The purpose of this paper is to investigate the relationship between hydride morphology, in particular the presence of radial hydrides (RHs), stress state and failure mechanisms associated with the ring compression test (RCT). Samples of ZIRLO®cladding were pre-hydrided and subjected to thermo-mechanical treatments to precipitate long radial hydrides. The results show that the reorientation treatment was very successful. A considerable fraction of RHs was generated, the radial hydride continuity factor being around 80 to 90% of the wall thickness. The samples with reoriented hydrides were tested using the RCT at room temperature. Macroscopic brittle failure was observed with sudden load drops for displacements around 0.5 mm, with a calculated “offset strain”between 0.5 and 1%. Crack nucleation occurs in RHs located in regions with the highest values of hoop stress. These locations are the inner diameter of cladding at the vertical plane of the sample (12 and 6 o’clock positions) and the outer diameter at the horizontal plane (3 and 9 o’clock positions). Noticeable load drops in the RCT are associated with unstable crack propagation events through the radial hydride network, the crack front reaching up to 90% of the wall thickness in some cases. The failure micro-mechanism is quasi-cleavage in the hydrides and micro-void nucleation, growth and coalescence in the Zr matrix, with ductile tearing patches connecting neighboring hydrides. The main conclusion is that radial hydride metrics is not the only parameter that determines cladding failure in the presence of RHs, but the interaction between the location and continuity of RHs and the stress normal to the hydride (the hoop stress in this case). Consequently, if a radial hydride is located at a position within the cladding where the hoop stress is small, a crack will not be initiated easily in the RCT.
Metal seals of O-ring form are often used in lid-systems of transport and storage casks for radioactive waste in Germany. To investigate their mechanical behaviour, three dimensional (3D) finite element (FE) models were created using solid elements for all of the seal components. The material behaviour of each component is described with a unified static elastic-plastic material model. The total strain is defined as the sum of linear elastic strain and plastic strain with power-law hardening. The model was carefully validated by comparison of Simulation results with experimental results. The influence of material fluctuation of each seal component due to varying properties and the sensitivity of different seal diameters on the seal force are analysed and discussed.
The results show that the material properties of helical spring have major influence on seal force and that the influence of seal diameters is negligible small in the studied range. This is very important to use the test results from seals with small diameter for the assessment of seal behaviour with larger diameter as used in transport and storage cask.
Transport casks for radioactive materials have to withstand the 9 m drop test, 1 m puncture drop test and dynamic crush test with regard to the mechanical requirements according to the IAEA regulations. The safety assessment of the package can be carried out on the basis of experimental investigations with prototypes or models of appropriate scale, calculations, by reference to previous satisfactory safety demonstrations of a sufficiently similar nature or a combination of these methods. Computational methods are increasingly used for the assessment of mechanical test scenarios. However, it must be guaranteed that the calculation methods provide reliable results. Important quality assurance measures at the Federal Institute for Materials Research and Testing are given concerning the preparation, run and evaluation of a numerical analysis with reference to the appropriate guidelines. Hence, a successful application of the finite element (FE) method requires a suitable mesh. An analysis of the 1 m puncture drop test using successively refined FE meshes was performed to find an acceptable mesh size and to study the mesh convergence using explicit dynamic FE codes. The FE model of the cask structure and the puncture bar is described. At the beginning a coarse mesh was created. Then this mesh was refined in two steps. In each step the size of the elements was bisected. The deformation of the mesh and the stresses were evaluated dependent on the mesh size. Finally, the results were extrapolated to an infinite fine mesh or the continuous body, respectively. The uncertainty of the numerical solution due to the discretisation of the continuous problem is given. A safety factor is discussed to account for the uncertainty.
Proper predictions of the behaviour of shock absorber materials are of utmost importance in safety assessments for licensing casks for transport and storage of highly active waste. After having identified significant discrepancies between numerical results and the actual response of polyurethane foam limiters subjected to accidental scenarios, a new research project ENREA was established by BAM. A major objective is to enhance and to develop advanced material models intended to simulate limiters under impact loading. They should account for all major factors influencing the load–deformation relationship like temperature, strain rate and specific stress state. The corresponding test program, applicable plasticity models, the overall parameter identification strategy based on local and global optimization techniques as well as experimental and numerical results are presented here in particular for closed cell foams.