Kerntechnische Entsorgung
Filtern
Dokumenttyp
- Vortrag (117)
- Beitrag zu einem Tagungsband (71)
- Posterpräsentation (28)
- Zeitschriftenartikel (21)
- Buchkapitel (7)
- Monografie (1)
- Beitrag zu einem Sammelband (1)
- Amtliche Bekanntmachung (1)
- Forschungsbericht (1)
Sprache
- Englisch (248) (entfernen)
Schlagworte
- Ageing (27)
- Drop test (17)
- Metal seal (17)
- Transport (17)
- Ring Compression Test (16)
- Spent Nuclear Fuel (16)
- Ageing Management (15)
- IAEA (15)
- Cladding Embrittlement (14)
- Compression set (13)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (248) (entfernen)
Paper des Monats
- ja (2)
Eingeladener Vortrag
- nein (117)
The investigation of the long-term performance of sealing systems employed in containers of radioactive waste and spent nuclear fuel is one research focus area for division 3.4 \Safety of Storage Containers" at the Bundesanstalt für Materialforschung und -prüfung. The behaviour of metallic seals, which are employed in interim storage casks for spent nuclear fuel and high active waste, over time is of high importance for ensuring safe enclosure. Therefore, investigations on these systems were started at BAM to get a general understanding of the relevant processes. Our investigations comprise investigations on different parameters which influence the seal Performance and the main part is focussed on the time and temperature dependent behaviour. Our aim is to understand the longterm behaviour of the sealing systems for evaluation of their performance during possible extended interim storage and subsequent transportation. In this contribution an overview of the performed tests and their respective results is given. A focus lies on a comparison between seals with large torus diameter in comparison to small diameters.
Outcomes of Three Large-Scale Fire Reference Tests Conducted in Propane Gas Fire Test Facility
(2020)
Packages for the transport of high-level radioactive material are designed to withstand severe accidents. Hypothetical severe accident conditions are defined in the IAEA Regulations for the Safe Transport of Radioactive Materials. One of these accident conditions is the thermal test, mainly consisting of a 30 minute fully engulfing 800°C pool fire or an equally severe fire test. The heat fluxes into the package depend substantially on the fire characteristics and the surface temperature of the package. Fire tests can be performed at BAM on a propane gas fire test facility. In order to investigate the heat fluxes over a wide range of surface temperatures in this test facility a fire reference package was designed for multiple use. The package represented the outer geometry of a specific transport cask for radioactive waste. The fire reference package is a closed steel sheet cylinder with a wall thickness of 10 mm, a length of 1500 mm and a diameter of 1050 mm. The package was instrumented with thermocouples and filled with heat resistant insulation material. Three open-air fire tests were performed in the BAM propane gas fire test facility. The flames exposure time period varied slightly for the fire tests. The wind direction as well as the wind speed were measured and changed between and during the tests. Test stand parameters such as wind shield location and propane gas volume flow were chosen constant for the three tests. The locally measured fire reference package steel sheet temperatures were used for the calculation of heat fluxes as function of time and surface temperature. The measured temperatures allowed further calculations. In a first approach effective fire characteristics of the propane gas fire, including the flame temperature, the fire convection coefficient and a radiation exchange coefficient mathematically describing the determined average heat flux over the surface temperature were calculated.
Safety of long term containment and storage of radioactive waste is an essential issue, which is increasingly gaining international attention. Extending interim storage beyond initial license periods is one of the major challenges worldwide.
BAM has been involved in all kinds of radioactive waste container safety evaluation for storage and transportation including their long term performance from the very beginning. Today, all work related to the safe management of radioactive waste is linked by the activity field “Nuclear Waste Management” within the Focus Area “Energy” at BAM and in conjunction with a research strategy and agenda. Most recently, the working group “Long Term Safety of Container Systems and Components” was established to launch and perform research projects related to safety issues concerning the extended interim storage of radioactive waste.
For example, within our project LaMEP, we investigate ageing effects of metal and elastomer seals as well as polymeric neutron shielding materials, which are container components that fulfil major safety functions. The results of the experiments help to understand the long term behaviour of these components. Likewise, our project BRUZL started at BAM in 2018 with the aim of developing a fracture mechanics approach to understand and describe a potential brittle failure mechanism of fuel cladding during long-term interim storage. BAM also contributes to the GRS project “Development of methods and models and international exchange for safety evaluation in the frame of interim storage of radioactive waste”. Additionally, BAM is involved in several international research programmes dealing with extended interim storage, such as the European Joint Programme on Radioactive Waste Management (EURAD), the Extended Storage Collaboration Program (ESCP) and IAEA Coordinated Research Projects.
The present contribution provides a comprehensive overview of BAM research activities contributing to national and international gap analyses and to filling knowledge gaps regarding the safe long term management of radioactive waste.
In Germany, spent nuclear fuel and vitrified high active waste is stored in dual purpose casks (DPC) at interim storage facilities. In order to ensure the transportability of the DPC to a final repository in future, the maintenance of the package design approval is realized. Therefore, the assessment of possible ageing effects during interim storage is necessary to ensure an evaluation of the transportability. The lecture presents BAM's current ageing evaluation concept in the field of trasnport law.
The containment system of transport packages for spent nuclear fuel and high-level waste usually includes bolted lids with metal gaskets. The specified transport condition imply high loading on the lids and the bolt connections of the package. The response of the lid systems on these load conditions is generally investigated by drop tests or numerically. BAM has started a research project to get a better understanding about the behavior of prestressed bolt connection under loadings typical for drop tests.
Packages for the transport of high-level radioactive material are designed to withstand severe accidents. Hypothetical severe accident conditions are defined in the IAEA Regulations for the Safe Transport of Radioactive Materials. One of these accident conditions is the thermal test, mainly consisting of a 30 minute fully engulfing 800°C pool fire or an equally severe fire test. The heat fluxes into the package depend substantially on the fire characteristics and the surface temperature of the package. Fire tests can be performed at BAM on a propane gas fire test facility. In order to investigate the heat fluxes over a wide range of surface temperatures in this test facility a fire reference package was designed for multiple use. The package represented the outer geometry of a specific transport cask for radioactive waste. The fire reference package is a closed steel sheet cylinder with a wall thickness of 10 mm, a length of 1500 mm and a diameter of 1050 mm. The package was instrumented with thermocouples and filled with heat resistant insulation material. Three open-air fire tests were performed in the BAM propane gas fire test facility. The flames exposure time period varied slightly for the fire tests. The wind direction as well as the wind speed were measured and changed between and during the tests. Test stand parameters such as wind shield location and propane gas volume flow were chosen constant for the three tests. The locally measured fire reference package steel sheet temperatures were used for the calculation of heat fluxes as function of time and surface temperature. The measured temperatures allowed further calculations. In a first approach effective fire characteristics of the propane gas fire, including the flame temperature, the fire convection coefficient and a radiation exchange coefficient mathematically describing the determined average heat flux over the surface temperature were calculated.
Damaged spent nuclear fuel (DSNF) can be loaded in German dual-purpose casks (DPC) for transport and interim storage. Encapsulations are needed to guarantee a safe handling and a tight closure, separated from the package enclosure. These encapsulations shall be durable and leak-tight for a long storage period, because they are usually not accessible within periodical inspections of the DPC. Due to the general design of DPCs for standard fuel assemblies, specific requirements have to be considered for the design of encapsulations for DSNF to ensure the loading in existing package designs. Especially the primary lid system of a DPC is designed for maximum loads due to the internal impact of the content during drop test conditions. The main difference of encapsulations for damaged spent nuclear fuel is that they have usually a much higher stiffness than standard fuel assemblies. Therefore the design of an internal shock absorber, e.g. at the head of an encapsulation is required to reduce mechanical loads to the primary lid system during impacts.
BAM as part of the German competent authority system is responsible for the safety assessment of the mechanical and thermal package design, the release of radioactive material and the quality assurance of package manufacturing and operation. Concerning the mechanical design of the encapsulation BAM was involved in the comprehensive assessment procedure during the package design approval process. An internal shock absorber was developed by the package designer with numerical analyses and experimental drop tests. Experimental drop tests are needed to cover limiting parameters regarding, e.g. temperature and wall thickness of the shock absorbing element to enable a detailed specification of the whole load-deformation behavior of the encapsulation shock absorber.
The paper gives an overview of the assessment work by BAM and points out the main findings which are relevant for an acceptable design of internal shock absorbers. The physical drop tests were planned on the basis of pre-investigations of the applicant concerning shape, dimension and material properties. In advance of the final drop tests the possible internal impact behavior had to be analyzed and the setup of the test facility had to be validated. The planning, performance and evaluation of the final drop tests were witnessed and assessed by BAM. In conclusion it could be approved that the German encapsulation system for damaged spent nuclear fuel with shock absorbing components can be handled similar to standard fuel assemblies in existing package designs.
Damaged spent nuclear fuel (DSNF) can be loaded in German dual-purpose casks (DPC) for transport and interim storage. Encapsulations are needed to guarantee a safe handling and a tight closure, separated from the package enclosure. These encapsulations shall be durable and leak-tight for a long storage period, because they are usually not accessible within periodical inspections of the DPC. Due to the general design of DPCs for standard fuel assemblies, specific requirements have to be considered for the design of encapsulations for DSNF to ensure the loading in existing package designs. Especially the primary lid system of a DPC is designed for maximum loads due to the internal impact of the content during drop test conditions. The main difference of encapsulations for damaged spent nuclear fuel is that they have usually a much higher stiffness than standard fuel assemblies. Therefore the design of an internal shock absorber, e.g. at the head of an encapsulation is required to reduce mechanical loads to the primary lid system during impacts.
BAM as part of the German competent authority system is responsible for the safety assessment of the mechanical and thermal package design, the release of radioactive material and the quality assurance of package manufacturing and operation. Concerning the mechanical design of the encapsulation BAM was involved in the comprehensive assessment procedure during the package design approval process. An internal shock absorber was developed by the package designer with numerical analyses and experimental drop tests. Experimental drop tests are needed to cover limiting parameters regarding, e.g. temperature and wall thickness of the shock absorbing element to enable a detailed specification of the whole load-deformation behavior of the encapsulation shock absorber.
The paper gives an overview of the assessment work by BAM and points out the main findings which are relevant for an acceptable design of internal shock absorbers. The physical drop tests were planned on the basis of pre-investigations of the applicant concerning shape, dimension and material properties. In advance of the final drop tests the possible internal impact behavior had to be analyzed and the setup of the test facility had to be validated. The planning, performance and evaluation of the final drop tests were witnessed and assessed by BAM. In conclusion it could be approved that the German encapsulation system for damaged spent nuclear fuel with shock absorbing components can be handled similar to standard fuel assemblies in existing package designs.
As part of the evaluation of a package for the safe transport of radioactive waste the regulations of the IAEA International Atomic Energy Agency shall be fulfilled. The regulations define requirements for the package and specify mechanical and thermal test conditions. Different methods are allowed for the test performance to demonstrate compliance with the regulations. Next to calculational approaches and the use of models of an appropriate scale, the performance of full-scale testing with prototype packages respectively full-scale models is applied.
The use of full-scale models has several advantages within the complete safety assessment procedure for a transport package approval. Scaling and corresponding similarity questions don’t have to be considered, additional material investigations can be limited and analyses to transfer test results to the original package design are reduced in number and complexity. Additionally, experience for future serial design procedures can be built up during manufacturing and assembling of the test model.
BAM operates different drop and fire test facilities south of Berlin, Germany. BAM has started to perform a drop test campaign with a full-scale model of 120 metric tons weight for a transport package approval procedure. The paper describes experience with test preparation, drop performance and additional analyses. The measurement concept is explained and test goals regarding the package safety assessment and evaluation of safety margins are introduced.
Packages for the transport of high-level radioactive material must withstand severe hypothetical accidents. Regulatory test conditions shall cover these severe accident conditions and consist of mechanical tests and a following thermal test. To withstand the mechanical tests heavy weight packages are often designed with impact limiters consisting of wood encapsulated in steel sheets. The thermal test is defined precisely in the IAEA-regulations as a 30 minute fully engulfing 800 °C fire. After the fire phase a pre-damaged impact limiter might continue burning or smouldering and influence the cask thermal behaviour with its energy release. The energy transferred from the impact limiter to the cask is of importance for the safety of transport packages. A full-scale fire test with an impact limiter of 2.3 m in diameter and filled with spruce wood was designed and performed. The impact limiter continued burning for 3 days. Energy transfer and temperature measurements were performed.
Elastomer seals are used in many industrial applications due to their excellent mechanical properties at a wide range of temperatures. Their high versatility and recovery potential under several load conditions make them well suitable for the application in containers designed for transport, storage and/or disposal of radioactive materials. In containers for low and intermediate level radioactive waste, elastomer seals are used as barrier seals, and as auxiliary seals in storage and transportation casks (dual purpose casks) for heat generating radioactive waste, such as spent fuel and high-level waste. While a seal exchange at defined intervals is typical in many conventional applications, it is impossible or at least hard to perform when principles of minimization of radiation exposure have to be considered and prohibit an unnecessary cask handling. An extensive knowledge of the change of the elastomer’s properties during aging and the availability of reliable end-of-lifetime criteria to guarantee the permanent safe enclosure of the radioactive material is mandatory. As BAM is involved in most of the national cask licensing procedures and in the evaluation of cask-related long-term safety issues, great efforts have been already made and are still planned to scientifically support this task.
Compression stress relaxation and compression set were identified as key indicators of elastomer long-term performance and quantitatively investigated in comprehensive test programs. Among other representative types of elastomers, specimens made from ethylene propylene diene rubber (EPDM) were tested before, during and after aging to capture the most important of their complex mechanical properties.
In the presented study, exemplary results were used to simulate the compression stress relaxation and the compression set of elastomer O-rings during aging. Regarding the influence of temperature, the time-temperature superposition principle is applied in the relaxation analysis of elastomer O-rings. The proposed model is implemented in the commercial finite element software ABAQUS/Standard® [1] with a sequential temperature displacement coupling. Numerical results match the experimental compression stress relaxation measurements well. The prediction of compression set values after long-term aging shows a relatively good agreement with the experimental results. Nevertheless, all input parameters derived from the specimen tests, additional assumptions concerning boundary conditions and modeling strategy are discussed with regard to the identified slight discrepancies.
The possibility to extend the finite element model to represent the O-ring seal’s ability to recover after a (fast) partial release is taken into account.
Understanding the failure mechanisms that lead to leakage of rubber seals at low temperatures is important. Rubber properties are highly temperature dependent. Changes in behaviour at low temperatures can result from the rubber-glass transition and for some rubbers by partial crystallisation. Experimental results on the low temperature behaviour of different rubber seals were discussed to help understand seal failure processes.
To improve the predictive capability of long-term stress relaxation of elastomers during thermo-oxidative ageing, a method to separate reversible and irreversible processes was adopted.
The separation is performed through the analysis of compression set after tempering. On the Basis of this separation, a numerical model for long-term stress relaxation during homogeneous ageing is proposed. The model consists of an additive contribution of physical and chemical relaxation.
Computer simulations of compression stress relaxation were performed for long ageing times and the results were validated with the Arrhenius treatment, the kinetic study and the time-temperature superposition technique based on experimental data. For chemical relaxation, two decay functions are introduced each with an activation energy and a degradative process. The first process with the lower activation energy dominates at lower ageing times, while the second one with the higher activation energy at longer ageing times. A degradation-rate based model for the evolution of each process and ist contribution to the total system during homogeneous ageing is proposed. The main advantage of the model is the possibility to quickly validate the interpolation at lower temperatures within the range of slower chemical processes without forcing a straight-line extrapolation.
Packages for the transport of high-level radioactive material are designed to withstand severe accidents. Hypothetical severe accident conditions are defined in the IAEA Regulations for the Safe Transport of Radioactive Materials.
One of these accident conditions is the thermal test, mainly consisting of a 30 minute fully engulfing 800°C pool fire or an equally severe fire test. The heat fluxes into the package depend substantially on the fire characteristics and the Surface temperature of the package.
Fire tests can be performed at BAM on a propane gas fire test facility. In order to investigate the heat fluxes over a wide range of surface temperatures in this test facility a fire reference package was designed for multiple use. The package represented the outer geometry of a specific transport cask for radioactive waste. The fire reference package is a closed steel sheet cylinder with a wall thickness of 10 mm, a length of 1500 mm and a diameter of 1050 mm. The package was instrumented with thermocouples and filled with heat resistant insulation material.
Three open-air fire tests were performed in the BAM propane gas fire test facility. The flames exposure time period varied slightly for the fire tests. The wind direction as well as the wind Speed were measured and changed between and during the tests. Test stand parameters such as wind shield location and propane gas volume flow were chosen constant for the three tests. The locally measured fire reference package steel sheet temperatures were used for the calculation of heat fluxes as function of time and surface temperature. The measured temperatures allowed further calculations. In a first approach effective fire characteristics of the propane gas fire, including the flame temperature, the fire convection coefficient and a Radiation exchange coefficient mathematically describing the determined average heat flux over the surface temperature were calculated.
Packages for the transport of high-level radioactive material are designed to withstand severe accidents. Hypothetical severe accident conditions are defined in the IAEA Regulations for the Safe Transport of Radioactive Materials.
One of these accident conditions is the thermal test, mainly consisting of a 30 minute fully engulfing 800°C pool fire or an equally severe fire test. The heat fluxes into the package depend substantially on the fire characteristics and the Surface temperature of the package.
Fire tests can be performed at BAM on a propane gas fire test facility. In order to investigate the heat fluxes over a wide range of surface temperatures in this test facility a fire reference package was designed for multiple use. The package represented the outer geometry of a specific transport cask for radioactive waste. The fire reference package is a closed steel sheet cylinder with a wall thickness of 10 mm, a length of 1500 mm and a diameter of 1050 mm. The package was instrumented with thermocouples and filled with heat resistant insulation material.
Three open-air fire tests were performed in the BAM propane gas fire test facility. The flames exposure time period varied slightly for the fire tests. The wind direction as well as the wind Speed were measured and changed between and during the tests. Test stand parameters such as wind shield location and propane gas volume flow were chosen constant for the three tests. The locally measured fire reference package steel sheet temperatures were used for the calculation of heat fluxes as function of time and surface temperature. The measured temperatures allowed further calculations. In a first approach effective fire characteristics of the propane gas fire, including the flame temperature, the fire convection coefficient and a Radiation exchange coefficient mathematically describing the determined average heat flux over the surface temperature were calculated.
Experimental and numerical analyses of spent nuclear fuel behavior under transport conditions
(2019)
Packages for the transport of spent nuclear fuel shall meet the International Atomic Energy Agency regulations to ensure safety under different transport conditions. The physical state of the spent fuel and the fuel rod cladding as well as the geometric configuration of fuel assemblies are important inputs for the evaluation of the package capabilities under these conditions. The mechanical behavior of spent fuel assemblies shall be analyzed with regard to the assumptions which are used in the containment and criticality safety analysis. The package as a mechanical system is characterized by a complex set of interactions, e. g. between the fuel rods within the assembly as well as between the fuel assemblies, the basket, and the cask containment. This complexity makes it difficult to assume appropriate mechanical loads for the spent fuel inside the package. Another challenge is the assumption of material properties which represent the variation of the fuel rods regarding cladding material, burn-up and the operation history sufficiently. The objective of this paper is to give an overview about the current approaches and research for the evaluation of spent fuel behavior within the package design approval procedure. In this context, analytical, numerical and experimental results are discussed. The presented work is achieved within a collaboration of BAM with national and international partners.
At the Bundesanstalt für Materialforschung und -prüfung (BAM) in Division 3.4 Safety of Storage Containers, one of our tasks is to evaluate the safety of containers designed for disposal of low and intermediate radioactive waste. As such containers might be transported before and stored until disposal, safe enclosure of the radioactive inventory is important for this time span. Elastomer O-rings are widely used as barrier seals in these containers. Thus, as for many other applications, an understanding of the practical effects of ageing degradation on elastomer seals during long-term exposure is mandatory for predicting the lifetime of such components. According to a long-term test programme on three kinds of rubbers (EPDM and FKM (relevant for application), HNBR (for comparison)), over several years we have studied the degradation and the change of mechanical properties (e.g. hardness, strain at break) at four different ageing temperatures (75 °C, 100 °C, 125 °C and 150 °C) as well as the change of sealing properties. Continuous and intermittent compression stress relaxation (CSR) measurements were performed in order to investigate the respective contribution of crosslinking and chain scission to the observed degradation effects. Thus, the degradation kinetics and mechanisms could be resolved more clearly. For assessing the seal performance, compression set (CS) and leakage rate measurements were conducted. The experimental results showed that the O-rings remained leak-tight under purely static conditions even when CSR, CS and mechanical properties already indicated far advanced degradation. For this reason, a modified leakage test involving a small and rapid partial decompression of the seal was developed that enabled determining an end-of-lifetime criterion for O-rings with a safety margin for thermal shrinkage and vibrations.
For disposal of the research reactor of the Technical University Munich FRM II a new transport and storage cask design was under approval assessment by the German authorities on the basis of International Atomic Energy Agency (IAEA) requirements. The cask body is made of ductile cast iron and closed by two bolted lid systems with metal seals. The material of the lids is stainless steel. On each end of the cask the wood-filled impact limiters are installed to reduce impact loads to the cask under drop test conditions. In the cavity of the cask a basket for five spent fuel elements is arranged.
This design has been assessed by the Bundesanstalt für Materialforschung und -prüfung (BAM) in view to the mechanical and thermal safety analyses, the activity release approaches, and subjects of quality assurance and surveillance for manufacturing and operation of the package.
For the mechanical safety analyses of the package a combination of experimental testing and analytical/numerical calculations were applied. In total, four drop tests were carried out at the BAM large drop test facility. Two tests were carried out as a full IAEA drop test sequence consisting of a 9m drop test onto an unyielding target and a 1m puncture bar drop test. The other two drop tests were performed as single 9m drop tests and completed by additional analyses for considering the effects of an IAEA drop test sequence.
The main objectives of the drop tests were the investigation of the integrity of the package and its safety against release of radioactive material as well as the test of the fastening system of the impact limiters. Furthermore, the acceleration and strain signals measured during the tests were used for the verification of finite-element (FE) models applied in the safety analysis of the package design.
O-rings made of HNBR, EPDM and FKM were aged in the compressed and uncompressed state at 150 °C, 125 °C, 100 °C, 75 °C, 60 °C and 23 °C for aging times of up to five years. Hardness was measured and increased with aging time and temperature for HNBR and EPDM, but it remained practically constant for FKM. Indenter modulus measurements were performed on the lateral O-ring surface (that was free of DLO effects) to assess an influence of the compression during aging, but none was detected. The equilibrium compression set (CS) exhibited faster and stronger degradation than hardness and was used for lifetime predictions using the time-temperature superposition (TTS) principle. With an end-of-lifetime criterion of 70 % CS, lifetimes of 4.5 years, 50 years and 526 years at 75 °C were estimated for HNBR, EPDM and FKM, respectively. The activation energies derived from an Arrhenius plot of the shift factors from the TTS were 85 kJ/mol, 99 kJ/mol and 78 kJ/mol for HNBR, EPDM and FKM, respectively, revealing that a higher activation energy does not necessarily mean that the material has a higher lifetime at lower temperatures. Furthermore, the measured lifetime of EPDM O-rings at 100 °C (5 years) was compared to that predicted on the basis of the lifetime at 150 °C as well as 125 °C using the corresponding shift factors. The error of the prediction was only ± 4 %. However, this precise prediction could only be achieved using the five-year long-term aging data. When using only data from aging times up to 0.5 years and 2 years, the lifetime of EPDM O-rings at 100 °C was underestimated by 31 % and 22 %, respectively.
The nuclear phase out in Germany will lead to a challenge finding skilled staff for all areas in nuclear business. Transport of spent fuel and high-level nuclear waste is an ongoing task over the next decades during the decommissioning of nuclear power plants and after the interim storage. The international regulations were adapted and address the issue of transports after storage now. The topic of aging and assessment of the development of the state-of-art technology are in focus. German research funds are supporting the investigations of future challenges of transport and storage of the nuclear heritage. BAM is involved and works on several topics related to the aging issue of packages. The behaviour of spent fuel claddings, long-term behaviour of metal and elastomeric gaskets and sensor/monitoring techniques of waste disposal are examples of research fields.
The investigation of the long-term performance of sealing systems employed in containers for radioactive waste and spent nuclear fuel is one research focus area for division 3.4 “Safety of Storage Containers” at the Bundesanstalt für Materialforschung und -prüfung. The behaviour of metallic seals, which are employed in interim storage casks for used fuel and high active waste, over time is of high importance for ensuring safe enclosure. Therefore, investigations on these systems were started at BAM to get a general understanding of the relevant processes. Our investigations comprise investigations on different parameters which influence the seal performance and the main part is focussed on the time and temperature dependent behaviour.
In this contribution an overview of the performed tests and their respective results will be given. A focus will lie on a comparison between seals with large torus diameter in comparison to small diameters.
Our aim is to understand the long-term behaviour of the sealing systems for evaluation of their performance during possible extended interim storage and subsequent transportation.
Compared with the original time-temperature superposition (TTS) principle, an extended non-linear time-temperature equivalent (TTE) principle is suggested in this work. Results shown us, all application of TTS and most of the TTE parameters, for example, the Orr-Sherby-Dorn, Manson-Succop, Larson-Müller, Manson-Haferd, Mendelson-Roberts-Manson parameters and the more general ‘single metamodel’ from Haque–Stewart are special cases of the new suggested principle. The merits of this new method are discussed.
This paper establishes different axisymmetric and two-dimensional models for a levitation device. Therein, the Maxwell equations are combined with the balance of linear momentum. Different possible formulations to describe the Maxwell equations are presented and compared and discussed in the example. A high order finite element discretization using Galerkin’s method in space and the generalized Newmark−alpha method in time are developed for the electro-magneto-mechanical approach. Several studies on spatial and temporal discretization with respect to convergence will be investigated. In addition, the boundary influences and the domain size with respect to the levitation device are also examined.
A new dual purpose cask design was developed for the safe transport and interim storage of spent fuel elements of German research reactors. In the framework of the safety assessment within the package approval procedure the Bundesanstalt für Materialforschung und –prüfung (BAM) as competent authority performed a series of drop tests according with the IAEA Transport Regulations. The package consists of a cylindrical thick-walled ductile cast iron cask body closed by a bolted lid system with metallic seals. A lid and bottom sided impact limiter consisting of a wood/steel construction limit the mechanical impact loading. The full-scale test specimen was equipped with a basket and assembled with dummy-fuel elements. The package and test specimen, respectively have a total mass of approximately 24 metric tons. The mechanical drop test program included three 9m free drop tests, in horizontal, vertical and oblique cask orientation onto the lid system. Additionally, a 1m-puncture bar drop test followed the horizontal drop test to consider an IAEA-drop test sequence. The horizontal and vertical drop tests were performed at a temperature of minus 40°C. During the oblique drop test the upper impact limiter was heated up to +80°C. The tests were conducted onto an unyielding target, fulfilling the IAEA requirements. The test specimen was considerably instrumented with strain gauges and accelerometers. Transient strains at selected locations of the inner and outer container walls, of the primary and secondary lid, as well as of the corresponding lid bolts were measured during the drop tests. Furthermore, decelerations in different locations at the cask body and the lids were measured. The complex geometrical deformation of the impact limiters due to the impact were determined by optical 3D- measurements. Before and after the drop tests the leakage rate of the lid system was determined by helium leakage testing. The experimental results contribute to the evaluation of the package response to mechanical tests, demonstrating safety under normal and accident conditions of transport and especially to the verification of the dynamic finite-element model of the package used in the package design safety report.
A new dual purpose cask design was developed for the safe transport and interim storage of spent fuel elements of German research reactors. In the framework of the safety assessment within the licensing procedure the Bundesanstalt für Materialforschung und –prüfung (BAM) as competent authority performed a series of drop tests according to the IAEA-Regulations. The package consists of a cylindrical thick-walled ductile cast iron cask body closed by a double lid system with metallic seals. A lid and bottom sided impact limiter consisting of a wood/steel construction limit the mechanical impact loading. The full-scale test specimen was equipped with a basket and assembled with dummy-fuel elements. The package and test specimen, respectively have a total mass of approximately 24 metric tons.
The mechanical test program included three 9m free drop tests, in horizontal, vertical and oblique cask orientation onto the lid system. Additionally, a 1m-puncture drop test followed the horizontal drop test to consider an IAEA-test sequence. The horizontal and vertical drop tests were performed at a temperature of minus 40°C. During the oblique drop test the upper impact limiter was heated to +80°C. The tests were conducted onto an unyielding target, fulfilling the requirements of the IAEA regulations.
The test specimen was considerably instrumented with strain gauges and accelerometers. Transient strains at selected locations of the inner and outer container walls, of the primary and secondary lid, as well as of the corresponding lid bolts were measured during the drop tests. Furthermore, decelerations in different locations at the cask body and the lids were measured. The complex geometrical deformation of the impact limiters due to the impact were determined by optical 3d- measurements using the projected fringe method in combination with multi-image photogrammetry. Before and after the drop tests the leakage rate of the lid system was determined by helium leakage testing.
The experimental results contribute to the evaluation of the package response to mechanical tests, demonstrating safety under normal and accident conditions of transport. Especially to the verification of the dynamic finiteelement model of the package used in the package design safety report. The paper describes the performance of the drop tests, selected test results focusing on the lid screws and the cask body and the deformation of the impact limiters as well as impact kinematics, respectively.
A new dual purpose cask design was developed for the safe transport and interim storage of spent fuel elements of German research reactors. In the framework of the safety assessment within the licensing procedure the Bundesanstalt für Materialforschung und –prüfung (BAM) as competent authority performed a series of drop tests according to the IAEA-Regulations. The package consists of a cylindrical thick-walled ductile cast iron cask body closed by a double lid system with metallic seals. A lid and bottom sided impact limiter consisting of a wood/steel construction limit the mechanical impact loading. The full-scale test specimen was equipped with a basket and assembled with dummy-fuel elements. The package and test specimen, respectively have a total mass of approximately 24 metric tons.
The mechanical test program included three 9m free drop tests, in horizontal, vertical and oblique cask orientation onto the lid system. Additionally, a 1m-puncture drop test followed the horizontal drop test to consider an IAEA-test sequence. The horizontal and vertical drop tests were performed at a temperature of minus 40°C. During the oblique drop test the upper impact limiter was heated to +80°C. The tests were conducted onto an unyielding target, fulfilling the requirements of the IAEA regulations.
The test specimen was considerably instrumented with strain gauges and accelerometers. Transient strains at selected locations of the inner and outer container walls, of the primary and secondary lid, as well as of the corresponding lid bolts were measured during the drop tests. Furthermore, decelerations in different locations at the cask body and the lids were measured. The complex geometrical deformation of the impact limiters due to the impact were determined by optical 3d- measurements using the projected fringe method in combination with multi-image photogrammetry. Before and after the drop tests the leakage rate of the lid system was determined by helium leakage testing.
The experimental results contribute to the evaluation of the package response to mechanical tests, demonstrating safety under normal and accident conditions of transport. Especially to the verification of the dynamic finiteelement model of the package used in the package design safety report. The paper describes the performance of the drop tests, selected test results focusing on the lid screws and the cask body and the deformation of the impact limiters as well as impact kinematics, respectively.
A new dual purpose cask design was developed for the safe transport and interim storage of spent fuel elements of German research reactors. In the framework of the safety assessment within the licensing procedure the Bundesanstalt für Materialforschung und –prüfung (BAM) as competent authority performed a series of drop tests according to the IAEA-Regulations [1]. The package consists of a cylindrical thick-walled ductile cast iron cask body closed by a double lid system with metallic seals. A lid and bottom sided impact limiter consisting of a wood/steel construction limit the mechanical impact loading. The full-scale test specimen was equipped with a basket and assembled with dummy-fuel elements. The package and test specimen, respectively have a total mass of approximately 24 metric tons.
The mechanical test program included three 9m free drop tests, in horizontal, vertical and oblique cask orientation onto the lid system. Additionally, a 1m-puncture drop test followed the horizontal drop test to consider an IAEA-test sequence. The horizontal and vertical drop tests were performed at a temperature of minus 40°C. During the oblique drop test the upper impact limiter was heated to +80°C. The tests were conducted onto an unyielding target, fulfilling the requirements of the IAEA regulations [1].
The test specimen was considerably instrumented with strain gauges and accelerometers. Transient strains at selected locations of the inner and outer container walls, of the primary and secondary lid, as well as of the corresponding lid bolts were measured during the drop tests. Furthermore, decelerations in different locations at the cask body and the lids were measured. The complex geometrical deformation of the impact limiters due to the impact were determined by optical 3d- measurements using the projected fringe method in combination with multi-image photogrammetry. Before and after the drop tests the leakage rate of the lid system was determined by helium leakage testing.
The experimental results contribute to the evaluation of the package response to mechanical tests, demonstrating safety under normal and accident conditions of transport. Especially to the verification of the dynamic finiteelement model of the package used in the package design safety report [2]. The paper describes the performance of the drop tests, selected test results focusing on the lid screws and the cask body and the deformation of the impact limiters as well as impact kinematics, respectively.
A new dual purpose cask design was developed for the safe transport and interim storage of spent fuel elements of German research reactors. In the framework of the safety assessment within the package approval procedure the Bundesanstalt für Materialforschung und –prüfung (BAM) as competent authority performed a series of drop tests according with the IAEA Transport Regulations. The package consists of a cylindrical thick-walled ductile cast iron cask body closed by a bolted lid system with metallic seals. A lid and bottom sided impact limiter consisting of a wood/steel construction limit the mechanical impact loading. The full-scale test specimen was equipped with a basket and assembled with dummy-fuel elements. The package and test specimen, respectively have a total mass of approximately 24 metric tons. The mechanical drop test program included three 9m free drop tests, in horizontal, vertical and oblique cask orientation onto the lid system. Additionally, a 1m-puncture bar drop test followed the horizontal drop test to consider an IAEA-drop test sequence. The horizontal and vertical drop tests were performed at a temperature of minus 40°C. During the oblique drop test the upper impact limiter was heated up to +80°C. The tests were conducted onto an unyielding target, fulfilling the IAEA requirements. The test specimen was considerably instrumented with strain gauges and accelerometers. Transient strains at selected locations of the inner and outer container walls, of the primary and secondary lid, as well as of the corresponding lid bolts were measured during the drop tests. Furthermore, decelerations in different locations at the cask body and the lids were measured. The complex geometrical deformation of the impact limiters due to the impact were determined by optical 3D- measurements. Before and after the drop tests the leakage rate of the lid system was determined by helium leakage testing. The experimental results contribute to the evaluation of the package response to mechanical tests, demonstrating safety under normal and accident conditions of transport and especially to the verification of the dynamic finite-element model of the package used in the package design safety report.
THz and mid IR spectroscopy of high-molecular PE (HMW) and ultra high-molecular PE (UHMW) reveals modifications of the molecular structure. Characteristic absorption bands are changed if the two materials are exposed by γ-Co60 radiation up to 600 kGy and subsequently stored at an annealing temperature of 398 K until for 729 days. UHMW-PE and HMW-PE behave differently during the ageing process because of their molecular weight and inherent structure distinctions. The spectroscopic data offer characteristic absorption bands, which have been used to describe the complete ageing process in more detail. For instance, the integral absorption in the B1u THz-region can be used to describe quantitatively the reduction of crystallinity. The formation of trans vinylene unsaturation and the decay of vinyl during ageing can be observed in detail in the mid IR range.
In this presentation the main requirements of BAM-GGR 016 regarding maintenance and periodic inspections were explained. BAM ensures during acceptance of the quality management program that specific and relevant instructions for maintenance and periodic inspections are developed and handed to the operator of the packaging. Examples are given.
For many sealing applications rubber O-rings are applied due to their special properties and easy use. In many applications as e.g. in aviation, traffic or process technology the material can be exposed to a variety of conditions during operation as e.g. low temperatures, elevated temperatures and different media. Therefore, it is important to know the material behaviour and the seal performance under those conditions. Additionally ageing of seals is an important factor which has an influence on the long term reliability.
In this contribution we would like to discuss different aspects affecting the seal performance, lifetime estimation and address open questions which should be addressed to come to a deeper understanding of these seals commonly understood as typical machine elements.
Results of running investigations at the Bundesanstalt für Materialforschung und -prüfung (BAM), Division 3.4 “Safety of Storage Containers” are presented and discussed.
At BAM, which is a federal institute for materials research and testing in Germany, it is one of our tasks to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes assessment of elastomeric seals applied in the casks. One of the aims is to identify a suitable method for estimating the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. Therefore, we started an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) which are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) for up to five years. In order to assess sealability, O-rings were aged in compression by 25 % (corresponding to the compression during service) between plates as well as in flanges that allow leakage rate measurements. For comparison, uncompressed O-rings were aged as well. In order to understand the underlying ageing mechanisms in each material, material properties such as hardness, density and tensile properties were examined. Additionally, compression set (CS), which represents the recovery behaviour of a seal after release from compression, is measured. For obtaining results closely related to practical conditions, O-rings with a full-scale cord diameter of 10 mm were aged. However, this set-up can lead to heterogeneous ageing caused by diffusion-limited oxidation (DLO) effects especially for HNBR, resulting in distorted bulk properties such as compression set. However, if DLO-affected data is excluded, extrapolations of CS data are possible using time-temperature shifts.
For selecting an appropriate end-of-lifetime criterion, leakage rate measurements were performed, since leakage rate is the only characteristic directly correlated to the performance of the sealing system. A significant increase in leakage rate was considered as the end of the lifetime. However, the O-rings remained leak tight under static conditions even though material properties had already degraded strongly. For this reason, a modified, more demanding leakage test involving a fast small decompression of the seal was developed that allowed determining a more conservative end-of-lifetime criterion with a safety margin for EPDM seals. FKM, which is a very heat and oxidation resistant material, exhibited only little degradation, even though it had the smallest activation energy.
Metal seals of O-ring form are often used in lid-systems of transport and storage casks for radioactive waste in Germany. To investigate their mechanical behaviour, three dimensional (3D) finite element (FE) models were created using solid elements for all of the seal components. The material behaviour of each component is described with a unified static elastic-plastic material model. The total strain is defined as the sum of linear elastic strain and plastic strain with power-law hardening. The model was carefully validated by comparison of Simulation results with experimental results. The influence of material fluctuation of each seal component due to varying properties and the sensitivity of different seal diameters on the seal force are analysed and discussed.
The results show that the material properties of helical spring have major influence on seal force and that the influence of seal diameters is negligible small in the studied range. This is very important to use the test results from seals with small diameter for the assessment of seal behaviour with larger diameter as used in transport and storage cask.
The first German package design approval certificate for a dual purpose cask intended for loading with damaged spent nuclear fuel was issued recently. BAM as part of the competent authority system in Germany carried out a comprehensive assessment procedure with respect to the mechanical and thermal design, the release of radioactive material and the quality assurance aspects of manufacturing and operation. Packages for the transport and storage of radioactive material have been assessed by BAM for many years, thus the common assessment procedure is well-known and good practice. Up to now only SNF without defects or HLW with well-defined properties were designated for long-term Interim storage and transports afterwards. Due to Germany’s nuclear phase out all other kinds of spent nuclear fuel in particular damaged spent nuclear fuel shall be packed as well. Damaged spent nuclear fuel needs a tight closure with Special encapsulations and clearly defined properties in Germany. In addition, these encapsulations shall be long-term durable, because they are not accessible after loading in a packaging within periodical inspections. The main difference to Standard package components is that encapsulations with a permanent closure achieve their specified conditions not after manufacturing but only during operation, after loading and closing. To ensure compliance with the specific conditions, special measures for quality assurance are necessary during operation of each encapsulation, e.g. drying and sealing, which were assessed by BAM. The present paper gives an overview of the conducted assessment from BAM and point out the findings concerning to the special closure lid of the approved encapsulation, which is screwed and welded. A wide verification concept is necessary to show the specific tightness under transport conditions. Together with quality assurance measures during first operation steps these encapsulations with damaged spent nuclear fuel can be handled like standard fuel assemblies in approved package designs.
Fire testing is an essential part of the hypothetical, cumulative mechanical and thermal test conditions that shall guarantee package safety in severe accidents. Within regulatory approval of transport or storage packages for radioactive material, specific thermal load tests are required in accordance to licensing conditions and international standards, respectively. The specifications of these thermal tests are based on test conditions with equivalent heat input to that of a hydrocarbon fuel fire. In the past, light heating oil, diesel or kerosene was mostly used as the fuel to generate the pool fire. In accordance with IAEA regulations for a fire in an accident, the temperature of 800 °C over a period of 30 minutes must be fulfilled. Furthermore, the delivery acceptance criteria for containers in nuclear waste repositories could reach for example average temperatures of 800 °C during a period of one hour in combination with defined requirements on activity release. BAM as a scientific and technical German federal government institute operates an open air Technical Safety Test Site for experimental investigations of dangerous good and its containment. In this areal a large fire test facility is under operation. Liquid Propane is utilized as fuel which is pumped via pipelines from a central storage tank to the fire exposed test facility areas. In the ring burner system, the gas is released from nozzles, and ignited by ignition burners. The paper includes examples of fire test performance with prototypes of a transport package and a storage container, respectively. In preparation of the thermal load, calorimeter tests have been performed using test specimens of appropriate size and behavior. For the fire test scenario is demonstrated that the IAEA thermal test requirements are fulfilled.
The safety demonstrations realized by applicants in the case of approval request for the package designs containing enriched UF6 have to take into account some specific technical issues. Concerning the shipment of enriched UF6, the package designs consist in general of a filled 30B cylinder surrounded by an overpack.
The description of the content, considering the UF6 origin, i.e. natural or reprocessed, shall be clearly justified especially when the UF6 isotopic composition exceeds the limits specified in ASTM standards.
Concerning the containment of the UF6, the applicant shall demonstrate in all conditions of transport the leak-tightness of the valve and plug of the cylinders filled with enriched UF6. In this regard, when mechanical justifications are based on numerical calculations, the absence of contact between these components of the cylinder and the internal surfaces of the overpack after the regulatory drop tests shall be shown to respect the IAEA regulations.
Furthermore, the representativeness of the ballast used to simulate the behaviour of the UF6 loaded within the cylinder shall be justified if drop tests are performed. The representativeness of the ballast should also be justified for numerical calculations.
In addition, the applicant shall demonstrate that the melting temperature of the valve and the plug, including the tinned joint, will not be exceeded during the regulatory fire test.
Finally, specific provisions relative to the use of plugs and the maintenance of cylinders should be included in the safety analysis report.
For transport package design and operation according to the IAEA regulations, the package shall be securely stowed and its retention system shall be capable to withstand load conditions of routine transport. The supporting IAEA Advisory Material SSG-26 provides information how to do that.
Up to now package designers in different countries use other load factors for the design of attachment points than those specified in the IAEA guidance material. In particular the acceleration values vary between different countries and lead to difficulties during the validation of foreign approval certificates. Therefore the IAEA started a discussion process to review the existing guidance text. An international working group was constituted in 2013. Representatives came from different stakeholders, e.g. transport operators, competent authorities and modal organizations. The discussions concluded especially on the transport conditions which has to be considered for stowage design, including on the one hand the relevance of the load factors used for strength and fatigue analysis and on the other hand the criteria which have to be considered for the attachment points.
The proposed acceleration values will be compared to those measured during recent multi-modal testing by Sandia National Laboratories that measured the acceleration levels experienced by a spent fuel flask during heavy-haul truck, sea, and rail transport.
The ISO standard 10276 is dealing with the load attachment systems of packages as well. This standard considers the trunnion design, manufacturing and operational aspects. The regular standard revision phase started in 2017. An expert group discussed new state-of-the-art technology, different analysis approaches for strength and fatigue analysis and proposed revised text for the ISO standard for international discussion. The finite-element analysis approach incl. appropriate acceptance criteria are described and referenced.
The paper describes relevant tie-down aspects, gives background argumentation relevant to analysis approaches, and tries to support harmonized application of the revised IAEA guidance material and the future revised ISO standard.
Since 2005, several European countries, coordinated by the European Association of Competent Authorities (EACA), have been developing a guide on contents and structure of the documentation demonstrating the compliance with the regulations for packages for the transport of radioactive material (package design safety report, PDSR). This guide has been periodically improved, considering feedback from Designers and authorities.
Taking into account the successful application of this guide in Europe, in 2013 the International Atomic Energy Agency (IAEA) decided to establish a similar guide as an IAEA document for promotion of worldwide use. The development of this IAEA guide started from the latest version of the European PDSR guide. In 2016/2017, during a 120-day review period, comments on the draft were received from member states and international organizations. These were incorporated into the draft in a series of meetings in 2017.
In another meeting in December 2018 the draft was updated to be in line with the latest revision of the IAEA Regulations for the Safe Transport of Radioactive Material (SSR-6).
In this process the draft has been improved significantly, regarding structure as well as implementation of a graded approach depending on the package type, and clarified.
This paper points to the major considerations in developing the guide and important improvements over the last version of the European PDSR guide.
Fire testing is an essential part of the hypothetical, cumulative mechanical and thermal test conditions that shall guarantee package safety in severe accidents. Within regulatory approval of transport or storage packages for radioactive material, specific thermal load tests are required in accordance to licensing conditions and international standards, respectively. The specifications of these thermal tests are based on test conditions with equivalent heat input to that of a hydrocarbon fuel fire. In the past, light heating oil, diesel or kerosene was mostly used as the fuel to generate the pool fire. In accordance with IAEA regulations for a fire in an accident, the temperature of 800 °C over a period of 30 minutes must be fulfilled. Furthermore, the delivery acceptance criteria for containers in nuclear waste repositories could reach for example average temperatures of 800 °C during a period of one hour in combination with defined requirements on activity release. BAM as a scientific and technical German federal government institute operates an open air Technical Safety Test Site for experimental investigations of dangerous good and its containment. In this areal a large fire test facility is under operation. Liquid Propane is utilized as fuel which is pumped via pipelines from a central storage tank to the fire exposed test facility areas. In the ring burner system, the gas is released from nozzles, and ignited by ignition burners. The paper includes examples of fire test performance with prototypes of a transport package and a storage container, respectively. In preparation of the thermal load, calorimeter tests have been performed using test specimens of appropriate size and behavior. For the fire test scenario is demonstrated that the IAEA thermal test requirements are fulfilled.
For transport package design and operation according to the IAEA regulations, the package shall be securely stowed and its retention system shall be capable to withstand load conditions of routine transport. The supporting IAEA Advisory Material SSG-26 provides information how to do that.
Up to now package designers in different countries use other load factors for the design of attachment points than those specified in the IAEA guidance material. In particular the acceleration values vary between different countries and lead to difficulties during the validation of foreign approval certificates. Therefore the IAEA started a discussion process to review the existing guidance text. An international working group was constituted in 2013. Representatives came from different stakeholders, e.g. transport operators, competent authorities and modal organizations. The discussions concluded especially on the transport conditions which has to be considered for stowage design, including on the one hand the relevance of the load factors used for strength and fatigue analysis and on the other hand the criteria which have to be considered for the attachment points.
The proposed acceleration values will be compared to those measured during recent multi-modal testing by Sandia National Laboratories that measured the acceleration levels experienced by a spent fuel flask during heavy-haul truck, sea, and rail transport.
The ISO standard 10276 is dealing with the load attachment systems of packages as well. This standard considers the trunnion design, manufacturing and operational aspects. The regular standard revision phase started in 2017. An expert group discussed new state-of-the-art technology, different analysis approaches for strength and fatigue analysis and proposed revised text for the ISO standard for international discussion. The finite-element analysis approach incl. appropriate acceptance criteria are described and referenced.
The paper describes relevant tie-down aspects, gives background argumentation relevant to analysis approaches, and tries to support harmonized application of the revised IAEA guidance material and the future revised ISO standard.
At the Bundesanstalt für Materialforschung und -prüfung (BAM) in Division 3.4 Safety of Storage Containers, one of our tasks is to evaluate the safety of containers designed for disposal of low and intermediate radioactive waste. As such containers might be transported before and stored until disposal, safe enclosure of the radioactive inventory is important for this time span.
Elastomer O-rings are widely used as barrier seals in these containers. Thus, as for many other applications, an understanding of the practical effects of ageing degradation on elastomer seals during long-term exposure is mandatory for predicting the lifetime of such components. According to a long-term test programme on three kinds of rubbers (EPDM and FKM (relevant for application), HNBR (for comparison)), over several years we have studied the degradation and the change of mechanical properties (e.g. hardness, strain at break) at four different ageing temperatures (75 °C, 100 °C, 125 °C and 150 °C) as well as the change of sealing properties. Continuous and intermittent compression stress relaxation (CSR) measurements were performed in order to investigate the respective contribution of crosslinking and chain scission to the observed degradation effects. Thus, the degradation kinetics and mechanisms could be resolved more clearly. For assessing the seal performance, compression set (CS) and leakage rate measurements were conducted. The experimental results showed that the O-rings remained leak-tight under purely static conditions even when CSR, CS and mechanical properties already indicated far advanced degradation. For this reason, a modified leakage test involving a small and rapid partial decompression of the seal was developed that enabled determining an end-of-lifetime criterion for O-rings with a safety margin for thermal shrinkage and vibrations.
In accident scenarios of transport packages or hypothetical crashes of containers in a storage facility or repository, the materials resistance against dynamic failure of the involved components is a deciding factor for package and container integrity during the handling, transport and storage for each type of radioactive material. For example, different dynamic impact tests on containers and components like lid sealing systems and specimens made of ductile cast iron and shock-absorbing materials are carried out by BAM. In order to perform dynamic impact tests with packages and its parts BAM operates two free-fall drop test facilities with maximum capacities of 200 t and 55 t, and a test bench for guided drop tests. This latter drop test machine enables a clearly specified component loading by a precisely positioned test object or drop weight and has been used recently for numerous investigations. The paper gives an overview of the wide range of experimental testing methods carried out within guided Impact and bending tests. Examples of methodological challenges are presented, especially such experimental analysis of dynamic impact conditions. In addition to known applied methods of dynamic, non-contact displacement measurements like high-speed 3-D surface deformation a recently patented 2-D tracking method is presented. By means of in-situ determination of fracture parameters with relevance to the materials stress intensity factor, the method has been successfully applied for a typical specimen geometry. Also shown are the possibility of detecting in-situ He-leakage rates on laterally impact loaded lid sealing systems as well as a method of acceleration sensor-temperature control under test conditions in the low temperature range.
In accident scenarios of transport packages or hypothetical crashes of containers in a storage facility or repository, the materials resistance against dynamic failure of the involved components is a deciding factor for package and container integrity during the handling, transport and storage for each type of radioactive material. For example, different dynamic impact tests on containers and components like lid sealing systems and specimens made of ductile cast iron and shock-absorbing materials are carried out by BAM. In order to perform dynamic impact tests with packages and its parts BAM operates two free-fall drop test facilities with maximum capacities of 200 t and 55 t, and a test bench for guided drop tests. This latter drop test machine enables a clearly specified component loading by a precisely positioned test object or drop weight and has been used recently for numerous investigations. The paper gives an overview of the wide range of experimental testing methods carried out within guided Impact and bending tests. Examples of methodological challenges are presented, especially such experimental analysis of dynamic impact conditions. In addition to known applied methods of dynamic, non-contact displacement measurements like high-speed 3-D surface deformation a recently patented 2-D tracking method is presented. By means of in-situ determination of fracture parameters with relevance to the materials stress intensity factor, the method has been successfully applied for a typical specimen geometry. Also shown are the possibility of detecting in-situ He-leakage rates on laterally impact loaded lid sealing systems as well as a method of acceleration sensor-temperature control under test conditions in the low temperature range.
In accordance with IAEA SSR-6 para 306 a management system shall be established and implemented to ensure compliance with the relevant provisions of the IAEA regulations. BAM has issued an update of the guideline: the BAM-GGR 011. The new revision describes necessary quality assurance measures for design, manufacture, testing, documentation, use, maintenance and inspection of packagings for package designs requiring competent authority approval for the transport of radioactive material.
The measures can be categorised as system-related and design-related. They are independently approved and monitored by the German competent authority BAM and its authorised expert (BAM/T). The qualification of the organisation applying for the design approval certificate is reviewed in the context of the design approval procedure. The quality assurance measures for manufacture consist of three main steps. Pre-assessment of manufacturing documents such as quality plans, specifications etc., Manufacturing inspections according the pre-assessed documents and inspection before commissioning including documentation review. Periodic inspections during operation as well as relevant specifications for use and maintenance ensure that the properties specified in the approval certificate are preserved over the package life time. Special provisions for the return on
experience regarding operational feedback for design, manufacture, use, maintenance and inspection are given. Special focus shall be given here to the rearranged and meanwhile established system of manufacturing inspections. This includes more transparent roles for a) the Producers authorised inspection 11282 representative, b) the independent inspection expert (S), acting on behalf of the manufacturer with acceptance of BAM, and c) BAM or its authorised expert (BAM/T). Additional attention shall be drawn to the management of deviations during manufacturing and provisions for maintenance and periodic inspections.
In accordance with IAEA SSR-6 para 306 a management system shall be established and implemented to ensure compliance with the relevant provisions of the IAEA regulations. BAM has issued an update of the guideline: the BAM-GGR 011. The new revision describes necessary quality assurance measures for design, manufacture, testing, documentation, use, maintenance and inspection of packagings for package designs requiring competent authority approval for the transport of radioactive material.
The measures can be categorised as system-related and design-related. They are independently approved and monitored by the German competent authority BAM and its authorised expert (BAM/T). The qualification of the organisation applying for the design approval certificate is reviewed in the context of the design approval procedure. The quality assurance measures for manufacture consist of three main steps. Pre-assessment of manufacturing documents such as quality plans, specifications etc., Manufacturing inspections according the pre-assessed documents and inspection before commissioning including documentation review. Periodic inspections during operation as well as relevant specifications for use and maintenance ensure that the properties specified in the approval certificate are preserved over the package life time. Special provisions for the return on experience regarding operational feedback for design, manufacture, use, maintenance and inspection are given.
Special focus shall be given here to the rearranged and meanwhile established system of manufacturing inspections. This includes more transparent roles for a) the producers authorised inspection 11282 representative, b) the independent inspection expert (S), acting on behalf of the manufacturer with acceptance of BAM, and c) BAM or its authorised expert (BAM/T). Additional attention shall be drawn to the management of deviations during manufacturing and provisions for maintenance and periodic inspections.
For disposal of the German research reactor of the Technical University Munich FRM II a new transport and storage cask design was under approval assessment by the German authorities. The Bundesanstalt für Materialforschung und -prüfung (BAM) assessed the mechanical and thermal package safety and performed drop tests. The activity release approaches and subjects of quality assurance and surveillance for manufacturing and operation of the package were assessed by BAM as well.
The cask body is made of ductile cast iron and closed by two bolted lid systems with metal seals. The material of the lids is stainless steel. On each end of the cask a wood-filled impact limiter is installed to reduce impact loads to the cask under drop test conditions. In the cavity of the cask a basket for five spent fuel assemblies is arranged.
For the safety case a combination of experimental testing and analytical/numerical calculations were applied. In total, four drop tests were carried out at the BAM large drop test facility. Two tests were carried out as a full IAEA drop test sequence consisting of a 9m drop test onto an unyielding target and a 1m puncture bar drop test. The other two drop test were performed as single 9m drop tests and completed by additional analyses for considering the effects of an IAEA drop test sequence.
The main objectives of the drop tests were the investigation of the integrity of the package and its safety against release of radioactive material as well as the test of the fastening system of the impact limiters. Furthermore, the acceleration and strain signals measured during the tests were used for the verification of Finite-Element-Analysis (FEA) used for the safety analysis of the package design.
The finite-element models incorporated in the package design safety report include the cask body, the lid system, the inventory and the impact limiters with the fastening system. In this context special attention was paid to the modeling of the encapsulated wood-filled impact limiters.
Additional calculations using the verified numerical models were done by the applicant and assessed by BAM to investigate e.g. the brittle fracture of the cask body made of ductile cask iron within the package design approval procedure.
This paper describes the package design assessment from the view of the competent authority BAM including the applied assessment strategy, the conducted drop tests and the additional calculations by using numerical and analytical methods.
The containment systems of transport and storage casks for spent fuel and highlevelradioactive waste usually include bolted lids with metallic or elastomeric seals. The mechanical and thermal loadings associated with the routine, normal and accident conditions of transport can have a significant effect on the leak tightness of such containment system.
Scaled cask models are often used for providing the required mechanical and thermal tests series.Leak tests have been conducted on those models.
It is also common practice to use scaled component tests to investigate the influence of deformations or displacements of the lids and the seals on the standard leakage rate as well as to study the temperature and time depending alteration of the seals.
In this paper questions of the transferability of scaled test results to the full size design of the containment system will be discussed.