Degradation von Werkstoffen
Filtern
Dokumenttyp
- Vortrag (823)
- Beitrag zu einem Tagungsband (167)
- Posterpräsentation (128)
- Zeitschriftenartikel (78)
- Sonstiges (23)
- Zeitschriftenheft (Herausgeberschaft für das komplette Heft) (20)
- Forschungsbericht (18)
- Buchkapitel (14)
- Dissertation (12)
- Beitrag zu einem Sammelband (7)
Sprache
- Englisch (743)
- Deutsch (546)
- Mehrsprachig (3)
- Russisch (2)
- Chinesisch (2)
- Französisch (1)
- Spanisch (1)
Referierte Publikation
- nein (1298) (entfernen)
Schlagworte
- Corrosion (103)
- Korrosion (94)
- Nichtrostender Stahl (55)
- Additive Fertigung (46)
- Welding (44)
- KorroPad (43)
- Hydrogen (41)
- Wasserstoff (41)
- Schweißen (39)
- Eigenspannungen (36)
Organisationseinheit der BAM
- 9 Komponentensicherheit (462)
- 7 Bauwerkssicherheit (343)
- 9.4 Integrität von Schweißverbindungen (290)
- 5 Werkstofftechnik (250)
- 7.6 Korrosion und Korrosionsschutz (242)
- 8 Zerstörungsfreie Prüfung (165)
- 9.2 Versuchsanlagen und Prüftechnik (136)
- 6 Materialchemie (117)
- 9.0 Abteilungsleitung und andere (109)
- 3 Gefahrgutumschließungen; Energiespeicher (97)
Paper des Monats
- ja (1)
Iron aluminides depict a sustainable and light-weight material class which could be employed in many applications requiring high strength at intermediate to high temperatures. According to first results, the alloy Fe-26Al-4Mo-0.5Ti-1B surpasses conventional materials in wet corrosion resistance and creep resistance up to 650 °C. For these reasons, the AiF research project “WAFEAL – Materials applications for iron aluminides” was initiated to transfer these findings into a standardised materials dataset and to derive best practices for processing. In the first place, a set of different microstructures adjusted by varying casting methods, wall thicknesses and heat treatments was investigated and correlated with hardness on macro and micro scale. Correlations were drawn between solidification rates and resulting grain sizes and hardness. The effect of vacancy hardening was only verified for wall thickness as low as 2.5 mm. Moreover, a common decrease of macrohardness after a heat treatment at 1000 °C for 100 h was observed irrespective of casting process or wall thickness. This effect was linked with an unexpected decrease of the complex boride phase fraction which acts as a hardening phase.
Due to the increasing scarcity of critical raw materials current high-temperature materials are sought to be replaced by alloys based on more abundant metals. One possibility within the class of intermetallics are iron aluminides, which combine sustainability and cost-efficiency with the prospect of mass savings. Iron aluminides show competitive specific strength up to 700 °C and excellent creep and wet corrosion resistance by small additions of Mo, Ti and B. Nevertheless, a Mo content of above 2 at.% which is needed for optimum corrosion resistance results in enhanced brittleness, especially at room temperature. This is why alloys with these Mo fractions were only mechanically tested under compressive loading so far. Still, testing of static and creep properties under tensile loading is required for reliable component design. Besides high standards for crack-free processing, data acquisition for tensile loads is especially complicated by environmental embrittling effects for iron aluminides. To cope with these challenges, the AiF research project “WAFEAL – Materials applications for iron aluminides” was initiated. The main goal is to collect standardised data on ambient and high-temperature tensile properties and creep properties. Samples with a nominal composition of Fe-26Al-4Mo-0.5Ti-1B [at.%] were manufactured via centrifugal casting in ceramic shell moulds followed by machining. Heat treatment for homogenisation and final polishing were carried out where appropriate. A summary of the achieved tensile and creep properties such as yield and tensile strength, maximum elongation, secondary creep rate and stress exponents will be given. Results will be also discussed regarding the influence of temperature, stress level and microstructure on the damage mechanisms. Furthermore, the effect of different alloy concentrations on the mechanical response at different temperatures will be outlined within a small experimental series.
With an increasing demand in more efficient fuel consumption to reduce CO2 emissions, weight reductions in high-temperature materials at affordable costs gain increasing attention. One potential candidate is the intermetallic material class of iron aluminides, combining the advantages in mass savings, high temperature performance and recyclability of resources. The alloy Fe-26Al-4Mo-0.5Ti-1B was selected to study the microstructural features evolving from two casting processes, five wall thicknesses and three final conditions. Conclusions are drawn upon the correlations of processing variables, grain sizes and hardness.
The increasing importance of resource availability and closed-loop material cycles are driving materials research to reduce alloying content in conventional materials or even substitute them with more sustainable alternatives. Intermetallic iron aluminide alloys (FeAl) present a potential alternative. Many alloy concepts for improved high-temperature properties or ductility have already been successfully implemented in casting technologies on a laboratory scale. However, successful testing of FeAl alloys on an industrial scale was still pending at the beginning of the project.
Therefore, the aim of the project was to develop simulation-based casting concepts for industrial casting processes using the base alloy Fe-26Al-4Mo-0.5Ti-1B and to narrow down process limits by means of hot cracking tests. Findings were transferred into practice-oriented guidelines for casting of iron aluminides, which is accessible to future applicants in SMEs. The focus was placed on centrifugal casting combined with investment casting or die casting. In addition to numerous design and casting process parameters, heat treatments and alloying additions (Al, Mo, B) were varied to determine the influence of alloying elements on castability, microstructure and mechanical properties. Data from microstructure analyses (microscopic imaging, determination of grain sizes as well as phase compositions and volume fractions, fractography), mechanical tests (hardness measurements, compression tests, ambient and high-temperature tensile tests, creep tests) as well as measurements of thermophysical properties could be generated on the base alloy. Correlations of materials data with process variables allowed conclusions to be drawn on strengthening mechanisms and ductility of the alloy and how they can be controlled in terms of processing and component design. Successful casting of highly complex components with thin wall thicknesses and optimised alloy compositions points out prospects for new fields of application.
The increasing importance of resource availability and closed-loop material cycles are driving materials research to reduce alloying content in conventional materials or even substitute them with more sustainable alternatives. Intermetallic iron aluminide alloys (FeAl) present a potential alternative. Many alloy concepts for improved high-temperature properties or ductility have already been successfully implemented in casting technologies on a laboratory scale. However, successful testing of FeAl alloys on an industrial scale was still pending at the beginning of the project.
Therefore, the aim of the project was to develop simulation based casting concepts for industrial casting processes using the base alloy Fe-26Al-4Mo-0.5Ti-1B and to narrow down process limits by means of hot cracking tests. Findings were transferred into practice-oriented guidelines for casting of iron aluminides, which is accessible to future applicants in SMEs. The focus was placed on centrifugal casting combined with investment casting or die casting. In addition to numerous design and casting process parameters, heat treatments and alloying additions (Al, Mo, B) were varied to determine the influence of alloying elements on castability, microstructure and mechanical properties. Data from microstructure analyses (microscopic imaging, determination of grain sizes as well as phase compositions and volume fractions, fractography), mechanical tests (hardness measurements, compression tests, ambient and high-temperature tensile tests, creep tests) as well as measurements of thermophysical properties could be generated on the base alloy. Correlations of materials data with process variables allowed conclusions to be drawn on strengthening mechanisms and ductility of the alloy and how they can be controlled in terms of processing and component design. Successful casting of highly complex components with thin wall thicknesses and optimised alloy compositions points out prospects for new fields of application.
Tracking waterborne microplastic (MP) in urban areas is a challenging task because of the various sources and transport pathways involved. Since MP occurs in low concentrations in most wastewater and stormwater streams, large sample volumes need to be captured, prepared, and carefully analyzed. The recent research in urban areas focused mainly on MP emissions at wastewater treatment plants (WWTPs), as obvious entry points into receiving waters. However, important transport pathways under wet-weather conditions are yet not been investigated thoroughly. In addition, the lack of comprehensive and comparable sampling strategies complicated the attempts for a deeper understanding of occurrence and sources. The goal of this paper is to (i) introduce and describe sampling strategies for MP at different locations in a municipal catchment area under dry and wet-weather conditions, (ii) quantify MP emissions from the entire catchment and two other smaller ones within the bigger catchment, and (iii) compare the emissions under dry and wet-weather conditions. WWTP has a high removal rate of MP (>96%), with an estimated emission rate of 189 kg/a or 0.94 g/[population equivalents (PEQ · a)], and polyethylene (PE) as the most abundant MP. The specific dry-weather emissions at a subcatchment were ≈30 g/(PEQ · a) higher than in the influent of WWTP with 23 g/(PEQ · a). Specific wet-weather emissions from large sub-catchment with higher traffic and population densities were 1952 g/(ha · a) higher than the emissions from smaller catchment (796 g/[ha · a]) with less population and traffic. The results suggest that wet-weather transport pathways are likely responsible for 2–4 times more MP emissions into receiving waters compared to dry-weather ones due to tire abrasion entered from streets through gullies. However, more investigations of wet-weather MP need to be carried out considering additional catchment attributes and storm event characteristics.
Im Vorhaben wurde eine forcierte Prüfmethode zur Bestimmung der Beständigkeit von metallenen Werkstoffen gegenüber Brennstoffen aus Mitteldestillaten und Gemischen aus Mitteldestillat und paraffinischen Kohlenwasserstoffen, die jeweils Fettsäuremethylester (FAME) als biogene Komponente enthalten, entwickelt. Bei der Prüfmethode werden Prüfkörper des jeweiligen Werkstoffes in speziellen Prüfmedien ausgelagert. Die Zusammensetzung von zwei Prüfmedien wurde im Vorhaben erarbeitet. Diese Prüfmedien erfassen die Effekte der Alterung des FAME, die zu erwarten sind, wenn der Brennstoff länger als 2 Jahre im Feld lagert. Sie decken den Bereich bis 20 % (V/V) FAME-Anteil ab. Die Auslagerung kann bei geringem Aufwand unter Atmosphärendruck durchgeführt werden.
Die Eignung einer Auswahl von metallenen Werkstoffen und Polymerwerkstoffen, die für Versorgungsanlagen für Mitteldestillat relevant sind, wurde durch Auslagerung in folgenden nicht gealterten Brennstoffen bestimmt: Heizöl EL schwefelarm (B0), Heizöl EL schwefelarm mit 20 % (V/V) FAME (B20), FAME (B100) und hydriertes Pflanzenöl (HVO). Die Werkstoffe wurden auch in einem 1 Jahr gealterten B20 und einem 8 Jahre gealtertem B10 ausgelagert. Die Temperatur bei der Auslagerung betrug 50 °C für die metallenen Werkstoffe und 40 °C und 70 °C für die Polymerwerkstoffe. Die Ergebnisse der Beständigkeitsbewertung wurden in Beständigkeitslisten zusammengefasst. Die mit B20 erhaltenen Bewertungen gelten generell für Gemische aus Heizöl EL schwefelarm und FAME mit einem FAME-Gehalt bis 20 % (V/V). Sie sind auch auf Gemische aus Dieselkraftstoff und FAME mit einem FAME-Gehalt bis 20 %(V/V) übertragbar.
Die forcierte Prüfmethode kann insbesondere KMUs bei der Weiterentwicklung von bestehenden Produkten und der Entwicklung von neuen Produkten als ein kostengünstiger Schnelltest zur Überprüfung der Werkstoff- und Bauteilbeständigkeit gegenüber Mitteldestillaten mit hohem FAME-Anteil dienen. Sie kann für die Hersteller die Sicherheit erhöhen, dass Bauteile die Freigabeprüfungen der Bauaufsicht bestehen, wobei die Freigabe jedoch nur für Deutschland gültig ist.
Die Erkenntnisse des Forschungsvorhabens können in eine harmonisierte Europäische Norm für alternative Brenn- und Kraftstoffe einfließen. Diese ist für die Bauteilhersteller die Voraussetzung für die Erschließung des europäischen Marktes.
Ni-base superalloy single crystals have been used in turbine blades for hot sections of gas turbines for over four decades. In order to increase the efficiency of the turbines, a continuous increase in the inlet temperature of combustion gases into the turbine has driven the design of turbine blades to complicated shapes and the presence of a complex pattern of cooling channels. These three-dimensional shapes, together with the inhomogeneous distribution of stresses along the blade, induce an also complicated triaxial stress state, which does not compare to uniaxial tests that are performed to characterize high temperature properties such as creep. A round notch on a test piece represents a simple configuration that generates a quasi-isostatic stress state across the notch. In the present contribution, the effect of a sharp round notch on the microstructural micromechanisms within the notched region cylindrical bars, loaded along [001] at 1020 °C and 160 MPa net stress, is studied. To this end, a series of interrupted creep tests is conducted on plain and notched bars and the microstructure is compared. Results are discussed in terms of degree microstructural coarsening, and dislocation activity. The effect of notch generation via grinding is also discussed in these terms. The presence of carbides evolving in from residual carbon is also shown and discussed. .Funding by the German Research Association (DFG) [grant number AG 191/1] is acknowledge
Unlike conventional alloys, which typically consist of one main element, high-entropy alloys (HEAs) contain five or more principal elements, which broaden chemical complexity and with it a realm of synergistic mechanisms. The AlMo0.5NbTa0.5TiZr HEA initiated a subclass of Al-containing refractory (r)HEAs that has recently drawn attention [2]. The alloy has a superalloy-resembling B2/bcc nanostructure, which inspired its name refractory high entropy superalloy (RSA). With high-temperature (HT) compressive strengths beyond conventional Ni-based superalloys, this nanostructure could be used for improved HT structural applications. However, in the application-relevant HT regime the Al-Zr-rich B2 phase decomposes to form a hexagonal Al-Zr-based intermetallic (Al4-xZr5; x: 0..1) [3,4]. This work explores the fascinating yet fatal micromechanisms associated to this phase transformation, in the context of creep, annealing and oxidation experiments performed between 800 and 1200 °C.
The material was produced by arc-melting and heat treatment in argon, which lead to grain boundaries decorated with up to 7%. Interrupted constant-load creep tests were performed under vacuum (at 10-4 Pa), at 900–1100 °C with external tensile stresses of 30–120 MPa. Oxidation experiments were separately conducted for 24 hours at 800 and 1000 °C in both dry (21% O2 + 79% N2) and humid (8% O2 + 74% N2 + 18% H2O) air. After the experiments, the samples were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy to reveal degradation mechanisms. Crystallographic texture, orientation relationships and stabilization of an oxygen-containing iso structure (Al4-xZr5(Ox-y); y: 0..x) of the Al-Zr-rich intermetallic are found and discussed.