Chemie und Prozesstechnik
Filtern
Dokumenttyp
- Vortrag (24)
- Zeitschriftenartikel (12)
- Beitrag zu einem Tagungsband (7)
- Posterpräsentation (7)
- Buchkapitel (1)
- Beitrag zu einem Sammelband (1)
- Dissertation (1)
- Sonstiges (1)
- Forschungsbericht (1)
Sprache
- Englisch (34)
- Deutsch (20)
- Mehrsprachig (1)
Schlagworte
- Wood materials (4)
- Acoustic emission (3)
- Coulometric sensors (3)
- Elektrolyseverfahren (3)
- Gas Source Localisation (3)
- Gas Spectroscopy (3)
- Individual cell tracking (3)
- Measurement uncertainty (3)
- QI-Digital (3)
- Schallemission (3)
Organisationseinheit der BAM
- 8.1 Sensorik, mess- und prüftechnische Verfahren (55) (entfernen)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (24)
In this study, nanoscopic particles of magnesium Fluoride (MgF2) and calcium fluoride (CaF2) also known as nano metal fluorides (NMFs), were evaluated for their potential to improve wood durability. Even though these fluorides are sparingly soluble, their synthesis in the form of nano-sized particles turns them into promising candidates for wood preservation. Their distinct property of low-water solubility is proposed to maintain long-lasting protection of treated wood by reducing the leaching of fluoride. Analytical methods were used to characterize the synthesized NMFs and their distribution in treated wood specimens. Transmission electron microscopy images showed that these fluoride particles are smaller than 10 nm. In nano metal fluoride (NMF) treated specimens, aggregates of these particles are uniformly distributed in the wood matrix as confirmed with scanning electron microscopy images and their corresponding energy-dispersive X-ray spectroscopy maps. The fluoride aggregates form a protective layer around the tracheid walls and block the bordered pits, thus reducing the possible flow path for water absorption into wood. This is reflected in the reduced swelling and increased hydrophobicity of wood treated with NMFs. The biocidal efficacy of NMFs was tested against brown-rot fungi (Coniophora puteanaand Rhodonia placenta), white-rot fungus (Trametes versicolor), and termites (Coptotermes formosanus). The fungal and termite tests were performed in accordance with the EN 113 (1996) and EN 117 (2012) standards, respectively. Prior to fungal tests, the NMF treated wood specimens were leached according to the EN 84 (1997)standard. Compared to untreated specimens, the NMF treated wood specimens have a higher resistance to decay caused by brown-rot fungi, white-rot fungus, and termites. Although all NMF treatments in wood reduce the mass loss caused by fungal decay, only the combined treatment of MgF2 and CaF2 has efficacy against both brown-rot fungi and white-rot fungus. Similarly, wood treated with the combined NMF formulation is the least susceptible to attack by C. formosanus.It is proposed that combining MgF2 and CaF2changes their overall solubility to promote the release of fluoride ions at the optimal concentration needed for biocidal efficacy against fungi and termites. In this thesis, it was proven that even after leaching, sufficient fluoride was present to protect NMF treated wood from fungal decay. This shows that NMFs are robust enough for above ground contact outdoor applications of wood, where permanent wetness cannot be avoided according to Use Class 3.2, as per the EN 335 (2013) standard. Also, they pose a low risk to human health and the environment because they are sparingly soluble. Since NMFs significantly reduce the decay of wood, the CO2 fixed in it will be retained for longer than in unpreserved wood. Overall, the novel results of this study show the potential of NMFs to increase the service life of building materials made from non-durable wood.
Um die Versagensabläufe über die verschiedenen Skalen im Holzwerkstoff verfolgen zu können, werden Zugversuche an Lagenhölzern mittels Schallemissionsmessung überwacht. Synchron erfolgen In-situ-Messungen mit Digitaler Bildkorrelation bzw. Synchrotron-Mikro-Computertomographie. Die Kombination aller Ergebnisse wie auch die Anwendung der frequenzbasierten Mustererkennung und die Simulation ausgewählter Versuche zielen auf die Identifizierung zugrunde liegender Mechanismen hin. Abschließend werden Ansätze für ein Monitoring von Holzstrukturen diskutiert.
The applicability of three methods developed by finite element analysis (FEM) and proposed in the literature are studied on steel S355. Instrumented indentation tests using spherical indenters of radius 200 and 500 μ m are performed in the macro range at depths of more than 6 μ m. The results of the selected methods are compared with the tensile test. To evaluate the partially strongly varying results, the uncertainties of the calculated strain hardening exponent, n, and yield stress, Y, are estimated. Recommendations for an appropriated procedure of the indentation test are given. The machine compliance and the determination of the zero point of Depth play an essential role. If the certain conditions are considered, the instrumented indentation Tests can be used, in particular for investigations of specimens with inhomogeneous elastoplasticity.
Against the background of sustainable resource management and efficiency, wood-based materials are currently experiencing a revival and, among others, plywood, Laminated Veneer Lumber and glued laminated timber are becoming increasingly more important in the building sector. Even though these materials are so-called engineered products, the element wood is naturally grown with intrinsic variability in mechanical properties and requires professional handling on-site. Otherwise, load-bearing structures made of wood materials may entail certain risks. Critical situations can, in principle, be avoided by implementing a structural health monitoring system into components or structures made from wood material. The aim is to indicate accumulation of mechanical damage and to eliminate or at least significantly reduce the risk of unexpected failure. Toward this purpose, the failure behavior of several layered wood materials under quasi-static tension was investigated in laboratory-scale experiments by means of acoustic emission (AE) measurement. Based on spectral analysis and pattern recognition, two classes of AE signals are identified for each investigated lay-up that are characterized by either low or high frequency contents in the respective power spectra. AE activity and intensity of both signal classes are analyzed, striving for predictors appropriate for AE monitoring concepts.
Against the background of sustainable resource management and efficiency, wood-based materials are currently experiencing a revival and, among others, plywood, Laminated Veneer Lumber and glued laminated timber are becoming increasingly more important in the building sector. Even though these materials are so-called engineered products, the element wood is naturally grown with intrinsic variability in mechanical properties and requires professional handling on-site. Otherwise, load-bearing structures made of wood materials may entail certain risks. Critical situations can, in principle, be avoided by implementing a structural health monitoring system into components or structures made from wood material. The aim is to indicate accumulation of mechanical damage and to eliminate or at least significantly reduce the risk of unexpected failure. Toward this purpose, the failure behavior of several layered wood materials under quasi-static tension was investigated in laboratory-scale experiments by means of acoustic emission (AE) measurement. Based on spectral analysis and pattern recognition, two classes of AE signals are identified for each investigated lay-up that are characterized by either low or high frequency contents in the respective power spectra. AE activity and intensity of both signal classes are analyzed, striving for predictors appropriate for AE monitoring concepts.
The finite volume method (FVM), like the finite element method (FEM), is a numerical method for determining an approximate solution for partial differential equations. The derivation of the two methods is based on very different considerations, as they have historically evolved from two distinct engineering disciplines, namely solid mechanics and fluid mechanics. This makes FVM difficult to learn for someone familiar with FEM. In this paper we want to show that a slight modification of the FEM procedure leads to an alternative derivation of the FVM. Both numerical methods are starting from the same strong formulation of the problem represented by differential equations, which are only satisfied by their exact solution. For an approximation of the exact solution, the strong formulation must be converted to a so-called weak form. From here on, the two numerical methods differ. By appropriate choice of the trial function and the test function, we can obtain different numerical methods for solving the weak formulation of the problem. While typically in FEM the basis functions of the trial function and test function are identical, in FVM they are chosen differently. In this paper, we show which trial and test function must be chosen to derive the FVM alternatively: The trial function of the FVM is a “shifted” trial function of the FEM, where the nodal points are now located in the middle of an integration interval rather than at the ends. Moreover, the basis functions of the test function are no longer the same as those of the trial function as in the FEM, but are shown to be a constant equal to 1. This is demonstrated by the example of a 1D Poisson equation.
Fluorides are well-known as wood preservatives. One of the limitations of fluoride-based wood preservatives is their high leachability. Alternative to current fluoride salts such as NaF used in wood protection are low water-soluble fluorides. However, impregnation of low water-soluble fluorides into wood poses a challenge. To address this challenge, low water-soluble fluorides like calcium fluoride (CaF2) and magnesium fluoride (MgF2) were synthesized as nanoparticles via the fluorolytic sol−gel synthesis and then impregnated into wood specimens. In this study, the toxicity of nano metal fluorides was assessed by termite mortality, mass loss and visual analysis of treated specimens after eight weeks of exposure to termites, Coptotermes formosanus. Nano metal fluorides with sol concentrations of 0.5 M and higher were found to be effective against termites resulting in 100% termite mortality and significantly inhibited termite feeding. Among the formulations tested, the least damage was found for specimens treated with combinations of CaF2 and MgF2 with an average mass loss less than 1% and visual rating of “1”. These results demonstrate the efficacy of low water-soluble nano metal fluorides to protect wood from termite attack.
In civil engineering, many structures are made of reinforced concrete. Most Degradation processes relevant to this material, e.g., corrosion, are related to an increased level of material moisture.
Therefore, moisture monitoring in reinforced concrete is regarded as a crucial method for structural health monitoring. In this study, passive radio frequency identification (RFID)-based sensors are embedded into the concrete. They are well suited for long-term operation over decades and are well protected against harsh environmental conditions. The energy supply and the data transfer of the humidity sensors are provided by RFID. The sensor casing materials are optimised to withstand the high alkaline environment in concrete, having pH values of more than 12. Membrane materials are also investigated to identify materials capable of enabling water vapour transport from the porous cement matrix to the embedded humidity sensor. By measuring the corresponding relative humidity with embedded passive RFID-based sensors, the cement hydration is monitored for 170 days.
Moreover, long-term moisture monitoring is performed for more than 1000 days. The Experiments show that embedded passive RFID-based sensors are highly suitable for long-term structural health monitoring in civil engineering.
The determination of the measurement uncertainty of quantitative and qualitative results is an important quality management tool, for example to describe measuring equipment, procedures, measurement results and the quality of products. The lecture presents the process description for the determination of the measurement uncertainty according to GUM, the determination of uncertainties in qualitative measurement results and the application of the measurement uncertainty for conformity assessment.
The evaluation of measurement uncertainty is essential for testing and calibration laboratories. This paper provides a general process description for the determination of the measurement uncertainty of quantitative data and its application to the conformity assessment with examples, and how to deal with the uncertainty of qualitative (Boolean) results, e. g. when "Alarm" or "No alarm" occours in an instrument display.