6.3 Strukturanalytik
Filtern
Dokumenttyp
- Vortrag (156)
- Posterpräsentation (100)
- Zeitschriftenartikel (20)
- Forschungsdatensatz (5)
- Sonstiges (4)
- Forschungsbericht (4)
- Beitrag zu einem Tagungsband (3)
- Dissertation (2)
- Buchkapitel (1)
- Tagungsband (Herausgeberschaft für den kompletten Band) (1)
Sprache
- Englisch (274)
- Deutsch (21)
- Mehrsprachig (2)
Referierte Publikation
- nein (297) (entfernen)
Schlagworte
- Mechanochemistry (56)
- Synchrotron (36)
- BAMline (26)
- In situ (24)
- XANES (18)
- XRF (14)
- Nanoparticles (13)
- XRD (11)
- Calcium sulfate (9)
- MALDI-TOF MS (9)
Organisationseinheit der BAM
- 6 Materialchemie (297)
- 6.3 Strukturanalytik (297)
- 1 Analytische Chemie; Referenzmaterialien (32)
- 6.0 Abteilungsleitung und andere (31)
- 5 Werkstofftechnik (19)
- 6.1 Oberflächen- und Dünnschichtanalyse (14)
- 4 Material und Umwelt (12)
- 5.1 Mikrostruktur Design und Degradation (11)
- 8 Zerstörungsfreie Prüfung (11)
- 1.4 Prozessanalytik (10)
The presentation includes aspects of material design and characterization with a focus on lignin. Examples are the structural elucidation of lignosulfonates by means of two-dimensional chromatography, the mechanochemical degradation and functionalization of Kraft-Lignin with accompanying analytics. Future projects involving the incorporation of lignin into polymers will be presented.
Die Probenpräparation ist ein wichtiger Schritt für die Qualität der Massenspektren in MALDI-TOF MS. Es werden Polymerproben, die lösungsmittelbasiert und lösungsmittelfrei präpariert worden sind, verglichen. Dabei werden die Intensitätsverhältnisse von ternären Mischungen von PEG-, PS- und PMMA-Polymeren beachtet.
MALDI TOF Massenspektrometrie wurde verwendet, um Kristallisationsprozesse in Polyestern (Polylactide, Polyglycolide) zu untersuchen. Dabei konnte gezeigt werden, dass Zyklen und Linearen simultan, aber in unterschiedlichen Kristalliten, kristallisieren. Die dabei ablaufenden Umesterungen (Transesterifizierungen) konnten mit der MALDI TOF Massenspektrometrie nachgewiesen werden. Damit wurde ein völlig neues Anwendungsgebiet dieser MS Methode demonstriert.
Owing to a growing shortage of fluorspar, a raw material used for producing fluorinated base chemicals, fluorspar has been named among the 30 critical raw materials in the EU. 1 However, the sustainable transfer of fluorine atoms from one molecule to another using heterogeneous catalysts has not yet been reported. Herein, we present the heterogeneous catalyst zirconium chloro fluoride (ZCF) that performs dehydrofluorination of a fluoroalkane and consecutive hydrofluorination of an alkyne at room temperature.
The variability and heterogeneity in their structural composition is significant for nearly all synthetic and natural polymers. Beside molar mass also functionality type distribution, copolymer composition distribution and architectural features are responsible for changing the material properties.
A wide range of analytical techniques are available to get insight into these parameters. However, in most cases it is essential to combine different sophisticated techniques to get closer to actual structures and to avoid statistical averages.
Different liquid chromatographic separation modes and their coupling in a two-dimensional way (SEC, LCCC, HILIC, 2D-LC) in combination with suitable detection techniques (e.g. UV, RI, LS, IR, MALDI/ESI-MS) as well as techniques like BET, DCS, SEM/TEM were applied to make structural features visible.
A few aspects are discussed for structural different polylactides from various synthesis routes and their behavior in LC-MS.
Glycolide was polymerized in bulk by means of four different ROPPOC catalysts: tin(II) 2-ethylhexanoate (SnOct2), dibutyltin bis(pentafluoro-phenoxide) (BuSnOPF),zinc biscaproate (ZnCap), and zinc bis(pentafluoro-phenyl sulfide) (ZnSPF). The temperature was varied between 110 and 180°C and the time between 3 h and 7 days. For the few polyglycolides (PGAs) that were soluble extremely high molecular masses were obtained. The MALDI TOF mass spectra had all a low signal-to-noise ration and displayed the peaks of cyclic PGAs with a“saw-tooth pattern ”indicating formation of extended-ring crystallites in the mass range below m/z 2500. The shape of DSC curves varied considerably with catalyst and reaction conditions, whereas the long-distance values measured by SAXS were small and varied little with the polymeriza-tion conditions.
Kemnitz et al. developed a fluorolytic route to access metal fluorides 2 such as AlF3 3 and MgF2 4 which possess a high surface area. In aluminium-based systems, the synthetic approach led to amorphous xerogels that can be further converted into Lewis superacids.3 Still, despite zirconium oxide being described as a stronger Lewis acid than other metal oxides 4 zirconium fluoride-based materials have only recently been reported or investigated. 6 In this work we extend the class of amorphous Lewis acidic heterogeneous catalysts to an amorphous ZrF4 that is active in C-F bond activation.
Amorphous materials play an important role in C-F bond activation but face the difficulty of limited available structural information by methods such as powder XRD and solid-state MAS NMR spectroscopy especially if the nucleus is not abundant enough. Here, we present heterogeneous catalysts, active in C-F bond activation, where EXAFS allowed specifically elucidating the local structure, which would have not been possible elsewise.
AbstractThe high-temperature corrosion behaviors of the equimolar CrCoNi medium-entropy alloy and CrMnFeCoNi high-entropy alloy were studied in a gas atmosphere consisting of a volumetric mixture of 10% H2O, 2% O2, 0.5% SO2, and 87.5% Ar at 800 °C for up to 96 h. Both alloys were initially single-phase fcc with a mean grain size of ~ 50 μm and a homogeneous chemical composition. The oxide layer thickness of CrMnFeCoNi increased linearly with exposure time while it remained constant at ~ 1 μm for CrCoNi. A Cr2O3 layer and minor amounts of (Co,Ni)Cr2O4 developed on the latter while three oxide layers were detected on the former, i.e., a thin and continuous chromium rich oxide layer at the oxide/alloy interface, a dense (Mn,Cr)3O4 layer in the center and a thick and porous layer of Mn3O4 and MnSO4 at the gas/oxide interface. Additionally, a few metal sulfides were observed in the CrMnFeCoNi matrix. These results were found to be in reasonable agreement with thermodynamic calculations.
Calcium sulfate hemihydrate (CaSO4ᐧ0.5H2O), also known as bassanite, has been used as a precursor to produce gypsum (dihydrate, CaSO4ᐧ2H2O) for various construction and decorative purposes since prehistoric times. The main route to obtain hemihydrate is a thermal treatment of gypsum at temperatures typically between 150 °C and 200 °C to remove some of the structural water.
In this contribution, we introduce (Fig. 1) a more efficient and sustainable method (T < 100 °C) that enables the direct, rapid, and reversibly conversion of gypsum to bassanite using reusable high salinity aqueous solutions (brines with c[NaCl] > 4 M). The optimum conditions for the efficientproduction of bassanite in a short time (< 5 min) involve the use of brines with c(NaCl) > 4 M and maintaining a temperature, T > 80 °C. When the solution containing bassanite crystals is cooled down to around room temperature, eventually gypsum is formed. When the temperature is raised again to T > 80 °C, bassanite is rapidly re-precipitated. This contrasts with the typical behaviour of the bassanite phase in low salt environments.
Traditionally, hemihydrate is obtained through a solid state thermal treatment because bassanite is considered to be metastable with respect to gypsum and anhydrite in aqueous solutions, and therefore gypsum-to-bassanite conversion should not occur in water. Its very occurrence actually contradicts numerical thermodynamic predictions regarding solubility of calcium sulfate phases. By following the evolution of crystalline phases with in situ and time-resolved X-ray diffraction/scattering and Raman spectroscopy, we demonstrated that the phase stability in brines at elevated temperatures is inaccurately represented in the thermodynamic databases. Most notably for c(NaCl) > 4 M, and T > 80 °C gypsum becomes readily more soluble than bassanite, which induces the direct precipitation of the latter from gypsum. The fact that these transformations are controlled by the solution provides extensive opportunities for precise manipulation of crystal formation. Our experiments confirmed that bassanite remained the sole crystalline structure for many hours before reverting into gypsum. This property is extremely advantageous for practical processing and efficient crystal extraction in industrial scenarios.