9.2 Versuchsanlagen und Prüftechnik
Filtern
Dokumenttyp
- Vortrag (147) (entfernen)
Referierte Publikation
- nein (147)
Schlagworte
- Additive Fertigung (36)
- Eigenspannungen (33)
- Ultraschallunterstütztes Fräsen (32)
- Hochfester Stahl (24)
- MAG-Schweißen (16)
- Legierungsmodifikation (15)
- Oberflächenintegrität (15)
- Welding (14)
- Additive manufacturing (13)
- Residual stress (11)
Organisationseinheit der BAM
- 9 Komponentensicherheit (147) (entfernen)
Residual stress formation during repeated gouging and repair welding cycles of high-strength steels
(2024)
The construction of foundation and erection structures for wind power plants requires the use of modern, sustainable and resource-efficient high-strength fine-grained structural steels. Weld defects due to the welding process are unacceptable. To overcome this issue, local thermal gouging followed by re-welding is a common and cost-effective method. The high shrinkage restraint of the gouge by the surrounding structure can cause crack initiation when design and re-weld induced residual stresses are superimposed. This risk is intensified by the progressive degradation of the microstructure and mechanical properties of high-strength steels during the weld repair process.
This investigation focuses on high-strength steels S500MLO for offshore applications and S960QL for mobile crane applications. The reduction and development of residual stresses caused by local thermal gouging and re-welding was investigated. Digital Image Correlated (DIC) stress-strain analysis was performed during preheating, welding and cooling. The results of the global DIC analysis and local longitudinal and transverse residual stresses of the weld determined by X-ray diffraction were found to be in good agreement. Furthermore, different stress levels were identified during gouging and welding. Repeated repair cycles led to an increase of longitudinal and transverse residual stresses in the weld metal as well as a hardness increase in the heat affected zone.
Der Bau von Gründungs- und Turmstrukturen für Windkraftanlagen erfordert den Einsatz moderner, nachhaltiger und ressourcenschonender hochfester Feinkornbaustähle. Durch den Schweißprozess verursachte Schweißnahtfehler sind nicht akzeptabel. Um diese zu beheben, ist das lokale thermische Fugenhobeln mit anschließendem Reparaturschweißen ein gängiges und wirtschaftliches Verfahren. Die hohe Schrumpfbehinderung um die ausgefugte Nut durch das umgebende Gefüge kann zu Rissbildung führen, wenn sich konstruktiv bedingte Spannungen und Eigenspannungen aus der Reparaturschweißung überlagern. Diese Gefahr wird durch die Verschlechterung der Mikrostruktur und der mechanischen Eigenschaften hochfester Stähle während des Schweißreparaturprozesses noch verstärkt.
The presentation gives an overview of BAM's activities on processing influences and application properties of MPEAs in the form of joined and machined high and medium entropy alloys (CoCrFeMnNi and CoCrNi). In the case of welding, the focus is on defect-free welded joints with sufficient mechanical properties. In the case of machining, the focus is on the possible influence on the surface quality of the materials through adequate milling parameters. In addition, the hydrogen absorption and diffusion properties as well as the electrochemical corrosion behavior are fundamentally examined.
Die additive Fertigung mittels Schweißverfahren bietet große ökonomische Vorteile für eine ressourceneffiziente Bauteilherstellung. Offene Fragen bezüglich Homogenität, Anisotropie der Schweißgefüge und den damit verbundenen Bauteileigenschaften stehen einer wirtschaftlichen Verarbeitung oftmals im Wege. Finale Bauteilgeometrie und Oberflächengüte erfordern meist komplementäre subtraktive Fertigungsschritte. Werkstoffe für hochbelastbare Komponenten sind oftmals schwer spanbar. In einem Vorhaben der BAM und des ISAF wurde untersucht, wie die Modifikation der AM-Schweißzusätze und das ultraschallunterstützte Fräsen (US) die Zerspanungssituation verbessern. Der vorliegende Artikel stellt wesentliche Zusammenhänge zwischen Legierung, Gefüge und Zerspanung zweier schwer spanbarer Hochleistungslegierungen (FeNi und CoCr) dar. Großes Potenzial zeigte neben dem US die Modifikation mit Zr und Hf bei Zulegierung in das Schweißgut mittels Beschichtung von Massivdrähten bzw. Herstellung von Fülldrähten.
Diese Studie konzentriert sich auf den Einfluss der Bearbeitung auf die Eigenspannungen und den Verzug von WAAM-Proben. Definierte Proben wurden vollautomatisch mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) mit unterschiedlichen geometrischen Designs geschweißt. Der Eigenspannungszustand vor und nach dem Abtrennen der AM-Struktur von der Substratplatte wurde mittels Röntgenbeugung an der Probenoberfläche analysiert und durch 3D-Verformungsanalysen mittels Photogrammetrie ergänzt. Die Ergebnisse zeigen einen signifikanten Einfluss der Geometrie auf die Relaxation und Umverteilung der Eigenspannungen.
Influence of machining on residual stresses in additive manufactured high-strength steel components
(2024)
This study focuses on the effect of machining on the residual stresses and distortion of WAAM specimens. Defined specimens were welded fully automatically with a special WAAM solid wire (yield strength >820 MPa) with different geometric designs. The residual stresses state before and after cutting of the AM structure from the substrate plate were analyzed by means of X-ray diffraction on the specimen surface and complementary by 3d deformation analyses using photogrammetry. The results reveal significant influences of the geometry on the relaxation and redistribution of residual stresses.
In der Abschlusspräsentation des ZIM-Kooperationsvorhabens "TeWuFeAl" werden die wichtigsten Ergebnisse zusammengefasst dargestellt. Ziel des Projektes war die Entwicklung einer Prozess- und Werkzeugtechnologie für das ultraschallunterstützte Fräsen von im Kokillenguss hergestellter Eisen- und Titan-Aluminid-Bauteilen. Auf Basis einer eigens entwickelten Werkzeugtechnologie und Prozessführung konnten die Belastungen auf das Werkzeug und die Oberfläche von Bauteilen aus dem schwer zerspanbaren Eisenaluminid bei der frästechnischen Bearbeitung signifikant verringert werden. Die Messung der Prozesskräfte und der thermischen Belastung der Werkzeugschneide ermöglicht die Ermittlung geeigneter Zerspanungsparameter für eine maximale Werkzeuglebensdauer. Die Anwendung des ultraschallunterstützten Fräsens (USAM) wirkt sich vorteilhaft auf den Zerspanprozess aus. Neben einer deutlichen verlängerung der Werkzeuglebensdauer, zeigen sich Vorteile in Bezug auf die topographischen, metallurgischen sowie mechanischen Eigenschaften der erzeugten Oberflächenintegrität. Die durch USAM erzeugte homogene Bauteiloberfläche weist eine reduzierte Defektdichte und verringerte Rauheitskennwerte auf. Besonders vielversprechend sind die Ergebnisse der Messungen der Eigenspannungen im Tiefenprofil der Oberfläche. Die Werkzeugoszillation bewirkt eine, vergleichbar zum Strahlprozess, Verdichtung der Oberfläche was in Druckeigenspannungen resultiert. Diese potenziell vorteilhaften Druckeigenspannungen können maßgeblich zur Risssicherheit hochbelasteter Komponenten und somit zum Leichtbau und Ressourceneffizienz beitragen.
Ultraschallunterstützte Zerspanung mit geometrisch bestimmter Schneide schwer spanbarer Werkstoffe
(2023)
Das hybride Fertigungsverfahren der ultraschallunterstützen Zerspanung wird mit geometrisch unbestimmter Schneide wie bspw. dem Schleifen bereits erfolgreich in der Industrie eingesetzt und verspricht auch unter Verwendung von Werkzeugen mit geometrisch bestimmter Schneide vielversprechende Vorteile gegenüber den konventionellen spanenden Fertigungsverfahren. In den letzten Jahren wurden an der BAM positive Ergebnisse beim ultraschallunterstützten Fräsen (USAM) von schwer spanbaren Werkstoffen wie z.B. Ni-/Co-Legierungen oder Eisenaluminid für den Leichtbau erzielt aber auch die Finishbearbeitung von schweißtechnisch generierten Bauteilen (AM) bspw. aus FeNi36 konnte hinsichtlich erreichbarer Werkzeuglebensdauer sowie Oberflächenintegrität zur Verbesserung der Komponentensicherheit beitragen. Die mittels USAM erzeugten Oberflächen erscheinen homogener und weisen weniger Defekte infolge des Materialabtrags auf, was sich ebenfalls in verringerten Rauheitskennwerten abbildet. Durch die geringere thermo-mechanische Belastung der Bauteiloberfläche sind Eigenschaftsdegradationen zusätzlich reduziert. Besonders großes Zukunftspotenzial besitzt das ultraschallunterstütze Fräsen durch die Erzeugung von erwünschten Druckeigenspannungen bis unter die Bauteiloberfläche, was auf die oszillierende Wirkung der Werkzeugschneide - vergleichbar mit einem Strahlprozess - zurückzuführen ist. Druckeigenspannungen tragen maßgeblich zur Risssicherheit hochbelasteter Komponenten bei wie sie bspw. in Turbinen vorzufinden sind und können somit zum Leichtbau und zur Ressourceneffizienz beitragen.
Additive manufacturing (AM) processes enable the efficient production of advanced constructions. New developments in topology optimization are leading to weight-optimized designs of increasing complexity. Direct energy deposition processes (DED) such as wire and arc-based additive manufacturing are an important method of additive manufacturing. The wire filler metals enable a wide range of materials, while the arc process provides a high deposition rate compared to laser and powder-based processes. Combined with the use of high-strength steels, the thickness of walls or components can be significantly reduced in the context of lightweight construction, which results in significant savings in energy, costs, time and resources. Suitable high-strength steel filler metals are commercially available for DED-arc AM processes. However, guidelines and quantitative knowledge about welding stresses and cold cracking issues during component production and service are lacking. This limits the industrial application considerably. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute- Villigen, Switzerland (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps compared to XRD. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times and less post heat treatment cycles of following AM layers in the area of the top layer.
Additive manufacturing (AM) processes enable the efficient production of advanced constructions. New developments in topology optimization are leading to weight-optimized designs of increasing complexity. Direct energy deposition processes (DED) such as wire and arc-based additive manufacturing are an important method of additive manufacturing. The wire filler metals enable a wide range of materials, while the arc process provides a high deposition rate compared to laser and powder-based processes. Combined with the use of high-strength steels, the thickness of walls or components can be significantly reduced in the context of lightweight construction, which results in significant savings in energy, costs, time and resources. Suitable high-strength steel filler metals are commercially available for DED-arc AM processes. However, guidelines and quantitative knowledge about welding stresses and cold cracking issues during component production and service are lacking. This limits the industrial application considerably. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute- Villigen, Switzerland (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps compared to XRD. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times and less post heat treatment cycles of following AM layers in the area of the top layer.
Additive manufacturing (AM) processes enable the efficient production of advanced constructions. New developments in topology optimization are leading to weight-optimized designs of increasing complexity. Direct energy deposition processes (DED) such as wire and arc-based additive manufacturing are an important method of additive manufacturing. The wire filler metals enable a wide range of materials, while the arc process provides a high deposition rate compared to laser and powder-based processes. Combined with the use of high-strength steels, the thickness of walls or components can be significantly reduced in the context of lightweight construction, which results in significant savings in energy, costs, time and resources. Suitable high-strength steel filler metals are commercially available for DED-arc AM processes. However, guidelines and quantitative knowledge about welding stresses and cold cracking issues during component production and service are lacking. This limits the industrial application considerably. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute- Villigen, Switzerland (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps compared to XRD. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times and less post heat treatment cycles of following AM layers in the area of the top layer.
Stresses in repair welding of high-strength steels Part 2: Heat Control and Stress Optimization
(2023)
In welding of high-strength steels, e.g., for foundations and erection structures of wind energy plants, unacceptable defects can occasionally be found in the weld area, which should be removed by thermal gouging and subsequent re-welding. High shrinkage restraint of repair welds may lead to crack formation and component failure, particularly in interaction with degraded microstructures and mechanical properties due to repair cycles. This study aims for elaboration of recommendations for repair concepts appropriate to the stresses and materials involved to avoid cold cracking, damage and expensive reworking. In part 1 [1] of this study systematic investigations of influences of shrinkage restraint on residual stresses and cold cracking risk during repair welding of two high-strength steels S500MLO for offshore application and S960QL for mobile crane structures were focussed. In this part 2, the microstructure and residual stresses due to gouging and influences of heat control parameters in repair welding are analysed. A clear reduction in residual stress after gouging can be observed, especially for the specimens with restrained transverse shrinkage. Gouging to a depth of approx. 2/3 of the seam height does not lead to a complete relaxation of the observed reaction forces. Particularly for the higher strength steel S960QL, there are pronounced areas influenced by the gouging process in which a degradation of the microstructure and properties should be assumed. Overall, the repair welds show a significant increase in the width of the weld and HAZ compared to the original weld, especially in the case of S960QL/G89. The repair welds show higher welding-induced stresses than the original welds, especially in the areas of the HAZ and the base metal close to the weld seam. This behaviour can be attributed overall to increased restraint conditions due to the remaining root weld or shorter gouge grooves. In good agreement with earlier investigations, the residual stresses transverse to the weld can be significantly reduced by upwardly limited working or interpass temperatures and the reaction stresses resulting from high restraint conditions can be effectively counteracted. The influence of the heat input on the stress formation is low compared to the interpass temperature for both test materials.
The sustainable and resource-efficient production of wind energy plants requires the use of modern high-strength fine-grain structural steels. This applies to both foundation and erection structures, like mobile or ship cranes. During the assembly of steel structures, unacceptable defects can occasionally be found in the weld area. In most cases, the economical solution would be local thermal gouging of the affected areas and re-welding. Due to the high shrinkage restraint of the joint groove in the overall structure, the superposition of global and local welding-induced stresses may lead to crack formation and component failure, particularly in interaction with the degradation of the microstructure and mechanical properties of high-strength steels during the repair process. However, manufacturers hardly have any information about these issues and there is a lack of recommendations and guidelines to take these safety-relevant aspects into account in adequate repair concepts. The aim of this research is to derive recommendations for repair concepts appropriate to the stresses and materials involved providing a basis for standards and guidelines to avoid cold cracking, damage and expensive reworking especially for high-strength steels. Part 1 of this study involves systematic investigations of influences of shrinkage restraint during repair welding of two high-strength steels S500MLO for offshore application and S960QL for mobile crane structures. The quantification of the shrinkage restraint of repair weld joints was achieved by means of experimental and numerical restraint intensity analysis. In welding experiments with self-restrained slot specimens, restraint intensity and introduction of hydrogen via the welding arc using anti spatter spray were varied systematically to analyse the effect on welding result, residual stresses, and cold cracking. It could be shown that increasing restraint intensities result in significantly higher transverse residual stress levels. In the case of hydrogen introduction S500MLO showed no cold cracking independent of the restraint conditions. However, S960QL was found to be considerably cold cracking sensitive if hydrogen is introduced. With increasing restraint intensity length and number of cold cracks increases significantly. Part 2 [1] of this study is focussed on microstructure and residual stresses due to gouging and stress optimization via adequate heat control parameters in repair welding.
Der Vortrag gibt einen Überblick über den Einfluss der Prozessparameter auf die Eigenspannungen sowie die Härte in additiv gefertigten Bauteilen aus hochfestem stahl. Des Weiteren wird dargestellt, wie sich das Bauteildesign und trennende Fertigungsschritte auf die Eigenspannungen der Bauteile auswirken.
Additive manufacturing (AM) processes enable the efficient production of advanced constructions. New developments in topology optimization are leading to weight-optimized designs of increasing complexity. Direct energy deposition processes (DED) such as wire and arc-based additive manufacturing are an important method of additive manufacturing. The wire filler metals enable a wide range of materials, while the arc process provides a high deposition rate compared to laser and powder-based processes. Combined with the use of high-strength steels, the thickness of walls or components can be significantly reduced in the context of lightweight construction, which results in significant savings in energy, costs, time and resources. Suitable high-strength steel filler metals are commercially available for DED-arc AM processes. However, guidelines and quantitative knowledge about welding stresses and cold cracking issues during component production and service are lacking. This limits the industrial application considerably. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute- Villigen, Switzerland (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps compared to XRD. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times and less post heat treatment cycles of following AM layers in the area of the top layer.
Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann.
Auf der Grundlage einer speziell entwickelten Werkzeugtechnologie sowie Prozessführung können die Belastungen auf das Werkzeug und die Bauteiloberfläche bei der frästechnischen Bearbeitung von Bauteilen aus dem innovativen jedoch schwer zerspanbaren Eisenaluminid deutlich reduziert werden. Die Messung der Prozesskräfte sowie der thermischen Belastung der Werkzeugschneide ermöglicht die Identifikation geeigneter Zerspanungsparameter hinsichtlich einer maximalen Werkzeuglebensdauer. Die Verwendung des ultraschallunterstützten Fräsens (USAM) besitzt vorteilhafte Einflüsse auf den Zerspanprozess, insbesondere hinsichtlich einer homogenen Bauteiloberfläche. Im Rahmen von Standzeitversuchen erfolgt durch USAM ein gleichmäßiger und im Vergleich zum konventionellen Fräsen (CM) deutlich reduzierter Werkzeugverschleiß. Mit wachsendem Zerspanvolumen verstärkt sich der positive Effekt von USAM und äußert sich in einer deutlichen Reduzierung der Rauheit und Defektdichte auf der Bauteiloberfläche.
Alloy Modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. In addition to increasing demands to replace conventional cobalt alloys with nickel alloys as a result of price and supply risks, there is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining is investigated. The alloy used is a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA). Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
Die Ziele zur Verringerung der CO2-Emissionen sind eng verknüpft mit der Entwicklung hocheffizienter und wirtschaftlicher Komponenten aus Stahl in der Anlagen-, Verfahrens- und Kraftwerktechnik, die für hohe kombinierte korrosive, tribologische, thermische und mechanische Beanspruchungen auf Anwendungsfall und Stahlwerkstoff abgestimmte Verschleißschutzschichten erfordern. Neben zunehmenden Forderungen infolge des Preis- und Lieferrisikos konventionelle Kobalt- durch Nickellegierungen zu ersetzen, wächst in der Industrie der Bedarf nach definierten Oberflächen hoher Güte bzw. Funktionsflächen für die Schutzschichten. Eine für Bauteile mit komplexer Geometrie erforderliche Fräsbearbeitung ist insbesondere für KMU aufgrund hohen Werkzeugverschleißes oftmals nicht wirtschaftlich realisierbar, jedoch für viele Einsatzfälle dringend notwendig.
In einem Gemeinschaftsvorhaben der BAM und des ISAF der TU Clausthal (Fosta P1550/IGF 21959 N) wird daher untersucht, wie mittels Legierungsmodifikationen der Schweißzusätze für nickelbasierte plasmaauftraggeschweißte Verschleißschutzschichten und durch Einsatz innovativer ultraschallunterstützter Fräsprozesse eine günstigere Zerspanbarkeit erreicht werden kann, ohne das Verschleißschutzpotential zu mindern.
Im vorliegenden Beitrag wird der Einfluss der mittels Legierungsmodifikation eingestellten Gefüge- und Ausscheidungsmorphologie auf die Zerspanung untersucht. Dies erfolgt anhand einer typischerweise für Schneckenmaschinen eingesetzte Verschließschutzlegierung zur Substitution entsprechender CoCr-Legierungen (Stellite), einer NiCrMoSiFeB-Legierung (Handelsname: Colmonoy 56 PTA). Durch metallurgische Untersuchungen und In-situ-Messung auftretender Prozesskräfte und Temperaturen an der Werkzeugschneide beim Fräsprozesses sowie der anschließenden Untersuchung von Werkzeugverschleiß und Oberflächenintegrität ist eine detaillierte Analyse und Korrelation zwischen den mikrostrukturellen Eigenschaften und der Zerspanbarkeit möglich. Die Vorgehensweise erlaubt einer Beurteilung des Einflusses der ultraschallunterstützten Fräsbearbeitung auf den Prozess sowie die resultierenden Oberflächenintegrität. Unter systematischer Anwendung dieser Methodik sowie der Berücksichtigung der Anbindung zum Stahlsubstratwerkstoff und der Wirksamkeit des Verschleißschutzes lässt sich letztlich eine gezielte Optimierung der Zerspanungssituation und des Verschleißschutzes erreichen. Die Erkenntnisse erlauben Handlungsanweisungen und Empfehlungen für Normen und Verarbeitungsrichtlinien, die besonders KMU eine sichere und wirtschaftliche Fertigung hochbelasteter Stahlkomponenten mit unkritischen, kostenreduzierten Werkstoffen ermöglichen sollen.
Reducing CO2 emissions to 62 percent up to 2030 and achieving greenhouse neutrality up to 2050 are the key goals of the EU's climate protection legislation. The expansion of technologies for climate-neutral energy generation is not the only important contribution to reducing greenhouse gases, the efficient use of material systems is also a key factor. In the area of plant engineering, steel components are provided with a wear-protection coating for efficient use to protect them against corrosive, tribological, thermal and mechanical stresses. The wear-protection coatings are primarily made of Co alloys, which are to be replaced by alternative materials, such as nickel alloys, because of the poor working conditions regarding the extraction of the cobalt and because of the health risks. In terms of corrosion behavior, many applications require a crack-free wear protection layer and additional machining. Machining by milling is not economical for wear materials, especially for SME because of the high tool wear, but it is essential to produce defined surfaces with high quality.
Alloy modifications of the filler metals for nickel-based plasma deposition welded wear protection coatings and the use of innovative ultrasonic-assisted milling processes are examined to determine how more favorable machinability can be achieved without reducing the wear protection potential. The focus is on the NiCrSiFeB alloy, which is intended to replace CoCr alloys in the area of screw machines. The modification of hard facing layers in terms of microstructure and precipitation morphology as well as suitability for machining is investigated and compared with the CoCr alloy. In this aspect, the alloy modifications are generated by a PTA process by systematically adjusting the preheating and interpass temperatures, a crack-free wear-resistant layer can be generated, which is subsequently machined by a milling process. In addition to the crack-free properties,
the microstructure, the bonding as well as the mixing between the NiCrFeB alloy and a 1.8550 as well as between the CoCr alloy and a 1.4828 are analyzed and compared in the joining areas. In addition, heating and cooling rates are determined and a chemical analysis of the weld metals is performed. This study provides important knowledge about the differences between NiCrFeB alloy and CoCr alloys in terms of microstructure morphology, bonding and mixing behavior in the joining zones to the basic material.
Alloy Modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. There is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining for a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA) is investigated. Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
Alloy Modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. There is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining for a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA) is investigated. Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
Alloy modification and ultrasonic assisted milling of wear resistant alloys with defined surfaces
(2023)
The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. In addition to increasing demands to replace conventional cobalt alloys with nickel alloys as a result of price and supply risks, there is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces.
A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process.
In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on machining is investigated. The alloy used is a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA). Through metallurgical investigations and in-situ measurement of cutting forces and temperatures at the cutting edge during the milling process as well as the subsequent investigation of tool wear and surface integrity, a detailed analysis and correlation between microstructural properties and machinability is feasible. The findings allow recommendations for standards and processing guidelines, enabling safe and economical production of highly stressed steel components with non-critical, cost-reduced materials.
In vielen Anwendungen werden aufgrund zunehmender Anforderungen an den Widerstand gegenüber hohen, kombinierten mechanischen, tribologischen, thermischen und korrosiven Beanspruchungen Hochleistungsle¬gierungen eingesetzt. Den vielfach komplexen Bauteilstrukturen, herausfordernden Fertigungseigenschaften und der Erhöhung der Ressourceneffizienz lässt sich heute mit der additiven Fertigung (AM) begegnen, dem oftmals noch unzureichende Kenntnisse über die resultierende Homogenität und Anisotropie der speziellen Gefüge und den damit verbundenen Eigenschaften entgegensteht. Viele Anwendungen benötigen zudem definierte Oberflächen mit hohen Anforderungen an die Oberflächenintegrität, dem durch komplementären Einsatz von additiven und abtragenden Fertigungsschritten Rechnung getragen wird. Hochleistungslegierungen auf der Basis von Nickel oder Kobalt sind infolge der niedrigen Wärmeleitfähigkeit verbunden mit hoher Festigkeit und Zähigkeit äußerst herausfordernd mit Blick auf eine wirtschaftliche Zerspanung mit geometrisch bestimmter Schneide. Ein Vorhaben (IGF-Nr. 20.979 N/DVS-Nr. 1.3211) der BAM und TU Clausthal/ISAF befasst sich mit der Lösung dieser Problemstellung durch gezielte Beeinflussung des Gefüges mittels Modifikation der Schweißzusatzwerkstoffe und den Einsatz des ultraschallunterstützten Fräsens (US), bei gleichzeitiger Sicherstellung der geforderten Eigenschaften der untersuchten Werkstoffe. Es werden die Ergebnisse der Mikrostruktur und der Zerspanbarkeit der Modifikationen der MSG-Schweißung der FeNi36-Referenzlegierung mit 0,4 Gew.-% Zr und der Modifikationen der MSG-Schweißung der CoCr-Referenzlegierung mit 1 Gew.-% Zr sowie Hf vorgestellt. Abschließend werden aus den Ergebnissen Handlungsempfehlungen abgeleitet.
Multiple principal element alloys (MPEA) represent a class of materials consisting of at least three alloying elements, each with 5 to 35 atomic %. The MPEAs encompass the so-called high-entropy (HEA) and medium-entropy alloys (MEAs) and are fundamentally different from conventional materials like the Fe-based steel. Within the last 20 years, highly innovative MPEA with individually adjustable properties for industrial applications were identified. However, the focus has been on pure material synthesis. With the increase in available material quantities, the focus is now on processing issues such as joining and welding. In that connection, the weldability of MPEAs has received very little attention so far and experience in dissimilar metal welds (DMWs) is lacking so far but. The present study summarizes comprehensive experimental results on the weldability of MPEA-DMWs and their resulting microstructure. For this purpose, two equiatomic MPEAs, CoCrFeMnNi (HEA) and CoCrNi (MEA) in cold-rolled and annealed conditions were joined by solid-state friction stir welding (FSW) to an austenitic stainless steel 316L. The DMWs showed very interesting microstructure features. In addition, the mechanical-technological properties were obtained by instrumented tensile tests, and the local straining was determined in-situ by digital image correlation (DIC). A significant influence of the FSW processing on the mechanical performance was identified,in terms of the formation of FSW-specific defects like whitebands or tunnel defects. The experiments proofed the general (but currently limited) FS weldability of the MPEAs to conventional austenitic steel grade AISI 304. This enables targeted further considerations of these highly innovative MPEAs.
Additive manufacturing (AM) processes enable the efficient production of advanced constructions. Direct energy deposition processes such as wire and arc-based additive manufacturing (DED-arc) are important methods. The wire filler metals enable a wide range of materials. In addition, the arc process provides a high deposition rate compared to laser and powder-based processes. Furthermore, components can be manufactured near-net-shape, offering significant savings in cost, time, and resources. Combined with the use of high-strength steels to reduce wall or component thicknesses in the context of lightweight design, great opportunities for saving energy and resources can be achieved. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times in the area of the top layer.
Influence of Residual Stresses on Stress Relief Cracking of Thick-Walled Creep-Resistant Steel Welds
(2023)
Controlling the residual stress level during welding of creep-resistant Cr-Mo-V steels is crucial to avoid so called stress relief cracking (SRC) during post weld heat treatment (PWHT) of large-scale components. In the present study, a laboratory scale test specimen (400 mm x 400 mm x 25 mm) was used to simulate thick-walled component welds made of 13CrMoV9-10. The aim was to identify the level and distribution of residual stresses to evaluate the suitability of the specimen for laboratory based SRC testing. High restraint was ensured by the specimen geometry with a narrow welding gap in the center. This gap was filled by submerged arc welding in a multi-layer technique. Two specimens were welded with identical parameters and compared in the as-welded state and after PWHT (705 °C for 10 h). Neutron diffraction was used to determine the residual stresses in the weld metal, the heat-affected zone (HAZ) and the base material at different depths longitudinal, transverse, and normal to the welding direction. The experiments were performed on the instrument E3 of the research reactor BERII of HZB Berlin, Germany. Complementarily, laboratory X-ray diffraction was applied to characterize the surface residual stresses. In the welded state, especially in the weld metal and the adjacent HAZ, the residual stress can reach the yield strength of the untreated material. The highest levels occur in the longitudinal direction. The transverse and normal directions are characterized by residual stress of lower magnitude. As expected, the residual stress is almost completely relieved after PWHT.
Die additive Fertigung (AM) durch schweißtechnische Verfahren eröffnet vielfach ökonomische Vorteile für eine ressourceneffiziente Bauteilherstellung. Gerade hinsichtlich der Homogenität und Anisotropie der resultierenden Schweißgefüge und den damit verbundenen Eigenschaften gibt es noch offene Fragestellungen. Die Einstellung der finalen Bauteilgeometrie und Oberflächengüte erfordert den komplementären Einsatz abtragender Fertigungsschritte. Hochleistungslegierungen auf der Basis von Nickel oder Kobalt sind aufgrund ihrer niedrigen Wärmeleitfähigkeit verbunden mit hoher Festigkeit und Zähigkeit schwer spanbar. Eine gezielte Gefügebeeinflussung mittels Modifikation der AM-Schweißzusatzwerkstoffe und der Einsatz des ultraschallunterstützten Fräsens (US) bietet das Potential insgesamt die Zerspanungssituation zu verbessern. Dieser Lösungsansatz unter Gewährleistung des Erhalts der geforderten Werkstoff- bzw. Bauteileigenschaften ist Untersuchungsgegenstand eines Gemeinschaftsvorhabens (IGF-Nr. 20.979 N/DVS-Nr. 1.3211) der BAM und TU Clausthal/ISAF. Der vorliegende Beitrag stellt Ergebnisse für die beiden untersuchten FeNi- und CoCr-Legierungen sowie wesentliche Zusammenhänge zwischen Legierungsmodifikation, entstehender Gefügemorphologie und Zerspanungseigenschaften der mittels MAG additiv gefertigter Proben vor. Das größte Potential für die Modifikation zeigten Zr und Hf. Die Zulegierung in das Schweißgut erfolgte durch Beschichtung von Massivdrähten sowie durch Herstellung von Fülldrähten.
Multielement-Legierungen (MPEA - Multiple Principal Element Alloys, gemeinhin auch als Hochentropielegierungen bezeichnet) stellen eine neue Klasse von Werkstoffen dar, die aus mindestens drei Legierungselementen mit jeweils 5 bis 35 Atom-% bestehen. Somit unterscheidet sich diese Legierungskonzept fundamental von konventionellen Werkstoffen wie Stahl oder Nickellegierungen. Hierzu werden die Legierungselemente gezielt ausgewählt und die Mikrostrukturen ein- und zum Teil auch mehrphasig eingestellt. Das Ziel ist dabei, hochinnovative MPEA mit individuell einstellbaren Eigenschaften für die industrielle Anwendung zu identifizieren. Dabei werden insbesondere Zielkonflikte, wie bspw. der Trade-off zwischen Festigkeit und Duktilität bei konventionellen Stählen, überwunden. Insbesondere die hohe mechanische Festigkeit bei höchster Korrosionsbeständigkeit sind bei bestimmten Legierungssystemen von hohem Interesse. Hier kann u.a. die Substitution klassischer hochlegierter Stähle oder von Ni-Basislegierungen perspektivisch erfolgen. In den letzten 20 Jahren lag der Fokus jedoch auf der reinen Materialsynthese. Mit der Zunahme verfügbarer Werkstoffquantitäten, stehen Verarbeitungsfragen, wie werkstoff- und beanspruchungsgerechte Füge- bzw. Schweißverfahren jetzt im Mittelpunkt. Der Schweißeignung von MPEA wurde bis Ende 2022 nur äußert wenig Aufmerksamkeit zuteil. Erfahrungen zu Mischverbindungen (sogenannte DMWs - Dissimilar Metal Welds) fehlen dabei vollständig, sind jedoch essenziell für die Anwendung dieser Werkstoffe in Verbindung mit konventionellen Werkstoffen. Die vorliegende Studie präsentiert erstmals im deutschen Sprachraum, die umfassenden experimentellen Ergebnisse zur Schweißeignung von MPEA-Mischverbindungen und der resultierenden Mikrostruktur. Dazu wurden zwei äquiatomare MPEAs CoCrFeMnNi (Hochentropie-) und CoCrNi (Mittelentropielegierung) mittels WIG- und Rührreibschweißen mit einem konventionellen, hochlegierten und austenitischen Cr-Ni-Stahl (1.4301) gefügt. Die erstmals untersuchten DMWs resultierten dabei in sehr interessanten Mikrostrukturen, mechanisch-technologische Eigenschaften wurden durch instrumentierte Zugversuche gewonnen, die gleichzeitig der Ermittlung der lokalen Verformung im Schweißnahtbereich dienten (durch Verwendung der berührungslosen DIC-Digital Image Correlation-Technik). Dabei zeigt sich für beide Schweißverfahren eine Erweichung in der WEZ der MPEAs sowie eine geringfügig verminderte Zugfestigkeit. Durch die Experimente konnte der prinzipielle Nachweis der Schweißeignung der MPEAs für DMWs mit konventionellen Werkstoffen erbracht werden, die auch eine dementsprechende mechanische Beanspruchbarkeit ermöglichen. Dies ermöglicht zielgerichtete weitere Betrachtungen dieser höchst innovativen Werkstoffe.
Dissimilar metal TIG weld joints of multiple principal element alloys (MPEA) to austenitic steel 304
(2023)
Multi-element alloys (MPEA - Multiple Principal Element Alloys) represent a new class of materials consisting of at least three alloying elements, each with 5 to 35 atomic %. This material class includes high-entropy alloys (HEA, with n ≥ 4 elements). The underlying alloying concept differs fundamentally from conventional materials such as the Fe-based steel. For this purpose, the alloying elements are specifically selected, and the microstructures are adjusted in a single-phase and, in some cases, multi-phase manner. The aim is to identify highly innovative MPEA with individually adjustable properties for industrial applications. In the last 20 years, however, the focus has been on pure material synthesis. With the increase in available material quantities, the focus is on processing issues such as joining and welding processes. In that connection, the weldability of MPEAs has received very little attention so far. Experience with dissimilar metal welds (DMWs) is completely lacking but is essential for the application of these materials if joint to conventional materials. This study presents selected experimental results on the weldability of MPEA-DMWs and the resulting microstructures. For this purpose, the equiatomic CoCrFeMnNi (HEA) was investigated in cold-rolled (CR) and heat-treated (HT) condition and joined by tungsten inert gas (TIG) welding to an austenitic stainless steel 304. The DMWs showed defect-free conditions (no lack of fusion, cracks and so on), whereas the cold-rolling increases the microhardness. The global mechanical properties were obtained by instrumented tensile tests of cross-weld samples and showed sufficient yield and tensile strength comparable to that of the individual base materials (BM). The local strain conditions were determined by digital image correlation and showed the highest local strains to occur in the intermixed weld metal. Indeed, the preferred fracture location of the cross-weld tensile samples was in the weld metal. Finally, the experiments proofed the weldability of the MPEAs to conventional 304. This enables targeted further considerations for example as structural materials.
Design and construction of a rainfall simulator to test metal runoff at atmospheric conditions
(2023)
A rainfall simulator was presented as an environmental assessment tool to quantify wash-off concentrations from metallic materials. It is part of the RUNOFF-project, which studies and re-assesses the durability of roofing and facade materials under current atmospheric conditions in Germany.
Studying building materials is important as they have a significant impact on achieving a variety of goals and targets within the sustainable developments goals (SDGs). The durability of materials is essential to reach sustainability. However, the durability of metallic materials is strongly depended on climate conditions, which have changed as a result of technical measures in industry, climate change and increasing urbanisation. In Germany at least, the data base is not up-to-date leading to prediction models regarding corrosion resistance and durability of metallic materials which can no longer be trusted and therefore need to be re-assessed and updated. Also, not only the demand for sustainable but also environmentally friendly building materials has increased dramatically. A number of construction materials produce chemical hazards, and therefore have negative impacts on water quality, soils health and ecosystems. To limit these impacts, environmental assessment methods and tools are needed to measure and quantify the inputs and outputs of building materials throughout their lifetime.
Mikrolegierungselemente, wie Nb und Ti, sind für die signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Nominalstreckgrenze ≥ 690 MPa unerlässlich. Normvorgaben zur chemischen Zusam-mensetzung geben dabei nur obere Grenzwerte für die Hersteller vor. Weiterhin wirken sich bereits kleine Abwei-chungen in der Legierungsroute teilweise drastisch auf die mechanischen Eigenschaften aus. Somit wird eine adä-quate Vorhersage der Schweißeignung und der Integrität der Schweißverbindung aufgrund der variierenden Mikro-gefüge erschwert bis unmöglich. Unerwünschte Nebeneffekte sind die mögliche Erweichung der Wärmeeinflusszone (WEZ) als auch der gegenteilige Effekt der Aufhärtung.
Multiple principal element alloys (MPEA) encompass the well-known high entropy alloys (HEAs). MPEA/HEA represent a new class of materials consisting of at least three alloying elements, each containing 5 to 35 at.-%. This alloying concept thus differs fundamentally from conventional materials such as steel or nickel alloys. For this purpose, the alloying elements are specifically selected, and the microstructures are adjusted in a single-phase and, in some cases, multi-phase manner. In particular, conflicting goals, such as the trade-off between strength and ductility in conventional steels, are overcome. In the last 20 years, however, the focus has been on material synthesis. With the increase in available material quantities, the focus is now on pro-cessing issues such as joining and welding processes. The weldability of MPEA has received very little atten-tion so far. Experience with dissimilar metal welds (DMWs) is completely lacking but is essential for the appli-cation of these materials in combination with conventional materials. The present study presents, comprehen-sive experimental results on the weldability of MPEA-DMWs. For that purpose, a Co20Cr20Fe20Mn20Ni20 HEA in cold-rolled and heat-treated condition was joined by means of tungsten inert gas welding (TIG) with the austenitic Cr-Ni steel AISI 304. The DMWs resulted in interesting mechanical properties. They were obtained by instrumented tensile tests as well as the local deformation in the weld area by using digital image correlation (DIC) technique. A significant softening in the heat-affected zone (HAZ) of the MPEAs as well as a slightly reduced tensile strength with a significant decrease of the elongation at fracture were found. The experiments provided proof in principle of the weldability of the MPEAs for DMWs with conventional materials that ensure a corresponding capability for mechanical loading. This allows further considerations on the application of these innovative materials.
High-strength steels offer great potential in weight-optimised modern steel structures. Additive manufacturing processes, such as Wire Arc Additive Manufacturing (WAAM), enable near-net-shape manufacturing of complex structures and more efficient manufacturing, offering significant savings in costs, time, and resources. Suitable filler materials for WAAM are already commercially available. However, the lack of knowledge or technical guidelines regarding welding residual stresses during manufacturing and operation in connection with cold cracking risk limit their industrial application significantly. In a project of BAM and TU Chemnitz, the influences and complex interactions of material, manufacturing process, design and processing steps on residual stress evolution are investigated. By developing process recommendations and a special cold cracking test, economic manufacturing, and stress-appropriate design of high-strength steel WAAM components are main objectives.
The present study focuses on determining the influence of heat control (interpass temperature, heat input, cooling time) and the design aspects of the components on the hardness and residual stresses, which are analysed by X-ray diffraction. Defined reference specimens, i.e., hollow cuboids, are automatically welded with a special WAAM solid wire. The influences of wall length, wall thickness and wall height on the residual stresses are analysed. Geometric properties can be selectively adjusted by wire feed and welding speed but cannot be varied arbitrarily. This was addressed by adapted build-up strategies. The results indicate a significant influence of the heat control and the wall height on the residual stresses. The interpass temperature, wall thickness and wall length are not significant. These analyses allow recommendations for standards and manufacturing guidelines, enabling a safe and economic manufacturing of high-strength steel components.
Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann.
Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann.
Das DVS-Vorhaben 01.3211 „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ ist ein Kooperationsprojekt der Bundesanstalt für Materialforschung und -prüfung (BAM) und dem Institut für Schweißtechnik und Trennende Fertigungsverfahren (ISAF) der Technischen Universität Clausthal. Das Übergeordnete Projektziel ist das Erlangen von Erkenntnissen für eine sichere und wirtschaftliche, kombinierte additive und abtragende Fertigung aus kostenintensiven Werkstoffen hochbelasteter Komponenten insbesondere für KMU. Dabei stehe die beiden Werkstoffe CoCr26Ni9Mo5W (2.4681) und FeNi36 (1.3912) im Fokus. Mittels Modifikation der Schweißzusätze sind homogen und isotrop ausgeprägte Werkstoffeigenschaften und eine Erhöhung der Prozessstabilität und Fertigungsfreiheitsgrade bei der additiven Fertigung erzielbar. Darüber hinaus wird der Einfluss nachfolgender abtragender Bearbeitungsschritte des ultraschallunterstützen und des konventionellen Fräsprozesses untersucht. Die mit dem Forschungsvorhaben verbundenen Nutzen für KMU sind die Stärkung der Innovationsfähigkeit und der Wirtschaftlichkeit sowie die Erhöhung der Wettbewerbsfähigkeit. In AP-3 wurden die Mikrostruktur der MSG-Schweißung der CoCr-Referenzlegierung untersucht. In AP-4 wurden Zerspanversuche an der MSG-Schweißung der CoCr-Referenzlegierung durchgeführt.
High entropy alloys (HEA) are a new class of materials that have been investigated since the early 2000s and offer great potential to replace conventional alloys. However, since they sometimes have significant contents of expensive alloying elements such as Co or Ni, their use is only conceivable in highly stressed areas of components. For this purpose, the weldability with conventional alloys such as high-alloy austenitic steels must be investigated. In addition to the resulting microstructure, the mechanical properties are also fundamental for the usability of HEAs in DMWs. For this purpose, TIG welds of CoCrFeMnNi HEA (cold rolled and recrystallized state) with AISI 304 austenitic steel are investigated. These mechanical properties are analyzed in this work by means of tensile tests and local hardness measurement. The local strain behavior of the welded joints is also characterized by means of Digital Image Correlation (DIC). The results of the local hardness measurement show a clear influence of the initial condition of the HEA on the HAZ. Thus, the HEA in the cold-rolled condition shows a clear softening because of recrystallization processes in the HAZ. On the other hand, there is no influence on the hardness of the weld metal, which is approx. 200 HV0.1 in both cases. The tensile tests show a consistent failure of the weld in the weld metal. However, regardless of the HEA condition, strengths in the range of the recrystallized HEA (RM ~ 550–600 MPa) are achieved, although with significantly reduced fracture elongations.
Einfluss der Schweiß- und Prüfparameter bei der Heißrissbewertung hochfester Schweißzusatzwerkstoffe
(2023)
Die Heißrissneigung beim Schweißen kann mittels einer ganzen Reihe von Prüfverfahren ermittelt werden. Eine etablierte Methode ist die sogenannte Varestraint-Prüfung, welche auch an der Bundesanstalt für Materialforschung und -prüfung (BAM) als modifizierter Varestraint/Transvarestraint-Test (MVT) zum Einsatz kommt. Die Ergebnisse von Varestraint-Prüfungen hängen jedoch stets in unterschiedlichem Maße von der individuellen Prüfmaschinenauslegung und den verwendeten Prüfparametern ab. Dies kann zu einer uneinheitlichen Bewertung des Rissverhaltens führen, wenn die Risslänge konventionell als Kriterium für die Rissneigung herangezogen wird. Scheinbare Abhängigkeiten von Prozessparametern erschweren dann die Interpretation der Ergebnisse. Eine neuartige Bewertungsmethodik entkoppelt den Maschineneinfluss vom Materialverhalten und verwendet die Dehnrate als Risskriterium in Analogie zu Prokhorovs Heißrissmodell. Die neue Auswertung wird anhand einer Studie hochfester Schweißzusatzwerkstoffe vorgestellt, deren Rissverhalten in Abhängigkeit der chemischen Zusammensetzung und der Schweißparameter bewertet wird.
High-strength fine-grained structural steels have great potential for modern weight optimized steel construc-tions. Efficient manufacturing and further weight savings are achievable due to Wire Arc Additive Manu-facturing (WAAM). First commercial high-strength welding consumables for WAAM are already available. However, the application is still severely limited due to a lack of knowledge and guidelines for the industry regarding welding residual stresses and component safety in manufacturing and operation. Residual stresses may be critical regarding the special microstructure of high-strength steels in context with the risk of cold cracking and component performance in service. Therefore, process- and material-related influences, as well as the design effects on residual stress formation and cold cracking, are being investi-gated in a research project (IGF 21162 BG) focusing a high-strength WAAM welding consumable with yield strength of over 800 MPa. Objectives are the establish-ment of special WAAM cold cracking tests and pro-cessing recommendations allowing economical, suita-ble, and crack-safe WAAM of high-strength steels. First studies on process-related influences showed transfor-mation residual stresses arising during cooling, which significantly influence stress evolution of the compo-nent during layer-wise build-up. This has not yet been investigated for WAAM of high-strength steels. Focus of this study is on the systematic investigation of interactions of the WAAM welding process and design with cooling time, hardness, and residual stresses.
Defined open hollow cuboids were welded and investi-gated under systematic variation (design of experi-ments, DoE) of the scale/dimensions (cf. Fig. 1a) and heat control (interlayer temperature Ti: 100–300 °C), heat input E: 200–650 kJ/m. The welding parameters were kept constant as possible to avoid any influence by the arc and the material transfer mode. The heat input adjusted primarily via the welding speed. The resulting different weald bead widths were considered by different build-up strategies (weld beads per layer) to ensure defined wall thicknesses. The hardness was determined on cross-sections taken from the manufac-tured hollow cuboids (Fig. 1c) and the analysis of the residual stress state was carried out by means of X-ray diffraction (XRD) at defined positions on the lateral wall (Fig. 1b).
The hardness is higher at the top compared to the lower weld beads, as shown in Fig. 1c exemplarily for central test parameters of the DoE = 425 kJ/mm, Ti = 200 °C). This may be attributed to the specific heat control of the top weld beads, i.e., quenching effects, which are not tempered by weld beads above as is the case for lower weld beads implying a higher hardness. It was observed that the hardness level decreases with increasing energy per unit length, while the in-terpass temperature has a rather low influence on the hardness
Residual stress analysis was performed on the lat-eral wall in the welding direction, cf. Fig. 1b, to deter-mine the influence of heat control and design. In the top area of the wall, maximum longitudinal residual stress-es of up to over 500 MPa exhibit, which corresponds to approx. 65% of the nominal yield strength of the mate-rial. The statistic evaluation of stress levels in welding direction of all test specimens show that adaption of heat input may reduce welding stresses up to 50%. In-terpass temperature has less pronounced effect on cool-ing times, microstructure, and on the residual level within parameter matrix. Overall, the results show a significant influence of heat input and component di-mensions on the residual stresses and minor effect of the interpass temperature. Hence, the properties of the specimens may be effectively adjusted via heat input. The working temperatures should be considered for global shrinkage behavior or restraints. Such investiga-tions of residual stress are necessary to further deter-mine local and global welding stresses regarding the consequences on the component safety during manu-facturing and service.
Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf die Abkühlbedingungen, Gefüge, mechanisch-technologischen Eigenschaften und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung und Probenabmessungen werden innerhalb eines statistischen Versuchsplans variiert. Die Schweißwärmeführung wird dabei so eingestellt, dass die t8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) sichergestellt sind. Hierzu ließen sich über zusätzliche thermo-physikalische Umformsimulationen mittels Dilatometer die komplexen Wärmezyklen abbilden und die resultierende Zugfestigkeit des Schweißgutes bestimmen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein.
Im Rahmen der Normungssitzung werden praktikable Verarbeitungsempfehlungen basierend auf den Erkenntnissen des Vh. mit Vertretern aus Industrie und Forschung diskutiert.