Antimony in incineration bottom ash – Leaching behavior and conclusions for treatment processes
(2020)
Antimony (Sb) is used in industrial products mainly as flame retardant in plastic material. Due to such additives in plastics, about a half of Sb ends up in municipal solid waste incineration at the end-of-life and consequently in relevant amounts in the generated bottom ash. In contact with water, the initial leachability is low, as antimonates form sparingly soluble compounds with Ca2+. Following the carbonation of the incineration bottom ash (IBA) during the proceeding ageing the pH in the leachates decreases. With decreasing concentration of Ca in the eluate the solution equilibrium changes and antimonates dissolve. In Germany it is intended to regulate Sb in IBA with the planned implementation of the so called Mantelverordnung (MantelVO, containing provisions on the utilisation of mineral waste) in the near future. The limit values set in the draft might be critical for IBA and therefore pose a risk for the utilisation of the mineral fraction of IBA in the well-established recycling routes.
Potential use of incineration bottom ash in construction – Evaluation of the environmental impact
(2020)
Knowledge of the long-term leaching behavior of potentially harmful substances is crucial for the assessment of the environmental compatibility of reusing municipal solid-waste incineration bottom ash (MSWI BA) in construction, i.e., as a road base layer.
BA fractions obtained from wet-processing aiming at the improvement of environmental quality were used to investigate the mobility of relevant substances. Eluates from laboratory-scaled leaching procedures (column percolation and lysimeters) were analyzed to learn about the long-term release of substances. Unsaturated conditions and artificial rainwater (AR) were used in the lysimeter tests to simulate field conditions. In addition, batch test eluates were generated at usual liquid-to-solid ratios (L/S) for compliance testing purposes. A variety of cations and anions was measured in the eluates.
The wet treatment reduces the leaching of chloride and particularly sulfate by more than 60%. The release of typical contaminants for the treated MSWI BA such as the heavy metals Cu and Cr was well below 1% in the conducted leaching tests.
An increase in the Sb concentration observed in the lysimeter experiments starting at L/S 0.75 L/kg and in the column experiment at L/S 4 L/kg is assumed to be related to decreasing concentrations of Ca and thus to the dissolution of sparingly soluble calcium antimonate. The same leaching mechanism applies with V, but the concentration levels observed are less critical regarding relevant limit values. However, on the long term the behavior of Sb could be problematic for the application of MSWI BA in construction.