Präsentation
Filtern
Erscheinungsjahr
- 2017 (4) (entfernen)
Dokumenttyp
- Vortrag (2)
- Posterpräsentation (2)
Sprache
- Englisch (4)
Referierte Publikation
- nein (4)
Schlagworte
- Core-shell nanoparticles (4) (entfernen)
Eingeladener Vortrag
- nein (2)
The presentation focuses on the current state of the optical spectroscopic studies on plasmon enhanced upconversion luminescent processes of silica-metal core-shell nanocomposites. A general introduction of the upconversion process, the theoretical basis of plasmonic enhancement, the theoretical requirements in regard to NP architecture for plasmon enhanced UC will be outlined. The first proof-of-concept measurements show the difficulty in realization the theoretical measurement parameters in laboratory conditions and underline the need for shifting the experiments to single particle level.“
SrF2 nanoparticles can be doped with trivalent earth metal ions such as Eu3+ and Tb3+ to generate materials exhibiting an intensive red or green fluorescence. A CaF2 shell increases intensity, fluorescence lifetie and quantum yield. The chemical composition of the nanoparticle core-shell region is investigated by XPS at different excitation energies corresponding to different information depths.
Investigation of core-shell nanoparticles using scanning transmission x-ray microscopy (STXM)
(2017)
A scanning transmission x-ray microscopy (STXM) based methodology is introduced for determining the dimensions (shell thickness, core and total diameter) of core-shell nanoparticles which exhibit a strong x-ray absorption contrast and a well-defined interface between core and shell material. A low radiation dosage during data acquisition and, therefore, less x-ray beam induced damage of the sample is achieved by recording STXM images only at two predetermined energies of maximum absorption contrast, instead of recording a stack of images across the whole absorption edge. A model core-shell nanoparticle, polytetrafluoroethylene (PTFE) cores with polystyrene (PS) shell, is used for demonstration. Near edge x-ray absorption fine structure (NEXAFS) spectroscopy confirms the significant difference in x-ray absorption behavior between PTFE and PS. Additionally, due to the insolubility of styrene in PTFE a well-defined interface between particle core and shell is expected. In order to validate the STXM results, both the naked PTFE cores as well as the complete core-shell nanoparticles are examined by scanning electron microscopy (SEM). The introduced STXM based methodology yields particle dimensions in good agreement with the SEM results (deviation equal or less than 10%) and provides additional information such as the position of the particle core which cannot be extracted from a SEM micrograph.
A scanning transmission x-ray microscopy (STXM) based methodology is introduced for determining the dimensions (shell thickness, core and total diameter) of core-shell nanoparticles which exhibit a strong x-ray absorption contrast and a well-defined interface between core and shell material. A low radiation dosage during data acquisition and, therefore, less x-ray beam induced damage of the sample is achieved by recording STXM images only at two predetermined energies of maximum absorption contrast, instead of recording a stack of images across the whole absorption edge. A model core-shell nanoparticle, polytetrafluoroethylene (PTFE) cores with polystyrene (PS) shell, is used for demonstration. Near edge x-ray absorption fine structure (NEXAFS) spectroscopy confirms the significant difference in x-ray absorption behavior between PTFE and PS. Additionally, due to the insolubility of styrene in PTFE a well-defined interface between particle core and shell is expected. In order to validate the STXM results, both the naked PTFE cores as well as the complete core-shell nanoparticles are examined by scanning electron microscopy (SEM). The introduced STXM based methodology yields particle dimensions in good agreement with the SEM results (deviation equal or less than 10%) and provides additional information such as the position of the particle core which cannot be extracted from a SEM micrograph.