Chemie und Prozesstechnik
Filtern
Dokumenttyp
- Zeitschriftenartikel (11)
- Vortrag (8)
- Beitrag zu einem Tagungsband (4)
- Posterpräsentation (1)
Schlagworte
- Additive Fertigung (8)
- Künstliche Bewitterung (6)
- Additive manufacturing (5)
- Kunststoffe (5)
- Thermografie (5)
- Zerstörungsfreie Prüfung (5)
- Polymer of intrinsic microporosity (3)
- Active thermography (2)
- Artificial weathering (2)
- Boson peak (2)
Organisationseinheit der BAM
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (24) (entfernen)
Eingeladener Vortrag
- nein (8)
We report dielectric and calorimetric studies on metathesis and addition-type polytricyclononenes, both based on the same monomer bearing three pendant OSiMe3 groups. For the addition-type polymer, dielectric spectroscopy reveals a β*-process related to the microporosity, whereas for its metathesis counterpart, the segmental dynamics manifests as an α-process related to a glass transition. Besides active dielectric processes, a significant conductivity contribution is detected for both samples which for the microporous additiontype polymer is three orders of magnitude greater than for the metathesis polymer. The broadband dielectric spectroscopy is complemented by detailed calorimetric investigations, comprising DSC, FSC, and TMDSC. The calorimetric methods detected the glass transition for the metathesis polymer in agreement with the observed dielectric α-process. Furthermore, the already reported gas transport properties for both polymers are compared, setting them in correlation with the observed molecular mobility and conductivity behavior. The discussed results reflect significant differences in molecular mobility of the two polymers affecting the appearance of microporosity which strongly determines the gas transport properties.
The microscopic diffusion and the low frequency density of states (VDOS) of PIM-EATB(CH3) are investigated by inelastic and quasi-elastic neutron scattering where also the demethylated counterpart of PIM-EA-TB(H2) is considered. These intrinsic microporous polymers are characterized by large BET surface area values of several hundred m2/g and pore sizes between 0.5 and 2 nm. Detailed comparison is made to the archetype of polymers of intrinsic microporosity, PIM-1, and polynorbornenes also bearing a microporosity. Due to the wavelength of neutrons, the diffusion and vibrations can be addressed on microscopic length and time scales. From the inelastic neutron scattering experiments the low frequency density of states (VDOS) is estimated which shows excess contributions to the Debye-type VDOS known as Boson peak. It was found that the maximum frequency of the Boson peak decreases with increasing microporosity characterized by the BET surface area. However, besides the BET surface area, additional factors such as the backbone stiffness govern the maximum frequency of the Boson peak. Further the mean squared displacement related to microscopic motions was estimated from elastic fixed window scans. At temperatures above 175 K, the mean squared displacement PIM-EA-TB(CH3) is higher than that for the demethylated counterpart PIM-EA-TB(H2). The additional contribution found for PIM-EATB(CH3) is ascribed to the rotation of the methyl group in this polymer because the only difference between the two structures is that PIM-EA-TB(CH3) has methyl groups where PIM-EA-TB(H2) has none. A detailed comparison of the molecular dynamics is also made to that of PIM-1 and the microporous polynorbornene PTCNSi1. The manuscript focuses on the importance of vibrations and the localized molecular mobility characterized by the microscopic diffusion on the gas Transport in polymeric separation membranes. In the frame of the random gate model localized fluctuations can open or close bottlenecks between pores to enable the diffusion of gas molecules.
The molecular dynamics of addition-type poly(tricyclononenes) with Si-substituted bulky side groups has been investigated by a combination of neutron time-of-flight and neutron backscattering spectroscopy methods on a time scale from 0.1 ps to ca. 3 ns. The investigated poly(tricyclononenes) PTCNSi1 and PTCNSi2g both bear a high microporosity which makes them promising candidates for active separation layers for gas separation membranes. At least for larger gas molecules it is assumed that the pathways for diffusion require an enlargement of pre-existing micropores in terms of an activated zone. A low temperature relaxation process was found for both polymers by the performed neutron scattering experiments. This process was assigned to the methyl group rotation. It was analysed in terms of a jump diffusion in a three-fold potential. The analysis of the dependence of the elastic incoherent structure factor on the scattering vector yields the number of methyl groups which might be immobilized. For PTCNSi1 (3 methyl groups in the monomeric unit) it was found that all methyl groups take part in the methyl group rotation whereas for PTCNSi2g (6 methyl groups in monomeric unit) a considerable number of methyl groups are blocked in their rotation. This immobilization of methyl groups is due to the sterically demanding arrangement of the methyl groups in PTCNSi2g. This conclusion is further supported by the result that the activation energy for the methyl group rotation is three times higher for PTCNSi2g than that of PTCNSi1.
Microplastic particles are currently detected in almost all environmental compartments. The results of detection vary widely, as a multitude of very different methods are used with very different requirements for analytical validity.
In this work four thermoanalytical methods are compared and their advantages and limitations are discussed. One of them is thermal extraction-desorption gas chromatography mass spectrometry (TED-GC/MS), an analysis method for microplastic detection that has become established in recent years. In addition, thermogravimetric analysis coupled with Fourier-transform infrared spectroscopy (TGA-FTIR) and mass spectrometry (TGA-MS) were applied, two methods that are less common in this field but are still used in other research areas. Finally, microscale combustion calorimeter (MCC) was applied, a method not yet used for microplastic detection.
The presented results are taken from a recently published interlaboratory comparison test by Becker et al. (2020). Here a reference material consisting of suspended matter and specified added polymer masses was examined, and only the results of the recoveries were presented. In the present paper, however, the results for the individual polymers are discussed in detail and individual perspectives for all instruments are shown.
It was found that TED-GC/MS is the most suitable method for samples with unknown matrix and unknown, variable kinds and contents of microplastic. TGA-FTIR is a robust method for samples with known matrix and with defined kinds of microplastic. TGA-MS may offer a solution for the detection of PVC particles in the future. MCC can be used as a very fast and simple screening method for the identification of a potential microplastic load of standard polymers in unknown samples.
For the first time, dielectric and calorimetric investigations of an homologous series of Janus polynorbornenes with rigid main backbones and flexible -Si(OR)3 side groups, of differing length alkyl chains (R = Propyl, Butyl, Hexyl, Octyl, Decyl) is reported. Generally, this class of polymers has some potential for applications in the field of gas separation membranes. Two dielectrically active processes are observed at low temperatures, denoted as β- and α- relaxation. The former can be assigned to localized fluctuations, whilst the latter is related to the glassy dynamics of the flexible -Si(OR)3 side groups, creating a nanophase separation in both the alkyl chain rich and backbone rich domains. This is confirmed through temperature modulated DSC measurements and X-ray scattering experiments. The glass transition temperatures of the backbone rich domains, which are beyond or near to their degradation temperatures in terms of conventional DSC, are determined for the first time using Fast Scanning Calorimetry employing both fast heating and cooling rates. This is complimented with scattering experiments that show how the size of the alkyl chain rich domains increases with chain length. Alongside these results, a significant conductivity contribution was observed for all poly(tricyclononenes) with -Si(OR)3 side groups, which is interpreted in terms of a percolation model.
Inelastic incoherent neutron time-of flight scattering was employed to measure the low frequency density of states for a series of addition polynorbornenes with bulky side groups. The rigid main chain in combination with the bulky side groups give rise to a microporosity of these polymers in the solid state. The microporosity characterized by the BET surfaces area varies systematically in the considered series. Such materials have some possible application as active separation layer in gas separation membranes.
All investigated materials show excess contributions to the Debye type density of states characteristic for glasses known as Boson peak. The maximum position of the Boson peak shifts to lower frequency values with increasing microporosity. Data for PIM-1 and Matrimid included for comparison are in good agreement to this dependency. This result supports the sound wave interpretation of the Boson peak.
Quasielastic neutron scattering by employing a combination of time-of-flight and backscattering techniques is carried out to explore the molecular mobility of a polymer of intrinsic microporosity (PIM-1) at microscopic time scales in comparison with a high-performance polyimide. Molecular fluctuations can change the structure of the temporary network of micropores and open or close pathways for gas molecules. Therefore, the investigation might help to understand the selectivity of PIMs in gas separation processes. The performed neutron scattering experiments provide evidence for a low-temperature relaxation process, which was assigned to methyl group rotation. This methyl group rotation was analyzed in terms of jump diffusion in a three-fold potential. The analysis results in a fraction of methyl groups which are immobilized. For PIM-1 it was found that the fraction of immobilized methyl groups decreases with increasing temperature up to 350 K. At higher temperatures the number of immobilized methyl group increases gain due to an underlying relaxation process. This motional process on a somewhat larger length scale might lead to a reversible structural rearrangement which partially hinders the strongly localized methyl group rotation. In addition, it was found that the activation energy for the methyl group rotation for PIM-1 and the polyimide is significantly higher than for conventional polymers.
Surface Properties and Porosity of Silica Particles Studied by Wide-Angle Soft X-ray Scattering
(2020)
Wide-angle soft X-ray scattering on free silica particles of different porosity prepared in a beam is reported. The explored q region is mostly dominated by features due to surface roughness and bulk porosity. A comprehensive experimental and theoretical analysis of silica particles of different porosity is presented for various incident photon energies. A correlation analysis, based on the theory of Porod, is used to test the validity of exact Mie theory in different pore density limits. The ability of the discrete dipole scattering model (DDSCAT) to resolve local effects, caused by various pore distributions, is discussed. Characteristic differences between the soft X-ray scattering patterns of the particle samples of different surface properties and porosity are detected. For all mentioned cases, it was confirmed that the effective radius concept of the Guinier model can be successfully extended to Mie theory and DDSCAT in describing the additive contributions of the primary particles, including a thin inhomogeneous solvent-rich surface shell and empty bulk pores. Close agreement, within ±15%, between the calculated and observed pore sizes and porosity values is reached. The influence of pores is alternatively described either in terms of secondary Mie scattering, which is modulated by the local internal electrical field within the particles, or by an independent Mie scattering process induced by the incident field on isolated pores. It is found that for the typical pore/particle size ratios the latter approach presents the best choice.
Es wurden Prüfkörper aus additiver Fertigung mittels Laser Sinter Verfahren (Polyamid 12, PA 12) und Fused Layer Modeling (Acrylnitril-Butadien-Styrol, ABS) sowie Prüfkörper aus dem Kunststoff-Spritzguss Verfahren (PA 12 und ABS) über 2000 Stunden künstlich bewittert. Vor, während und nach der Bewitterung erfolgte eine zerstörungsfreie Prüfung mittels Thermografie, optischer Mikroskopie und spektralen Methoden (UV/VIS-Spektroskopie und spektrale Reflexion), um den Alterungsfortschritt zu untersuchen und Schäden durch die künstliche Bewitterung sowie eingedruckte Defekte zu identifizieren und zu detektieren.
Zusätzlich wurden zerstörende Zugprüfungen vorgenommen, welche mit einer IR-Kamera verfolgt wurden. Auf diese Weise konnten lokale Temperaturänderungen, hervorgerufen durch elastische sowie plastische Verformungen, zeitaufgelöst erfasst und ausgewertet werden.
Additively manufactured test specimens made of polyamide 12 (PA 12) by Laser Sintering as well as of acrylonitrile butadiene styrene (ABS) by Fused Layer Modelling, were characterised with active thermography directly after manufacturing and after artificial weathering. For this, two different excitation methods (flash and pulse heating) were used and compared, regarding their suitability for the detection of constructed and imprinted defects inside the test specimens. To increase the quality of the thermograms, data processing methods like thermal signal reconstruction (TSR) and Fourier Transformation after TSR were applied. To further investigate the long-term stability of the additively manufactured test specimens towards environmental stress, like UV radiation, heat, humidity, water contact and frost with active thermography, an artificial weathering test over 2000 hours (~3 months) was applied to the specimens. The monitoring of the changes in the optical properties of the weathered plastics was supplemented by spectral reflectance and UV/VIS spectroscopy.