7.5 Technische Eigenschaften von Polymerwerkstoffen
Filtern
Dokumenttyp
- Zeitschriftenartikel (129)
- Vortrag (106)
- Beitrag zu einem Tagungsband (29)
- Posterpräsentation (28)
- Buchkapitel (10)
- Beitrag zu einem Sammelband (2)
- Zeitschriftenheft (Herausgeberschaft für das komplette Heft) (2)
- Forschungsdatensatz (2)
- Monografie (1)
- Dissertation (1)
Sprache
- Englisch (252)
- Deutsch (58)
- Mehrsprachig (1)
Schlagworte
- Flame retardant (36)
- Flame retardancy (25)
- Graphene (14)
- Flammability (13)
- Rubber (12)
- Weathering (12)
- Durability (11)
- Evacuation (11)
- Additive Fertigung (10)
- Brandschutz (9)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (311)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (311)
- 6 Materialchemie (38)
- 6.6 Physik und chemische Analytik der Polymere (33)
- 5 Werkstofftechnik (29)
- 5.3 Polymere Verbundwerkstoffe (28)
- 3 Gefahrgutumschließungen; Energiespeicher (20)
- 8 Zerstörungsfreie Prüfung (19)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (15)
- 7.3 Brandingenieurwesen (12)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (106)
Die Präsentation gibt einen Überblick über die Arbeiten im German Pilot des EU-Projekts TREEADS. Es werden klein-, mittel- und großskalige Versuche an Waldboden mit einheimischer Vegetation durchgeführt. Begleitend werden numerische Untersuchungen durchgeführt, die eine Variation der Parameter, wie Bodenfeuchte, Temperaturen und Wind über die Experimente hinaus erlauben. Die gemessenen Materialparameter dienen als Input für die numerischen Berechnungen. Die numerischen Modelle werden mit den mittel- und großskaligen Experimenten validiert.
Weltweit stellen Waldbrände eine große Bedrohung für Umwelt, Wirtschaft und menschliches Leben dar. Der fortschreitende Klimawandel verstärkt Trockenheit und Dürre, wodurch die Größe und Intensität von Waldbränden sowie das daraus resultierende Gefahrenpotential zusätzlich erhöht werden. Um im Risikofall eine schnelle und effektive Waldbrandbekämpfung zu gewährleisten, sollen Einsatzkräfte in Zukunft von KI-basierten Ausbreitungsmodellen unterstützt werden.
Der Einsatz von maschinellem Lernen ermöglicht dabei schnelle und zielgerichtete Ausbreitungsvorhersagen in Echtzeit, die in den Prozess der Brandbekämpfung als zusätzliche Information einfließen können. Im Rahmen des durch das EU-Förderprogram Horizon 2020 finanzierte Projekt TREEADS wird ein solches Modell für Europa entwickelt.
Dazu wird mit verschiedenen Satellitendaten des Copernicus-Programms und der NASA ein auf räumlicher und zeitlicher Ebene aufgelöster Datensatz zu europäischen Waldbränden aufgebaut. Zu den erfassten Waldbränden werden wichtigen Faktoren, die Einfluss auf die Brandausbreitung haben, ergänzt. Dazu gehören das von Copernicus bereitgestellte, digitale Geländemodell Europas und verschiedene, von Sentinel-2 Messungen abgeleitete Informationen zu Vegetation und Landnutzung. Dieser 2D-Trainingsdatensatz zu realen Waldbränden wird durch die zeitlich hochaufgelösten, meteorologischen Reanalyse-Produkte – Copernicus European Regional ReAnalysis (CERRA) und ERA5-Land – vervollständigt und ist die Grundlage für ein Modell zur Ausbreitungsvorhersage von Waldbränden.
Methoden des Maschinellen Lernens können komplexe Muster in den gesammelten Daten erkennen und so zu einer verbesserten Vorhersage der Brandausbreitung beitragen. Die vielfältigen, von Copernicus bereitgestellten Daten sind dabei ein unabdingbarer Bestandteil des Modells, mit dem den Einsatzkräften ein zusätzliches Tool für den effizienten Einsatz ihrer limitierten Ressourcen zur Verfügung steht.
Die Umweltwirkungen auf ein Material werden als Überlapp der Funktionskurven von Materialempfindlichkeit und einwirkenden Umweltparametern betrachtet. Wenn entweder die Empfindlichkeit oder die Beanspruchungen Null sind, ergibt sich auch keine Umweltwirkung und bei beidseitig Werten größer Null das jeweilige Produkt der beiden. Die Akkumulation der nicht-reversiblen Effekte über die Zeit und allen Eigenschaftsänderungen entspricht der Alterung des Materials für den jeweiligen Expositionszeitraum.
Die digitale Umweltsimulation gliedert sich hier in drei Teilaspekte. Ein erster, rein materialwissenschaftlicher Teil hat die Aufgabe, alle relevanten Materialempfindlichkeiten experimentell zu quantifizieren. Ein zweiter – unter Umständen numerischer Teil – hat die Aufgabe, das Bauteil und seine Einbaulage zu digitalisieren und aus den makroskopischen Umgebungsbedingungen die relevanten mikroklimatischen Umweltparameter für alle Oberflächen- oder Volumenelemente zu bestimmen. In einem dritten Teil werden die Einwirkungen über den betrachteten Zeitraum berechnet und kumuliert. Dieses Konzept, das auf den so genannten Expositions-Reaktions-Funktionen (ERF) basiert, wird an Beispielen der Photoxidation erläutert. Dieses Vorgehen wurde schon beim ViPQuali-Projekt als Numerische Umweltsimulation umgesetzt.
Überprüft werden muss das Modell unbedingt an einer realitätsnahen Validierungsbeanspruchung. Hier werden die ermittelten ERFs mit über den kompletten Beanspruchungszeitraum geloggten Umweltparametern gekoppelt, um die berechnete mit der experimentell erfahrenen Alterungswirkung zu vergleichen. Nur so kann sichergestellt sein, dass alle für die Anwendungsumgebung relevanten Materialempfindlichkeiten einbezogen wurden.
This is the stable version of the full-notch creep test ontology (OntoFNCT) that ontologically represents the full-notch creep test. OntoFNCT has been developed in accordance with the corresponding test standard ISO 16770:2019-09 Plastics - Determination of environmental stress cracking (ESC) of polyethylene - Full-notch creep test (FNCT).
The OntoFNCT provides conceptualizations that are supposed to be valid for the description of full-notch creep tests and associated data in accordance with the corresponding test standard. By using OntoFNCT for storing full-notch creep test data, all data will be well structured and based on a common vocabulary agreed on by an expert group (generation of FAIR data) which is meant to lead to enhanced data interoperability. This comprises several data categories such as primary data, secondary data and metadata. Data will be human and machine readable. The usage of OntoFNCT facilitates data retrieval and downstream usage. Due to a close connection to the mid-level PMD core ontology (PMDco), the interoperability of full-notch creep test data is enhanced and querying in combination with other aspects and data within the broad field of materials science and engineering (MSE) is facilitated.
The class structure of OntoFNCT forms a comprehensible and semantic layer for unified storage of data generated in a full-notch creep test including the possibility to record data from analysis and re-evaluation. Furthermore, extensive metadata allows to assess data quality and reliability. Following the open world assumption, object properties are deliberately low restrictive and sparse.
Die Umweltwirkungen auf ein Material werden als Überlapp der Funktionskurven von Materialempfindlichkeit und einwirkenden Umweltparametern betrachtet. Wenn entweder die Empfindlichkeit oder die Beanspruchungen Null sind, ergibt sich auch keine Umweltwirkung und bei beidseitig Werten größer Null das jeweilige Produkt der beiden. Die Akkumulation der nicht-reversiblen Effekte über die Zeit und allen Eigenschaftsänderungen entspricht der Alterung des Materials für den jeweiligen Expositionszeitraum.
Die digitale Umweltsimulation gliedert sich hier in drei Teilaspekte. Ein erster, rein materialwissenschaftlicher Teil hat die Aufgabe, alle relevanten Materialempfindlichkeiten experimentell zu quantifizieren. Ein zweiter – unter Umständen numerischer Teil – hat die Aufgabe, das Bauteil und seine Einbaulage zu digitalisieren und aus den makroskopischen Umgebungsbedingungen die relevanten mikroklimatischen Umweltparameter für alle Oberflächen- oder Volumenelemente zu bestimmen. In einem dritten Teil werden die Einwirkungen über den betrachteten Zeitraum berechnet und kumuliert. Dieses Konzept, das auf den so genannten Expositions-Reaktions-Funktionen (ERF) basiert, wird an Beispielen der Photoxidation erläutert. Dieses Vorgehen wurde schon beim ViPQuali-Projekt als Numerische Umweltsimulation umgesetzt.
Überprüft werden muss das Modell unbedingt an einer realitätsnahen Validierungsbeanspruchung. Hier werden die ermittelten ERFs mit über den kompletten Beanspruchungszeitraum geloggten Umweltparametern gekoppelt, um die berechnete mit der experimentell erfahrenen Alterungswirkung zu vergleichen. Nur so kann sichergestellt sein, dass alle für die Anwendungsumgebung relevanten Materialempfindlichkeiten einbezogen wurden.
The dripping behaviour of polymers is often observed experimentally through the UL94 flammability standard test. In this work, polymeric dripping under fire is investigated numerically using particle finite element method. A parametric analysis was carried out to observe the influence of a single property on overall dripping behaviour via a UL94 vertical test model. Surrogates and property ranges were defined for variation of the following parameters: glass transition temperature (Tg), melting temperature (Tm), decomposition temperature (Td), density (ρ), specific heat capacity (Cp), apparent effective heat of combustion of the volatiles, char yield (μ), thermal conductivity (k), and viscosity (η). Polyamide, poly(ether ether ketone), poly(methyl methacrylate), and polysulfone were used as benchmarks. Simulated results showed that specific heat capacity, thermal conductivity, and char yield allied with viscosity were the properties that most influenced dripping behaviour (starting time and occurrence).
EPDM, HNBR and FKM materials were exposed at 150 ◦C to air under atmospheric pressure and to hydrogen at 50 bar for different ageing times. All measurements after hydrogen exposure were conducted on samples in degassed condition to assess irreversible effects resulting from that exposure and to compare them to those after ageing in air. Density, hardness, tensile properties, compression set, and hydrogen permeability of all samples were analysed. In both ageing environments, HNBR exhibited the most significant changes of material properties.
However, for both EPDM and HNBR, considerably less severe ageing effects were observed under hydrogen in comparison to ageing in air. On the other hand, FKM showed about the same low level of deterioration in both ageing environments but exhibited poor resistance against damage due to rapid gas decompression in hydrogen environment that can lead to seal failure. The obtained results may serve as a guidance toward a better understanding for design and utilisation of elastomeric materials in future hydrogen infrastructure components.
Two-dimensional covalent organic frameworks (COFs) based on phosphinine and thiophene building blocks have been synthesized with two different side groups. The materials are denoted as CPSF-MeO and CPSF-EtO where CxxF correspond to the covalent framework, whereas P and S are related to heteroatoms phosphorous and sulfur. MeO and EtO indicate the substituents, i.e. methoxy and ethoxy.
Their morphologies were studied by scanning electron microcopy and X-ray scattering. The absence of crystalline reflexes in the X-ray pattern reveal that both materials are amorphous and can be considered as glasses. Furthermore, N2 adsorption measurements indicate substantial Brunauer–Emmett–Teller (BET) surface area values pointing to the formation of three-dimensional pores by stacking of the aromatic 2D layer. An analysis of the porosity of both COFs showed a mean radius of the pores to be of ca. 4 nm, consistent with their chemical structure. The COFs form nanoparticles with a radius of around 100 nm. The thermal behavior of the COFs was further investigated by fast scanning calorimetry. These investigations showed that both COFs undergo a glass transition. The glass transition temperature of CPSF-EtO is found to be ca. 100 K higher than that for CPSF-MeO. This large difference in the glass transition is discussed to be due to a change in the interaction of the COF sheets induced by the longer ethoxy group. It might be assumed that for CPSF-EtO more individual COF sheets assemble to larger stacks than for CPSF-MeO. This agrees with the much larger surface area value found for CPSF-EtO compared to CPSF-MeO. To corroborate the results obtained be fast scanning calorimetry dielectric measurements were conducted which confirm the occurrence of a dynamic glass transition. The estimated temperature dependence of the relaxation rates of the dielectric relaxation and their absolute values agrees well with the data obtained by fast scanning calorimetry. Considering the fragility approach to the glass transition, it was further found that CPSF-MeO is a fragile glass former whereas CPSF-EtO behaves as a strong glass forming material. This difference in the fragility points also to distinct differences in the interaction between the 2D COF molecules in both materials.
Combining buffing leather fibers from industrial waste streams with ammonium polyphosphate and bentonite clay is proposed as a flame-retardant additive for polypropylene. The paper addresses how they can be processed into attractive composites with the desired mechanical properties. Buffing leather fibers function as a multifunctional bio-filler and as a synergist for the flame retardant, resulting in fire retardancy successful enough to increase the oxygen index (LOI) by up to 7 vol.-% and to achieve a V0 UL 94 classification. Impressively reduced heat release rates are obtained in the cone calorimeter at 50 kW/m2 irradiation; for instance, the maximum average rate heat evolved (MARHE) drops from 765 to below 200 kW m 2. The synergistic effects are quantified and shown to be very strong for LOI and MARHE. This work opens the door to use waste buffing leather fibers as a promising multifunctional and synergistic bio-filler.
To ensure fire safety, polymers are filled with flame retardants and smoke suppressants. To meet the highest requirements, it is essential to understand the decomposition of those polymeric materials. This study reveals interactions between polymer, smoke suppressants, and flame retardants, and discusses their impact on the materials’ flame retardancy, smoke emission, smoke toxicity, and particle emission in conventional loadings to provide deeper general understanding. Low melting oxide glass, melem, spherical silica, sepiolite, melamine polyphosphate, and boehmite in an aluminum diethylphosphinate flame-retarded polyamide 6.6 were investigated. All smoke suppressants improve the protective layer and act as an adjuvant. Silica and melem performed best under forced flaming conditions. Spherical silica reduces the peak of heat release rate by 39% and the total heat evolved by 14%, whereas 10 wt% melem lowers the total smoke production by 41%. Melem alters the mode of action of aluminum diethylphosphinate from gas to more condensed phase activity. This change reduces flame inhibition and hence smoke toxicity, but further improves the protective layer due to charring reactions in the decomposition mechanism. In addition, the sizes of the smoke particles decrease because of the prolonged time in the pyrolytic zone. This study highlights that interactions between polymer, flame retardants, and smoke suppressants can significantly determine the smoking and burning behavior.
Polymers with intrinsic microporosity (PIMs) are gaining attention as gas separation membranes. Nevertheless, they face limitations due to pronounced physical aging. In this study a covalent organic framework containing λ5-phosphinine moieties, CPSF-EtO were incorporated as a nanofiller (concentration range 0-10 wt%) into a PIM-1 matrix forming dense films with a thickness of ca. 100 μm. The aim of the investigation was to investigate possible enhancements of gas transport properties and mitigating effects on physical aging. The incorporation of the nanofiller occurred on aggregate level with domains up to 100 nm as observed by T-SEM and confirmed by X-ray scattering. Moreover, the X-ray data show that the structure of the microporous network of the PIM-1 matrix is changed by the nanofiller.
As the molecular mobility is fundamental for gas transport as well as for physical aging, the study includes dielectric investigations of pure PIM-1 and PIM-1/CPSF-EtO mixed matrix membranes to establish a correlation between the molecular mobility and the gas transport properties. Using the time-lag method the gas permeability and the permselectivity were determined for N2, O2, CH4 and CO2 for samples with variation in filler content. A significant increase in the permeability of CH4 and CO2 (50 % increase compared to pure PIM-1) was observed for a concentration of 5 wt% of the nanofiller. Furthermore, the most pronounced change in the permselectivity was found for the gas pair CO2/N2 at a filler concentration of 7 wt%.
AbstractThe increasing threat of forest fires on a global scale is not only a matter of concern due to the potential harm they may cause to both human and animal life but also due to their significant role in exacerbating climate change. In light of these circumstances, one might inquire as to whether forest soil can self‐ignite and, if so, under what conditions and at what temperatures this phenomenon may occur. This question is being addressed in the German pilot “Fire science of wildfires and safety measures” of the EU project TREEADS, and the first results are presented below. The importance of basic research into the self‐ignition of forest soil cannot be underestimated, as it provides crucial knowledge to prevent forest fires and protect human and animal health. Furthermore, mitigating the occurrence of forest fires can also play a role in reducing greenhouse gas emissions, contributing to global efforts to combat climate change. The procedure of the hot storage test is an effective means of determining whether a material can self‐ignite. During the investigation of six soil samples, it was found that five of them were indeed capable of self‐ignition. In addition to determining whether the material ignites, the modified hot storage test also analyzed the resulting smoke gases and measured their concentration. The research question of whether regional forest soil is capable of self‐ignition can be answered with yes based on these initial tests. Further experiments are needed to determine if self‐ignition causes forest fires.
Pressure-sensitive adhesive tapes are used in several industrial applications such as con-struction, railway vehicles and the automotive sector,where the burning behavior is ofcrucial importance. Flame retarded adhesivetapes are developed and provided, however,often without considering the interaction of adhesive tapes and the bonded materialsduring burning nor the contribution of the tapes to fire protection goal of the bondedcomponents in distinct fire tests. This publication delivers an empirical comprehensiveknowledge how adhesive tapes and their flame retardancy effect the burning behaviorof bonded materials. With a special focus on the interaction between the single compo-nents, one flame retarded tape and one tapewithout flame retardant are examined inscenarios of emerging and developing fires, along with their bonds with the commonmaterials wood, zinc-plated steel, mineral wool, polycarbonate, and polymethylmethacry-late. The flame retardant significantly improved the flame retardancy of the tape as afree-standing object and yielded a V-2 rating in UL 94 vertical test and raised the OxygenIndex by 5 vol.%. In bonds, or rather laminates, the investigations prove that the choiceof carrier and substrates are the factors with the greatest impact on the fire propertiesand can change the peak of heat release rate and the maximum average rate of heatemission up to 25%. This research yielded a good empirical overall understanding of thefire behavior of adhesive tapes and bonded materials. Thus, it serves as a guide for tapemanufacturers and applicants to develop tapes and bonds more substrate specific.
The residual post-fire mechanical properties of fiber-reinforced epoxy composites are influenced by their fire residues after burning. This study uses intumescent/low-melting glass flame retardants to tailor fire residues in epoxy resin. Processibility of prepregs and their quality are analysed for transfer of the flame-retardant epoxy resins to layered glass-fiber reinforced composites. Minimal effects were found on the pre-fire flexural strengths of the composites due to low loading of the flame retardants. However, when transferred to glass-fiber reinforced composites, the fire residues diminish significantly. Further studies are required to improve theoretical and experimental estimations of the post-fire mechanics of the composites.
The residual post-fire mechanical properties of fiber-reinforced epoxy composites are influenced by their fire residues after burning. This study uses intumescent/low-melting glass flame retardants to tailor fire residues in epoxy resin. Processibility of prepregs and their quality are analysed for transfer of the flame-retardant epoxy resins to layered glass-fiber reinforced composites. Minimal effects were found on the pre-fire flexural strengths of the composites due to low loading of the flame retardants. However, when transferred to glass-fiber reinforced composites, the fire residues diminish significantly. Further studies are required to improve theoretical and experimental estimations of the post-fire mechanics of the composites.
The transfer of flame-retardant epoxy resin formulations to composites for structural and lightweight applications in the energy and transport sector can be complex and requires systematic investigation. Here, uncoated and silane-coated ammonium polyphosphate (APP, Si-APP) intumescent compounds are transferred to prepregs using a Bisphenol A diglycidyl ether (DGEBA) resin matrix to 0/90o bidirectional glass fibers with an aerial weight of 600 g/m2. Inorganic silicates (InSi) are added to improve the fire residues of the composites after combustion and the total amount of flame retardants in the resin formulations was 10% by weight. The prepregs' fiber volume content (FVC) is corroborated using in-process measurements and thermogravimetric analysis. This was found to be approximately 60% for the composites containing APP, which is ideal for load-bearing applications with high mechanical strength. However, the Si-APP containing prepregs showed an inconsistent FVC potentially due to interactions with the commercial sizing of the glass fibers. The composites subsequently prepared are analysed for potential filtration effects of the additives via SEM after immobilization in a cured resin and platinum sputtering. The inter-laminar shear strength and the mechanical strength of the composites are compared via three-point bending tests. Additionally, the fire performance of the composites is analysed using cone calorimetry. It was found there was minimal impact of the loading of the flame retardants on the delamination of the composites and the flexural strength. However, the high density of the glass fibers possibly results in a suppression of the mode of action of the flame retardants in the composites. Therefore, the fire residues of the composites are further compared using SEM, and the flame-retardant modes of action upon transfer are investigated.
Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. These polymers are characterized by a high permeability and reasonable permselectivity. The latter point is somehow surprising because for microporous systems a more Knudson-like diffusion is expected then a size dependent temperature activated sieving process. It was argued in the framework of a random gate model that molecular fluctuations on a time scale from ps to ns are responsible for the permselectivity.
Here series of polymers of intrinsic microporosity (PIMs) as well as microporous polynorbornenes with bulky Si side groups and a rigid backbone are considered. The polymers have different microporosity characterized by high BET surface area values.
First inelastic time-of-flight neutron scattering measurements were carried out to investigate the low frequency density of state (VDOS). The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. It was found that the frequency of the maximum position of the Boson peak correlates with the BET surface area value.
Secondly elastic scans as well as quasielastic neutron scattering measurements by a combination of neutron time-of-flight and backscattering have been out. A low temperature relaxation process was found for both polymers. This process was assigned to the methyl group rotation. It was analysed in terms of a jump diffusion in a three-fold potential. The analysis of the dependence of the elastic incoherent structure factor on the scattering vector yields the number of methyl groups which might be immobilized.
The neutron scattering experiments were accompanied by fast scanning calorimetry and broadband dielectric investigations as well as atomistic molecular dynamic simulations.
We report the selective ring opening copolymerisation (ROCOP) of
oxetane and phthalic thioanhydride by a heterobimetallic Cr(III)K
catalyst precisely yielding semi-crystalline alternating poly(esteralt-
thioesters) which show improved degradability due to the
thioester links in the polymer backbone.
Leather is a widely used material for thousands of years and in modern days it is produced on industrial scale. This production produces high amounts of organic waste during the tannery process. These fibers can become a resource and act as a multi-functional bio-filler in flame retardant composites.
This project investigates two leather fibers towards their ability to enhance the flame-retardancy in different composites. These composites use ammonium polyphosphate (APP) or aluminum trihydroxide (ATH) as flame retardants. Different silicon based synergists support polymers with ATH to reduce the load of flame retardant. The different modes of action (charring, gas phase activity, barrier effect) can be quantified of each composite.
The new composites form a stable char layer resulting in an increase in residue, lower peak heat release rates (pHRR) and higher limiting oxygen index (LOI). In addition, the ratings in the UL94-classification increased up to V-0.
Short overview is given of BAM's research within the topic "Flame Retardancy of Polymeric Materials". Fire science is identified as a crucial compentenc of BAM following our mission "Safety in Technology and Chemistry". In the area of polymers we work interdisciplinary, in the dimensions from nm to 2m, and we love to combine experiment and simulation. Multimethodical examples are given to describe the burning phenomena and flame-retardant modes of action. Further some examples are presented for tailored bench-scale fire testing and assessing concepts. Our goal is to provide the fundaments for a evidenced-based development of future materials.
The dataset provided in this repository comprises data obtained from a series of full-notch creep tests (FNCT) performed on selected high-density polyethylene (PE-HD) materials (for further details, see section 1 Materials in this document) in accordance with the corresponding standard ISO 16770.
The FNCT is one of the mechanical testing procedures used to characterize polymer materials with respect to their environmental stress cracking (ESC) behavior. It is widely applied for PE-HD materials, that are predominantly used for pipe and container applications. It is based on the determination of the time to failure for a test specimen under constant mechanical load in a well-defined and temperature controlled liquid environment. The test device used here also allows for continuous monitoring of applied force, specimen elongation and temperature.
For intumescent coatings durability is an important aspect. Due to ageing, which is caused by climatic conditions, the thermal protection performance of intumescent coatings can be reduced during the working life. The national German and the European procedures to assess the durability of intumescent coatings presume a working life of 10 years. For a longer period, additional investigations are required. However, the European assessment procedure does not provide specific information how to prove a durability of more than 10 years. In addition to this formal reason, also from a scientifical position, it is necessary to investigate the degradation of intumescent coatings in detail to propose a corresponding test concept for a durability of more than 10 years.
The presentation summarises the existing knowledge about the degradation behaviour and ageing of intumescent coatings. Furthermore, the results of different approaches from a recently conducted research project are presented. Starting from a water-based and an epoxy-based guide formulation, in a first approach a degradation of the intumescent coating was carried out directly during the production process, i.e. by reducing the concentration of functionally relevant chemical components. In another approach, the duration of the short-term weathering tests was significantly extended, i.e. by multiple repetition of the artificial weathering. The thermal protection performance of the intumescent coating was assessed by fire tests and tests with electrical heating source. In addition, small-scale tests were carried out to determine the thermal material properties of the intumescent coating and thermo-analytical methods were applied to characterise the degradation. Derived from this knowledge, possibilities to test and assess a working life for a period of more than 10 years are proposed.
Polyamide 4.6 (PA46) is a high-heat-resistant polymer, but it has no dripping resistance under fire. Three commercial grades of PA46 are investigated under UL 94 vertical fire test conditions. Their performances are discussed based on the materials’ structural, thermal, and rheological properties. PA46 presents flaming drops, whereas dripping is prevented in the flame-retarded PA46.
Friction-modified PA46 has increased flaming dripping. Temperature profiles of the specimens under fire and the temperature of the drops are measured by thermocouples. A UL 94 vertical test configuration consisting of two flame applications is designed to assess the quantitative dripping behavior of the set of materials by the particle finite element method (PFEM). Polymer properties (activation energy and Arrhenius coefficient of decomposition, char yield, density, effective heat of combustion, heat of decomposition, specific heat capacity, and thermal conductivity) in addition to rheological responses in high temperatures are estimated and measured as input parameters for the simulations. The dripping behavior obtained by simulated materials corresponds with the experimental results in terms of time and drop size. A consistent picture of the interplay of the different phenomena controlling dripping under fire appears to deliver a better understanding of the role of different materials’ properties
Thermal runaway investigations were performed by subjecting single and double NMC pouch cells to thermal abuse condition inside an air-tight reactor vessel with an internal volume of 100 dm³. The study was divided into two series. The findings revealed the thermal runaway-induced explosion in the cells results in a rate of temperature increase greater than 10 K/s. The highest gaseous production was achieved at a range of 90 – 100% SOC and higher battery capacities 0.79 L/Wh (Series 1, 10 Ah cell) and 0.87 L/Wh (Series 2, 32 Ah cell). The investigation showed between 25 m³ and 84 m³ of explosible gas mixture could be released from electric vehicles of nominal useable electrical energy from 32 kWh up to 108 kWh at thermal runaway. It was also found that, the release of these explosible gases could undergo a secondary explosion.
Only the nano-scaled structure of the nanocomposite and the dispersion of nanoparticles within the polymer matrix harbor multifunctional potential including superior fire retardancy. Thus, this chapter focuses on the dispersion of nanoplates, based mainly on studies of layered silicates and graphene/graphene-related nanoplates. The nanostructure and properties of the nanocomposites are dependent mainly on thermodynamic and kinetic factors during preparation. Improving nano-dispersion often directly improves flame retardancy. Therefore, the modification of the nanoplates as well as the preparation of nanocomposites becomes very important to control this dispersion. The dispersion of nanoplates functions as a prerequisite for the formation of an efficient protective layer, changing the melt flow and dripping behavior, or the improvement of the char properties.
Leather is a widely used material for thousands of years and in modern days it is produced on industrial scale. This production produces high amounts of organic waste during the tannery process. These fibers can become a resource and act as a multi-functional bio-filler in flame retardant composites.
This project investigates two leather fibers towards their ability to enhance the flame-retardancy in different composites. These composites use ammonium polyphosphate (APP) or aluminum trihydroxide (ATH) as flame retardants. Different synergists support polymers with ATH.
The new composites form a stable char layer resulting in an increase in residue, lower peak heat release rates (pHRR) and higher limiting oxygen index (LOI). In addition, the ratings in the UL94-classification increased up to V-0.
Avoiding antimony – effect of Ca(H2PO2)2 on smoke emission and fire behaviour in brominated ABS
(2023)
The replacement of antimony trioxide (Sb2O3) in brominated flame-retardant ABS (ABS/FR) is of great interest. This study investigates the influence of calcium hypophosphite (CaP) in ABS/FR on flame retardancy and smoke emission. Different amounts of talc are added to ABS/FR/CaP to evaluate the influence of an inorganic barrier on smoke emission and flame retardancy. The cone calorimeter unveiled a reduction by 46% in PHRR for ABS/FR/CaP. Additional 8 wt.-% talc (ABS/FR/CaP/8Talc) reduced the PHRR by 61%. ABS/FR/CaP exhibited a more condensed phase action, which resulted in less smoke emission. The study investigates the influence of CaP in ABS/FR on the smoke toxicity, smoke density and the smoke particles distribution in the smoke density chamber (ISO 5659-2) coupled to a FTIR spectrometer and electrical low pressure cascade impactor (ELPI).
Bench-scale fire stability testing - Protective layers in carbon fibre reinforced polymer laminates
(2023)
Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) composites usually demands intermediate-scale or full-scale testing. In this study, a bench-scale test is presented as a practicable and efficient method to assess the improvement in structural integrity of CFRP with different protective interlayers during fire.
This study presents the processability, fire behavior, and mechanical performance between the flame retarded pure epoxy resin and flame retarded glass-fiber-reinforced plastic before, during, and after a fire event. This enables a deeper understanding of the transferability of flame retardants, modes of action, char enhancement, and flame inhibition on composite materials
The site of Schöningen (Germany), dated to ca. 300,000 years ago, yielded the earliest large-scale record of humanly-made wooden tools. These include wooden spears and shorter double-pointed sticks, discovered in association with herbivores that were hunted and butchered along a lakeshore. Wooden tools have not been systematically analysed to the same standard as other Palaeolithic technologies, such as lithic or bone tools. Our multianalytical study includes micro-CT scanning, 3-dimensional microscopy, and Fourier transform infrared spectroscopy, supporting a systematic technological and taphonomic analysis, thus setting a new standard for wooden tool analysis. In illustrating the biography of one of Schöningen’s double-pointed sticks, we demonstrate new human behaviours for this time period, including sophisticated woodworking techniques. The hominins selected a spruce branch which they then debarked and shaped into an aerodynamic and ergonomic tool. They likely seasoned the wood to avoid cracking and warping. After a long period of use, it was probably lost while hunting, and was then rapidly buried in mud. Taphonomic alterations include damage from trampling, fungal attack, root damage and compression. Through our detailed analysis we show that Middle Pleistocene humans had a rich awareness of raw material properties, and possessed sophisticated woodworking skills. Alongside new detailed morphometrics of the object, an ethnographic review supports a primary function as a throwing stick for hunting, indicating potential hunting strategies and social contexts including for communal hunts involving children. The Schöningen throwing sticks may have been used to strategically disadvantage larger ungulates, potentially from distances of up to 30 metres. They also demonstrate that the hominins were technologically capable of capturing smaller fast prey and avian fauna, a behaviour evidenced at contemporaneous Middle Pleistocene archaeological sites.
Inelastic incoherent neutron time-of-flight scattering was employed to investigate the low-frequency vibrational density of states (VDOSs) for a series of glassy Janus-poly(tricyclononenes), which consist of a rigid main chain and flexible alkyl side chains. Here, the length of the flexible side chains was systematically varied from propyl to octyl. Such materials have potential applications as active separation layers in gas separation membranes as a green future technology, especially for the separation of higher hydrocarbons. From the morphological point of view, the Janus polynorbornenes undergo a nanophase separation into alkyl side chain-rich nanodomains surrounded by a rigid polynorbornene matrix. Here, the influence of the nanophase-separated structure on the low-frequency VDOS is investigated from a fundamental point of view. The low-frequency VDOSs of these Janus polynorbornene show excess contributions to the Debye type VDOS known as the Boson peak (BP) for all side chain lengths. Due to the high incoherent scattering cross-section of hydrogen, most of the scattering comes from the alkyl side chain-rich domains.
Compared to conventional glass-forming materials, in the considered Janus polynorbornenes, the BP has a much lower intensity and its frequency position is shifted to higher values. These experimental results are discussed in terms of the nanophase-separated structure where the alkyl chain-rich domains were constrained by the surrounding matrix dominated by the rigid backbone. With increasing alkyl chain length, the size of the alkyl chain-rich domains increases. The frequency position of the BP shifts linearly to lower frequencies with the size of these nanodomains estimated from X-ray measurements. The obtained results support the sound wave interpretation to the BP
For a comprehensive safety assessment of stationary lithium-ion-battery applications, it is necessary to better understand the consequences of thermal runaway (TR). In this study, experimental tests comprising twelve TR experiments including four single-cell tests, two cell stack tests and six second-life module tests (2.65 kW h and 6.85 kW h) with an NMC-cathode under similar initial conditions were conducted. The temperature (direct at cells/modules and in near field), mass loss, cell/module voltage, and qualitative vent gas composition (Fourier transform infrared (FTIR) and diode laser spectroscopy (DLS) for HF) were measured. The results of the tests showed that the battery TR is accompanied by severe and in some cases violent chemical reactions. In most cases, TR was not accompanied by pregassing of the modules. Jet flames up to a length of 5 m and fragment throwing to distances to more than 30 m were detected. The TR of the tested modules was accompanied by significant mass loss of up to 82%. The maximum HF concentration measured was 76 ppm, whereby the measured HF concentrations in the module tests were not necessarily higher than that in the cell stack tests.
Subsequently, an explosion of the released vent gas occurred in one of the tests, resulting in the intensification of the negative consequences. According to the evaluation of the gas measurements with regard to toxicity base on the “Acute Exposure Guideline Levels” (AEGL), there is some concern with regards to CO, which may be equally as important to consider as the release of HF.
Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) composites usually demands intermediate-scale or full-scale testing. In this study, a bench-scale test is presented as a practicable and efficient method to assess the improvement in structural integrity of CFRP with different protective interlayers during fire.
Fire stability is one of the biggest issues of carbon fibre reinforced polymer (CFRP) composites, particularly when they are using in load bearing applications. As soon as the glass transition temperature of polymer matrix (100-200°C) is achieved, the composite loses its structural integrity, what leads to the distortion and failure. The principal fire stability test is based on simultaneous application of fire and mechanical load. Since the carbon fibres can transfer the tensile loads quite well, the compression load is chosen as a required mechanical load for a test. The fire tests were preceded by a static load test at room temperature to determine ultimate failure load. The specimen was loaded with a compression force until the failure load was reached, which was observed as a buckling. For the fire tests, 10% of compression failure load and direct flame of a fully developed fire (heat flux ≈ 180 kW m-2) were applied simultaneously to the specimen, while the time to failure was measured.
The possibilities of bench-scale fire stability testing were presented by investigating new types of laminate structures, which exhibit promising flame retardancy and fireproof properties. The new approach of CFRP laminate differs with a protective concept. Every system consists of two different interlayers (titanium foil, thermoplastic foil PEI, ceramic layer WHIPOX, rubber tape Pyrostat, basalt fibres and kenaf fibres), where the one layer constitutes the fireproof protection, that delays the rise of temperature in the rest of laminate, and the second layer provides very good structural connection with carbon fibre layers, thus improves the mechanical integrity of CFRP composite in fire.
The time to failure of CFRP composite was 17s. Protective systems significantly enhance the fire stability and increased time to failure by 3 to 10 times. Thicker specimens showed longer resistance time, however CFRP laminate with ceramic layer and titanium foil presented outstanding results and the best performance. The protection with Kenaf and basalt fibres offered a natural fibre solution with also good fire resistance performance
Although bench-scale tests are limited with respect to assessing the performance of components and structures, they are valuable in the assessment of different materials concepts. Furthermore, the reduced effort of conducting bench-scale test (lower costs, time, personnel resources) makes it more practical and effective.
Fire resistance of fiber-reinforced polymers (FRPs) has been an important area of research for many years since FRPs are mainly used in the transportation and construction sectors. This study presents the fire behavior, and mechanical performance between the flame retarded pure epoxy resin and flame retarded glass-fiber composites before, during, and after a fire event. This enables a deeper understanding of the transferability of flame retardants on composite materials.
Main message: Sustainability, or in other words, exploiting environmental conservation for the economic welfare and prosperity for all, would revolutionise the plastics industry were it to become predominant practice as a linear, fossil-fuel–based economy is switched to a carbon circular economy. Food for though is given by dint of a critical overview of the current trends in sustainable flame-retardant polymeric materials.
Introduction:
Transforming the plastics industry into a carbon circular economy over the next 30 years requires an immediate revolution entailing the development of cutting-edge materials and the planning of future industrial production plants. Hence, the innovative field of flame-retardant polymeric materials should lend its strength to drive this challenge. Visionary solutions are proposed to inspire us, while the implementation of economically feasible concepts can take us forward into the future.
Experimental The synthesis, processing, polymer analysis, thermal analysis, and investigation of fire behaviour from our own research are performed according to the state of the art, mostly in accordance with the pertinent ISO standards. Indeed, some of our equipment is part of the accredited lab; for the other methods we fulfil equivalent quality standards in terms of maintenance, calibration, participation in round robins, etc. Work steps such as the synthesis or preparation of new materials are usually outsourced or done with partners that have the relevant core competence. The talk also presents examples from other groups whose experimental is described in the corresponding scientific papers.
Results and Discussion An overview of current trends towards producing sustainable, flame-retardant polymeric materials is presented, using examples from the literature and by sketching our own projects performed in recent years. The examples are structured along a common theme leading from the use of old and new natural materials with some intrinsic flame retardancy, via flame-retardant biopolymers and biocomposites, to using renewable sources for flame retardants with the objective of exploiting natural sources available as industrial waste streams. Natural flame retardants and adjuvants are highlighted, although the status of most may be assessed as merely motivating our vision. Nevertheless, there are natural material streams finding their way into polymer mass production as fillers, adjuvants, polymers, or renewable educt sources. Natural substances originating from industrial waste streams open the door to sustainable solutions, because they are often available at low cost and avoid competition for land with farming or virgin forests. Aside from this main topic, remarks will address the recycling of flame-retarded polymeric materials; vitrimers are mentioned as a potential material for recyclable thermosets. At the end of the day, only convincing property profiles will prevail both for exploiting renewable sources and circular design, including cost effectiveness, sufficient availability, consistent quality, processibility, mechanical properties, and flame retardancy. However, sustainability must not be merely tolerated as an additional demand, but should instead be recognized as a solution, because sustainability aspires to ensure our economic welfare now and in the future.
Acknowledgement:
The examples shown from own project were supported by funding grants: BMBF WTZ: 01DN16040, DFG Scha 730/19-1, VW-Stiftung: Experiment No: 97437, DFG Scha 730/20-1, BMBF KMU Innovativ 031B1289B.
Slow crack growth (SCG) under the influence of external fluid media, usually termed environmental stress cracking (ESC), is still one of the most frequent origins of severe damage and failure of polymeric materials. For polyethylene (PE) this is relevant for mass products, like bottles for consumer products, but also for high-performance materials for pipes or industrial packaging, including containers for chemicals and other dangerous goods. Especially for high-density polyethylene (PE-HD) the susceptibility to SGC and ESC is depending on the complex interplay between molecular weight and architecture and the resulting semicrystalline morphology, especially the formation of tie-molecules.
A reliable assessment of the resistance against this damage phenomenon is essential for demanding as well as safety-critical applications and has to take into account suitable testing methodologies and conditions in combination with environmental media reflecting the properties representative for typical fillings and relevant components causing ESC. In this context a better understanding of different influencing factors, such as sorption, swelling or surface activity is necessary together with a detailed characterization of different stages of crack propagation and underlying mechanisms. Therefor well-established testing methods, such as the Full Notch Creep Test (FNCT), were complemented by detailed fracture surface analysis using e.g. LSM and SEM in combination with a time-dependent optical monitoring of the progressing crack growth.
For the crack growth also the ratio of fibrillated craze zone to crack opening is important for the deeper understanding of crack propagation and related material parameters which can be additionally addressed by X-ray computed tomography.
A few layer/multilayer graphene (MLG) with a specific surface area of BET ≥ 250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution or latex premixing of master batches followed by conventional two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of ca. 35, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR).[1-5] 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM).[6-8] The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
Composition and Explosibility of Gas Emissions from Lithium-Ion Batteries Undergoing Thermal Runaway
(2023)
Lithium-based batteries have the potential to undergo thermal runaway (TR), during which mixtures of gases are released. The purpose of this study was to assess the explosibility of the gaseous emission from LIBs of an NMC-based cathode during thermal runaway. In the current project, a series of pouch lithium-based battery cells was exposed to abuse conditions (thermal) to study the total amount of gases released and the composition of the gas mixture. First, the battery cells were placed in a closed vessel, and the pressure and temperature rise inside the vessel were measured. In a second step, the composition of gases was analysed using a Fourier transform Infrared (FTIR) spectrometer.
We found that the amount of released gases was up to 102 ± 4 L, with a clear dependence on the battery capacity. This study showed that the concentration of gaseous emissions such as carbon monoxide (CO), methane (CH4), ethylene (C2H4), ethane (C2H6), and hydrogen cyanide (HCN) increased with higher cell capacity. Of the five studied flammable gases, the maximum concentrations of carbon monoxide (16.85 vol%), methane (7.6 vol%), and ethylene (7.86 vol%) were identified to be within their explosible range. Applying Le Chatelier’s law, a calculated lower explosion limit (LEL) of 7% in volume fraction was obtained for the gas mixture. The upper explosion limit (UEL) of the gas mixture was also found to be 31% in volume. A filter comprising pyrobubbles was used for the removal of the studied gas components released during the thermal abuse. The investigation revealed that the pyrobubbles filter was highly effect in the removal of HCN (up to 94% removal) and CO2 (up to 100% removal). Herein, we report the dependency of the method of thermal runaway trigger on the measured maximum temperature.
In recent years, fire safety requirements for bus interior materials have been increased and introduced into international regulations. Fire safety requirements for the burning rate, melting and dripping behaviour of interior materials already exist for many years. However, it remains unclear to what extent the release of smoke, combustion products and their toxicity should be limited. Therefore, a research and development project 82.0723 funded by BASt (Federal Highway Research Institute) was initiated to develop a simplified procedure for testing the toxicity and smoke development in case of fire of interior materials used in buses. The scope of the research included calculations to assess the toxicity of fire gases and the derivation of specifications for the formation of practicable limit values for smoke toxicity. Further investigations are needed to derive these limit values for smoke toxicity in order to be applicable for real fire scenarios in buses.
Das EU Projekt TREEADS „A Holistic Fire Management Ecosystem for Prevention, Detection and Restoration of Environmental
Desasters” beschäftigt sich mit der Erforschung der drei Phasen „Prävention und Bereitschaft“, „Detektion und Reaktion“ und
„Aufforsten und Anpassen“ der Waldbrandverhütung. Im Projekt gibt es acht ausgewiesene Pilotregionen, in denen Deutschland
auch mit einer Pilotregion in Sachsen-Anhalt bzw. in Brandenburg vertreten ist. Unsere Arbeit auf Charakterisierung des Waldbodens und numerische Simulation wird vorgestellt.
Although fire safety regulations for buses have been adapted in recent years regarding, for example, fire detection and engine fire suppression systems, the changes in regulations for bus interior materials are minimal. A comparison of fire safety regulations for interior materials in other transport sectors for trains, ships or aircraft reveals a much lower level of requirements for bus materials. Although repeated bus accidents as well as fire statistics show the danger a bus fire can pose to passengers.
In particular, the combination of a fire incident and passengers with reduced mobility led to severe disasters in Germany and other European countries. To enhance the fire safety for passengers, the interior bus materials are crucial as the fire development in the bus cabin determines whether escape and rescue is possible. Against this background, bus interior materials were tested in different fire test scenarios. Measurement of a wide variety of parameters, for example, the mass loss, ignition time, smoke gas composition, heat release rate among others were carried out. Tested materials complied to the newest set of requirements. For this purpose, interior materials and their components had to be identified according to their chemical structure. Parts of the tests were funded by BASt (Federal Highway Research Institute) in the project 82.0723/2018. Experimental results show reaction-to-fire behaviour which lead to very limited times for escape and rescue in case of fire in a bus cabin. Based on the studies on fire behaviour and toxicity assessment, recommendations for improved fire safety regulations for interior materials could be made.
Das EU Projekt EU FireStat SI2.830108, das vom Europäischen Parlament finanziert und von der DG GROW der Europäischen Kommission in Auftrag gegeben wurde, hat aufgearbeitet, welche Terminologie in den europäische Mitgliedsstaaten verwendet wird und die von den Mitgliedstaaten erhobenen Daten über Gebäudebrände zu analysieren. Dabei wurden die Schwierigkeiten bei der Erfassung und die Unterschiede bei der Auslegung ermittelt und eine gemeinsame Terminologie sowie eine Methode zur Erfassung der erforderlichen Daten vorgeschlagen.
Folgende Schwerpunkte wurden bearbeitet: Zunächst erfolgte eine Diagnose von Terminologie-, Datenerhebungs- und Auslegungsproblemen, Erhebung der Terminologie und der Datenerfassung, Identifizierung der für die Entscheidungsfindung benötigten Daten, Analyse der Methoden zur Datenerhebung Definition einer gemeinsamen Terminologie, Methodik der Kosten-/Nutzenbewertung zur Unterstützung politischer Entscheidungen, Fallstudie zur Anwendung der Methode der Kosten-/Nutzenbewertung, Beschreibung einer zukünftigen Datenerhebungsmethode.
Das Ergebnis des Projekts ist eine Empfehlung, welche Daten in den Mitgliedstaaten erhoben werden sollten, um wissensbasierte Entscheidungen in Bezug auf den Brandschutz zu ermöglichen. Damit wird die Grundlage für Maßnahmen und Initiativen geschaffen, die den Brandschutz und die Brandverhütung der Mitgliedstaaten unterstützen, so dass knappe Ressourcen gezielt eingesetzt werden können.
Das EU Projekt EU FireStat SI2.830108, das vom Europäischen Parlament finanziert und von der DG GROW der Europäischen Kommission in Auftrag gegeben wurde, hat aufgearbeitet, welche Terminologie in den europäische Mitgliedsstaaten verwendet wird und die von den Mitgliedstaaten erhobenen Daten über Gebäudebrände zu analysieren. Dabei wurden die Schwierigkeiten bei der Erfassung und die Unterschiede bei der Auslegung ermittelt und eine gemeinsame Terminologie sowie eine Methode zur Erfassung der erforderlichen Daten vorgeschlagen.
Folgende Schwerpunkte wurden bearbeitet: Zunächst erfolgte eine Diagnose von Terminologie-, Datenerhebungs- und Auslegungsproblemen, Erhebung der Terminologie und der Datenerfassung, Identifizierung der für die Entscheidungsfindung benötigten Daten, Analyse der Methoden zur Datenerhebung Definition einer gemeinsamen Terminologie, Methodik der Kosten-/Nutzenbewertung zur Unterstützung politischer Entscheidungen, Fallstudie zur Anwendung der Methode der Kosten-/Nutzenbewertung, Beschreibung einer zukünftigen Datenerhebungsmethode.
Das Ergebnis des Projekts ist eine Empfehlung, welche Daten in den Mitgliedstaaten erhoben werden sollten, um wissensbasierte Entscheidungen in Bezug auf den Brandschutz zu ermöglichen. Damit wird die Grundlage für Maßnahmen und Initiativen geschaffen, die den Brandschutz und die Brandverhütung der Mitgliedstaaten unterstützen, so dass knappe Ressourcen gezielt eingesetzt werden können.
A well-defined terminology of fire-related variables is important for correct analyses and supporting knowledge-based decisions regarding the evaluation of building fires at the European level. After developing an overview of current practices for fire statistics in Part I, the terminology used and the data collected by the EU Member States and eight other countries regarding fire incidents, property damage and human losses were mapped to increase awareness of their practice and support a comprehensive assessment of several fire statistical datasets. A questionnaire was distributed to relevant authorities responsible for the collection, elaboration/analysis, and fire statistical data publications to define and select the essential variables for an appropriate fire assessment and fire incident description. Based on the results of the questionnaire able to identify the essential fire statistical variables and a detailed analysis of current definitions adopted in the fire statistics of the EU Member States and other countries, a common terminology is proposed to collect the necessary data in the EU Member States and obtain meaningful datasets based on standardised terms and definitions. The results will generate essential outputs to move towards harmonised fire statistics at the EU level and contribute to an appropriate analysis able to improve fire prevention and fire mitigation in building fires.
This study provides an analysis on the fire safety of passengers and the fire protection of coaches and buses. A brief review of major bus fire incidents, an overview of current regulations in Europe, and their limitations are presented. The study finds that the current small-scale fire test methods described in UN ECE Reg No. 118 need to be replaced by test methods that can assess the reaction to fire of materials when exposed to ignition sources of varying sizes. To address these shortcomings, the study proposed an expert recommendation to update the material fire safety requirements and testing for buses. Additional measures are proposed, derived from objectives and strategies applied in other transport sectors, and can be tested through existing European and international standards, which are widely used by several industries. These measures aim to extend the time with tenable conditions for a safe evacuation in case of fire, reduce the degree of damage to buses, reduce the risk for fast and excessive thermal exposure on modern energy carriers needed for a more sustainable transport sector.
The addition of nanoparticles as reinforcing fillers in elastomers yields nanocomposites with unique property profiles, which opens the door for various new application fields. Major factors influencing the performance of nanocomposites are studied by varying the type and shape of nanoparticles and their dispersion in the natural rubber matrix. The industrial applicability of these nanocomposites is put into focus using two types of graphene and a nanoscale carbon black, all commercially available, and scalable processing techniques in the form of a highly filled masterbatch production via latex premixing by simple stirring or ultrasonically assisted dispersing with surfactant followed by conventional two-roll milling and hot pressing. Different processing and measurement methods reveal the potential for possible improvements: rheology, curing behavior, static and dynamic mechanical properties, swelling, and fire behavior. The aspect ratio of the nanoparticles and their interaction with the surrounding matrix prove to be crucial for the development of superior nanocomposites. An enhanced dispersing method enables the utilization of the improvement potential at low filler loadings (3 parts per hundred of rubber [phr]) and yields multifunctional rubber nanocomposites: two-dimensional layered particles (graphene) result in anisotropic material behavior with strong reinforcement in the in-plane direction (157% increase in the Young's modulus). The peak heat release rate in the cone calorimeter is reduced by 55% by incorporating 3 phr of few-layer graphene via an optimized dispersing process.
The analysis of the current state of fire statistics and data collection in Europe and other countries is needed to increase awareness of how fire incidents affect buildings and to support pan-European fire prevention and fire mitigation measures.
The terminology and data collected regarding fire incidents in buildings in the EU Member States were mapped to obtain meaningful datasets to determine common terminology, collection methodology, and data interpretation system. An extensive literature review showed that fire data collection systems have been instrumental in informing firefighting strategies, evidence-based planning, prevention, and educational programmes. Differences and similarities between fire data collection systems were also investigated. The amount and quality of the information in fire statistical recording systems appear to be influenced by the complexity and structure with which the data are collected. The analysis also examined the existing fire statistics in the EU Member States and a few other countries. Finally, a detailed investigation of the number of fires, fire deaths, and injuries from 2009 to 2018 in several countries was examined based on data from a report by CTIF. The trends showed differences attributable to the existing fire statistical practices in terms of terminology and data
collection, and interpretation. Part II proposes a common terminology for selected fire statistical variables. The results provide relevant information regarding fire safety at the European level and should be used to guide the development of more uniform fire statistics across Europe.
A series of flexible polyurethane foams (FPUFs) were prepared with single and different combinations of flame retardants and additives. Expandable graphite (EG), phosphorous polyol (OP), copper (II) oxide (CuO), and/or castor oil (CAS) were added to FPUF during the foam preparation in a one-step process. The purpose of the study is to evaluate the synergistic effects of the flame retardants, additives, and the presence of bio-based content on the mechanical properties, flame retardancy, and smoke behavior of FPUFs. The combination of 10 wt % EG and 5 wt % OP in FPUF significantly improves the char yield. In the cone calorimeter experiment, the char yield is nearly three times higher than that with 10 wt % EG alone. The smoke behavior is additionally evaluated in a smoke density chamber (SDC). Comparing the samples with a single flame retardant, 10 wt % EG in FPUF considerably reduces the amount of smoke released and the emission of toxic gases. Replacing the amount of 10 wt % polyether polyol in FPUF with CAS maintains the physical and mechanical properties and fire behavior and enhances the bio-based content. The presence of 0.1 wt % CuO in FPUF effectively reduces the emission of hydrogen cyanide. As a result, this study proposes a multicomponent flame retardant strategy for FPUF to enhance the biomass content and address the weaknesses in flame retardancy, smoke, and toxic gas emissions. A starting point is disclosed for future product development.
Packaging containers for dangerous goods that include aggressive liquids require that any packaging material that is based on high-density polyethylene has a high degree of stability and durability. This work is focused on testing the environmental stress cracking of the high-density polyethylenes used for such containers in contact with crop protection formulations, in particular, two model liquids established in Germany as standardized test media representatives for crop protection formulations containing the various admixtures typical for such products. One of the liquids is water-based and contains mostly surface-active ingredients, while the other is solvent-based and includes some emulsifiers. Originally established for pin impression tests, these model liquids and their individual components were here used for the first time as environmental media in the Full Notch Creep Test, which addresses the resistance against environmental stress cracking. The Full Notch Creep Test was carried out on five high-density polyethylene types with both model liquids, and also on one selected material with its components. The evaluation was focused on the fracture surface structures, which were visualized by a scanning electron microscope and by optical in situ imaging of the notch opening. While the water-based model liquid and its surface-active individual components induced environmental stress cracking with the characteristic pattern for a craze-crack mechanism and so-called brittle fracture on the surface, the solvent-based model liquid and its soluble ingredients exhibited rather ductile failure behavior, caused by the plasticizing effect on the polymer that reduced the yield stress of the high-density polyethylene.
For both cases, fracture surface analysis, together with side views of the crack opening, showed a clear relation between surface pattern, notch deformation (e.g., by blunting), or crack opening due to crack growth with time to failure and the solubility of the liquids in high-density polyethylene.
Aufgrund des tieferen Eindringens der solaren Strahlung treten bei transparenten und bei transluzenten (durchscheinenden) Kunststoffen veränderte Bedingungen gegenüber opaken Proben auf. Dies kann zu speziellen Effekten und damit zu einem abweichenden Bewitterungsverhalten führen. Auch aus Mangel an geeigneten Normen werden diese Effekte häufig vernachlässigt. Deshalb initiiert der DIN-FNK auf ISO-Ebene ein entsprechendes Dokument.
Die Norm ist in der Form eines Technical Reports geplant. In einem ersten Teil sollen die Besonderheiten transparenter oder transluzenter Kunststoffe erläutert werden, um den Nutzer für mögliche Probleme zu sensibilisieren. Im zweiten Teil werden Empfehlungen für Bestrahlung oder Bewitterung herausgearbeitet. In einem dritten Teil geht es dann um Besonderheiten bei der Messung von Eigenschaftsänderungen transparenter bzw. transluzenter Kunststoffe. In informativen Anhängen sollen verschiedene Beispiele die Thematik illustrieren.
Im Rahmen des Forschungsprojektes IGF 20470N wurden Untersuchungen zum Alterungsverhalten von reaktiven Brandschutzsystemen (RBS) auf Stahlbauteilen durchgeführt. Mithilfe der Ergebnisse einer umfangreichen Literaturrecherche sowie experimentellen und numerischen Untersuchungen sollte ein Vorschlag für ein Prüfkonzept zum Nachweis einer Nutzungsdauer von RBS von mehr als 10 Jahren auf Basis von Kurzzeitversuchen abgeleitet werden. Dabei setzt die Bewertung des Alterungsverhaltens von RBS voraus, dass die Mechanismen der Alterung hinreichend bekannt sind.
Dafür wurden zunächst systematisch Daten von Kurz- und Langzeitversuchen von nationalen Zulassungsprüfungen der letzten Jahrzehnte ausgewertet. Anschließend wurden umfangreiche experimentelle Untersuchungen an einer wasserbasierten sowie einer epoxidharzbasierten Richtrezeptur durchgeführt. Da aus der Literatur bekannt ist, dass die Einflüsse der Bewitterung zu einer Veränderung der Konzentration der Bestandteile innerhalb der Beschichtung führen können, wurden Untersuchungen mit Mangelrezepturen durchgeführt, wobei systematisch einzelne Bestandteile reduziert wurden. Neben optischen Untersuchungen wurden thermoanalytische Verfahren (DSC-TG-, ATR-FTIR-, Elementar-, Farbanalyse) angewandt sowie Brandversuche an beschichteten Stahlplatten durchgeführt. Des Weiteren wurden die Richtrezepturen den beschleunigten Kurzzeitversuchen gemäß EAD 350402-00-1106 (2017) unterzogen, welche die Zulassung von Produkten auf europäischer Ebene regelt. Für die wasserbasierte Richtrezeptur wurden die Bewitterung für den feuchten Innenraum (Typ Z1) mehrfach wiederholt (1x, 3x, 6x). Für die epoxidharzbasierte Richtrezeptur entsprach die Bewitterung dem Zyklus für die Außenanwendung (Typ X). In Brandversuchen sowie thermoanalytischen und optischen Untersuchungen wurde das Alterungsverhalten sowie die thermische Schutzwirkung analysiert.
Anschließend wurden numerische Simulationen von Stahlbauteilen mit gealterten RBS durchgeführt und anhand der experimentellen Untersuchungen validiert. Mithilfe der numerischen Modelle kann eine Bewertung der thermischen Schutzwirkung von Stahlbauteilen mit gealterten RBS vorgenommen werden.
Mithilfe der gesammelten Erkenntnisse wurde ein Vorschlag für ein Prüfkonzept für den Nachweis einer Nutzungsdauer von mehr als 10 Jahren abgeleitet. Das Prüfkonzept besteht dabei aus einem Katalog von Möglichkeiten, die aktuellen Zulassungsprüfungen auf europäischer Ebene für eine Nutzungsdauer von 10 Jahren auf einen längeren Zeitraum zu erweitern.
In the processing of nanocomposites, high shear stresses at elevated tempera-tures orient two-dimensional nanoparticles like graphene. This orientationleads to anisotropic mechanical, thermal or barrier properties of the nanocom-posite. This anisotropy is addressed in this study by comparing graphene (few-layer graphene, FLG) with a nanoscaled carbon black (nCB) at a filler contentof 3 phr, by varying the vulcanization, and by comparing different FLG con-tents. Transmission electron microscopy gives insight into the qualitative ori-entation in the nanocomposite with FLG or nCB. The storage moduli paralleland normal to the orientation reveal the direction dependency of reinforce-ment through dynamic mechanical analysis (DMA). Dimensional swellingmeasurements show a restriction of the expansion parallel to the FLG orienta-tion, and an increased expansion normal to the orientation. The vulcanizationsystem and crosslinking determine the respective level of property values, andhigher crosslinking densities increase the anisotropy in DMA resulting invalues of up to 2.9 for the quantified anisotropy factor. With increasing FLGcontent, the anisotropy increases. A comparison of the results reveals swellingmeasurements as the most suitable method for the determination of anisot-ropy. Compared to recent literature, the presented processing induces higheranisotropy, leading to higher reinforcing effects in the direction of orientation
Produkte, Bauteile und Konstruktionen im Transport- und Bauwesen bestehen mehr und mehr aus Klebverbunden. Allein die Menge des verwendeten Klebstoffes oder die Anzahl geklebter Verbindungen schließen für eine verlässliche Betrachtung und Bewertung der Brandrisiken aus, deren Beitrag zur Brandentstehung, Flammenausbreitung oder Feuerwiderstand von Baugruppen und Konstruktionen zu vernachlässigen. Anforderungen an die Leistungsbeschreibungen von flammgeschützten Klebstoffen bzw. Haftklebebändern werden definiert, oft ohne ein ausreichendes Verständnis der Beiträge von Klebverbunden zum Brandverhalten der Bauteile zu haben. Der Vortrag beleuchtet diese Problematik und stellt die verschiedenen komplexen Anforderungen aus dem Brandschutz in Hinblick auf Auswahlkriterien und Entwicklungsziele für flammgeschützte Klebstoffe dar. Dabei ist dieser Transfer des Brandverhaltens, sprich der Systemantwort einer Komponente oder Bauteils in einem spezifischen Brandszenario, in Materialeigenschaften des Klebstoffes eine intrinsische und anspruchsvolle Herausforderung. Im abgeschlossenen IGF-Projekt Nr. 20762 N (Forschungsvereinigung DECHEMA) haben wir für Klebebänder eine systematisch-wissenschaftliche Studie durchgeführt und aussagekräftige Erkenntnisse zu Verfügung gestellt. Die Untersuchungen zur Entflammbarkeit zu Brandbeginn, zur Flammenausbreitung (Wärmeentwicklung) im sich entwickelnden Brand und zum Feuerwiderstand im Vollbrand machen die sehr unterschiedlichen Einflüsse von Klebverbunden, d. h. auch die unterschiedlichen Anforderungen an die Modifikation der Klebebänder, deutlich. Die thermische Analyse verschiedener Klebstoffe zusammen mit den Brandtest freistehender Haftklebebänder, an einseitig geklebten Substraten und an Klebverbundprobekörpern skizzieren eindrucksvoll die komplexen Zusammenhänge zwischen Materialeigenschaften der Klebebänder und dem Brandverhalten von Klebverbunden. Der Vergleich von verschiedenen Substraten wie Stahlbleche, Holz, Mineralwolle und verschiedene Polymermaterialien belegt darüber hinaus, dass der Einfluss der Klebverbindungen auf das Brandverhalten der Klebverbunde substratspezifisch ist. Gerade der Vergleich zwischen Holz, Polymethylmethacrylat (PMMA) und Bisphenol A Polycarbonat (PC) liefert überraschend unterschiedliche Ergebnisse. Die Variation der Klebstoffe und Trägermaterialien der Klebebänder skizziert die verschiedenen Möglichkeiten für die Materialentwicklung. Abhängig vom Material und Brandszenario können Klebverbunde im Vergleich zu gleich dicken Probekörpern aus demselben Substrat sowohl eine deutliche Erhöhung der Brandrisiken, ein praktisch unverändertes Brandverhalten oder eine Reduktion des Brandrisikos hervorrufen. Grundsätzlich kann keine Lösung bzw. kein Tape gefunden werden, die mit allen Substraten einen guten Brandschutz gewährleistet. Substrate, Carrier und Klebstoff müssen nicht nur aufeinander abgestimmt werden, sondern auch auf das Brandszenario, in welchem der Verbund eine gute Performance liefern soll.Das IGF-Projekt (20762) der Forschungsgemeinschaft (DECHEMA Deutsche Gesellschaft für Chemische Technik und Biotechnologie e V, Theodor Heuss Allee 25, 60486 Frankfurt am Main) wurde durch die AiF im Rahmen des Programms „Förderung der Industriellen Gemeinschaftsforschung (IGF)” des Bundesministeriums für Wirtschaft und Klimaschutz aufgrund eines Beschlusses des Deutschen Bundestages gefördert.
As most of polymeric materials are inherently flammable, flame retardants (FR) are commonly used to reduce their fire risks. Nevertheless, these flame retardant materials are often detrimental to smoke parameters like specific optical density or smoke toxicity. The influence of several smoke suppressants (SP)-zinc stannate, zinc phosphate, titanium oxide and hydrotalcite-were investigated with respect to flame retardancy, smoke emission, particle emission and smoke toxicity in a diethyl aluminum phosphinate (AlPi) flame retardant polyamide 6.6 (PA6.6). It was shown that the interaction between SP, FR and polymer is crucial for smoke and fire properties and can change the mode of action of the FR as well the decomposition mechanism of the polymer. Small amounts of SP show less effect on forced flaming behavior and the optical density, but they can influence flammability and the particle size distribution of the soot particles. The flame retardancy was significantly enhanced by 5 wt.-% zinc stannate in PA6.6 under forced flaming conditions. The charring mechanism was improved, and the mode of action of AlPi switched from the gas to the condensed phase. This resulted of in a reduced PHRR and TSP and an increase in residue yield. The smoke toxicity and optical density were reduced in the smoke density chamber as well. The smoke particles shifted to smaller sizes as the time in the pyrolytic zone increased. The formation of a dense char is assumed to be the key factor to enhance smoke suppression and flame retardancy properties.
Meta-analysis of heat release and smoke gas emission during thermal runaway of lithium-ion batteries
(2023)
Herein a meta-analysis of 76 experimental research papers from 2000 to 2021 is given about possible effects on the thermal runaway of lithium-ion battery cells. Data on the hazards of gas emissions and released heat are related to each other and differentiated by cell properties such as, cell geometry, cathode type or state of charge. Quantitative information on the total heat release in the range of 2.0–112.0 kJ Wh−1, the peak heat release rate in the range of 0.006–2.8 kW Wh−1and the smoke gas emission were extracted, normalized in terms of cell energy (Wh), combined in a data library and compared graphically. The total amount of gas emitted (3–48 mmol Wh−1) as well as the released amount of carbon monoxide (1–161 mg Wh−1) and hydrogen fluoride (2–197 mg Wh−1) were investigated as a function of the state of charge and cell geometry. The analysis reveals that the measured values are significantly influenced by the types of calorimeters and smoke gas analyzers used as well as by the type of thermal runaway trigger. This meta-analysis can serve as an important basis for any risk assessment of lithium-ion batteries.
The impact of phosphorus-containing flame retardants (FR) on rigid polyisocyanurate (PIR) foams is studied by systematic variation of the chemical structure of the FR, including non-NCO-reactive and NCO-reactive dibenzo[d,f][1,3,2]dioxaphosphepine 6-oxide (BPPO)- and 9,10 dihydro-9-oxa-10 phosphaphenanthrene-10-oxide (DOPO)-containing compounds, among them a number of compounds not reported so far. These PIR foams are compared with PIR foams without FR and with standard FRs with respect to foam properties, thermal decomposition, and fire behavior. Although BPPO and DOPO differ by just one oxygen atom, the impact on the FR properties is very significant: when the FR is a filler or a dangling (dead) end in the PIR polymer network, DOPO is more effective than BPPO. When the FR is a subunit of a diol and it is fully incorporated in the PIR network, BPPO delivers superior results.
Polyurethane foams (PUF) are generally flammable, so they are limited in some applications due to strict fire safety requirements. In this study, three distinct industrial benchmark polyurethane foams containing synergistic combinations of expandable graphite (EG) and phosphorous flame retardants (P-FR) were investigated one by one for their fire performance and smoke behavior. This paper aims to substantiate the hypothesis that the combination of EG and P-FR used in polyurethane foams yields a top-notch composite in terms of flame retardancy and smoke behavior by meeting the demanding requirement of low maximum average heat emission (MARHE) and smoke emission in a variety of applications, like advanced materials in construction, lightweight materials for railways, and more.
Leather is considered a luxury good when used in seating and upholstery. To improve safety, flame retardancy in leather is usually achieved through various finishing processes such as spray or roller coating. These treatments require processing steps that cost time and are laborintensive. One avenue to achieving flame retardancy in leather is to add flame retardants during the tanning process. However, the influence on flame retardancy exerted by specific intumescent additives specifically added during leather tanning has yet to be investigated. This work explores the roles played by intumescent additive compounds in flame retarding leather when they are added during tanning instead of applied as a coating. Via a systematic investigation of various compound mixtures, the flame retardant effects in the condensed and the gas phases are elucidated. The results show a strong impact of melamine in the gas phase and of polyphosphates in the condensed phase. Their impact was quantified in fire and smoke analysis, showing a 14% reduction in the peak of heat release rate, strongly reduced burning lengths, and a 20% reduction in total smoke release compared to nontreated leather. These results illuminate the key role played by specific compounds in the flame retardancy of leather, particularly when they are added specifically during the tanning process instead of being applied as a coating.
This method has great potential to reduce processing steps, lower costs, and improve material safety.
Reaktive Brandschutzsysteme finden im baulichen Brandschutz Anwendung zur Erhöhung des Feuerwiderstands von Stahlkonstruktionen. Neben den Anforderungen an die Feuerwiderstandsdauer können damit auch Ansprüche an die Ästhetik erfüllt werden. Die profilfolgende Applikation und die geringen Trockenschichtdicken der Produkte ermöglichen es, das filigrane Erscheinungsbild von Stahlkonstruktionen aufrechtzuerhalten. Neben der thermischen Schutzwirkung muss auch die Dauerhaftigkeit der Brandschutzbeschichtung sichergestellt werden. Die Bewertungsmethoden, die auf europäischer Ebene durch das EAD 350402-00-1106 zur Verfügung stehen, zielen auf eine Nutzungsdauer von zehn Jahren ab. Prüfverfahren für einen darüber hinausgehenden Zeitraum sind nicht beschrieben. In diesem Beitrag werden experimentelle Untersuchungen zum Einfluss der Bewitterung auf das Expansionsverhalten, zur thermischen Schutzwirkung und zu den während des Aufschäumens im Brandfall stattfindenden Reaktionen vorgestellt. Die Versuche wurden an einem wasserbasierten und einem epoxidharzbasierten reaktiven Brandschutzsystem durchgeführt. Die Ergebnisse wurden im Rahmen des IGF-Forschungsvorhabens 20470 N erzielt.
Composites in Fire and Flame
(2022)
Overview over the research results of the BAM in the field fire retardancy of composites. In different applications the flame retardancy of composites targets on different fire protection goals in the fire scenarios ignition, developing fire, and fully developed fire. Efficient solutions are tailored to pass a distinct fire test and to fit to a specific material. Flame inhibition as main flame retardancy mode of action combined with a minor mode of action in the condensed phase is general very efficient approach for composites. Alternatively residue design is demanded to achieve good results with only condensed phase mechanisms. Improving the fire stability asks for protective fire residues.
Investigation of the Thermal Stability of Proteinase K for the Melt Processing of Poly(L‑lactide)
(2022)
The enzymatic degradation of aliphatic polyesters offers unique opportunities for various use cases in materials science. Although evidently desirable, the implementation of enzymes in technical applications of polyesters is generally challenging due to the thermal lability of enzymes. To prospectively overcome this intrinsic limitation, we here explored the thermal stability of proteinase K at conditions applicable for polymer melt processing, given that this hydrolytic enzyme is well established for its ability to degrade poly(L-lactide) (PLLA). Using assorted spectroscopic methods and enzymatic assays, we investigated the effects of high temperatures on the structure and specific activity of proteinase K. Whereas in solution, irreversible unfolding occurred at temperatures above 75−80 °C, in the dry, bulk state, proteinase K withstood prolonged incubation at elevated temperatures. Unexpectedly little activity loss occurred during incubation at up to 130 °C, and intermediate levels of catalytic activity were preserved at up to 150 °C. The resistance of bulk proteinase K to thermal treatment was slightly enhanced by absorption into polyacrylamide (PAM) particles. Under these conditions, after 5 min at a temperature of 200 °C, which is required for the melt processing of PLLA, proteinase K was not completely denatured but retained around 2% enzymatic activity. Our findings reveal that the thermal processing of proteinase K in the dry state is principally feasible, but equally, they also identify needs and prospects for improvement. The experimental pipeline we establish for proteinase K analysis stands to benefit efforts directed to this end. More broadly, our work sheds light on enzymatically degradable polymers and the thermal processing of enzymes, which are of increasing economical and societal relevance.
Tailored crosslinking in elastomers is crucial for their technical applications. The incorporation of nanoparticles with high surface-to-volume ratios not only leads to the formation of physical networks and influences the ultimate performance of nanocomposites, but it also affects the chemical crosslinking reactions. The influence of few-layer graphene (FLG) on the crosslinking behavior of natural rubber is investigated. Four different curing systems, two sulfur-based with different accelerator-to-sulfur ratios, and two peroxide-based with different peroxide concentrations, are combined with different FLG contents. Using differential scanning calorimetry (DSC), vulcametry (MDR) and swelling measurements, the results show an accelerating effect of FLG on the kinetics of the sulfur-based curing systems, with an exothermic reaction peak in DSC shifted to lower temperatures and lower scorch and curing times in the MDR. While a higher accelerator-to-sulfur ratio in combination with FLG leads to reduced crosslinking densities, the peroxide crosslinkers are hardly affected by the presence of FLG. The good agreement of crosslink densities obtained from the swelling behavior confirms the suitability of vulcameter measurements for monitoring the complex vulcanization process of such nanocomposite systems in a simple and efficient way. The reinforcing effect of FLG shows the highest relative improvements in weakly crosslinked nanocomposites.
Überblick über den State-of-the-Art und aktuelle Trends mit den Schwerpunkten:
- nachwachsende Rohstoffe in flammgeschützten Polymerwerkstoffen (flammgeschützte Biopolymere und Biokomposite; biomass-basierte Flammschutzmittel, nachwachsende Hilfsstoffe aus Abfallströmen)
- Nachhaltigkeit und Flammschutz
- Konzepte von Analogie bis Out-of-the-Box.
Overview of the state of the art and current trends with the main topics:
- renewable sources in flame retardant polymers (flame retarded bio-polymers and biocomposites; bio-flame retardants, renewable adjuvants from industrial waste)
- flame retardancy meets sustainability
- concepts between analogy and out-of-the-box.
The fracture surface of slow and continuous crack propagation during environmental stress cracking of a semicrystalline polyethylene exhibits isotropic roughness exponents at the local scale but resolved across the macroscopic fracture surface a clear position dependence is found. The spatially resolved roughness exponent admits values in the range between 0.1 and 0.4, demonstrating nontrivial exponents in the small length-scale regime. Instead, they vary across the fracture surface according to the stress-state distribution, which suggests that the exponents are intimately linked to the locally dominating dissipation processes during craze cracking.
Polymeric membranes represent a cost- and energy-efficient solution for gas separation. Recently Polymers of Intrinsic Microporosity (PIMs) have been in a great interest because of their outstanding BET surface area larger than 700m2/g and pore size smaller than 1 nm. PIMs are a promising candidate in gas separation with high permeability and appealing selectivity due to their inefficient packing derived from a combination of ladder-like rigid segments with sites of contortion. However, it is recognized this class of polymers suffer from decrease in performance with time due to physical aging. The initial microporous structures approach a denser state via local chain rearrangements, leading to a dramatic reduction in permeability. As chain packing during film casting and physical aging are the key factors determine the performance in separation applications, characterization of the molecular mobility in these materials has been proved to provide valuable information. In recent research on PIM-1 the archetypal PIM, a molecular relaxation process with high activation energy together with a significant conductivity in the glassy state has been found and explained with the formation of local intermolecular agglomerates due to interaction of π-electrons in aromatic moieties of the polymer backbone. In this work, the dielectric behavior of the polymeric films and their response upon heating (aging) were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range down to 133K for the first time. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. Up to now, no other work has studied the role of porosity and thermal history of PIM-1 film in dielectric processes. The goal is by eliminating thermal history and considering storing conditions provide better understanding on aging and plasticizing in high free volume glassy polymer PIM-1.
Especially now in times of the energy revolution, the demand for energy-efficient separation processes promotes the advancement of new high-performance materials for use as highly selective separation membranes. Polymers with intrinsic microporosity (PIMs) are of high interest in the field of gas separation membranes. Currently the application of PIMs for membrane technology is still restrained by their strong tendency to physical aging involving a significant loss of their good gas separation properties. Physical aging phenomenon is related to the molecular mobility of PIMs which was investigated by broadband dielectric spectroscopy (BDS) previously [1]. In this work, covalent phosphinine-based framework (Eto-CPSF) was used as a nanofiller (0-10 wt %) in a PIM-1 matrix to potentially enhance the gas transport properties and prevent physical aging. Since molecular mobility is a fundamental parameter determining gas transport as well as physical aging in such a material, our study includes dielectric investigations by BDS of pure PIM-1 and PIM-1/Eto-CPSF mixed matrix membranes to establish a correlation between molecular mobility and gas transport properties. In addition, gas permeability was determined by the time-lag method (0-10 bar pressure) at 35 °C for N2, O2, CH4 and CO2 for all MMMs.
The dielectric behavior of the polymeric films and their response upon heating were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range up to 250 °C. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. As main result for MMMs, the permeability of PIM-1 for CH4 and CO2 gases were increased significantly with only 5 wt% of nanofiller within the polymer matrix. However, this is not observed for Eto-CPSF concentrations higher than ca. 7 wt% probably due to a microphase separated morphology of the nanocomposite system. Furthermore, the permselectivity of membranes for pair gases O2/N2 and CO2/N2 show enhancement up to a concentration of about 7 wt% Eto-CPSF filler.
Polymers of intrinsic microporosity (PIMs) are promising candidates for the active layer in gas separation membranes due to their high permeability and reasonable permselectivity. These appealing properties originate from a microporous structure as a result of inefficient segment packing in the condensed state due to a combination of a ladder-like rigid backbone and sites of contortion. However, this class of polymers suffers from a significant decrease in the permeability with time due to physical aging, whereby typically, the permselectivity increases. The initial microporous structures approach a denser state via local rearrangements, leading to the reduction of the permeability. Hence, a detailed characterization of the molecular mobility in such materials can provide valuable information on physical aging. In this work, the dielectric behavior of PIM-1 films and their behavior upon heating (aging) were revisited by isothermal frequency scans during different heating/cooling cycles over a broad temperature range between 133 and 523 K (−140 to 250 °C). In addition, the obtained results were compared with data of samples that were annealed at ambient temperatures over different time scales. Multiple dielectric processes were observed: several relaxation processes due to local fluctuations and a Maxwell−Wagner−Sillars polarization effect related to the microporosity. The temperature dependence of the rates of all processes follows the Arrhenius law where the estimated activation energy depends on the nature of the process. The influence of the thermal history (aging) on the processes is discussed in detail.
The phenomenon of environmental stress cracking is still a major issue in materials engineering as well as from a scientific perspective. Especially in the case of packaging materials made of high-density polyethylene, assessing the potential of premature damage due to environmental stress cracking is complex because of the large number of components in possible liquid filling goods. As a first guideline, the well-known effect of detergents and dispersants is usually considered, but the interplay with other components, such as organic solvents is often unknown. Particularly challenging in this respect are crop protection products, consisting of several different admixtures in addition to the biologically active ingredients. This study is based on two model liquids representing these admixtures that were established for testing in this context. The model liquids as well as their constituting components were used as liquid media in the Full Notch Creep Test to characterize the environmental stress cracking behavior of a typical high-density polyethylene. Complementary to the time-to failure of a notched specimen obtained from these tests, the crack opening was monitored optically, and the fracture surface was analyzed post-failure by laser scanning microscopy as well as scanning electron microscopy. Based on the results, the effect of various surfactants as well as the influence of organic solvents on environmental stress cracking are discussed.
Genormte künstliche Bewitterungstests sind häufig nicht spezifisch für die Anwendungssituation oder das Material. Das macht die Entwicklung spezifischer Tests erforderlich. Für deren Entwicklung müssen Maximalparameter der Anwendungssituation bekannt sein, womit dann der künstliche Test formuliert wird und dessen Bedingungen werden dann solange optimiert, bis die Korrelation der Effekte von natürlichem und künstlichem Test ausreichend ist.
Für Untersuchungen der Freisetzung kann der verbleibende Rest in der Probe und/oder die freigesetzte Menge in Luft, Boden, Wasser bestimmt werden.
Im ersten Beispiel der Witterungswirkung wurde die Freisetzung von Kohlenstoff-Nanoröhrchen (CNT) aus Polymer-Kompositen untersucht (unter Verwendung von empfindlich-nachweisbarer radioaktiver 14C-Markierung für einzelne CNT-Partikel), in einem zweiten die Freisetzung von anorganischen und organischen Bestandteilen aus elastomeren Bestandteilen von Sportböden (Bahnen und Kunstrasen) in Wasser.
The incorporation of nanoscale particles into elastomers enable a boost in performance and/or a distinct reduction of conventional filler loadings due to their high surface to volume ratio. 2D layered nanoparticles like graphene and graphene-related materials provide a great potential as effective fillers in rubber, especially by enhancing mechanical and barrier properties. The type and properties of the nanoparticles, their interface and the elastomeric matrix materials influence the technical behavior, and therefore the potential application fields of such rubber nanocomposites. Especially crucial for the efficiency of the nanofiller, however, is its best possible incorporation into the elastomer. The dispersing of nanoparticles without agglomerates usually constitutes a challenge when using conventional two-roll milling or internal mixing. Academic approaches for highly dispersed nanocomposites solve this problem but are often energy and time consuming with no feasible scale up possibility. Therefore, an ultrasonic assisted NR latex premixing process was established to produce highly filled masterbatches, enabling the main processing with conventional rubber processing techniques.
Two carbon-based nanoparticles with similar specific surface areas were investigated and incorporated in natural rubber as nanocomposites: A commercially available multilayer graphene (MLG) and a nanoscale carbon black (nCB). The mentioned premixed masterbatches were further processed to nanocomposites by the addition of matrix NR, two-roll milling, and hot pressing (vulcanization). By this procedure an increase in Young’s modulus of 157% (MLG) and 71% (nCB) could be obtained at a concentration level of 3 phr. As anisotropic material behavior was observable for the nanocomposites containing MLG, different measurement methods were investigated to quantify the orientation of the nanoparticles in the nanocomposites: Sorption measurements (swelling in 2 dimensions), hardness and dynamical mechanical analysis (in-plane vs. cross-plane), X-Ray diffraction and transmission and scanning electron microscopy.
A few layer/multilayer graphene (MLG) with a specific surface area of BET=250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution mixing of master batches followed by two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of 34, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR). 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability, the latter shown by the reduction in heat release rate in the cone calorimeter. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM). The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
Due to the high flammability and smoke toxicity of polyurethane foams (PUFs) during burning, distinct efficient combinations of flame retardants are demanded to improve the fire safety of PUFs in practical applications. This feature article focuses on one of the most impressive halogen-free combinations in PUFs: expandable graphite (EG) and phosphorus-based flame retardants (P-FRs). The synergistic effect of EG and P-FRs mainly superimposes the two modes of action, charring and maintaining a thermally insulating residue morphology, to bring effective flame retardancy to PUFs. Specific interactions between EG and P-FRs, including the agglutination of the fire residue consisting of expanded-graphite worms, yields an outstanding synergistic effect, making this approach the latest champion to fulfill the demanding requirements for flame-retarded PUFs. Current and future topics such as the increasing use of renewable feedstock are also discussed in this article.
In the recent years, more and more products in construction and automotive industry are bonded by adhesive tapes instead of mechanical fasteners but there is no sufficient understanding of how these bonded, layered materials behave in fires. Our research project gives an insight of how adhesives and substrates interact with each other in different fire scenarios and how flame retardants function in pressure sensitive adhesive (PSA) tapes. A systematic investigation on the burning behavior of PSA tapes as free-standing films, as top layers on different substrates and as sandwich-like adhesive joints was performed. The burning behavior of free-standing PSA tapes and those used as a coating was significantly improved by using phosphorus-based flame retardants. Furthermore, it was shown that, depending on tape structure and substrate, the PSA tape can lower the fire risk by acting as an intermediate protection layer in bonded materials.
The crack propagation rate of environmental stress cracking was studied on high-density polyethylene compact tension specimens under static loading. Selected environmental liquids are distilled water, 2 wt% aqueous Arkopal N100 solution, and two model liquid mixtures, one based on solvents and one on detergents, representing stress cracking test liquids for commercial crop protection products. The different surface tensions and solubilities, which affect the energetic facilitation of void nucleation and craze development, are studied. Crack growth in surface-active media is strongly accelerated as the solvents induce plasticization, followed by strong blunting significantly retarding both crack initiation and crack propagation. The crack propagation rate for static load as a function of the stress intensity factor within all environments is found to follow the Paris–Erdogan law. Scanning electron micrographs of the fracture surface highlight more pronounced structures with both extensive degrees of plasticization and reduced crack propagation rate, addressing the distinct creep behavior of fibrils. Additionally, the limitations of linear elastic fracture mechanisms for visco-elastic polymers exposed to environmental liquids are discussed.
Emanating from developing flame retarded biocomposites, we have proposed renewable natural fibers (including keratin) taken from industrial waste as an authentic sustainable approach. More recently, we have investigated non-vegan flame retardant approaches. This paper loves to give you an insight into our ongoing projects on biogenic industrial wastes like leather, bone meal, and insects. Materials were characterized multi-methodically, flame retardant modes of action quantified, decomposition mechanism proposed, and synergisms explained. Considering the large quantities of leather waste (LW) in industrial-scale production, we underline LW as multifunctional bio-adjuvants. LW enhances the flame retardancy of poly(ethylene-vinyl acetate) (EVA) containing phosphorus flame retardants (P-FR). Products/by-products of the invertebrate and vertebrate farming, respectively, are promising bio-based adjuvants in flame retarded bio-epoxy thermosets. While the addition of bone meal yields the formation of an inorganic shield, protein-based powders from insects provide an intumescent behavior. In combination with a P-FR superior charring and self-extinguishing are obtained.
Acknowledgement: In part of this work was supported by the Volkswagen Foundation grant “Experiment!” No. 97437.
In a laboratory test, transparent high‐density polyethylene (HDPE) jerrycans have been exposed to both UV radiation and 55 wt‐% nitric acid solution at (41 ± 2)°C, for up to 20 days. For comparison, UV radiant exposure (21 days) and nitric acid exposure (up to 6 weeks) were performed separately, at nearly equal temperatures. The damages are compared with FTIR spectroscopy in ATR and HT‐gel permeation chromatography(GPC) on a molecular level and with hydraulic internal pressure testing as a component test. For the used jerrycans, relevant oxidation can only be found after the combined exposure. This is caused by the decomposition of nitric acid into nitrous gases by UV radiation, which is also observed at lower concentrations (28 wt‐%). After 6 days of laboratory exposure, this is rated as critical, which corresponds to about 1/10 year in Central Europe, according to the UV radiant exposure. The gradual increase in oxidative damage shows the reproducibility of the test.
Renewable alternatives for common thermoset resins are demanded to go for sustainability. The objective is to create a flame retarded epoxy resin from a commercial bio epoxy resin with halogen free inorganic and organic flame retardants, respectively. Alumina trihydrate, aluminum diethyl phosphinate, a DOPO-based phosphonamidate and ammonium polyphosphate seem to have promising performances. Properties are enhanced with different bio fillers: pyrolyzed cocoa shells and plant waste (provided by Otto A. Müller Recycling GmbH, thanks!), short fibers and nonwovens of the natural fiber kenaf, hydroxypropyl-ß-cyclodextrin and sulfobutylether-ß-cyclodextrin.
Fire performance is investigated by cone calorimeter examinations, LOI and UL-94 ratings. Thermal analysis is given by TG-FTIR and DSC measurements.
Combinations of flame retardants and bio-fillers lead to reduced PHRR and THR, reach V0 in UL-94 and have a significant increase in LOI of up to 37 vol.-%. 10 % ammonium polyphosphate with 10 % pyrolyzed cocoa shell performs best, builds a magnificent protective layer, and shows good intumescence.
Material solutions that meet both circular bioeconomy policies and high technical requirements have become a matter of particular interest. In this work, a prospectively abundant proteinrich waste resource for the manufacturing of flame-retardant epoxy biocomposites, as well as for the synthesis of biobased flame retardants or adjuvants, is introduced. Different biomass fillers sourced from the cultivation of the mealworm beetle Tenebrio molitor are embedded in a bioepoxy resin cured with tannic acid and investigated regarding the fire performance of the thermosets. By means of spectroscopic and thermal analysis (attenuated total reflectance FTIR spectroscopy, thermogravimetric analysis-coupled FTIR spectroscopy, and differential scanning calorimetry), the influence of the biomass microparticles on the curing and thermal degradation behavior is evaluated. The final performance of the biocomposites is assessed based on fire testing methodology (limited oxygen index, UL-94, and cone calorimetry). Providing a high charring efficiency in the specific tannic acid-based epoxy matrix, the protein-rich adult beetle is further investigated in combination with commercial environmentally benign flame retardants in view of its potential as an adjuvant. The results highlight a char forming effect of nonvegan fillers in the presence of tannic acid, particularly during thermal decomposition, and point toward the potential of protein-based flame retardants from industrial insect rearing for future formulations.
Brände zerstören immer wieder wichtige Kulturgüter und gefährden nationales Kulturerbe. Das Projekt BRAWA erarbeitet neue Strategien und innovative Technologien, um die Brandsicherheit historischer Gebäude zu erhöhen. Dabei basiert das Konzept auf der Vernetzung von Sensoren, die bereits beim Auftreten bestimmter Gase in der Frühphase der Brandentstehung Alarm auslösen. Durch ein neuartiges Helferkonzept soll eine frühe Branderkennung und -bekämpfung ermöglicht werden.
2D layered nanoparticles enable a distinct reduction of filler loadings in rubber compounds combined with a boost in performance due to their high surface to volume ratio. They often enable unique property profiles providing a great potential as effective fillers in rubber, especially by enhancing mechanical and barrier properties.
As the best possible incorporation into the elastomer matrix is crucial for the efficiency of the nanofiller, dispersing and exfoliation of the nanoparticles without formation of agglomerates usually constitutes an outstanding challenge - especially when using conventional processing methods. Laboratory-scale approaches for highly dispersed nanocomposites sometimes solve this problem, but these are often too energy and time consuming and provide no scale up possibility for real applications. Therefore, a latex premixing process was established to produce highly filled masterbatches, enabling the processing with conventional techniques.
The presence of nanoparticles greatly impacts the behavior of elastomeric compounds, besides affecting the properties of the final product also the processing is influenced (rheology, crosslinking).
In this study, nanocomposites of natural rubber and multilayer graphene (MLG) were prepared via a latex masterbatch route. Different strategies for masterbatch premixing are compared (stirring vs. ultrasonication, coagulation vs. drying). Dispersion and exfoliation of MLG were determined by transmission electron microscopy. The reinforcing effect of MLG affects the viscosity while the dispersed graphene layers may also act as diffusion barrier/absorbent for the crosslinking agents. In contrast to that, MLG forms physical crosslinks in the final product. Swelling measurements and differential scanning calorimetry allow a differentiation between chemical and physical network links. Different technical properties of the nanocomposites were measured with respect to mechanical and application relevant behavior.
Das langsame Risswachstum (slow crack growth, SCG) sowie der umgebungsbedingte Spannungsriss (environmental stress cracking, ESC) sind relevante Schädigungsmechanismen für teilkristalline Werkstoffe auf Basis von Polyethylen hoher Dichte (PE-HD).
Der Vortrag gibt einerseits einen Überblick über die grundlegenden Struktur-Eigenschafts-Beziehungen in diesem Kontext, andererseits werden auch verschiedene praxisorientierte Prüfverfahren vorgestellt. Letztere wurden in gemeinsamen Forschungsprojekten von BAM und LBF mit dem Schwerpunkt Gefahrgutbehälter bzw. Pflanzenschutzmittel vergleichend untersucht und durch weitergehende Analytik ergänzt.
The chapter gives a brief introduction to (nano)compositecomposite materials having the focus on polymer-based nanocomposites. The different dimensionalities of nanoparticles are introduced, along with their distribution in the matrix.
Different application fields of polymer-based nanocomposites, like flame retardancy, filled rubbers, nanofilled thermosets and thermoplastics, separation membranes and nanodielectrics, are considered in greater detail.
Brandschutz
(2022)
In den letzten Jahrzehnten wurde die Degradation der polymeren Matrix von flammgeschützten Polymeren eingehend untersucht. Erst in den letzten Jahren jedoch hat sich die Frage der Lebensdauer der Funktionalität des Flammschutzes selbst als wichtige Fragestellung herauskristallisiert, z.B. bei Kabeln. Deshalb sollte diese Fragestellung durch systematisch-variierte künstliche Klima- und Bewitterungstests an flammgeschützten Polymerwerkstoffen untersucht werden
In den letzten Jahrzehnten wurde die Degradation der polymeren Matrix von flammgeschützten Polymeren eingehend untersucht. Erst in den letzten Jahren jedoch hat sich die Frage der Lebensdauer der Funktionalität des Flammschutzes selbst als wichtige Fragestellung herauskristallisiert, z.B. bei Kabeln. Deshalb sollte diese Fragestellung durch systematisch-variierte künstliche Klima- und Bewitterungstests an flammgeschützten Polymerwerkstoffen untersucht werden.
Valorizing “non-vegan” bio-fillers: Synergists for phosphorus flame retardants in epoxy resins
(2022)
Sustainable, biogenic flame retardant adjuvants for epoxy resins are receiving increased focus. Zoological products like insects, bone meal, and eggshells are available in large quantities, but remain uninvestigated as functional fillers to epoxy resins, although they are potential synergists to flame retardants. The efficacy and flame retardancy of “non-vegan” additives in combination with flame retardants is investigated and the fire behavior and thermal decomposition of bio-sourced epoxy resin composites is characterized. By comparing the fire performance of composites containing flame retardants or fillers at varying loadings (5, 10, and 20%), their role as synergists that enhance the function of organophosphorus flame retardants in bio-epoxy composites is identified and quantified. Peak heat release rates were 44% lower in composites containing both filler and flame retardant versus those containing only flame retardants, and fire loads were reduced by 44% versus the pure resin, highlighting the ability of “non-vegan” fillers to function as synergists.
The important take home message of this chapter: When multicomponent flame retardant systems are applied to polymeric materials, it becomes possible to address multiple fire properties, increase efficiency, and minimize flame retardant use to maximize polymer property balance. Flame retardants are combined or used together with adjuvants or synergists; fibers and fillers make a crucial contribution to their fire properties. Multicomponent systems are discussed in their capacity as an overall powerful strategy for achieving and optimizing non-halogenated flame-retardant polymeric materials.
The valorization of macroalgae digestate as a secondary resource for high value chemicals and nutrients will promote the sustainability and circularity of anaerobic digestion based biorefinery. In this study, three digestates from A. nodosum C.linum and L. digitata were separated into liquid and solid fractions to investigate the production of high value added chemicals through pyrolysis using Pyrolysis Gas Chromatography Mass Spectroscopy (Py-GC/MS) while the filtered liquid fractions were tested as an alternative culture media to grow C. sorokiniana under mixotrophic conditions. The digestates showed different thermal degradation and an improvement of bio-oil profiles compared to the starter material. Pyrolyzates from raw macroalgae were characterized by a high anhydrosugar content in contrast to high aromatics observed in the case of their digestates. Toluene, benzofuran and vinylphenol, base chemicals for many industries, represented together 30–37% of the total chemicals produced during pyrolysis of the three macroalgae digestate. On the other hand, C. sorokiniana cultured on digestate-based media showed a higher lipid content with an increase in monounsaturated fatty acids and a lower poly-unsaturated fatty acid content in comparison to microalgae grown in standard tris-acetate-phosphate media. Thus, the acyl composition was shifted in a direction more suitable for biodiesel production by this process. In addition, the increase of Chemical Oxygen Demand and Volatile Fatty Acids concentration in the digestate was found to reduce ammonium toxicity. Finally, 94% of Chemical Oxygen Demand and 83% of ammonium were removed by microalgae from the digestate-based media which will reduce the pollution risk of the biorefinery. Overall, the results indicate that using macroalgae solid digestates can generate improvements in the quality of
products obtained by pyrolysis and the liquid digestate can positively influence microalgae growth and its products.
The incorporation of nanoparticles like multilayer graphene (MLG) into elastomeric composites boosts their technical performance, such as their mechanical behavior and electrical conductivity. Common filler types (carbon black (CB) and aluminum trihydroxide (ATH)) generally fulfill single, specific purposes and are often used in high loadings. CB typically reinforces rubber mechanically, while ATH increases flame retardancy. Small amounts of MLG reduce these high filler contents and maintain the multifunctional characteristics of rubber composites. In chlorosulfonated polyethylene (CSM) + ATH, an intrinsically flame-retardant rubber was designed to achieve the highest standards such as maximum average of heat emission (MARHE) <90 kW m−2, 3 phrMLG was substituted for 15 phr CB and/or 3 phr ATH via an industrially applicable processing approach. Replacing either CB or ATH resulted in a property profile that was multifunctionally improved in terms of features such as mechanical performance, reduced sorption, and flame retardance. MLG nanocomposites are reported to show promise as an industrially utilizable route to obtain multifunctional high-performance rubbers.
We report dielectric and calorimetric studies on metathesis and addition-type polytricyclononenes, both based on the same monomer bearing three pendant OSiMe3 groups. For the addition-type polymer, dielectric spectroscopy reveals a β*-process related to the microporosity, whereas for its metathesis counterpart, the segmental dynamics manifests as an α-process related to a glass transition. Besides active dielectric processes, a significant conductivity contribution is detected for both samples which for the microporous additiontype polymer is three orders of magnitude greater than for the metathesis polymer. The broadband dielectric spectroscopy is complemented by detailed calorimetric investigations, comprising DSC, FSC, and TMDSC. The calorimetric methods detected the glass transition for the metathesis polymer in agreement with the observed dielectric α-process. Furthermore, the already reported gas transport properties for both polymers are compared, setting them in correlation with the observed molecular mobility and conductivity behavior. The discussed results reflect significant differences in molecular mobility of the two polymers affecting the appearance of microporosity which strongly determines the gas transport properties.
Die Forderung, dass der Flammschutz von Kunststoffen nicht nur zum bei der Herstellung der jeweiligen Produkte, sondern auch über die gesamte Einsatzdauer im geforderten Maß wirksam ist, stellt eine große Aufgabe dar. Ferner ist die Anforderung für viele Produkte in der Praxis neu, da bisher vor allem der Einfluss der Flammschutzmittel auf die Stabilität der Polymerwerkstoffe, nicht aber die Stabilität des Flammschutzes untersucht wurde. Das Langzeitverhalten halogenfreier Systeme ist bis heute wenig untersucht, insbesondere weil Phosphor- und Stickstoff-basierte Systeme die oxidative Beständigkeit von Polymeren weniger zu beeinflussen scheinen als halogenhaltige FSM. Die Frage, wie zuverlässig der Flammschutz wirkt, wenn Kunststoffe einige Jahre im Innen- und Außenbereich im Einsatz sind und dabei wechselnden Beanspruchungen ausgesetzt waren, wurde bislang nur vereinzelt untersucht. Mögliche Auswirkungen von Witterungseinflüssen auf flammgeschützte Polymerwerkstoffe sind, dass die Flammschutzmittel selbst abbauen, ausgewaschen werden, oder auch durch Wechselwirkung mit den eingesetzten Additiven oder mit den Alterungsprodukten der Polymermatrix in ihrer Wirkung nachlassen. Hier bestand großer Forschungsbedarf, um an den Punkt zu gelangen, die Beständigkeit der Flammschutzeigenschaften eines Produktes über seine gesamte Lebensdauer zuverlässig garantieren zu können. Diese Fragestellung greift das durchgeführte Forschungsvorhaben auf.
Ziel war die Untersuchung der Langzeitstabilität der Flammschutzwirkung von halogenfrei flammgeschützten Polymerwerkstoffen unter diversen Witterungseinflüssen. Dazu wurden die Schädigungsmechanismen der Polymerwerkstoffe und der Flammschutzmittel sowie die auftretenden Wechselwirkungen analysiert, um ein Verständnis für die ablaufenden Prozesse zu entwickeln und Empfehlung für die Reduzierung der Alterung zu erarbeiten. Gegenstand der Untersuchungen waren anwendungsrelevante Flammschutz-Konzepte, die miteinander verglichen wurden. Die Erarbeitung von Struktur-Eigenschafts-Beziehungen ermöglichte die Beschreibung der Empfindlichkeiten und den Vergleich zwischen den Systemen. Darauf basierend wurden für die FSM spezifische Leitlinien für die Optimierung der Langzeitstabilität des Flammschutzes erstellt.
Simulation of the burning and dripping cables in fire using the particle finite element method
(2022)
The behavior of the cable jacket in fire characterized by the tendency to melt and drip constitutes a major source of fire hazard. The reason is that the melted material may convey the flame from one point to another, expanding fire and contributing to the fire load. In this article, the capability of a new computational strategy based on the particle finite element method for simulating a bench-scale cables burning test is analyzed. The use bench-scale test has been previously used to simulate the full-scale test described in EN 50399. As the air effect is neglected, a simple combustion model is included. The samples selected are two cables consisting of a copper core and differently flame retarded thermoplastic polyurethane sheets. The key modeling parameters were determined from different literature sources as well as experimentally. During the experiment, the specimen was burned under the test set-up condition recording the process and measuring the temperature evolution by means of three thermocouples. Next, the test was reproduced numerically and compared with a real fire test. The numerical results show that the particle finite element method can accurately predict the evolution of the temperature and the melting of the jacket.
A systematic series of flexible polyurethane foams (FPUF) with different concentrations of flame retardants, bis([dimethoxyphosphoryl]methyl) phenyl phosphate (BDMPP), and melamine (MA) or expandable graphite (EG) was prepared. The mechanical properties of the FPUFs were evaluated by a universal testing machine. The pyrolysis behaviors and the evolved gas analysis were done by thermogravimetric analysis (TGA) and TGA coupled with Fourier-transform infrared (TG-FTIR), respectively. The fire behaviors were studied by limiting oxygen index (LOI), UL 94 test for horizontal burning of cellular materials (UL 94 HBF), and cone calorimeter measurement. Scanning electronic microscopy (SEM) was used to examine the cellular structure's morphology and the postfire char residue of the FPUFs. LOI and UL 94 HBF tests of all the flame retarded samples show improved flame retardancy. BDMPP plays an essential role in the gas phase because it significantly reduces the effective heat of combustion (EHC). This study highlights the synergistic effect caused by the combination of BDMPP and EG. The measured char yield from TGA is greater than the sum of individual effects. No dripping phenomenon occurs during burning for FPUF-BDMPP-EGs, as demonstrated by the result of the UL 94 HBF test. EG performs excellently on smoke suppression during burning, as evident in the result of the cone calorimeter test. MA reduces the peak heat release rate (pHRR) significantly. The synergistic effect of the combination of BDMPP and EG as well as MA offers an approach to enhance flame retardancy and smoke suppression.