Chemische Charakterisierung und Spurenanalytik
Filtern
Dokumenttyp
- Zeitschriftenartikel (31)
Sprache
- Englisch (31)
Referierte Publikation
- ja (31) (entfernen)
Schlagworte
- ICP-MS (11)
- Laser ablation (10)
- Nanoparticle (8)
- Cell (7)
- Imaging (4)
- LA-ICP-MS (3)
- Bioconjugation (2)
- HR-CS-MAS (2)
- Mass spectrometry (2)
- Nanomaterials (2)
Organisationseinheit der BAM
The mechanism of action of zirconium permanent modifiers on graphite surfaces was investigated in order to understand its influence on the analytical signal in atomic and molecular absorption spectrometry (AAS/MAS). For this, the molecule formation of CaF was studied, which is used for the indirect analytical determination of fluorine in high-resolution continuum source graphite furnace molecular absorption spectrometry (HR-CS-GFMAS). The kinetics of this reaction was established by monitoring its molecular spectrum at different atomisation temperatures. An Arrhenius plot showed a pseudo-first order reaction with respect to fluorine (n = 1). An intermediate state was isolated, and its structure was elucidated by spectroscopic methods: scanning electron microscopy with energy dispersive X-ray spectroscopy (SEMEDX), X-ray photoelectron spectroscopy (XPS), X-ray absorption spectroscopy (XANES and EXAFS), and Raman microspectroscopy. We propose here a mechanism, where ZrO2 acts as a heterogeneous catalyst: after a pyrolytic step, an intermediate state of ZrO(OCaF) is activated, and at higher temperatures, CaF(g) is released from the zirconium-coated graphite surface. No evidence of the formation of zirconium carbide was found. Consequently, as the CaF formation is catalysed by a heterogeneous catalyst, surface modifications with ZrO2 nanoparticles and ZrO xerogels were investigated in order to increase the surface area. Their influence was evaluated in the molecule formation of CaF, CaCl, CaBr, and CaI. Graphite furnace modification with zirconium oxide nanoparticles proves to be the best choice for fluorine analysis with a signal enhancement of more than eleven times with respect a non-coated graphite furnace. However, the influence of zirconium modifications in the analytical signals of Cl, and I is lower than the F signals or even negative in case of the Br. Understanding zirconium modifiers as heterogeneous catalysts offers a new perspective to AAS and MAS, and reveals the potential of surface analytical methods for development of improved permanent modifiers and graphite furnace coatings.
A fast and simple method for sulfur quantification in crude oils was developed by using high-resolution continuum source graphite furnace molecular absorption spectrometry (HR-CS-GFMAS). For this, heavy crude oil samples were prepared as microemulsion (shake) and injected into a graphite furnace (shut). Finally, the concentration of sulfur was determined by monitoring in situ the transient molecular spectrum of GeS at wavelength 295.205nm after adding a germanium solution as molecular forming agent (and go). Zirconium dioxide in the form of nanoparticles (45–55nm) was employed as a permanent modifier of the graphite furnace. Calibration was done with an aqueous solution standard of ammonium sulfate, and a characteristic mass (m0) of 7.5ng was achieved. The effectiveness of the proposed method was evaluated analizing, ten heavy crude oil samples with Sulfur amounts ranging between 0.3 and 4.5% as well as two NIST standard reference materials, 1620c and 1622e. Results were compared with those obtained by routine ICP-OES analysis, and no statistical relevant differences were found.
We have efficiently produced collagen-rich microstructures in fibroblast multicellular spheroids (MCSs) as a three-dimensional in vitro tissue analog to investigate silver (Ag) nanoparticle (NP) penetration. The MCS production was examined by changing the seeding cell number (500 to 40,000 cells) and the growth period (1 to 10 days). MCSs were incubated with Ag NP suspensions with a concentration of 5 μg/mL for 24 h. For this study, laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) was used to visualize Ag NP localization quantitatively. Thin sections of MCSs were analyzed by LA-ICP-MS with a laser spot size of 8 μm to image distributions of 109Ag, 31P, 63Cu, 66Zn, and 79Br. A calibration using a NP suspension was applied to convert the measured Ag intensity into the number of NPs present. The determined numbers of NPs ranged from 30 to 7200 particles in an outer rim of MCS. The particle distribution was clearly correlated with the presence of 31P and 66Zn and was localized in the outer rim of proliferating cells with a width that was equal to about twice the diameter of single cells. Moreover, abundant collagens were found in the outer rim of MCSs. For only the highest seeding cell number, NPs were completely captured at the outer rim, in a natural barrier reducing particle transport, whereas Eosin (79Br) used as a probe of small molecules penetrated into the core of MCSs already after 1 min of exposure.
We applied high resolution laser ablation inductively coupled plasma time-of-flight mass spectrometry (LA-ICP-TOF-MS) with cellular spatial resolution for bioimaging of nanoparticles uptaken by fibroblast multicellular spheroids (MCS). This was used to quantitatively investigate interactions of silver nanoparticles (Ag NPs) and the distributions of intrinsic minerals and biologically relevant elements within thin sections of a fibroblast MCS as a three-dimensional in vitro tissue model. We designed matrix-matched calibration standards for this purpose and printed them using a noncontact piezo-driven array spotter with a Ag NP suspension and multielement standards. The limits of detection for Ag, Mg, P, K, Mn, Fe, Co, Cu, and Zn were at the femtogram (fg) level, which is sufficient to investigate intrinsic minerals in thin MCS sections (20 μm thick). After incubation for 48 h, Ag NPs were enriched in the outer rim of the MCS but not detected in the core. The localization of Ag NPs was inhomogeneous in the outer rim, and they were colocalized with a single-cell-like structure visualized by Fe distribution (pixel size of elemental images: 5 × 0.5 μm). The quantitative value for the total mass of Ag NPs in a thin section by the present method agreed with that obtained by ICP-sector field (SF)-MS with a liquid mode after acid digestion.
We investigated the penetration of silver nanoparticles (Ag NPs) into a three-dimensional in vitro tissue analog using NPs with various sizes and surface coatings, and with different incubation times. A high-Resolution laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) time-of-flight (TOF) instrument was applied for imaging the distributions of elements in thin sample sections (20 μm thick). A fibroblast multicellular spheroid (MCS) was selected as the model system and cultured for more than 8 days to produce a natural barrier formed by the extracellular matrix containing collagen. The MCS was then exposed for up to 48 h to one of four types of Ag NPs (∅ 5 nm citrate coated, ∅ 20 nm citrate coated, ∅ 20 nm polyvinylpyrrolidone coated, and ∅ 50 nm citrate coated). Imaging showed that the penetration pathway was strongly related to steric networks formed by collagen fibrils, and Ag NPs with a hydrodynamic diameter of more than 41 nm were completely trapped in an outer rim of the MCSs even after incubation for 48 h. In addition, we examined the impact of these NPs on essential elements (P, Fe, Cu, and Zn) in
areas of Ag NP accumulation. We observed a linear increase at the sub-femtogram level in the total concentration of Cu (fg per pixel) in samples treated with small or large Ag NPs (∅ 5 nm or ∅ 50 nm) for 48 h.
Metal tags find application in a multitude of biomedical systems and the combination with laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) offers an opportunity for multiplexing. To lay the foundation for an increase of the signal intensities in such processes, we herein present a general approach for efficient functionalization of a well-defined metal oxido cluster [Bi6O4(OH)(4)(SO3CF3)(6)(CH3CN)(6)].2 CH3CN (1), which can be realized by selecting 7mer peptide sequences via combinatorial means from large one-bead one-compound peptide libraries. Selective cluster-binding peptide sequences (CBS) for 1 were discriminated from non-binders by treatment with H2S gas to form the reduction product Bi2S3, clearly visible to the naked eye. Interactions were further confirmed by NMR experiments. Extension of a binding peptide with a maleimide linker (Mal) introduces the possibility to covalently attach thiol-bearing moieties such as biological probes and for their analysis the presence of the cluster instead of mononuclear entities should lead to an increase of signal intensities in LA-ICP-MS measurements. To prove this, CBS-Mal was covalently bound onto thiol-presenting glass substrates, which then captured 1 effectively, so that LA-ICP-MS measurements demonstrated drastic signal amplification compared to single lanthanide tags.
Online immunocapture ICP‑MS for the determination of the metalloprotein ceruloplasmin in human serum
(2018)
The human copper-protein ceruloplasmin (Cp) is the major copper-containing protein in the human body. The accurate determination of Cp is mandatory for the reliable diagnosis of several diseases. However, the analysis of Cp has proven to be difficult. The aim of our work was a proof of concept for the determination of a metalloprotein-based on online immunocapture ICP-MS. The immuno-affinity step is responsible for the enrichment and isolation of the analyte from serum, whereas the compound-independent quantitation with ICP-MS delivers the sensitivity,
precision, and large dynamic range. Off-line ELISA (enzyme-linked immunosorbent assay) was used in parallel to confirm the elution profile of the analyte with a structure-selective method. The total protein elution was observed with the 32S mass trace. The ICP-MS signals were normalized on a 59Co signal. The human copper-protein Cp could be selectively determined. This was shown with pure Cp and with a sample of human serum. The good correlation with off-line ELISA shows that Cp could be captured and eluted selectively from the anti-Cp affinity column and subsequently determined by the copper signal of ICP-MS.
An immunohistochemical method is described to visualize the distribution of metallothioneins 1/2 (MT 1/2) and metallothionein 3 (MT 3) in human ocular tissue. It is making use of (a) antibodies conjugated to gold nanoclusters (AuNCs) acting as labels, and (b) laser ablation (LA) coupled to inductively coupled plasma – mass spectrometry (ICP-MS).Water-soluble fluorescent AuNCs (with an average size of 2.7 nm) were synthesized and then conjugated to antibody by carbodiimide coupling. The surface of the modified AuNCs was then blocked with hydroxylamine to avoid nonspecific interactions with biological tissue. Immunoassays for MT 1/2 and MT 3 in ocular tissue sections (5 μm thick) from two post mortem human donors were performed. Imaging studies were then performed by fluorescence using confocal microscopy, and LA-ICP-MS was performed in the retina to measure the signal for gold. Signal amplification by the >500 gold atoms in each nanocluster allowed the antigens (MT 1/2 and MT 3) to be imaged by LA-ICP-MS using a laser spot size as small as 4 μm. The image patterns found in retina are in good agreement with those obtained by conventional fluorescence immunohistochemistry which was used as an established reference method.
Recent recommendations by the Food and Drug Administration1 and the European Medicines Agency2 are to limit the clinical use of linear gadolinium-based contrast agents (GBCAs) due to convincing evidence of deposition in tissues. Macrocyclic GBCA continued to be considered safe, provided that patients have normal renal function. To date, given the low sensitivity of conventional MRI, there has been a debate about the signal increase following the injections of a macrocyclic GBCA.
Well-absorbed iron-based nanoparticulated materials are a promise for the oral management of iron deficient anemia. In this work, a battery of in vitro and in situ experiments are combined for the evaluation of the uptake, distribution and toxicity of new synthesized ultrasmall (4 nm core) Fe2O3 nanoparticles coated with tartaric/adipic acid with potential to be used as oral Fe supplements. First, the in vitro simulated gastric acid solubility studies by TEM and HPLC-ICP-MS reveal a partial reduction of the core size of about 40% after 90 min at pH3. Such scenario confirms the arrival of the nanoparticulate material in the small intestine. In the next step, the in vivo absorption through the small intestine by intestinal perfusion experiments is conducted using the sought nanoparticles in Wistar rats. The quantification of Fe in the NPs Suspension before and after perfusion shows Fe absorption levels above 79%, never reported for other Fe treatments. Such high absorption levels do not seem to compromise cell viability, evaluated in enterocytes-like models (Caco-2 and HT-29) using cytotoxicity, ROS production, genotoxicity and lipid peroxidation tests. Moreover, regional differences in terms of Fe concentration are obtained among different parts of the small intestine as duodenum>jejunum>ileum. Complementary transmission electron microscopy (TEM) images show the presence of the intact particles around the intestinal microvilli without significant tissue damage. These studies show the high potential of these NP preparations for their use as oral management of anemia.