Präsentation
Filtern
Dokumenttyp
- Vortrag (424)
- Posterpräsentation (88)
- Beitrag zu einem Tagungsband (9)
Sprache
- Englisch (344)
- Deutsch (176)
- Mehrsprachig (1)
Schlagworte
- Hydrogen (28)
- Safety (26)
- Ageing (21)
- Gefahrgut (21)
- Gefahrguttransport (21)
- Gefahrgutverpackungen (18)
- Transport (18)
- Wasserstoff (18)
- Drop test (16)
- Dangerous Goods Database (14)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (521) (entfernen)
Cryogenic liquefied gases, such as liquid hydrogen (LH2) and liquefied natural gas (LNG), are becoming more popular as eco-friendly energy sources. However, using these gases more often increases the risk of accidents, making it important to conduct thorough risk assessments. The storage systems for these gases rely on thermal superinsulation (TSI), which can fail under extreme heat, especially during fires. Therefore, it is essential to study how and why TSI fails. This research (part of PhD topic) aims to examine insulation performance, thereby improving the overall safety of cryogenic storage systems.
To reduce carbon dioxide emissions, energy carries such as hydrogen consider to be a solution. Consumption of hydrogen as a fuel meets several restrictions such as its low volumetric energy density in gas phase. To tackle this problem, storage as well as transportation in liquid phase is recommended. To be able to handle this component in liquid phase, an efficient thermal insulation e.g., MLI insulation is required. Some studies have been revealed vulnerability of this type of insulation against high heat flux, for instance a fire accident. Some investigations have been depicted the importance of consideration of the MLI thermal degradation in terms of its reflective layer. However, limited number of studies have been focused on the thermal degradation of spacer material and its effect on the overall heat flux.
In this study, through systematic experimental measurements, the effect of thermal loads on glass fleece, glass paper as well as polyester spacers are investigated. The results are reported in various temperature and heat flux profiles. Interpreting the temperature profiles revealed as the number of spacers in the medium increases, the peak temperature detectable by the temperature sensor on the measurement plate decreases. Moreover, the contribution of each individual spacer in all cases regarding the experimental temperature range is assessed to be around 8%. This value may increase to around 50% for glass paper and polyester spacers, and to around 25% for glass fleece spacers as the number of spacer layers increases up to six layers.
To utilize the outcomes of the experiment later and integrate the results into numerical and CFD simulations, a model is proposed for the mentioned experimental temperature range up to 300°C to predict a heat flux attenuation factor. The model proposes a fitting factor that can reproduce the least square fitted line to the experimental data.
In the course of decarbonizing the energy industry, cryogenic energy carriers as liquefied hydrogen (LH2) and liquefied natural gas (LNG) are seen as having great potential. In technical applications, the challenge is to keep these energy carriers cold for a long time. This is achieved in the road transport sector and also stationary applications by thermal super insulations (TSI) which based on double-walled tanks with vacuum and multilayer insulation (MLI) in the interspace. This study focuses on the behaviour of widely used combustible MLI in a fire scenario, at vacuum and atmospheric pressure conditions. The former corresponds to the typical design condition and the latter to the condition after an outer hull rapture of a tank. Furthermore, two fire scenarios were taken into account: a standard-oriented approach and a hydrocarbon fire-oriented approach. For the study, a test rig was applied that allows testing of TSI at industrial conditions and subsequent analysis of TSI samples. The test rig allows thermal loading and performance analysis of TSI samples at the same time. Comparing the tests, the samples degraded differently. However, no sudden failure of the entire MLI was observed in any test. These results are relevant for the evaluation of incidents with tanks for the storage of cryogenic fluids and can thus contribute to the improvement of TSI and the development of emergency measures for the protection of persons and infrastructures.
A damaging action of HNO3-55% only occurs in combination with its decomposition into nitrous gases, which can be caused by UV radiation. In a laboratory test, transparent HDPE jerrycans have been exposed to both UV radiation and 55 wt-% nitric acid solution at (41 ± 2)°C, for up to 20 days. For comparison, UV radiant exposure (21 days) and nitric acid exposure (up to 6 weeks) were performed separately, at nearly equal temperatures. The respective damages are compared with FTIR spectroscopy in ATR and HT-gel permeation chromatography (GPC) on a molecular level and with hydraulic internal pressure testing as a component test. For the used jerrycans, relevant oxidation can only be found after the combined exposure. The gradual increase in oxidative damage shows the good reproducibility of the lab exposure. The decomposition of nitric acid into nitrous gases by UV radiation – as well as the jerrycan oxidation – is also observed at lower HNO3 concentration (28 wt- %). Similar results are obtained after outdoor tests. Again, the damage occurs only after combined exposure, in contrast to the exposures to UV only and to HNO3 only, which were conducted in parallel. Outdoor exposures are most readily accepted as they represent possible end-use conditions. However, the reproducibility of these exposures is poor due to the large temporal variations in weather. There are also several safety risks, which is why the number of replicates remains limited. Since the outdoor and lab exposure tests show the same qualitative results, it is appropriate to conduct systematic studies in the laboratory. After 6 days of lab exposure, the oxidation damage is rated as critical, which corresponds to about 1/10 year in Central Europe, according to the UV radiant exposure. It should be noted that this amount can also occur in two sunny weeks.
Non-Destructive Testing (NDT) of type 4 composite pressure vessels can be seen as key to better understanding the behaviour of the composite structure and the impact of the manufacturing process on its quality. In this presentation, NDT methods used in the “Trustworthy Hydrogen” project are introduced. A brief discussion of the observed phenomena is provided.
Hydrogen Fire Testing
(2024)
In this presentation we present a new hydrogen-based test rig for an ongoing feasibility study of using hydrogen as an energy source for the thermal testing of transport packages containing radioactive materials. The test rig will be capable of combusting hydrogen for a wide range of different burner geometries, mass flows and if necessary hydrogen blends. As this type of fire test according to the IAEA boundary conditions does not yet exist, a large number of preliminary investigations, safety assessments and calculations must be carried out in order to develop a viable concept for hydrogen fires. In the first step of the feasibility study, the temperature, structure, and radiation of various hydrogen flames are surveyed. In future works, the results will make it possible to design burner frames that are suitable for fire reference tests in order to make comparisons with pool and propane fires used in assessment procedures today. In parallel comparative numerical simulations are conducted to model the thermal behaviour of hydrogen flames using the software package Ansys®. On the one hand, the numerical simulations support the experiments by providing an overview of numerous parameters and the measuring range; on the other hand, they will help with the design of the burner frame in future work. This paper gives an overview in the design and capabilities of the test rig. Furthermore, the results of the parameter studies show that burner geometry and mass flow provide a significant design margin for the thermal shape of the hydrogen flames. In addition, the results of the initial numerical calculations will be used to determine the necessary sensors, the positions, and their operating range. Only the optimal interaction allows a controlled system that permits user-defined hydrogen fires.
Introduction and Necessity of the Investigation
The IAEA regulations for the safe transport of radioactive material (IAEA SSR-6) define the safety requirements for different package types and consider different transport conditions. The accident conditions of transport specify different mechanical and thermal tests based on investigations of real accident scenarios.
Considering the rapid development of new boundary conditions of transport such as electric mobility and the use of hydrogen as energy source for trucks and other kind of vehicles, potential effects of battery and hydrogen fires in transport accidents should be investigated. The aim is to evaluate the existing test requirements developed and derived decades ago, whether they are covering the current transport situation.
This concept paper will briefly present the reasons for detailed investigations as bases for a coordinated research project under the roof of the IAEA.
Brittle Failure Limits of Spent Fuel Claddings Subjected to Long-Term Dry Interim Storage Conditions
(2024)
The mechanical properties of spent fuel claddings can be adversely affected under the conditions of long-term dry interim storage, so that the failure limits may be reached in case of mechanical loads during handling or transport after storage. Pre-storage drying and the early stage of interim storage can expose the cladding to higher temperatures and higher tensile hoop stresses than those associated with in-reactor operation and pool storage. During slow cooling of a cladding tube under internal pressure, radial hydrides may precipitate in zirconium-based cladding alloys. This can lead to embrittlement of the material and sudden failure of the cladding integrity under mechanical stress. In order to prevent brittle failure, numerical methods are being developed to predict the mechanical behaviour and identify limiting conditions. Experimental investigations, numerical analyses and evaluation methods are discussed.
An established experimental method for characterising cladding materials is the Ring Compression Test (RCT). Some test results on irradiated cladding tubes after operation in pressure water reactors are publicly available. However, it is helpful to carry out studies on unirradiated surrogate claddings with similar material properties to reduce the effort associated with irradiated samples in hot cells and to perform material tests with a wider range of parameters. On the basis of such experimental data, load-displacement curves have been numerically analysed for a selection of cladding materials.
Radial hydrides can cause a sample to break suddenly due to fracture even at low deformation. Noticeable load drops in the RCT are caused by unstable crack propagation through the radial hydride network. The failure mechanism is quasi-cleavage in the hydrides and micro-void nucleation, growth, and coalescence in the zirconium matrix, with ductile tearing patches connecting adjacent hydrides. The cohesive zone approach was used to simulate the failure process taking into account the radial hydride morphology.
The developed method can adequately describe both the deformation and failure behaviour of irradiated as well as unirradiated claddings of zirconium-based alloys with radial hydrides under RCT conditions. Limiting conditions can be expressed in terms of fracture energy and cohesive strength.
Distributed fiber optic strain sensing for structural health monitoring of 70 MPa hydrogen vessels
(2024)
We report on the development and testing of 70 MPa hydrogen pressure
vessels with integrated fiber optic sensing fibers for automotive use. The paper deals with the condition monitoring of such composite pressure vessels (CPVs) using the optical backscatter reflectometry (OBR) applied for a distributed fiber optic strain sensing along fully integrated polyimide-coated single-mode glass optical fiber (SM-GOF). The sensing fibers were embedded into the vessel structure by wrapping them over the polymer liner during the manufacturing process of the carbon fiber reinforced polymer (CFRP). Detecting local strain events by the integrated fiber optic sensors can be an opportunity for monitoring the material degradation of CPVs under static and cyclic loading.
Hydrogen pressure vessels are among the most essential components for reliable hydrogen technology. Under current regulations, a mostly conservative strategy is employed, restricting the usage time of hydrogen pressure vessels without providing information on the real remaining lifetime. During the service life, pressure vessels are inspected periodically. However, no established method that can provide continuous monitoring or information on the remaining safe service life of the vessel. In this paper, we propose a sensor network for Structural Health Monitoring (SHM) of hydrogen pressure vessels where data from all sensors are collected and centrally evaluated. Specifically, we integrate three different SHM sensing technologies namely Guided Wave ultrasonics (GW), Acoustic Emission testing (AT), and distributed Fiber Optic Sensing (FOS). This integrated approach offers significantly more information and could therefore enable a transition from costly and time-consuming periodic inspections to more efficient and modern predictive maintenance strategies, including Artificial Intelligence (AI)-based evaluation. This does not only have a positive effect on the operational costs but enhances safety through early identification of critical conditions in the overall system in real-time. We demonstrate an experimental set-up of a lifetime test where a Type IV Composite Overwrapped Pressure Vessel (COPV) is investigated under cyclic loading instrumented with AT, FOS, and GW methods. We acquired data from the sensor network until the pressure vessel failed due to material degradation. The data collected using the three different SHM sensor technologies is planned to be evaluated individually, using data fusion, and AI. In the future, we aim to integrate the measurement setup into a hydrogen refueling station with the data stream implemented into a digital signal processing chain and a digital twin.