaviour is under investigation in order to derive analytical descriptions for the long-term seal performance. Thus, standardized tests on the basic seal materials, with focus on aluminium, and additional investigations on the seals as a component are conducted. The current investigations include compression and tension creep measurements as well as tensile testing. Furthermore, ageing of seal segments provides information on the development of the contact area width, jacket thickness and microstructural changes in dependence of time and temperature. The obtained data are used for the development of material models and an analytical approach to describe and predict the time and temperature dependent sealing behaviour in the long-term.
Übersicht über die gefahrgutrechtlichen Anforderungen zur Bauartprüfung und dem Qualitätsmanagement für Verpackungen für nicht zulassungspflichtige Versandstücke.
After restarting the site selection process for a final repository for spent nuclear fuel (SNF) and heat-generating radioactive waste, all areas with one of the three potential host rock formations considered in Germany – salt, clay and crystalline rock – are under review. The project “KoBrA“, run by BGE TECHNOLOGY and BAM, collects and reviews requirements, criteria and proposals for final disposal container concepts complying with the current safety standards, taking into consideration international experience in the field of high-level nuclear waste (HLW) management.
The European Joint Programme on Radioactive Waste Management (EURAD) has been launched to coordinate activities on agreed priorities of common interest between European partners. The main actions include scientific and technical activities on radioactive waste characterization and processing, interim storage of radioactive waste as well as predisposal and disposal solutions. As part of the programme, the work package on Spent Fuel Characterization and Evolution until Disposal (SFC) was proposed and accepted by the European Commission. The objectives of this work package include the development of beyond-state-of-the-art characterization techniques for spent nuclear fuel during its evolution from reactor unloading until disposal, the understanding of the spent fuel performance during prolonged storage, transport and emplacement in a deep geological repository, the understanding of the behaviour of fuel, cladding, pellet-cladding interaction and ageing effect under normal and postulated accident scenarios until disposal, and contributions to operational safety concepts for fuel handling at spent nuclear fuel packaging facilities.
For many sealing applications rubbers are applied due to their special material properties and easy use. In many applications as e.g. in aviation, traffic or process technology the material can be exposed to low temperatures during operation. Therefore, it is important to know the material behaviour at those low temperatures to determine the temperature range that allows a safe operation of the seal.
In this work, we focus on the behaviour of elastomer seals at low temperatures with regard to potential decrease of leak-tightness or catastrophic seal failure of O-ring rubber seals. This is required as material properties of rubbers are strongly temperature dependent but their temperature application range is not always clearly defined.
Based on previous investigations which considered the physical material properties and the seal behaviour under purely static conditions we widen the focus on the sealing performance after a fast partial relief of compressed seals and additional materials.
For the investigations, different typical rubber seal materials were used as e.g. fluorocarbon (FKM), ethylene propylene diene (EPDM) and hydrogenated acrylonitrile-butadiene (HNBR) rubber.
The correlation of the physical material properties with seal performance is studied. This includes as well purely static sealing applications as the performance during/after fast partial relief of seals at low temperatures.
Understanding the failure mechanisms that lead to leakage of rubber seals at low temperatures is important. Rubber properties are highly temperature dependent. Changes in behaviour at low temperatures can result from the rubber-glass transition and for some rubbers by partial crystallisation. Experimental results on the low temperature behaviour of different rubber seals were discussed to help understand seal failure processes.
The investigation of the long-term performance of sealing systems employed in containers for radioactive waste and spent nuclear fuel is one research focus area for division 3.4 “Safety of Storage Containers” at the Bundesanstalt für Materialforschung und -prüfung. The behaviour of metallic seals, which are employed in interim storage casks for used fuel and high active waste, over time is of high importance for ensuring safe enclosure. Therefore, investigations on these systems were started at BAM to get a general understanding of the relevant processes. Our investigations comprise investigations on different parameters which influence the seal performance and the main part is focussed on the time and temperature dependent behaviour.
In this contribution an overview of the performed tests and their respective results will be given. A focus will lie on a comparison between seals with large torus diameter in comparison to small diameters.
Our aim is to understand the long-term behaviour of the sealing systems for evaluation of their performance during possible extended interim storage and subsequent transportation.
For many sealing applications rubber O-rings are applied due to their special properties and easy use. In many applications as e.g. in aviation, traffic or process technology the material can be exposed to a variety of conditions during operation as e.g. low temperatures, elevated temperatures and different media. Therefore, it is important to know the material behaviour and the seal performance under those conditions. Additionally ageing of seals is an important factor which has an influence on the long term reliability.
In this contribution we would like to discuss different aspects affecting the seal performance, lifetime estimation and address open questions which should be addressed to come to a deeper understanding of these seals commonly understood as typical machine elements.
Results of running investigations at the Bundesanstalt für Materialforschung und -prüfung (BAM), Division 3.4 “Safety of Storage Containers” are presented and discussed.
Editorial
(2019)
Dear Readers, a new year started for all of us (as I write these lines, possibly it was already some time ago when these lines are finally available) and this is the time for the so-called New Year’s resolutions. Setting goals and changing our behavior as well in a private as in a professional context.
For Scientists the resolutions may comprise tasks like finalizing a longago started publication, picking up the loose ends of an application for funding or just bringing the running projects in a greater structure.