7.5 Technische Eigenschaften von Polymerwerkstoffen
Filtern
Dokumenttyp
- Vortrag (106)
- Beitrag zu einem Tagungsband (28)
- Posterpräsentation (28)
- Zeitschriftenartikel (10)
- Buchkapitel (9)
- Beitrag zu einem Sammelband (2)
- Zeitschriftenheft (Herausgeberschaft für das komplette Heft) (2)
- Forschungsdatensatz (2)
- Monografie (1)
- Dissertation (1)
Sprache
- Englisch (135)
- Deutsch (54)
- Mehrsprachig (1)
Referierte Publikation
- nein (190) (entfernen)
Schlagworte
- Flame retardant (18)
- Flame retardancy (13)
- Additive Fertigung (10)
- Evacuation (9)
- Graphene (9)
- Künstliche Bewitterung (9)
- Durability (8)
- Flammability (8)
- Flammschutz (8)
- Pyrolysis (8)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (190)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (190)
- 6 Materialchemie (19)
- 5 Werkstofftechnik (17)
- 5.3 Polymere Verbundwerkstoffe (17)
- 6.6 Physik und chemische Analytik der Polymere (17)
- 3 Gefahrgutumschließungen; Energiespeicher (13)
- 8 Zerstörungsfreie Prüfung (13)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (11)
- 8.0 Abteilungsleitung und andere (10)
Eingeladener Vortrag
- nein (106)
Die Präsentation gibt einen Überblick über die Arbeiten im German Pilot des EU-Projekts TREEADS. Es werden klein-, mittel- und großskalige Versuche an Waldboden mit einheimischer Vegetation durchgeführt. Begleitend werden numerische Untersuchungen durchgeführt, die eine Variation der Parameter, wie Bodenfeuchte, Temperaturen und Wind über die Experimente hinaus erlauben. Die gemessenen Materialparameter dienen als Input für die numerischen Berechnungen. Die numerischen Modelle werden mit den mittel- und großskaligen Experimenten validiert.
Weltweit stellen Waldbrände eine große Bedrohung für Umwelt, Wirtschaft und menschliches Leben dar. Der fortschreitende Klimawandel verstärkt Trockenheit und Dürre, wodurch die Größe und Intensität von Waldbränden sowie das daraus resultierende Gefahrenpotential zusätzlich erhöht werden. Um im Risikofall eine schnelle und effektive Waldbrandbekämpfung zu gewährleisten, sollen Einsatzkräfte in Zukunft von KI-basierten Ausbreitungsmodellen unterstützt werden.
Der Einsatz von maschinellem Lernen ermöglicht dabei schnelle und zielgerichtete Ausbreitungsvorhersagen in Echtzeit, die in den Prozess der Brandbekämpfung als zusätzliche Information einfließen können. Im Rahmen des durch das EU-Förderprogram Horizon 2020 finanzierte Projekt TREEADS wird ein solches Modell für Europa entwickelt.
Dazu wird mit verschiedenen Satellitendaten des Copernicus-Programms und der NASA ein auf räumlicher und zeitlicher Ebene aufgelöster Datensatz zu europäischen Waldbränden aufgebaut. Zu den erfassten Waldbränden werden wichtigen Faktoren, die Einfluss auf die Brandausbreitung haben, ergänzt. Dazu gehören das von Copernicus bereitgestellte, digitale Geländemodell Europas und verschiedene, von Sentinel-2 Messungen abgeleitete Informationen zu Vegetation und Landnutzung. Dieser 2D-Trainingsdatensatz zu realen Waldbränden wird durch die zeitlich hochaufgelösten, meteorologischen Reanalyse-Produkte – Copernicus European Regional ReAnalysis (CERRA) und ERA5-Land – vervollständigt und ist die Grundlage für ein Modell zur Ausbreitungsvorhersage von Waldbränden.
Methoden des Maschinellen Lernens können komplexe Muster in den gesammelten Daten erkennen und so zu einer verbesserten Vorhersage der Brandausbreitung beitragen. Die vielfältigen, von Copernicus bereitgestellten Daten sind dabei ein unabdingbarer Bestandteil des Modells, mit dem den Einsatzkräften ein zusätzliches Tool für den effizienten Einsatz ihrer limitierten Ressourcen zur Verfügung steht.
Die Umweltwirkungen auf ein Material werden als Überlapp der Funktionskurven von Materialempfindlichkeit und einwirkenden Umweltparametern betrachtet. Wenn entweder die Empfindlichkeit oder die Beanspruchungen Null sind, ergibt sich auch keine Umweltwirkung und bei beidseitig Werten größer Null das jeweilige Produkt der beiden. Die Akkumulation der nicht-reversiblen Effekte über die Zeit und allen Eigenschaftsänderungen entspricht der Alterung des Materials für den jeweiligen Expositionszeitraum.
Die digitale Umweltsimulation gliedert sich hier in drei Teilaspekte. Ein erster, rein materialwissenschaftlicher Teil hat die Aufgabe, alle relevanten Materialempfindlichkeiten experimentell zu quantifizieren. Ein zweiter – unter Umständen numerischer Teil – hat die Aufgabe, das Bauteil und seine Einbaulage zu digitalisieren und aus den makroskopischen Umgebungsbedingungen die relevanten mikroklimatischen Umweltparameter für alle Oberflächen- oder Volumenelemente zu bestimmen. In einem dritten Teil werden die Einwirkungen über den betrachteten Zeitraum berechnet und kumuliert. Dieses Konzept, das auf den so genannten Expositions-Reaktions-Funktionen (ERF) basiert, wird an Beispielen der Photoxidation erläutert. Dieses Vorgehen wurde schon beim ViPQuali-Projekt als Numerische Umweltsimulation umgesetzt.
Überprüft werden muss das Modell unbedingt an einer realitätsnahen Validierungsbeanspruchung. Hier werden die ermittelten ERFs mit über den kompletten Beanspruchungszeitraum geloggten Umweltparametern gekoppelt, um die berechnete mit der experimentell erfahrenen Alterungswirkung zu vergleichen. Nur so kann sichergestellt sein, dass alle für die Anwendungsumgebung relevanten Materialempfindlichkeiten einbezogen wurden.
This is the stable version of the full-notch creep test ontology (OntoFNCT) that ontologically represents the full-notch creep test. OntoFNCT has been developed in accordance with the corresponding test standard ISO 16770:2019-09 Plastics - Determination of environmental stress cracking (ESC) of polyethylene - Full-notch creep test (FNCT).
The OntoFNCT provides conceptualizations that are supposed to be valid for the description of full-notch creep tests and associated data in accordance with the corresponding test standard. By using OntoFNCT for storing full-notch creep test data, all data will be well structured and based on a common vocabulary agreed on by an expert group (generation of FAIR data) which is meant to lead to enhanced data interoperability. This comprises several data categories such as primary data, secondary data and metadata. Data will be human and machine readable. The usage of OntoFNCT facilitates data retrieval and downstream usage. Due to a close connection to the mid-level PMD core ontology (PMDco), the interoperability of full-notch creep test data is enhanced and querying in combination with other aspects and data within the broad field of materials science and engineering (MSE) is facilitated.
The class structure of OntoFNCT forms a comprehensible and semantic layer for unified storage of data generated in a full-notch creep test including the possibility to record data from analysis and re-evaluation. Furthermore, extensive metadata allows to assess data quality and reliability. Following the open world assumption, object properties are deliberately low restrictive and sparse.
Die Umweltwirkungen auf ein Material werden als Überlapp der Funktionskurven von Materialempfindlichkeit und einwirkenden Umweltparametern betrachtet. Wenn entweder die Empfindlichkeit oder die Beanspruchungen Null sind, ergibt sich auch keine Umweltwirkung und bei beidseitig Werten größer Null das jeweilige Produkt der beiden. Die Akkumulation der nicht-reversiblen Effekte über die Zeit und allen Eigenschaftsänderungen entspricht der Alterung des Materials für den jeweiligen Expositionszeitraum.
Die digitale Umweltsimulation gliedert sich hier in drei Teilaspekte. Ein erster, rein materialwissenschaftlicher Teil hat die Aufgabe, alle relevanten Materialempfindlichkeiten experimentell zu quantifizieren. Ein zweiter – unter Umständen numerischer Teil – hat die Aufgabe, das Bauteil und seine Einbaulage zu digitalisieren und aus den makroskopischen Umgebungsbedingungen die relevanten mikroklimatischen Umweltparameter für alle Oberflächen- oder Volumenelemente zu bestimmen. In einem dritten Teil werden die Einwirkungen über den betrachteten Zeitraum berechnet und kumuliert. Dieses Konzept, das auf den so genannten Expositions-Reaktions-Funktionen (ERF) basiert, wird an Beispielen der Photoxidation erläutert. Dieses Vorgehen wurde schon beim ViPQuali-Projekt als Numerische Umweltsimulation umgesetzt.
Überprüft werden muss das Modell unbedingt an einer realitätsnahen Validierungsbeanspruchung. Hier werden die ermittelten ERFs mit über den kompletten Beanspruchungszeitraum geloggten Umweltparametern gekoppelt, um die berechnete mit der experimentell erfahrenen Alterungswirkung zu vergleichen. Nur so kann sichergestellt sein, dass alle für die Anwendungsumgebung relevanten Materialempfindlichkeiten einbezogen wurden.
The dripping behaviour of polymers is often observed experimentally through the UL94 flammability standard test. In this work, polymeric dripping under fire is investigated numerically using particle finite element method. A parametric analysis was carried out to observe the influence of a single property on overall dripping behaviour via a UL94 vertical test model. Surrogates and property ranges were defined for variation of the following parameters: glass transition temperature (Tg), melting temperature (Tm), decomposition temperature (Td), density (ρ), specific heat capacity (Cp), apparent effective heat of combustion of the volatiles, char yield (μ), thermal conductivity (k), and viscosity (η). Polyamide, poly(ether ether ketone), poly(methyl methacrylate), and polysulfone were used as benchmarks. Simulated results showed that specific heat capacity, thermal conductivity, and char yield allied with viscosity were the properties that most influenced dripping behaviour (starting time and occurrence).
EPDM, HNBR and FKM materials were exposed at 150 ◦C to air under atmospheric pressure and to hydrogen at 50 bar for different ageing times. All measurements after hydrogen exposure were conducted on samples in degassed condition to assess irreversible effects resulting from that exposure and to compare them to those after ageing in air. Density, hardness, tensile properties, compression set, and hydrogen permeability of all samples were analysed. In both ageing environments, HNBR exhibited the most significant changes of material properties.
However, for both EPDM and HNBR, considerably less severe ageing effects were observed under hydrogen in comparison to ageing in air. On the other hand, FKM showed about the same low level of deterioration in both ageing environments but exhibited poor resistance against damage due to rapid gas decompression in hydrogen environment that can lead to seal failure. The obtained results may serve as a guidance toward a better understanding for design and utilisation of elastomeric materials in future hydrogen infrastructure components.
The residual post-fire mechanical properties of fiber-reinforced epoxy composites are influenced by their fire residues after burning. This study uses intumescent/low-melting glass flame retardants to tailor fire residues in epoxy resin. Processibility of prepregs and their quality are analysed for transfer of the flame-retardant epoxy resins to layered glass-fiber reinforced composites. Minimal effects were found on the pre-fire flexural strengths of the composites due to low loading of the flame retardants. However, when transferred to glass-fiber reinforced composites, the fire residues diminish significantly. Further studies are required to improve theoretical and experimental estimations of the post-fire mechanics of the composites.
The residual post-fire mechanical properties of fiber-reinforced epoxy composites are influenced by their fire residues after burning. This study uses intumescent/low-melting glass flame retardants to tailor fire residues in epoxy resin. Processibility of prepregs and their quality are analysed for transfer of the flame-retardant epoxy resins to layered glass-fiber reinforced composites. Minimal effects were found on the pre-fire flexural strengths of the composites due to low loading of the flame retardants. However, when transferred to glass-fiber reinforced composites, the fire residues diminish significantly. Further studies are required to improve theoretical and experimental estimations of the post-fire mechanics of the composites.
The transfer of flame-retardant epoxy resin formulations to composites for structural and lightweight applications in the energy and transport sector can be complex and requires systematic investigation. Here, uncoated and silane-coated ammonium polyphosphate (APP, Si-APP) intumescent compounds are transferred to prepregs using a Bisphenol A diglycidyl ether (DGEBA) resin matrix to 0/90o bidirectional glass fibers with an aerial weight of 600 g/m2. Inorganic silicates (InSi) are added to improve the fire residues of the composites after combustion and the total amount of flame retardants in the resin formulations was 10% by weight. The prepregs' fiber volume content (FVC) is corroborated using in-process measurements and thermogravimetric analysis. This was found to be approximately 60% for the composites containing APP, which is ideal for load-bearing applications with high mechanical strength. However, the Si-APP containing prepregs showed an inconsistent FVC potentially due to interactions with the commercial sizing of the glass fibers. The composites subsequently prepared are analysed for potential filtration effects of the additives via SEM after immobilization in a cured resin and platinum sputtering. The inter-laminar shear strength and the mechanical strength of the composites are compared via three-point bending tests. Additionally, the fire performance of the composites is analysed using cone calorimetry. It was found there was minimal impact of the loading of the flame retardants on the delamination of the composites and the flexural strength. However, the high density of the glass fibers possibly results in a suppression of the mode of action of the flame retardants in the composites. Therefore, the fire residues of the composites are further compared using SEM, and the flame-retardant modes of action upon transfer are investigated.
Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. These polymers are characterized by a high permeability and reasonable permselectivity. The latter point is somehow surprising because for microporous systems a more Knudson-like diffusion is expected then a size dependent temperature activated sieving process. It was argued in the framework of a random gate model that molecular fluctuations on a time scale from ps to ns are responsible for the permselectivity.
Here series of polymers of intrinsic microporosity (PIMs) as well as microporous polynorbornenes with bulky Si side groups and a rigid backbone are considered. The polymers have different microporosity characterized by high BET surface area values.
First inelastic time-of-flight neutron scattering measurements were carried out to investigate the low frequency density of state (VDOS). The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. It was found that the frequency of the maximum position of the Boson peak correlates with the BET surface area value.
Secondly elastic scans as well as quasielastic neutron scattering measurements by a combination of neutron time-of-flight and backscattering have been out. A low temperature relaxation process was found for both polymers. This process was assigned to the methyl group rotation. It was analysed in terms of a jump diffusion in a three-fold potential. The analysis of the dependence of the elastic incoherent structure factor on the scattering vector yields the number of methyl groups which might be immobilized.
The neutron scattering experiments were accompanied by fast scanning calorimetry and broadband dielectric investigations as well as atomistic molecular dynamic simulations.
Leather is a widely used material for thousands of years and in modern days it is produced on industrial scale. This production produces high amounts of organic waste during the tannery process. These fibers can become a resource and act as a multi-functional bio-filler in flame retardant composites.
This project investigates two leather fibers towards their ability to enhance the flame-retardancy in different composites. These composites use ammonium polyphosphate (APP) or aluminum trihydroxide (ATH) as flame retardants. Different silicon based synergists support polymers with ATH to reduce the load of flame retardant. The different modes of action (charring, gas phase activity, barrier effect) can be quantified of each composite.
The new composites form a stable char layer resulting in an increase in residue, lower peak heat release rates (pHRR) and higher limiting oxygen index (LOI). In addition, the ratings in the UL94-classification increased up to V-0.
Short overview is given of BAM's research within the topic "Flame Retardancy of Polymeric Materials". Fire science is identified as a crucial compentenc of BAM following our mission "Safety in Technology and Chemistry". In the area of polymers we work interdisciplinary, in the dimensions from nm to 2m, and we love to combine experiment and simulation. Multimethodical examples are given to describe the burning phenomena and flame-retardant modes of action. Further some examples are presented for tailored bench-scale fire testing and assessing concepts. Our goal is to provide the fundaments for a evidenced-based development of future materials.
The dataset provided in this repository comprises data obtained from a series of full-notch creep tests (FNCT) performed on selected high-density polyethylene (PE-HD) materials (for further details, see section 1 Materials in this document) in accordance with the corresponding standard ISO 16770.
The FNCT is one of the mechanical testing procedures used to characterize polymer materials with respect to their environmental stress cracking (ESC) behavior. It is widely applied for PE-HD materials, that are predominantly used for pipe and container applications. It is based on the determination of the time to failure for a test specimen under constant mechanical load in a well-defined and temperature controlled liquid environment. The test device used here also allows for continuous monitoring of applied force, specimen elongation and temperature.
For intumescent coatings durability is an important aspect. Due to ageing, which is caused by climatic conditions, the thermal protection performance of intumescent coatings can be reduced during the working life. The national German and the European procedures to assess the durability of intumescent coatings presume a working life of 10 years. For a longer period, additional investigations are required. However, the European assessment procedure does not provide specific information how to prove a durability of more than 10 years. In addition to this formal reason, also from a scientifical position, it is necessary to investigate the degradation of intumescent coatings in detail to propose a corresponding test concept for a durability of more than 10 years.
The presentation summarises the existing knowledge about the degradation behaviour and ageing of intumescent coatings. Furthermore, the results of different approaches from a recently conducted research project are presented. Starting from a water-based and an epoxy-based guide formulation, in a first approach a degradation of the intumescent coating was carried out directly during the production process, i.e. by reducing the concentration of functionally relevant chemical components. In another approach, the duration of the short-term weathering tests was significantly extended, i.e. by multiple repetition of the artificial weathering. The thermal protection performance of the intumescent coating was assessed by fire tests and tests with electrical heating source. In addition, small-scale tests were carried out to determine the thermal material properties of the intumescent coating and thermo-analytical methods were applied to characterise the degradation. Derived from this knowledge, possibilities to test and assess a working life for a period of more than 10 years are proposed.
Thermal runaway investigations were performed by subjecting single and double NMC pouch cells to thermal abuse condition inside an air-tight reactor vessel with an internal volume of 100 dm³. The study was divided into two series. The findings revealed the thermal runaway-induced explosion in the cells results in a rate of temperature increase greater than 10 K/s. The highest gaseous production was achieved at a range of 90 – 100% SOC and higher battery capacities 0.79 L/Wh (Series 1, 10 Ah cell) and 0.87 L/Wh (Series 2, 32 Ah cell). The investigation showed between 25 m³ and 84 m³ of explosible gas mixture could be released from electric vehicles of nominal useable electrical energy from 32 kWh up to 108 kWh at thermal runaway. It was also found that, the release of these explosible gases could undergo a secondary explosion.
Only the nano-scaled structure of the nanocomposite and the dispersion of nanoparticles within the polymer matrix harbor multifunctional potential including superior fire retardancy. Thus, this chapter focuses on the dispersion of nanoplates, based mainly on studies of layered silicates and graphene/graphene-related nanoplates. The nanostructure and properties of the nanocomposites are dependent mainly on thermodynamic and kinetic factors during preparation. Improving nano-dispersion often directly improves flame retardancy. Therefore, the modification of the nanoplates as well as the preparation of nanocomposites becomes very important to control this dispersion. The dispersion of nanoplates functions as a prerequisite for the formation of an efficient protective layer, changing the melt flow and dripping behavior, or the improvement of the char properties.
Leather is a widely used material for thousands of years and in modern days it is produced on industrial scale. This production produces high amounts of organic waste during the tannery process. These fibers can become a resource and act as a multi-functional bio-filler in flame retardant composites.
This project investigates two leather fibers towards their ability to enhance the flame-retardancy in different composites. These composites use ammonium polyphosphate (APP) or aluminum trihydroxide (ATH) as flame retardants. Different synergists support polymers with ATH.
The new composites form a stable char layer resulting in an increase in residue, lower peak heat release rates (pHRR) and higher limiting oxygen index (LOI). In addition, the ratings in the UL94-classification increased up to V-0.
Avoiding antimony – effect of Ca(H2PO2)2 on smoke emission and fire behaviour in brominated ABS
(2023)
The replacement of antimony trioxide (Sb2O3) in brominated flame-retardant ABS (ABS/FR) is of great interest. This study investigates the influence of calcium hypophosphite (CaP) in ABS/FR on flame retardancy and smoke emission. Different amounts of talc are added to ABS/FR/CaP to evaluate the influence of an inorganic barrier on smoke emission and flame retardancy. The cone calorimeter unveiled a reduction by 46% in PHRR for ABS/FR/CaP. Additional 8 wt.-% talc (ABS/FR/CaP/8Talc) reduced the PHRR by 61%. ABS/FR/CaP exhibited a more condensed phase action, which resulted in less smoke emission. The study investigates the influence of CaP in ABS/FR on the smoke toxicity, smoke density and the smoke particles distribution in the smoke density chamber (ISO 5659-2) coupled to a FTIR spectrometer and electrical low pressure cascade impactor (ELPI).
Bench-scale fire stability testing - Protective layers in carbon fibre reinforced polymer laminates
(2023)
Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) composites usually demands intermediate-scale or full-scale testing. In this study, a bench-scale test is presented as a practicable and efficient method to assess the improvement in structural integrity of CFRP with different protective interlayers during fire.
This study presents the processability, fire behavior, and mechanical performance between the flame retarded pure epoxy resin and flame retarded glass-fiber-reinforced plastic before, during, and after a fire event. This enables a deeper understanding of the transferability of flame retardants, modes of action, char enhancement, and flame inhibition on composite materials
Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) composites usually demands intermediate-scale or full-scale testing. In this study, a bench-scale test is presented as a practicable and efficient method to assess the improvement in structural integrity of CFRP with different protective interlayers during fire.
Fire stability is one of the biggest issues of carbon fibre reinforced polymer (CFRP) composites, particularly when they are using in load bearing applications. As soon as the glass transition temperature of polymer matrix (100-200°C) is achieved, the composite loses its structural integrity, what leads to the distortion and failure. The principal fire stability test is based on simultaneous application of fire and mechanical load. Since the carbon fibres can transfer the tensile loads quite well, the compression load is chosen as a required mechanical load for a test. The fire tests were preceded by a static load test at room temperature to determine ultimate failure load. The specimen was loaded with a compression force until the failure load was reached, which was observed as a buckling. For the fire tests, 10% of compression failure load and direct flame of a fully developed fire (heat flux ≈ 180 kW m-2) were applied simultaneously to the specimen, while the time to failure was measured.
The possibilities of bench-scale fire stability testing were presented by investigating new types of laminate structures, which exhibit promising flame retardancy and fireproof properties. The new approach of CFRP laminate differs with a protective concept. Every system consists of two different interlayers (titanium foil, thermoplastic foil PEI, ceramic layer WHIPOX, rubber tape Pyrostat, basalt fibres and kenaf fibres), where the one layer constitutes the fireproof protection, that delays the rise of temperature in the rest of laminate, and the second layer provides very good structural connection with carbon fibre layers, thus improves the mechanical integrity of CFRP composite in fire.
The time to failure of CFRP composite was 17s. Protective systems significantly enhance the fire stability and increased time to failure by 3 to 10 times. Thicker specimens showed longer resistance time, however CFRP laminate with ceramic layer and titanium foil presented outstanding results and the best performance. The protection with Kenaf and basalt fibres offered a natural fibre solution with also good fire resistance performance
Although bench-scale tests are limited with respect to assessing the performance of components and structures, they are valuable in the assessment of different materials concepts. Furthermore, the reduced effort of conducting bench-scale test (lower costs, time, personnel resources) makes it more practical and effective.
Fire resistance of fiber-reinforced polymers (FRPs) has been an important area of research for many years since FRPs are mainly used in the transportation and construction sectors. This study presents the fire behavior, and mechanical performance between the flame retarded pure epoxy resin and flame retarded glass-fiber composites before, during, and after a fire event. This enables a deeper understanding of the transferability of flame retardants on composite materials.
Main message: Sustainability, or in other words, exploiting environmental conservation for the economic welfare and prosperity for all, would revolutionise the plastics industry were it to become predominant practice as a linear, fossil-fuel–based economy is switched to a carbon circular economy. Food for though is given by dint of a critical overview of the current trends in sustainable flame-retardant polymeric materials.
Introduction:
Transforming the plastics industry into a carbon circular economy over the next 30 years requires an immediate revolution entailing the development of cutting-edge materials and the planning of future industrial production plants. Hence, the innovative field of flame-retardant polymeric materials should lend its strength to drive this challenge. Visionary solutions are proposed to inspire us, while the implementation of economically feasible concepts can take us forward into the future.
Experimental The synthesis, processing, polymer analysis, thermal analysis, and investigation of fire behaviour from our own research are performed according to the state of the art, mostly in accordance with the pertinent ISO standards. Indeed, some of our equipment is part of the accredited lab; for the other methods we fulfil equivalent quality standards in terms of maintenance, calibration, participation in round robins, etc. Work steps such as the synthesis or preparation of new materials are usually outsourced or done with partners that have the relevant core competence. The talk also presents examples from other groups whose experimental is described in the corresponding scientific papers.
Results and Discussion An overview of current trends towards producing sustainable, flame-retardant polymeric materials is presented, using examples from the literature and by sketching our own projects performed in recent years. The examples are structured along a common theme leading from the use of old and new natural materials with some intrinsic flame retardancy, via flame-retardant biopolymers and biocomposites, to using renewable sources for flame retardants with the objective of exploiting natural sources available as industrial waste streams. Natural flame retardants and adjuvants are highlighted, although the status of most may be assessed as merely motivating our vision. Nevertheless, there are natural material streams finding their way into polymer mass production as fillers, adjuvants, polymers, or renewable educt sources. Natural substances originating from industrial waste streams open the door to sustainable solutions, because they are often available at low cost and avoid competition for land with farming or virgin forests. Aside from this main topic, remarks will address the recycling of flame-retarded polymeric materials; vitrimers are mentioned as a potential material for recyclable thermosets. At the end of the day, only convincing property profiles will prevail both for exploiting renewable sources and circular design, including cost effectiveness, sufficient availability, consistent quality, processibility, mechanical properties, and flame retardancy. However, sustainability must not be merely tolerated as an additional demand, but should instead be recognized as a solution, because sustainability aspires to ensure our economic welfare now and in the future.
Acknowledgement:
The examples shown from own project were supported by funding grants: BMBF WTZ: 01DN16040, DFG Scha 730/19-1, VW-Stiftung: Experiment No: 97437, DFG Scha 730/20-1, BMBF KMU Innovativ 031B1289B.
Slow crack growth (SCG) under the influence of external fluid media, usually termed environmental stress cracking (ESC), is still one of the most frequent origins of severe damage and failure of polymeric materials. For polyethylene (PE) this is relevant for mass products, like bottles for consumer products, but also for high-performance materials for pipes or industrial packaging, including containers for chemicals and other dangerous goods. Especially for high-density polyethylene (PE-HD) the susceptibility to SGC and ESC is depending on the complex interplay between molecular weight and architecture and the resulting semicrystalline morphology, especially the formation of tie-molecules.
A reliable assessment of the resistance against this damage phenomenon is essential for demanding as well as safety-critical applications and has to take into account suitable testing methodologies and conditions in combination with environmental media reflecting the properties representative for typical fillings and relevant components causing ESC. In this context a better understanding of different influencing factors, such as sorption, swelling or surface activity is necessary together with a detailed characterization of different stages of crack propagation and underlying mechanisms. Therefor well-established testing methods, such as the Full Notch Creep Test (FNCT), were complemented by detailed fracture surface analysis using e.g. LSM and SEM in combination with a time-dependent optical monitoring of the progressing crack growth.
For the crack growth also the ratio of fibrillated craze zone to crack opening is important for the deeper understanding of crack propagation and related material parameters which can be additionally addressed by X-ray computed tomography.
A few layer/multilayer graphene (MLG) with a specific surface area of BET ≥ 250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution or latex premixing of master batches followed by conventional two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of ca. 35, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR).[1-5] 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM).[6-8] The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
In recent years, fire safety requirements for bus interior materials have been increased and introduced into international regulations. Fire safety requirements for the burning rate, melting and dripping behaviour of interior materials already exist for many years. However, it remains unclear to what extent the release of smoke, combustion products and their toxicity should be limited. Therefore, a research and development project 82.0723 funded by BASt (Federal Highway Research Institute) was initiated to develop a simplified procedure for testing the toxicity and smoke development in case of fire of interior materials used in buses. The scope of the research included calculations to assess the toxicity of fire gases and the derivation of specifications for the formation of practicable limit values for smoke toxicity. Further investigations are needed to derive these limit values for smoke toxicity in order to be applicable for real fire scenarios in buses.
Das EU Projekt TREEADS „A Holistic Fire Management Ecosystem for Prevention, Detection and Restoration of Environmental
Desasters” beschäftigt sich mit der Erforschung der drei Phasen „Prävention und Bereitschaft“, „Detektion und Reaktion“ und
„Aufforsten und Anpassen“ der Waldbrandverhütung. Im Projekt gibt es acht ausgewiesene Pilotregionen, in denen Deutschland
auch mit einer Pilotregion in Sachsen-Anhalt bzw. in Brandenburg vertreten ist. Unsere Arbeit auf Charakterisierung des Waldbodens und numerische Simulation wird vorgestellt.
Das EU Projekt EU FireStat SI2.830108, das vom Europäischen Parlament finanziert und von der DG GROW der Europäischen Kommission in Auftrag gegeben wurde, hat aufgearbeitet, welche Terminologie in den europäische Mitgliedsstaaten verwendet wird und die von den Mitgliedstaaten erhobenen Daten über Gebäudebrände zu analysieren. Dabei wurden die Schwierigkeiten bei der Erfassung und die Unterschiede bei der Auslegung ermittelt und eine gemeinsame Terminologie sowie eine Methode zur Erfassung der erforderlichen Daten vorgeschlagen.
Folgende Schwerpunkte wurden bearbeitet: Zunächst erfolgte eine Diagnose von Terminologie-, Datenerhebungs- und Auslegungsproblemen, Erhebung der Terminologie und der Datenerfassung, Identifizierung der für die Entscheidungsfindung benötigten Daten, Analyse der Methoden zur Datenerhebung Definition einer gemeinsamen Terminologie, Methodik der Kosten-/Nutzenbewertung zur Unterstützung politischer Entscheidungen, Fallstudie zur Anwendung der Methode der Kosten-/Nutzenbewertung, Beschreibung einer zukünftigen Datenerhebungsmethode.
Das Ergebnis des Projekts ist eine Empfehlung, welche Daten in den Mitgliedstaaten erhoben werden sollten, um wissensbasierte Entscheidungen in Bezug auf den Brandschutz zu ermöglichen. Damit wird die Grundlage für Maßnahmen und Initiativen geschaffen, die den Brandschutz und die Brandverhütung der Mitgliedstaaten unterstützen, so dass knappe Ressourcen gezielt eingesetzt werden können.
Das EU Projekt EU FireStat SI2.830108, das vom Europäischen Parlament finanziert und von der DG GROW der Europäischen Kommission in Auftrag gegeben wurde, hat aufgearbeitet, welche Terminologie in den europäische Mitgliedsstaaten verwendet wird und die von den Mitgliedstaaten erhobenen Daten über Gebäudebrände zu analysieren. Dabei wurden die Schwierigkeiten bei der Erfassung und die Unterschiede bei der Auslegung ermittelt und eine gemeinsame Terminologie sowie eine Methode zur Erfassung der erforderlichen Daten vorgeschlagen.
Folgende Schwerpunkte wurden bearbeitet: Zunächst erfolgte eine Diagnose von Terminologie-, Datenerhebungs- und Auslegungsproblemen, Erhebung der Terminologie und der Datenerfassung, Identifizierung der für die Entscheidungsfindung benötigten Daten, Analyse der Methoden zur Datenerhebung Definition einer gemeinsamen Terminologie, Methodik der Kosten-/Nutzenbewertung zur Unterstützung politischer Entscheidungen, Fallstudie zur Anwendung der Methode der Kosten-/Nutzenbewertung, Beschreibung einer zukünftigen Datenerhebungsmethode.
Das Ergebnis des Projekts ist eine Empfehlung, welche Daten in den Mitgliedstaaten erhoben werden sollten, um wissensbasierte Entscheidungen in Bezug auf den Brandschutz zu ermöglichen. Damit wird die Grundlage für Maßnahmen und Initiativen geschaffen, die den Brandschutz und die Brandverhütung der Mitgliedstaaten unterstützen, so dass knappe Ressourcen gezielt eingesetzt werden können.
A well-defined terminology of fire-related variables is important for correct analyses and supporting knowledge-based decisions regarding the evaluation of building fires at the European level. After developing an overview of current practices for fire statistics in Part I, the terminology used and the data collected by the EU Member States and eight other countries regarding fire incidents, property damage and human losses were mapped to increase awareness of their practice and support a comprehensive assessment of several fire statistical datasets. A questionnaire was distributed to relevant authorities responsible for the collection, elaboration/analysis, and fire statistical data publications to define and select the essential variables for an appropriate fire assessment and fire incident description. Based on the results of the questionnaire able to identify the essential fire statistical variables and a detailed analysis of current definitions adopted in the fire statistics of the EU Member States and other countries, a common terminology is proposed to collect the necessary data in the EU Member States and obtain meaningful datasets based on standardised terms and definitions. The results will generate essential outputs to move towards harmonised fire statistics at the EU level and contribute to an appropriate analysis able to improve fire prevention and fire mitigation in building fires.
Packaging containers for dangerous goods that include aggressive liquids require that any packaging material that is based on high-density polyethylene has a high degree of stability and durability. This work is focused on testing the environmental stress cracking of the high-density polyethylenes used for such containers in contact with crop protection formulations, in particular, two model liquids established in Germany as standardized test media representatives for crop protection formulations containing the various admixtures typical for such products. One of the liquids is water-based and contains mostly surface-active ingredients, while the other is solvent-based and includes some emulsifiers. Originally established for pin impression tests, these model liquids and their individual components were here used for the first time as environmental media in the Full Notch Creep Test, which addresses the resistance against environmental stress cracking. The Full Notch Creep Test was carried out on five high-density polyethylene types with both model liquids, and also on one selected material with its components. The evaluation was focused on the fracture surface structures, which were visualized by a scanning electron microscope and by optical in situ imaging of the notch opening. While the water-based model liquid and its surface-active individual components induced environmental stress cracking with the characteristic pattern for a craze-crack mechanism and so-called brittle fracture on the surface, the solvent-based model liquid and its soluble ingredients exhibited rather ductile failure behavior, caused by the plasticizing effect on the polymer that reduced the yield stress of the high-density polyethylene.
For both cases, fracture surface analysis, together with side views of the crack opening, showed a clear relation between surface pattern, notch deformation (e.g., by blunting), or crack opening due to crack growth with time to failure and the solubility of the liquids in high-density polyethylene.
Aufgrund des tieferen Eindringens der solaren Strahlung treten bei transparenten und bei transluzenten (durchscheinenden) Kunststoffen veränderte Bedingungen gegenüber opaken Proben auf. Dies kann zu speziellen Effekten und damit zu einem abweichenden Bewitterungsverhalten führen. Auch aus Mangel an geeigneten Normen werden diese Effekte häufig vernachlässigt. Deshalb initiiert der DIN-FNK auf ISO-Ebene ein entsprechendes Dokument.
Die Norm ist in der Form eines Technical Reports geplant. In einem ersten Teil sollen die Besonderheiten transparenter oder transluzenter Kunststoffe erläutert werden, um den Nutzer für mögliche Probleme zu sensibilisieren. Im zweiten Teil werden Empfehlungen für Bestrahlung oder Bewitterung herausgearbeitet. In einem dritten Teil geht es dann um Besonderheiten bei der Messung von Eigenschaftsänderungen transparenter bzw. transluzenter Kunststoffe. In informativen Anhängen sollen verschiedene Beispiele die Thematik illustrieren.
Im Rahmen des Forschungsprojektes IGF 20470N wurden Untersuchungen zum Alterungsverhalten von reaktiven Brandschutzsystemen (RBS) auf Stahlbauteilen durchgeführt. Mithilfe der Ergebnisse einer umfangreichen Literaturrecherche sowie experimentellen und numerischen Untersuchungen sollte ein Vorschlag für ein Prüfkonzept zum Nachweis einer Nutzungsdauer von RBS von mehr als 10 Jahren auf Basis von Kurzzeitversuchen abgeleitet werden. Dabei setzt die Bewertung des Alterungsverhaltens von RBS voraus, dass die Mechanismen der Alterung hinreichend bekannt sind.
Dafür wurden zunächst systematisch Daten von Kurz- und Langzeitversuchen von nationalen Zulassungsprüfungen der letzten Jahrzehnte ausgewertet. Anschließend wurden umfangreiche experimentelle Untersuchungen an einer wasserbasierten sowie einer epoxidharzbasierten Richtrezeptur durchgeführt. Da aus der Literatur bekannt ist, dass die Einflüsse der Bewitterung zu einer Veränderung der Konzentration der Bestandteile innerhalb der Beschichtung führen können, wurden Untersuchungen mit Mangelrezepturen durchgeführt, wobei systematisch einzelne Bestandteile reduziert wurden. Neben optischen Untersuchungen wurden thermoanalytische Verfahren (DSC-TG-, ATR-FTIR-, Elementar-, Farbanalyse) angewandt sowie Brandversuche an beschichteten Stahlplatten durchgeführt. Des Weiteren wurden die Richtrezepturen den beschleunigten Kurzzeitversuchen gemäß EAD 350402-00-1106 (2017) unterzogen, welche die Zulassung von Produkten auf europäischer Ebene regelt. Für die wasserbasierte Richtrezeptur wurden die Bewitterung für den feuchten Innenraum (Typ Z1) mehrfach wiederholt (1x, 3x, 6x). Für die epoxidharzbasierte Richtrezeptur entsprach die Bewitterung dem Zyklus für die Außenanwendung (Typ X). In Brandversuchen sowie thermoanalytischen und optischen Untersuchungen wurde das Alterungsverhalten sowie die thermische Schutzwirkung analysiert.
Anschließend wurden numerische Simulationen von Stahlbauteilen mit gealterten RBS durchgeführt und anhand der experimentellen Untersuchungen validiert. Mithilfe der numerischen Modelle kann eine Bewertung der thermischen Schutzwirkung von Stahlbauteilen mit gealterten RBS vorgenommen werden.
Mithilfe der gesammelten Erkenntnisse wurde ein Vorschlag für ein Prüfkonzept für den Nachweis einer Nutzungsdauer von mehr als 10 Jahren abgeleitet. Das Prüfkonzept besteht dabei aus einem Katalog von Möglichkeiten, die aktuellen Zulassungsprüfungen auf europäischer Ebene für eine Nutzungsdauer von 10 Jahren auf einen längeren Zeitraum zu erweitern.
Produkte, Bauteile und Konstruktionen im Transport- und Bauwesen bestehen mehr und mehr aus Klebverbunden. Allein die Menge des verwendeten Klebstoffes oder die Anzahl geklebter Verbindungen schließen für eine verlässliche Betrachtung und Bewertung der Brandrisiken aus, deren Beitrag zur Brandentstehung, Flammenausbreitung oder Feuerwiderstand von Baugruppen und Konstruktionen zu vernachlässigen. Anforderungen an die Leistungsbeschreibungen von flammgeschützten Klebstoffen bzw. Haftklebebändern werden definiert, oft ohne ein ausreichendes Verständnis der Beiträge von Klebverbunden zum Brandverhalten der Bauteile zu haben. Der Vortrag beleuchtet diese Problematik und stellt die verschiedenen komplexen Anforderungen aus dem Brandschutz in Hinblick auf Auswahlkriterien und Entwicklungsziele für flammgeschützte Klebstoffe dar. Dabei ist dieser Transfer des Brandverhaltens, sprich der Systemantwort einer Komponente oder Bauteils in einem spezifischen Brandszenario, in Materialeigenschaften des Klebstoffes eine intrinsische und anspruchsvolle Herausforderung. Im abgeschlossenen IGF-Projekt Nr. 20762 N (Forschungsvereinigung DECHEMA) haben wir für Klebebänder eine systematisch-wissenschaftliche Studie durchgeführt und aussagekräftige Erkenntnisse zu Verfügung gestellt. Die Untersuchungen zur Entflammbarkeit zu Brandbeginn, zur Flammenausbreitung (Wärmeentwicklung) im sich entwickelnden Brand und zum Feuerwiderstand im Vollbrand machen die sehr unterschiedlichen Einflüsse von Klebverbunden, d. h. auch die unterschiedlichen Anforderungen an die Modifikation der Klebebänder, deutlich. Die thermische Analyse verschiedener Klebstoffe zusammen mit den Brandtest freistehender Haftklebebänder, an einseitig geklebten Substraten und an Klebverbundprobekörpern skizzieren eindrucksvoll die komplexen Zusammenhänge zwischen Materialeigenschaften der Klebebänder und dem Brandverhalten von Klebverbunden. Der Vergleich von verschiedenen Substraten wie Stahlbleche, Holz, Mineralwolle und verschiedene Polymermaterialien belegt darüber hinaus, dass der Einfluss der Klebverbindungen auf das Brandverhalten der Klebverbunde substratspezifisch ist. Gerade der Vergleich zwischen Holz, Polymethylmethacrylat (PMMA) und Bisphenol A Polycarbonat (PC) liefert überraschend unterschiedliche Ergebnisse. Die Variation der Klebstoffe und Trägermaterialien der Klebebänder skizziert die verschiedenen Möglichkeiten für die Materialentwicklung. Abhängig vom Material und Brandszenario können Klebverbunde im Vergleich zu gleich dicken Probekörpern aus demselben Substrat sowohl eine deutliche Erhöhung der Brandrisiken, ein praktisch unverändertes Brandverhalten oder eine Reduktion des Brandrisikos hervorrufen. Grundsätzlich kann keine Lösung bzw. kein Tape gefunden werden, die mit allen Substraten einen guten Brandschutz gewährleistet. Substrate, Carrier und Klebstoff müssen nicht nur aufeinander abgestimmt werden, sondern auch auf das Brandszenario, in welchem der Verbund eine gute Performance liefern soll.Das IGF-Projekt (20762) der Forschungsgemeinschaft (DECHEMA Deutsche Gesellschaft für Chemische Technik und Biotechnologie e V, Theodor Heuss Allee 25, 60486 Frankfurt am Main) wurde durch die AiF im Rahmen des Programms „Förderung der Industriellen Gemeinschaftsforschung (IGF)” des Bundesministeriums für Wirtschaft und Klimaschutz aufgrund eines Beschlusses des Deutschen Bundestages gefördert.
Composites in Fire and Flame
(2022)
Overview over the research results of the BAM in the field fire retardancy of composites. In different applications the flame retardancy of composites targets on different fire protection goals in the fire scenarios ignition, developing fire, and fully developed fire. Efficient solutions are tailored to pass a distinct fire test and to fit to a specific material. Flame inhibition as main flame retardancy mode of action combined with a minor mode of action in the condensed phase is general very efficient approach for composites. Alternatively residue design is demanded to achieve good results with only condensed phase mechanisms. Improving the fire stability asks for protective fire residues.
Überblick über den State-of-the-Art und aktuelle Trends mit den Schwerpunkten:
- nachwachsende Rohstoffe in flammgeschützten Polymerwerkstoffen (flammgeschützte Biopolymere und Biokomposite; biomass-basierte Flammschutzmittel, nachwachsende Hilfsstoffe aus Abfallströmen)
- Nachhaltigkeit und Flammschutz
- Konzepte von Analogie bis Out-of-the-Box.
Overview of the state of the art and current trends with the main topics:
- renewable sources in flame retardant polymers (flame retarded bio-polymers and biocomposites; bio-flame retardants, renewable adjuvants from industrial waste)
- flame retardancy meets sustainability
- concepts between analogy and out-of-the-box.
Polymeric membranes represent a cost- and energy-efficient solution for gas separation. Recently Polymers of Intrinsic Microporosity (PIMs) have been in a great interest because of their outstanding BET surface area larger than 700m2/g and pore size smaller than 1 nm. PIMs are a promising candidate in gas separation with high permeability and appealing selectivity due to their inefficient packing derived from a combination of ladder-like rigid segments with sites of contortion. However, it is recognized this class of polymers suffer from decrease in performance with time due to physical aging. The initial microporous structures approach a denser state via local chain rearrangements, leading to a dramatic reduction in permeability. As chain packing during film casting and physical aging are the key factors determine the performance in separation applications, characterization of the molecular mobility in these materials has been proved to provide valuable information. In recent research on PIM-1 the archetypal PIM, a molecular relaxation process with high activation energy together with a significant conductivity in the glassy state has been found and explained with the formation of local intermolecular agglomerates due to interaction of π-electrons in aromatic moieties of the polymer backbone. In this work, the dielectric behavior of the polymeric films and their response upon heating (aging) were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range down to 133K for the first time. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. Up to now, no other work has studied the role of porosity and thermal history of PIM-1 film in dielectric processes. The goal is by eliminating thermal history and considering storing conditions provide better understanding on aging and plasticizing in high free volume glassy polymer PIM-1.
Especially now in times of the energy revolution, the demand for energy-efficient separation processes promotes the advancement of new high-performance materials for use as highly selective separation membranes. Polymers with intrinsic microporosity (PIMs) are of high interest in the field of gas separation membranes. Currently the application of PIMs for membrane technology is still restrained by their strong tendency to physical aging involving a significant loss of their good gas separation properties. Physical aging phenomenon is related to the molecular mobility of PIMs which was investigated by broadband dielectric spectroscopy (BDS) previously [1]. In this work, covalent phosphinine-based framework (Eto-CPSF) was used as a nanofiller (0-10 wt %) in a PIM-1 matrix to potentially enhance the gas transport properties and prevent physical aging. Since molecular mobility is a fundamental parameter determining gas transport as well as physical aging in such a material, our study includes dielectric investigations by BDS of pure PIM-1 and PIM-1/Eto-CPSF mixed matrix membranes to establish a correlation between molecular mobility and gas transport properties. In addition, gas permeability was determined by the time-lag method (0-10 bar pressure) at 35 °C for N2, O2, CH4 and CO2 for all MMMs.
The dielectric behavior of the polymeric films and their response upon heating were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range up to 250 °C. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. As main result for MMMs, the permeability of PIM-1 for CH4 and CO2 gases were increased significantly with only 5 wt% of nanofiller within the polymer matrix. However, this is not observed for Eto-CPSF concentrations higher than ca. 7 wt% probably due to a microphase separated morphology of the nanocomposite system. Furthermore, the permselectivity of membranes for pair gases O2/N2 and CO2/N2 show enhancement up to a concentration of about 7 wt% Eto-CPSF filler.
Genormte künstliche Bewitterungstests sind häufig nicht spezifisch für die Anwendungssituation oder das Material. Das macht die Entwicklung spezifischer Tests erforderlich. Für deren Entwicklung müssen Maximalparameter der Anwendungssituation bekannt sein, womit dann der künstliche Test formuliert wird und dessen Bedingungen werden dann solange optimiert, bis die Korrelation der Effekte von natürlichem und künstlichem Test ausreichend ist.
Für Untersuchungen der Freisetzung kann der verbleibende Rest in der Probe und/oder die freigesetzte Menge in Luft, Boden, Wasser bestimmt werden.
Im ersten Beispiel der Witterungswirkung wurde die Freisetzung von Kohlenstoff-Nanoröhrchen (CNT) aus Polymer-Kompositen untersucht (unter Verwendung von empfindlich-nachweisbarer radioaktiver 14C-Markierung für einzelne CNT-Partikel), in einem zweiten die Freisetzung von anorganischen und organischen Bestandteilen aus elastomeren Bestandteilen von Sportböden (Bahnen und Kunstrasen) in Wasser.
The incorporation of nanoscale particles into elastomers enable a boost in performance and/or a distinct reduction of conventional filler loadings due to their high surface to volume ratio. 2D layered nanoparticles like graphene and graphene-related materials provide a great potential as effective fillers in rubber, especially by enhancing mechanical and barrier properties. The type and properties of the nanoparticles, their interface and the elastomeric matrix materials influence the technical behavior, and therefore the potential application fields of such rubber nanocomposites. Especially crucial for the efficiency of the nanofiller, however, is its best possible incorporation into the elastomer. The dispersing of nanoparticles without agglomerates usually constitutes a challenge when using conventional two-roll milling or internal mixing. Academic approaches for highly dispersed nanocomposites solve this problem but are often energy and time consuming with no feasible scale up possibility. Therefore, an ultrasonic assisted NR latex premixing process was established to produce highly filled masterbatches, enabling the main processing with conventional rubber processing techniques.
Two carbon-based nanoparticles with similar specific surface areas were investigated and incorporated in natural rubber as nanocomposites: A commercially available multilayer graphene (MLG) and a nanoscale carbon black (nCB). The mentioned premixed masterbatches were further processed to nanocomposites by the addition of matrix NR, two-roll milling, and hot pressing (vulcanization). By this procedure an increase in Young’s modulus of 157% (MLG) and 71% (nCB) could be obtained at a concentration level of 3 phr. As anisotropic material behavior was observable for the nanocomposites containing MLG, different measurement methods were investigated to quantify the orientation of the nanoparticles in the nanocomposites: Sorption measurements (swelling in 2 dimensions), hardness and dynamical mechanical analysis (in-plane vs. cross-plane), X-Ray diffraction and transmission and scanning electron microscopy.
A few layer/multilayer graphene (MLG) with a specific surface area of BET=250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution mixing of master batches followed by two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of 34, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR). 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability, the latter shown by the reduction in heat release rate in the cone calorimeter. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM). The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
In the recent years, more and more products in construction and automotive industry are bonded by adhesive tapes instead of mechanical fasteners but there is no sufficient understanding of how these bonded, layered materials behave in fires. Our research project gives an insight of how adhesives and substrates interact with each other in different fire scenarios and how flame retardants function in pressure sensitive adhesive (PSA) tapes. A systematic investigation on the burning behavior of PSA tapes as free-standing films, as top layers on different substrates and as sandwich-like adhesive joints was performed. The burning behavior of free-standing PSA tapes and those used as a coating was significantly improved by using phosphorus-based flame retardants. Furthermore, it was shown that, depending on tape structure and substrate, the PSA tape can lower the fire risk by acting as an intermediate protection layer in bonded materials.