Polymers with intrinsic microporosity (PIMs) represent a novel, innovative class of materials with great potential in various applications from high-performance gas separation membranes to electronic devices. Here for the first time, for PIM-1, as the archetypal PIM, fast scanning calorimetry provides definitive evidence for a glass transition (Tg=715 K, heating rate 3·10^4 K/s) by decoupling the time-scales responsible for glass transition and decomposition. As the rigid molecular structure of PIM-1 prevents any conformational changes, small-scale bend and flex fluctuations must be considered the origin of its glass transition. This result has strong implications for the fundamental understanding of the glass transition and for the physical aging of PIMs and other complex polymers, both topical problems of materials science.
Microplastic particles are currently detected in almost all environmental compartments. The results of detection vary widely, as a multitude of very different methods are used with very different requirements for analytical validity.
In this work four thermoanalytical methods are compared and their advantages and limitations are discussed. One of them is thermal extraction-desorption gas chromatography mass spectrometry (TED-GC/MS), an analysis method for microplastic detection that has become established in recent years. In addition, thermogravimetric analysis coupled with Fourier-transform infrared spectroscopy (TGA-FTIR) and mass spectrometry (TGA-MS) were applied, two methods that are less common in this field but are still used in other research areas. Finally, microscale combustion calorimeter (MCC) was applied, a method not yet used for microplastic detection.
The presented results are taken from a recently published interlaboratory comparison test by Becker et al. (2020). Here a reference material consisting of suspended matter and specified added polymer masses was examined, and only the results of the recoveries were presented. In the present paper, however, the results for the individual polymers are discussed in detail and individual perspectives for all instruments are shown.
It was found that TED-GC/MS is the most suitable method for samples with unknown matrix and unknown, variable kinds and contents of microplastic. TGA-FTIR is a robust method for samples with known matrix and with defined kinds of microplastic. TGA-MS may offer a solution for the detection of PVC particles in the future. MCC can be used as a very fast and simple screening method for the identification of a potential microplastic load of standard polymers in unknown samples.
Novel agar-based test electrolytes are used to perform electrochemical corrosion investigations on ZnFe and ZnNi binary as well as ZnFeMo ternary zinc coatings. The objectives of the electrochemical investigations include the characterization of the corrosion behavior, the description of the protective effect of the coatings as well as the investigation of the layer formation and degradation under artificial aging. ZnFe and ZnFeMo coatings are applied with varying iron content as well as an additional passivation layer, respectively, to study the effect on corrosion resistance. The results show that the protective effect of the coatings is not negatively influenced by different iron contents or the addition of molybdenum. Additional passivation of the ZnFe-containing coatings by means of a passivating agent leads to a significant improvement in the protective effect. Artificial aging leads to slight degradation of the additional passivation layer whereas coatings without post-treatment enhance their protective effect by the formation of corrosion product layers.
The electrochemical behavior of UNS N08031 was investigated as a function of electrode potential in Green-Death solution at 40 °C. The UNS N08031 surface is in a stable passive state during cyclic potentiodynamic polarization without an initiation and/or propagation of localized corrosion. In potentiostatic polarization of UNS N08031 for 3600 s, passive current density increases with an increase in the passivation potential from 0.7 to 1.0 VSSE (silver/silver chloride reference electrode in saturated potassium chloride) Electrochemical impedance spectroscopy (EIS) and Mott-Schottky (M-S) analysis showed that a more defective n-type semiconductive passive film forms as the potential increases. X-ray photoelectron spectroscopy (XPS) revealed that passive film consists of mainly chromium and minor iron and nickel oxides. The mechanism of the defective passive film formation is discussed. The increase of the applied potential is considered to be a reason for the change in passive film stability.
Einkomponentige alkaliaktivierte Bindemittel (AAB), d. h. AAB, bei denen der Aktivator als Feststoff im Bindemittel vorliegt, weisen Vorteile hinsichtlich der praktischen Anwendung im Bauwesen gegenüber konventionellen AAB auf. Einkomponentige AAB lassen sich als Gemische aus reaktiver Silica und Natriumaluminat herstellen, wobei die Reaktionsprodukte von der eingesetzten Silica und den Verhältnissen Na2O/Al2O3/SiO2/H2O abhängen: Während Mikrosilica und ähnliche Reststoffe zu zeolithreichen Produkten führen, erhält man aus Reisschalenasche vollständig amorphe Gele (sog. «Geopolymere »). Mörtel auf Basis solcher Bindemittel entsprechen den Anforderungen von DIN 19573:2016-03 hinsichtlich des Widerstands gegen Schwefelsäureangriff (Prüfung bei pH = 1 für 70 d) und sind damit potentiell als Reparatursysteme für Abwasserinfrastruktur geeignet. Untersuchungen mittels 29Si-MAS-NMR und 1H-29Si-Kreuzpolarisations(CP)-MAS-NMR sowie REM-Aufnahmen von erhärteten und dem Schwefelsäureangriff ausgesetzten AAB zeigen, dass der hohe Säurewiderstand v. a. auf die Fällung von Silicagel an der Grenzfläche Mörtel/Säure zurückzuführen ist, wodurch der Korrosionsfortschritt in darunterliegenden Schichten verlangsamt wird.
Einkomponentige alkaliaktivierte Bindemittel (AAB), d. h. AAB, bei denen der Aktivator als Feststoff im Bindemittel vorliegt, weisen Vorteile hinsichtlich der praktischen Anwendung im Bauwesen gegenüber konventionellen AAB auf. Einkomponentige AAB lassen sich als Gemische aus reaktiver Silica und Natriumaluminat herstellen, wobei die Reaktionsprodukte von der eingesetzten Silica und den Verhältnissen Na2O/Al2O3/SiO2/H2O abhängen: Während Mikrosilica und ähnliche Reststoffe zu zeolithreichen Produkten führen, erhält man aus Reisschalenasche vollständig amorphe Gele (sog. «Geopolymere»). Mörtel auf Basis solcher Bindemittel entsprechen den Anforderungen von DIN 19573:2016-03 hinsichtlich des Widerstands gegen Schwefelsäureangriff (Prüfung bei pH = 1 für 70 d) und sind damit potentiell als Reparatursysteme für Abwasserinfrastruktur geeignet. Untersuchungen mittels 29Si-MAS-NMR und 1H-29Si-Kreuzpolarisations(CP)-MAS-NMR sowie REM-Aufnahmen von erhärteten und dem Schwefelsäureangriff ausgesetzten AAB zeigen, dass der hohe Säurewiderstand v. a. auf die Fällung von Silicagel an der Grenzfläche Mörtel/Säure zurückzuführen ist, wodurch der Korrosionsfortschritt in darunterliegenden Schichten verlangsamt wird.
Die Rheologie von fließfähigen zementären Systemen mit Fließmitteln wird durch eine Vielzahl parallel stattfindender Effekte beeinflusst. Zu diesen Effekten zählen Wechselwirkungen zwischen den Polymeren und Ionen in der Porenlösung, frühe Phasenbildung, zeitabhängige und kompetitive Adsorption zwischen anionischen Polymeren und Sulfationen, Bildung von Phasen in der Porenlösung sowie Morphologieänderungen an Partikeloberflächen. Die frühe Hydratation von Zement, die durch Lösungs- und Fällungsprozesse angetrieben wird, beeinflusst diese Effekte erheblich. Das permanente Ungleichgewicht der Porenlösung führt zu Veränderungen der Partikeloberflächen, welches widerum zur Folge hat, dass rheometrische Messungen dieser Zementleime anfällig für Streuungen sind. Um die Einflüsse aus der Zementhydratation zu minimieren, wurden die rheometrischen Untersuchungen mit Zement in Porenlösung durchgeführt. Die Experimente wurden mit verschiedenen Feststoffvolumenfraktionen durchgeführt und mit den Ergebnissen identischer Systeme mit Wasser anstelle von Porenlösung verglichen. Zusätzlich wurden die gleichen Systeme mit Zugabe von Polycarboxylatethern untersucht.
Die Ergebnisse zeigen, dass die Leime mit Wasser niedrigere Werte für Fließgrenze und plastische Viskosität aufweisen, als die Systeme mit Porenlösung. Während die Polymere eine Verminderung der Fließgrenze zur Folge hatte, war die Wirkung von Polymeren auf die plastische Viskosität vernachlässigbar. Zusätzlich wurde die frühe Hydratation unter Verwendung von Wärmeflusskalorimetrie, Rasterelektronenmikroskopie und Nadeleindringtiefe beobachtet.
Die Rheologie von fließfähigen zementären Systemen mit Fließmitteln wird durch eine Vielzahl parallel stattfindender Effekte beeinflusst. Zu diesen Effekten zählen Wechselwirkungen zwischen den Polymeren und Ionen in der Porenlösung, frühe Phasenbildung, zeitabhängige und kompetitive Adsorption zwischen anionischen Polymeren und Sulfationen, Bildung von Phasen in der Porenlösung sowie Morphologieänderungen an Partikeloberflächen. Die frühe Hydratation von Zement, die durch Lösungs- und Fällungsprozesse angetrieben wird, beeinflusst diese Effekte erheblich. Das permanente Ungleichgewicht der Porenlösung führt zu Veränderungen der Partikeloberflächen, welches widerum zur Folge hat, dass rheometrische Messungen dieser Zementleime anfällig für Streuungen sind. Um die Einflüsse aus der Zementhydratation zu minimieren, wurden die rheometrischen Untersuchungen mit Zement in Wasser, wässriger Phase von Zementleim bzw. mit vorhydratisiertem Zement durchgeführt. Zusätzlich wurden die gleichen Systeme mit Zugabe von Polycarboxylatethern untersucht.
Die Ergebnisse zeigen, dass die Leime mit Wasser niedrigere Werte für Fließgrenze und plastische Viskosität aufweisen, als die Systeme mit der wässrigen Phase von Zementleim. Während die Polymere eine Verminderung der Fließgrenze zur Folge hatte, war die Wirkung von Polymeren auf die plastische Viskosität vernachlässigbar. Zusätzlich wurde die frühe Hydratation unter Verwendung von Wärmeflusskalorimetrie, Rasterelektronenmikroskopie und Nadeleindringtiefe beobachtet.
The effects of weathering exposure on unfilled and filled thermoplastic polyurethanes (TPU) materials are described as performed under different humidity conditions. For this purpose, a weathering device was used with UV-A 340 nm lamps at a constant temperature of 40 °C. The effects of environmental (UV and humidity condition) degradation on the frictional properties of TPU materials are presented along with surface analyses to characterize the chemistry of the degradative process. Photooxidative degradation of unfilled polymer leads to deterioration of physical and mechanical properties, which affects its tribological behavior significantly. Due to crosslinking, the stiffness of the material increases, reducing drastically the friction coefficient of unfilled TPUs. The frictional behavior of glass fiber reinforced TPU is less affected by radiation.
Polymers of Intrinsic Microporosity (PIMs) of high performance have developed as materials with a wide application range in gas separation and other energy-related fields. Further optimization and long-term behavior of devices with PIMs require an understanding of the structure-property relationships including physical aging. In this context the glass transi-tion plays a central role, but with conventional thermal analysis a glass transition is usually not detectable for PIMs be-fore their thermal decomposition. Fast scanning calorimetry provides evidence of the glass transition for a series of PIMs, as the time scales responsible for thermal degradation and for the glass transition are decoupled by employing ultrafast heating rates of tens of thousands K s-1. The investigated PIMs were chosen considering the chain rigidity. The estimated glass transition temperatures follow the order of the rigidity of the backbone of the PIMs.
In this study, a multi-proxy approach combining 29Si, 27Al and 1H MAS-NMR, FEG-EPMA, XANES at the Cu K-edge and XRD analytics with hydrochemical tools such as ICP-OES analyses, oxygen-isotope signatures, and thermodynamic modelling was applied to K-silicate-activated metakaolin specimens - with and without CuSO4·5H2O addition - exposed to sulfuric acid at pH = 2 for 35 days. The results revealed a multistage deterioration mechanism governed by (i) acid diffusion, (ii) leaching of K-A-S-H, (iii) microstructural damage related to precipitation of expansive (K,Ca,Al)-sulfate-hydrate phases (iv) complete dissolution of the K-A-S-H framework, (v) and formation of silica gel in the outermost corroded regions. Copper ions were mainly located in layered spertiniite-chrysocolla-like phases in the as-cured materials. The results demonstrate an overall negative effect of Cu addition on chemical material durability, implying that the reported higher durability of Cu-doped AAM in biocorrosion environments can be best explained by bacteriostatic effects.
Design and construction of a rainfall simulator to test metal runoff at atmospheric conditions
(2023)
A rainfall simulator was presented as an environmental assessment tool to quantify wash-off concentrations from metallic materials. It is part of the RUNOFF-project, which studies and re-assesses the durability of roofing and facade materials under current atmospheric conditions in Germany.
Studying building materials is important as they have a significant impact on achieving a variety of goals and targets within the sustainable developments goals (SDGs). The durability of materials is essential to reach sustainability. However, the durability of metallic materials is strongly depended on climate conditions, which have changed as a result of technical measures in industry, climate change and increasing urbanisation. In Germany at least, the data base is not up-to-date leading to prediction models regarding corrosion resistance and durability of metallic materials which can no longer be trusted and therefore need to be re-assessed and updated. Also, not only the demand for sustainable but also environmentally friendly building materials has increased dramatically. A number of construction materials produce chemical hazards, and therefore have negative impacts on water quality, soils health and ecosystems. To limit these impacts, environmental assessment methods and tools are needed to measure and quantify the inputs and outputs of building materials throughout their lifetime.
Metakaolin-based alkali activated mortars (AAM) - with and without CuSO4·5H2O and ZnO addition (mass ratio Mn+/solid binder 0.08% to 1.7%) - were casted and exposed within an extensive long-term field campaign over the period of 20 months to a sewer basin, strongly affected by biogenic acid corrosion. (Un-)exposed AAM were tested regarding their physicochemical and microstructural properties, bioreceptivity and overall durability. Metal addition led to a retarding effect during alkali-activation reaction, as well as to an increase in open porosity of up to 3.0% and corresponding lower compressive strength of up to 10.9%. Reduced microbial colonization and diversity were observed on AAM with Cu, while Zn addition led to increased biodiversity. We propose that the observed higher durability of Cu-doped AAM is due to antibacterial effects and associated reduction of biogenic acid production, superseding overall negative effects of metal-dosage on physical material properties. Observed lower durability of Zn-doped AAM was related to combined negative physicochemical and microbial effects.
In a laboratory test, transparent high‐density polyethylene (HDPE) jerrycans have been exposed to both UV radiation and 55 wt‐% nitric acid solution at (41 ± 2)°C, for up to 20 days. For comparison, UV radiant exposure (21 days) and nitric acid exposure (up to 6 weeks) were performed separately, at nearly equal temperatures. The damages are compared with FTIR spectroscopy in ATR and HT‐gel permeation chromatography(GPC) on a molecular level and with hydraulic internal pressure testing as a component test. For the used jerrycans, relevant oxidation can only be found after the combined exposure. This is caused by the decomposition of nitric acid into nitrous gases by UV radiation, which is also observed at lower concentrations (28 wt‐%). After 6 days of laboratory exposure, this is rated as critical, which corresponds to about 1/10 year in Central Europe, according to the UV radiant exposure. The gradual increase in oxidative damage shows the reproducibility of the test.
In recent years superglassy polymers exhibiting intrinsic microporosity established a new perspective for a number of applications, especially for gas separation membranes as These polymers Combine extremely high permeabilities with attractive selectivities. The essential factor governing the structure Formation in the solid film or layer is either a contorted rigid Backbone (polymers of intrinsic microporosity - PIMs) or extremely bulky side groups (polynorbornenes and polytricyclonenenes).
For a deeper understanding of both types of such high-Performance polymers for gas separation membranes and their further development broadband dielectric spectroscopy (BDS) can provide a substantial contribution.
BDS addresses molecular relaxations characterizing the dynamics of the solid polymer as a major factor determining the gas transport properties but also the physical aging behavior which is an essential issue for such polymers.
BDS is applied on PIMs where fluctuations of molecular dipoles connected to the backbone can be directly monitored. Furthermore, also polynorbornenes were investigated which carry no dipole moment in their repeat unit - the high resolution of modern equipment allows for the detailed analysis also for very small dielectric losses originating from partially oxidized moieties or marginal catalyst residues.
Additionally, from interfacial polarization phenomena, such as Maxwell-Wagner-Sillars (MWS) polarization due to blocking of charge carriers at internal interfacial boundaries on a mesoscopic length scale, valuable information on the intrinsic microporosity and its changes induced by physical aging can be obtained.
Finally, also conductivity can be characterized in detail in such polymeric systems revealing contributions of interactions of aromatic moieties (π-π-stacking) or the drift motion of charge carriers. These features also determine the structure formation in the solid state.
Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. Here, the vibrational density of states (VDOS) for PIM-1, the prototypical polymer with intrinsic microporosity, is investigated by means of inelastic neutron scattering. The results are compared to data measured for a more conventional high-performance polyimide used in gas separation membranes (Matrimid). The measured data show the characteristic low frequency excess contribution to VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. In comparison to the Boson peak of Matrimid, that of PIM-1 is shifted to lower frequencies. This shift is discussed considering the microporous, sponge-like structure of PIM-1 as providing a higher compressibility at the molecular scale than for conventional polymers. For an annealed PIM-1 sample, the Boson peak shifts to higher frequencies in comparison to the un-annealed sample. These changes in the VDOS of the annealed PIM-1 sample are related to changes in the microporous structure as confirmed by X-ray scattering.
Polyether and -ester urethanes (PU) were exposed to artificial weathering at 40 °C and artificial UV radiation in a weathering chamber. In 3 parallel exposures, humidity was varied between dry, humid, and wet conditions. Material alteration was investigated by various analytical techniques like size exclusion chromatography
(SEC), liquid chromatography-infrared spectroscopy (LC-FTIR), thermal-desorption gas chromatography-mass spectrometry (TD-GC-MS), fluorescence mapping and dynamic mechanical analysis (DMA). Our results show that depending on the weathering conditions, different degradation effects can be observed. By means of SEC an initial strong decrease of the molar masses and a broadening of the mass distributions was found. After a material dependent time span this was followed by a plateau where molar mass changes were less significant. A minor moisture-dependent degradation effect was only found for polyester PU. Fluorescence measurements on two materials revealed an increase in the luminescence intensity upon weathering process reaching a saturation level after about 500 h. The changes in the optical properties observed after different exposure conditions and times were very similar. The TD-GC-MS data showed the fate of the stabilizers and antioxidant in the course of weathering. LC-FTIR measurements revealed a change in peak intensities and the ratio of urethane and carbonyl bands.
Organic/inorganic mixtures were prepared from ordinary Portland cement (OPC), water (w/c 0.22), a fluorescent dye in aqueous solution (stable at alkaline pH; BAM-I), and two different comb shape polycarboxylates (PCEs), i.e., high charge (PCE-HC) and low charge (PCE-LC), respectively. Rheological and calorimetric measurements were performed prior to optical studies in order to select PCE concentrations. Absorption and fluorescence spectroscopy of the system OPC + BAM-I (CBAM-I) revealed maxima of dye BAM-I located at 645 nm and 663 nm, respectively. In presence of PCE-HC and PCE-LC, these mixtures displayed a small red shift in reflectance and a faster decrease in intensity compared to studies with CBAM-I; however, only slight differences were observed between the different PCEs. With time, all systems exhibited a decrease in intensity of BAM-I in absorption/reflectance and emission. This could be caused by dye adsorption and possibly decomposition when in contact with cement particles or hydration products.
The influence of starting materials and synthesis route on the properties and the structure of cementitious sodium aluminosilicate gels is not fully understood, partly due their amorphous nature and the fact that they often contain residual reactants, which can make the results of single-pulse NMR spectroscopy applied to these materials difficult to interpret or ambiguous. To overcome some of these limitations, 29Si{27Al} TRAPDOR NMR as well as 27Al{29Si} and 27Al{1H} REDOR NMR spectroscopy were applied to materials synthesized by the one-part alkali-activation route from three different amorphous silica starting materials, including rice husk ash. The latter led to formation of a fully amorphous sodium aluminosilicate gel (geopolymer), while the materials produced from the other silicas contained amorphous phase and crystalline zeolites. Application of the double-resonance NMR methods allowed to identify hydrous alumina gel domains in the rice husk ash-based material as well as significantly differing amounts of residual silica in the three cured materials. Four-coordinated Al existed not only in the aluminosilicate gel framework but also in a water-rich chemical environment with only a small amount of Si in proximity, likely in the alumina gel or possibly present as extra-framework Al in the aluminosilicate gel. The results demonstrate how the employment of different silica starting materials determines the phase assemblage of one-part alkali-activated materials, which in turn influences their engineering properties such as the resistance against chemically/biologically aggressive media.
The chapter gives a brief introduction to (nano)compositecomposite materials having the focus on polymer-based nanocomposites. The different dimensionalities of nanoparticles are introduced, along with their distribution in the matrix.
Different application fields of polymer-based nanocomposites, like flame retardancy, filled rubbers, nanofilled thermosets and thermoplastics, separation membranes and nanodielectrics, are considered in greater detail.