9 Komponentensicherheit
Filtern
Erscheinungsjahr
- 2023 (3) (entfernen)
Dokumenttyp
- Vortrag (3)
Sprache
- Englisch (3)
Referierte Publikation
- nein (3)
Schlagworte
- Digital image correlation (2)
- AISI 316L (1)
- Additive Manufacturing (1)
- Adiabatic shear bands (1)
- Computed Tomography (1)
- Creep (1)
- Dissimilar metal weld (1)
- Finite element analysis (1)
- Gradient-enhanced damage (1)
- Laser Powder Bed Fusion (1)
- Mechanical properties (1)
- Microstructure (1)
- Multi-principal element alloys (1)
- PBF-LB/M/316L (1)
- Split Hopkinson bar (1)
- Viscoplasticity (1)
- Welding (1)
Organisationseinheit der BAM
- 5 Werkstofftechnik (3) (entfernen)
Eingeladener Vortrag
- nein (3) (entfernen)
The damage mechanisms of metallic components produced by process laser powder bed fusion differ significantly from those typically observed in conventionally manufactured variants of the same alloy. This is due to the unique microstructures of additively manufactured materials. Herein, the focus is on the study of the evolution of creep damage in stainless steel 316L specimens produced by laser powder bed fusion. X-ray computed tomography is used to unravel the influence of the process-specific microstructure from the influence of the initial void distribution on creep damage mechanisms. The void distribution of two specimens tested at 600 °C and 650 °C is analyzed before a creep test, after an interruption, and after fracture. The results indicate that the formation of damage is not connected to the initial void distribution. Instead, damage accumulation at grain boundaries resulting from intergranular cracking is observed.
The essence of dynamic failure is closely linked to the formation of adiabatic shear bands (ASB), which result from the localization of shear strain under high deformation speeds accompanied by a rapid temperature increase. Understanding this phenomenon is crucial in view of safety issues when impacts of fast rotating machine components (i.e. aircraft turbine blades) may occur. Our contribution addresses both the experimental evidence and characterization of ASBs due to high-speed impact tests at the Split HOPKINSON pressure bar (SHPB) setup and the finite element analysis to determine the parameters of the underlying constitutive model, which is closely related to JOHNSON-COOK (JC) material model.
Experimental investigations were performed on notched shear specimens made of the fine -grained structural steel S690QL and the displacements in the regions affected by shear localization were measured with subset-based local Digital Image Correlation (DIC). The displacement fields, obtained in the SHPB tests, were considered as an objective to validate and to identify the constitutive parameters with. The JC model could reasonably reproduce the displacement distribution. In order to overcome the issues with mesh dependency we provide a nonlocal extension based on the implicit gradient model approach.
High entropy alloys (HEA) are a new class of materials that have been investigated since the early 2000s and offer great potential to replace conventional alloys. However, since they sometimes have significant contents of expensive alloying elements such as Co or Ni, their use is only conceivable in highly stressed areas of components. For this purpose, the weldability with conventional alloys such as high-alloy austenitic steels must be investigated. In addition to the resulting microstructure, the mechanical properties are also fundamental for the usability of HEAs in DMWs. For this purpose, TIG welds of CoCrFeMnNi HEA (cold rolled and recrystallized state) with AISI 304 austenitic steel are investigated. These mechanical properties are analyzed in this work by means of tensile tests and local hardness measurement. The local strain behavior of the welded joints is also characterized by means of Digital Image Correlation (DIC). The results of the local hardness measurement show a clear influence of the initial condition of the HEA on the HAZ. Thus, the HEA in the cold-rolled condition shows a clear softening because of recrystallization processes in the HAZ. On the other hand, there is no influence on the hardness of the weld metal, which is approx. 200 HV0.1 in both cases. The tensile tests show a consistent failure of the weld in the weld metal. However, regardless of the HEA condition, strengths in the range of the recrystallized HEA (RM ~ 550–600 MPa) are achieved, although with significantly reduced fracture elongations.