5 Werkstofftechnik
Filtern
Erscheinungsjahr
- 2019 (187) (entfernen)
Dokumenttyp
- Vortrag (73)
- Zeitschriftenartikel (55)
- Posterpräsentation (31)
- Beitrag zu einem Tagungsband (19)
- Buchkapitel (2)
- Sonstiges (2)
- Forschungsbericht (2)
- Monografie (1)
- Dissertation (1)
- Forschungsdatensatz (1)
Sprache
- Englisch (156)
- Deutsch (30)
- Mehrsprachig (1)
Schlagworte
- Corrosion (17)
- Additive Manufacturing (14)
- Glass (12)
- Carbon steel (8)
- Low Cycle Fatigue (8)
- Microstructure (7)
- CO2 (6)
- Degradation (6)
- Fatigue (6)
- Water content (6)
- Additive manufacturing (5)
- CCS (5)
- Ceramic (5)
- Crack growth (5)
- Crystallization (5)
- EBSD (5)
- Oxidation (5)
- 3D printing (4)
- LCF (4)
- Mikrostruktur (4)
- P92 (4)
- Ti-6Al-4V (4)
- Transmission electron microscopy (4)
- 316L (3)
- Alloy 2618A (3)
- Anisotropy (3)
- Carbon capture (3)
- Ceramic spring (3)
- Ceramics (3)
- DCB (3)
- Diesel (3)
- Diffraction (3)
- Diopside (3)
- Full-Notch Creep Test (FNCT) (3)
- High temperature corrosion (3)
- In situ (3)
- Modeling (3)
- Orientation (3)
- Pitting (3)
- Polymer (3)
- Sandwich (3)
- Simulation (3)
- Sintering (3)
- Slurry (3)
- Steel (3)
- Sulfidation (3)
- Tempered Martensite Ferritic Steels (3)
- Thermo-Mechanical Fatigue (3)
- Utilization (3)
- Water speciation (3)
- µ-gravity (3)
- 3D (2)
- AISI 316L (2)
- Additive Fertigung (2)
- Al-Cu-Li alloys (2)
- Alterung (2)
- Aluminium (2)
- Betriebsfestigkeit (2)
- Bioactive glass (2)
- Bioceramics (2)
- CCU (2)
- CCUS (2)
- CT (2)
- Capture (2)
- Carbon (2)
- Coarsening (2)
- Composite (2)
- Computed Tomography (2)
- Condensate (2)
- Condensation (2)
- Corrosion Fatigue (2)
- Crack Propagation (2)
- Crack propagation (2)
- Creep-Fatigue (2)
- Crevice corrosion (2)
- Crystal plasticity (2)
- Dehnungsfehler (2)
- Digital material representation (2)
- Distribution function (2)
- Ductile iron (2)
- Early oxidation (2)
- Elastic constants (2)
- Electron energy (2)
- Energy distribution (2)
- Extensometer (2)
- FeCr- alloys (2)
- Fiber reinforced polymer (2)
- Fracture surface analysis (2)
- Fraktografie (2)
- Geothermal (2)
- Glas (2)
- Glass fiber reinforced polymers (2)
- Glass-ceramic (2)
- High Alloyed Steel (2)
- High Temperature Testing (2)
- High temperature (2)
- IN 718 (2)
- IR (2)
- Impurities (2)
- Internal friction (2)
- Kavitation (2)
- Kikuchi pattern (2)
- Kleinprobenprüfung (2)
- Laminography (2)
- Layerwise (2)
- Layerwise slurry deposition (2)
- Lightweight materials (2)
- Material degradation (2)
- Microhardness (2)
- Mixed Ca-K-Na phosphates (2)
- Monte-Carlo Simulation (2)
- NMR spectroscopy (2)
- Na and K rhenanites (2)
- Niobium alloying (2)
- Non-destructive testing (2)
- Phase diagram (2)
- Phase transformations (2)
- Photon counting detector (2)
- Pipelines (2)
- Polyethylene, PE-HD (2)
- Polymer matrix composites (2)
- Pores (2)
- Powder (2)
- Probengrößeneffekt (2)
- Roughness (2)
- Röntgenbeugung (2)
- Röntgenrefraktion (2)
- Scale-bridging (2)
- Schadensanalyse (2)
- Schädigung (2)
- Selective laser melting (2)
- Silicon Carbide (2)
- Soda-lime silicate glass (2)
- Soda-lime-silica glass (2)
- Storage (2)
- Surface (2)
- Surface crystallization (2)
- Synthetic air (2)
- TMF (2)
- Temperaturschwankungen (2)
- Tensile Properties (2)
- Ti64 (2)
- TiAl5V4 (2)
- Titan (2)
- Titanium (2)
- Topografie (2)
- Utilization, and storage (CCUS) technology (2)
- VSSA (2)
- Vickers indentation (2)
- Virtual experiments (2)
- Weibull Distribution (2)
- Werkstoffprüfung (2)
- Wind energy (2)
- Wind turbine blades (2)
- Zero-g (2)
- Zugeigenschaften (2)
- Zugversuch (2)
- 3D imaging (1)
- 5G (1)
- AFM based test methods (1)
- AISI 304L (1)
- AM (1)
- Abrasion (1)
- Aggressive environment (1)
- Alkali-activated materials (1)
- Alumina (1)
- Aluminosilicate glasses (1)
- Analytische Zentrifuge (1)
- Anwendungen (1)
- Aquifer (1)
- Artificial weathering (1)
- Atomization (1)
- Aufbau von Festkörpern (1)
- Aussonderugnsrate (1)
- BTS (1)
- Berstdruck (1)
- Biodiesel (1)
- Biogeochemical cycling (1)
- Biomineralisation (1)
- Biopolymer (1)
- Blähen (1)
- Breakdown strength (1)
- Brittle fracture (1)
- Bruchflächenanalyse (1)
- Bubble formation (1)
- C. lap-shear (1)
- CALPHAD (1)
- CALPHAD databases analysis (1)
- CFRP (1)
- CO2 Corrosion (1)
- CO2 separation membranes (1)
- CO2-Speicherung (1)
- CO2-storage (1)
- Calcination (1)
- Calcium cobaltite (1)
- Calibration (1)
- Carbidic austempered ductile iron (1)
- Carbon Capture, Utilization and Storage (CCUS) (1)
- Carbon capture, utilization and storage technology (1)
- Carbon fibres (1)
- Carbon storage (1)
- Cavitation (1)
- Cellulose (1)
- Cement (1)
- Certification Standard 22 (1)
- Chalcogenides (1)
- Characterisation (1)
- Chemically Complex Alloy (1)
- Chemische Analyse (1)
- Chemo-mechanical coupling (1)
- Co-axial monitoring (1)
- Coefficient of thermal expansion (1)
- Complex concentrated alloy (CCA) (1)
- Contact angle (1)
- Contact fatigue (1)
- Copper vacancies (1)
- Corrosion and storage (CCUS) technology (1)
- Corrosion pits (1)
- Corrosion resistance (1)
- Crack arrest (1)
- Crack healing (1)
- Creep (1)
- Crosslinking (1)
- Crystal Plasticity Modelling (1)
- Crystal Texture (1)
- Crystal orientation (1)
- Cyclic softening (1)
- D. aging (1)
- D. creep D. viscoelasticity (1)
- DED-L (1)
- Damage (1)
- Dark-field transmission electron microscopy (DFTEM) (1)
- Data storage (1)
- Defects (1)
- Deformation behavior (1)
- Dense phase (1)
- Destabilization (1)
- Deuterium (1)
- Dielectric breakdown (1)
- Dielectric strength (1)
- Diesel Fuel (1)
- Dislocation (1)
- Dislocations (1)
- Distributed fiber optic sensing (1)
- Distributed fiber optic sensors (1)
- Droplet (1)
- Droplet corrosion (1)
- Druckgasspeicher (1)
- Dual-energy (1)
- Dynamic mechanical analysis (1)
- Dynamisch Mechanische Analyse (1)
- EASA (1)
- EIS (1)
- Early sulfidation (1)
- Eigenschaften (1)
- Electrochemical characterisation (1)
- Electrochemical deposition (1)
- Electrochemical dressing (1)
- Electrochemical impedance spectroscopy (1)
- Electromicroscopy (1)
- Electron backscattered diffraction (EBSD) (1)
- Electron microscopy (1)
- Electropolishing (1)
- Endurance Limit (1)
- Energiespeicherung (1)
- Environment (1)
- Environmental Stress Cracking (ESC) (1)
- Environmental stress cracking (1)
- Environmental stress cracking (ESC) (1)
- Environmentally assisted cracking (1)
- Ermüdung (1)
- Erneuerbare Energien (1)
- Explosionsschutz (1)
- Exposed metal sites (1)
- FSDC (1)
- Fabrication (1)
- Facilitated activation (1)
- Failure test (1)
- Faser-Kunststoff-Verbunde (1)
- Faserkunststoffverbunde (1)
- Fatigue Life Evaluation (1)
- Fatigue Testing (1)
- Fatigue crack propagation stages (1)
- Ferritic steels (1)
- Ferritic–martensitic steel (1)
- Fiber reinforced polymers (1)
- Fine Powder (1)
- Finite element analysis (1)
- Flowability (1)
- Foaming (1)
- Focused Ion Beam (1)
- Force-distance diagram (1)
- Four-point bending test (1)
- Fracture (1)
- Fracture mechanics (1)
- Freeze Drying (1)
- Freeze casting (1)
- Fresnoit (1)
- Friction Stir Welding (1)
- Frozen state photopolymerization (1)
- GFRP (1)
- Gasdetektion (1)
- Gassensorik (1)
- Gefügeuntersuchung (1)
- Glass ceramic (1)
- Glass matrix composite (1)
- Glass powder (1)
- Glass screening device (1)
- Glasspeicher (1)
- Gleichgewicht (1)
- Gold (1)
- Grain boundary (1)
- Grünfolieneigenschaften (1)
- HDPE Soprption (1)
- HDPE Sorption (1)
- Hard machining (1)
- Hardness (1)
- Heat treatment (1)
- Heißgasextraktion (1)
- Heißgaskorrosion (1)
- Hierarchical porosities (1)
- High alloyed steel (1)
- High entropy alloys (1)
- High pressure (1)
- High-entropy alloys (1)
- High-temperature corrosion (1)
- High-temperature oxidation (1)
- High-temperature properties (1)
- High-voltage testing (1)
- Hochentropielegierungen (1)
- Hochtemperaturermüdung (1)
- Honing (1)
- Honing Stone (1)
- Hydrogel (1)
- Hydrogen (1)
- Hydrogen diffusivity (1)
- Hygrothermal (1)
- Impact damage (1)
- In-situ Process Monitoring (1)
- Inclusion cluster (1)
- Inclusion size (1)
- Inconel 625 (1)
- Inconel 686 (1)
- Incremental lifetime models (1)
- Infrared nano AFM (1)
- Infrared spectroscopy (1)
- Intermodulation AFM (1)
- Internal Surfaces (1)
- Internal oxidation (1)
- Interphase (1)
- Ionic porosity (1)
- Iron meteorite (1)
- Irregular topography (1)
- Keramikfeder (1)
- Keramische Folien (1)
- Korrosion (1)
- Kreislaufwirtschaft (1)
- Kriechen (1)
- Kristallisation (1)
- Kristallsystem (1)
- Kurzfaser-verstärkte Thermoplaste (1)
- LMD (1)
- LSD print (1)
- LTCC multilayer (1)
- Langzeitstabilität (1)
- Laser Beam Melting (1)
- Laser Scanning Microscopy (1)
- Laser Scanning Microscopy (LSM) (1)
- Laser beam melting (1)
- Laser cladding (1)
- Laser-induced slip casting (1)
- Laserbearbeitung (1)
- Laserscanningmikroskopie (LSM) (1)
- Layer system (1)
- Layerwise Slurry Deposition (1)
- Lebensdauer (1)
- Long-term storage (1)
- Low cycle fatigue (1)
- MOF-74 (1)
- Machine Learning (1)
- Magmatic and hydrothermal processes (1)
- Magnetic domains (1)
- Magnetische Domänen (1)
- Magnetoelastic effect (1)
- Magnetoelastischer Effekt (1)
- Martensite (1)
- Mass transport (1)
- Materialkreislauf (1)
- Materialprüfung (1)
- Materials science (1)
- Mechanical behavior (1)
- Mechanical properties (1)
- Mehrachsige Verformung (1)
- Metal powder characterization (1)
- Metrology (1)
- Micro-shrinkages (1)
- Micromechanical model (1)
- Microstructure analysis (1)
- Microstructure characterisation (1)
- Microstructure evolution (1)
- Microstructure modification (1)
- Mikrostrukturuntersuchung (1)
- Mindedestberstdruck (1)
- Mini-UAV (1)
- Mis-match (1)
- Mixed-linkers (1)
- Modell (1)
- Moisture (1)
- Mortel (1)
- Multiaxial deformation (1)
- Multiple cracks (1)
- NDT (1)
- NMR (1)
- Nano particle (1)
- Nano screening (1)
- Nanocomposites (1)
- Nanomaterial (1)
- Nanoparticles (1)
- Natural (1)
- Neutron diffraction (1)
- New standards (1)
- Ni-Resist (1)
- Nitride (1)
- Non-destructive Materials (1)
- Non-metallic inclusions (1)
- Nondestructive testing (1)
- Normung (1)
- Ooxidation (1)
- Optical criterion (1)
- Orientation relationship (1)
- Oxidation protection (1)
- PE-HD Sorption (1)
- Parabolic flight (1)
- Particle size (1)
- Partikelgrößenverteilung (1)
- Permeability (1)
- Phase transformation (1)
- Phase-field (1)
- Phase-field simulation (1)
- Phosphate (1)
- Physically based material model (1)
- Pipeline (1)
- Pitting corrosion (1)
- Plastic deformation (1)
- Platinum-group-metals (1)
- Polyaniline (1)
- Polyethylen hoher Dichte (1)
- Polyurethane (1)
- Power plant (1)
- Power-to-Gas (1)
- Preceramic polymer (1)
- Pressure-assisted sintering (1)
- Process Monitoring (1)
- Process development (1)
- Process monitoring (1)
- Processing window (1)
- Pultruded fiber rods (1)
- REM (1)
- Referenzmaterial (1)
- Referenzorganismus (1)
- Referenzverfahren (1)
- Relaxation fatigue (1)
- Repair patch (1)
- Residual stress (1)
- Resonance testing (1)
- Restberstfestigkeit (1)
- Risikoanalyse (1)
- Rohrprobekörper (1)
- SDC (1)
- STEM (1)
- Safety (1)
- Sailplane Development Panel (1)
- Salt melt (1)
- Samarium doped ceria (1)
- Sample preparation (1)
- Sandwich structures (1)
- Scaffolds (1)
- Scanning Electron Microscopy (SEM) (1)
- Scanning electron microscopy (1)
- Scavenging effect of iron (1)
- Scratches (1)
- Semiconductor materials (1)
- Sensor (1)
- Sensorik (1)
- Silicoborate glasses (1)
- Silver glass paste (1)
- Sintern (1)
- Slip-rolling (1)
- Slow Crack Growth (SCG) (1)
- Slow crack growth (1)
- Soda-lime-silica (1)
- Sodium ion batteries (1)
- Sol-gel coating (1)
- Sorption (1)
- Spannungs-Dehnungs-Verhalten (1)
- Spannungsriss (1)
- Spar cap design (1)
- Spectroscopy (1)
- Spring constant (1)
- Spring constant (1)
- Standardisation (1)
- Stanzen (1)
- Statistics (1)
- Stress intensity factor (1)
- Stress-strain behavior (1)
- Streuung (1)
- Structural composites (1)
- Structural defects (1)
- Structural health monitoring (1)
- Structural steel (1)
- Struktur (1)
- Subcritical crack growth (1)
- Superalloy (1)
- Superconducting magnet (1)
- Supercritical CO2 (1)
- Supercritical/dense phase CO2 (1)
- Surface treatments (1)
- Swept wavelength interferometry (1)
- Synthesis (1)
- TEM (1)
- Tempered martensite ferritic steel (1)
- Tempered martensite ferritic steels (1)
- Tensile testing (1)
- Thermodynamic analysis (1)
- Thermoelectric properties (1)
- Thermomechanics (1)
- Thermomechanik (1)
- Thiol-ene click chemistry (1)
- ToF-SIMS (1)
- Transmission electron microscopy (TEM) (1)
- Tribologie (1)
- Tungsten-Rhenium (1)
- Ultrasound (1)
- Ungleichgewicht (1)
- Unlegierter Baustahl (1)
- VM12 SHC (1)
- Vacuum hot extraction (1)
- Vickers (1)
- Viscoelastic model (1)
- Viscous sintering (1)
- Viskoplastisch (1)
- WAXS (1)
- Wasserstoff (1)
- Wasserstofferzeugung (1)
- Werkstoffmechanische Prüfung (1)
- Wetting (1)
- Wind turbine blade shells (1)
- Windenergie (1)
- X-ray absorption spectroscopy (1)
- X-ray refraction (1)
- XRD (1)
- Young´s modulus (1)
- Zerstörungsfreie Prüfung (1)
- ZnO (1)
- Zug-Druck-Schubprüfung (1)
- alumina (1)
- arbidic austempered ductile iron (1)
- arbon capture (1)
- ausfgallfreie Lastwechsel (1)
- bioactive (1)
- biomaterials (1)
- bone (1)
- carbon steel (1)
- ceramics (1)
- coarsening (1)
- condensate (1)
- corrosion (1)
- electrochemical characterization (1)
- hardness (1)
- high pressure (1)
- impurities (1)
- infrared spectroscopy (1)
- microstructure analysis (1)
- phosphate glasses (1)
- pitting corrosion (1)
- selective laser melting (1)
- statistische Auswertung (1)
- utilization, and storage (CCUS) technology (1)
- volume resistivity (1)
- water speciation (1)
Organisationseinheit der BAM
- 5 Werkstofftechnik (187) (entfernen)
Eingeladener Vortrag
- nein (73)
Additive manufacturing (AM) offers diverse advantages compared to conventional manufacturing. In this work the microstructure of austenitic steel 316L, manufactured with Selective Laser Melting (SLM), was analyzed and compared to microstructure of 316L hot rolled material. Methods used for analysis are microprobe, optical microscopy and electron backscatter diffraction.
Alkali and alkaline earth chlorides are discussed as heat storage media and are characterized by their low price and high availability. Disadvantages are a high corrosion rate and formation of Cr6+ ions in the melt, as observed in various binary chlorine salt melts. In our work the system NaCl-KCl-MgCl2 is considered. The storage capacity in this salt system is between 2 and 3 MWh per 10 t salt, depending on composition, melting temperature and working temperature. At the same time the system offers a eutectic line, which allows a high variance of the composition and possibly different corrosion rates can be observed. Corrosion tests in melts were carried out and the corrosion layers investigated. The tests with chloride melts on 12% Cr steel show an inner corrosion zone of up to 40 µm depth after 96 hours. The corrosion mechanisms and potential solutions are discussed.
Der vorliegende Vortrag gibt einen Überblick über Probenpräparationen mit der Focused Ion Beam (FIB) für AFM-basierte Untersuchungsverfahren. Anhand zweier Beispiele wird gezeigt, wie ionenstrahlpolierte Lamellen aus Halbleiter-Schichtsystemen elektrisch leitfähig auf Substrate platziert werden, so dass in-situ und in-operando Messungen mit Scanning Microwave Microscope (SMM) bzw. Spectroscopic infrared scanning near-field optical microscope (IR-SNOM) durchgeführt werden können.
This work examined the factors that influence the droplet corrosion of CO2 pipeline steels caused by oxyfuel flue gases in dense phase CO2 at 278 K, simulating the underground transport conditions. The wetting properties were studied by contact angle measurement, revealing pH and time dependency on the reactive wetting behaviors of carbon steel X70. Exposure tests with CO2 saturated water droplet on steel surface showed that the impurities (220 ppmv SO2 and 6700 ppmv O2) diffused into the droplet and then reacted with metal surfaces in dense phase condition, forming the corrosion products. The corrosion rate was confirmed strongly depending on the droplet volume as well as the SO2 concentration. Condensation experiments carried out on freshly polished coupons in CO2 with 200 ppmv H2O, 220 ppmv SO2 and 6700 ppmv O2, showed that the formation and aggregation of droplets is time and temperature dependent. At 278 K, condensation happened stronger and the corrosion products, mainly consisted of dense hydrated FeSO3/FeSO4. While at 288 K, more fluffy corrosion products consisting of iron oxide/hydroxide and hydrated FeSO3/FeSO4 were found. Further exposure tests on carbon steel coupons with different surface roughness did not reveal the difference in weight loss/gain and therefore the corrosion rate.
This contribution provides current findings regarding materials susceptibility for carbon capture, utilization and storage (CCUS) applications. Basing on results gathered in 2 German long-term projects (COORAL and CLUSTER) suitable materials are introduced as well as dominating impurities of the CO2-stream and corrosion mechanisms. Investigations cover the whole CCUS process chain and provide material recommendations for certain parts.
The current trend towards cyclic, “flexible” operation of fossil-fueled power plants constitutes a major issue regarding lifetime and operational safety of the respective installations and their components, as was outlined in our complementary contribution (Part 1). The present contribution reports on the investigation of the microstructure evolution in cyclically loaded ferritic-martensitic steels and its representation in a physically-based micromechanical model.
For this purpose, specimens of P92 steel grade from the mechanical test programme outlined in our companion contribution (Part 1) were analyzed by scanning electron microscopy (SEM), including backscattered diffraction (EBSD) mapping, and transmission electron microscopy (TEM). A novel method was implemented to improve angular resolution of EBSD scans. Additionally, a correlative microscopy approach was developed and used to correlate EBSD and TEM measurements on the same locations of thick regions of electron transparent specimens. By applying these techniques, a detailed quantitative microstructure description of the as-received material condition, namely in terms of subgrain morphology and dislocation density/distributions, was established. Comparisons of as-received and cyclically loaded conditions from tests interrupted at different stages of lifetime indicate a rapid redistribution of in-grain dislocations with a strong interaction between mobile dislocations and low angle grain boundaries (LABs).
The proposed micromechanical model is formulated in a viscoplastic self-consistent (VPSC) scheme, which is a mean-field approach that allows us to include the crystal details at the level of slip systems while avoiding the considerable computational costs of full-field approaches (such as the classical crystal plasticity finite element analysis). Being physically-based, the model uses dislocation densities and includes the interaction between dislocations, e.g. annihilation of mobile dislocations, and evolution of microstructure, e.g. the grain coarsening. Particularly, the constitutive laws for dislocation evolution and interaction between dislocations and low angle boundaries are calibrated based on two-dimensional discrete dislocation dynamic (2D DDD) simulations, which are performed at a micro-/meso-scale. The results of the beforementioned EBSD experiments are considered as a direct input, involving e.g. the amount of geometrically necessary dislocations, average misorientations and grain characteristics.
Polyether and -ester urethanes (PU) were exposed to artificial weathering at 40 °C and artificial UV radiation in a weathering chamber. In 3 parallel exposures, humidity was varied between dry, humid, and wet conditions. Material alteration was investigated by various analytical techniques like size exclusion chromatography
(SEC), liquid chromatography-infrared spectroscopy (LC-FTIR), thermal-desorption gas chromatography-mass spectrometry (TD-GC-MS), fluorescence mapping and dynamic mechanical analysis (DMA). Our results show that depending on the weathering conditions, different degradation effects can be observed. By means of SEC an initial strong decrease of the molar masses and a broadening of the mass distributions was found. After a material dependent time span this was followed by a plateau where molar mass changes were less significant. A minor moisture-dependent degradation effect was only found for polyester PU. Fluorescence measurements on two materials revealed an increase in the luminescence intensity upon weathering process reaching a saturation level after about 500 h. The changes in the optical properties observed after different exposure conditions and times were very similar. The TD-GC-MS data showed the fate of the stabilizers and antioxidant in the course of weathering. LC-FTIR measurements revealed a change in peak intensities and the ratio of urethane and carbonyl bands.
Assessing the structural integrity of carbon-fibre sandwich panels in fire: Bench-scale approach
(2019)
The fire resistance of lightweight sandwich panels (SW) with carbon fibre/epoxy skins and a poly(methacryl imide) (PMI) foam core is investigated in compression under direct application of a severe flame (heat flux=200 kW m−2). A bench-scale test procedure was used, with the sample held vertically. The epoxy decomposition temperature was quickly exceeded, with rapid flash-over and progressive core softening and decomposition.
There is a change in failure mode depending on whether the load is greater or less than 50% of the unexposed failure load, or in other words if one or two skins carry the load. At high loads, failure involved both skins with a single clear linear separation across each face. There is an inflection in the failure time relationship in the ∼50% load region, corresponding to the time taken for heat to be transmitted to the rear face, along with a change in the rear skin failure mode from separation to the formation of a plastic hinge. The integrity of the carbon front face, even with the resin burnt out, and the low thermal diffusivity of the core, both play key roles in prolonging rear face integrity, something to be borne in mind for future panel design. Intumescent coatings prolong the period before failure occurs. The ratio of times to failure with and without protection is proposed as a measure of their effectiveness. Apart from insulation properties, their adhesion and stability under severe fire impact play a key role.
Within the perspective of increasing reliability of AM processes, real-time monitoring allows part inspection while it is built and simultaneous defect detection. Further developments of real-time monitoring can also bring to self-regulating process controls. Key points to reach such a goal are the extensive research and knowledge of correlations between sensor signals and their causes in the process.
Understanding the interaction between boehmite and epoxy and the formation of their interphases with different mechanical and chemical structures is crucial to predict and optimize the properties of epoxy-boehmite nanocomposites. Probing the interfacial properties with atomic force microscopy (AFM)-based methods, especially particle-matrix long-range interactions, is challenging. This is due to size limitations of various analytical methods in resolving nanoparticles and their interphases, the overlap of interphases, and the effect of buried particles that prevent the accurate interphase property measurement. Here, we develop a layered model system in which the epoxy is cured in contact with a thin layer of hydrothermally synthesized boehmite. Different microscopy methods are employed to evaluate the interfacial properties. With intermodulation atomic force microscopy (ImAFM) and amplitude dependence force spectroscopy (ADFS), which contain information about stiffness, electrostatic, and van der Waals forces, a soft interphase was detected between the epoxy and boehmite. Surface potential maps obtained by scanning Kelvin probe microscopy (SKPM) revealed another interphase about one order of magnitude larger than the mechanical interphase. The AFM-infrared spectroscopy (AFM-IR) technique reveals that the soft interphase consists of unreacted curing agent. The long-range electrical interphase is attributed to the chemical alteration of the bulk epoxy and the formation of new absorption bands.
Calcium cobaltite (Ca3Co4O9) is considered as one of the most promising thermoelectric p-type oxides for energy harvesting applications at temperatures above 500 °C. It is challenging to sinter this material as its stability is limited to 920 °C. To facilitate a practicable and scalable production of Ca3Co4O9 for multilayer generators, a systematic study of the influence of powder calcination, Bi-doping, reaction sintering, and pressure-assisted sintering (PAS) on microstructure and thermoelectric properties is presented. Batches of doped, undoped, calcined, and not calcined powders were prepared, tape-cast, and sintered with and without uniaxial pressure at 900 °C. The resulting phase compositions, microstructures and thermoelectric properties were analysed. It is shown that the beneficial effect of Bi-doping observed on pressureless sintered samples cannot be transferred to PAS. Liquid phase formation induces distortions and abnormal grain growth. Although the Seebeck coefficient is increased to 139 µV/K by Bi-doping, the power factor is low due to poor electrical conductivity. The best results were achieved by PAS of calcined powder. The dense and textured microstructure exhibits a high power factor of 326 µW/mK² at 800 °C but adversely high thermal conductivity in the relevant direction. The figure of merit is higher than 0.08 at 700 °C.
Efficient studies of scarce or expensive materials require material saving processes. Therefore, a high yield concept for small batch preparation of ready-to-press powder is exemplarily presented for yttria stabilized nano-zirconia (d50 < 50 nm).
The concept involves small batch preparation in an ultrasound resonator, dispersant selection based on zeta potential measurements, evaluation of slurry stability using an analytical centrifuge, and preparation of ready-to-press powder by freeze drying.
Freeze drying offers key advantages. Process efficiency and high yield above 95 % are independent of sample size. The dried product does not require further mechanical treatment like milling or grinding. Side effects like migration of additives are avoided.
An optimized freeze drying process tolerates slurries with moderate stability. Thus, efforts for slurry development can be reduced. Generally, identifying a suitable dispersing agent requires only 3-5 zeta potential measurements. Slurry stability is rechecked using an analytical centrifuge, which also accounts for steric stabilization. An ultrasound resonator is used to disperse the powder without contamination, which becomes critical for small batches.
The described route is exemplarily presented for the development of an additive recipe for nano-sized zirconia powder, targeting for good pressing behavior and high green density. Therefore, a variety of binding and lubricating agents were tested.
Following the presented route, 80 g zirconia powder were sufficient to conduct a study including slurry development and five sample sets with varying composition, each set comprising five discs (d = 20 mm and h = 2 mm).
The introduction of the 5G technology and automotive radar applications moving into higher frequency ranges trigger further miniaturization of LTCC technology (low temperature co-fired ceramics). To assess dimensional tolerances of inner metal structures of an industrially produced LTCC multilayer, computer tomography (CT) scans were evaluated by machine learning segmentation.
The tested multilayer consists of several layers of a glass ceramic substrate with low resistance silver-based vertical interconnect access (VIA). The VIAs are punched into the LTCC green tape and then filled with silver-based pastes before stacking and sintering. These geometries must abide by strict tolerance requirements to ensure the high frequency properties.
This poster presents a method to extract shape and size specific data from these VIAs. For this purpose, 4 measurements, each containing 3 to 4 samples, were segmented using the trainable WEKA segmentation, a non-commercial machine learning tool. The dimensional stability of the VIA can be evaluated regarding the edge-displacement as well as the cross-sectional area. Deviation from the ideal tubular shape is best measured by aspect ratio of each individual layer. The herein described method allows for a fast and semi-automatic analysis of considerable amount of structural data. This data can then be quantified by shape descriptors to illustrate 3-dimensional information in a concise manner. Inter alia, a 45 % periodical change of cross-sectional area is demonstrated.
Dielectric breakdown of ceramics is widely believed to originate from microstructural defects. Still, there is no commonly accepted model for the origin and process of dielectric failure that covers all observed phenomena and dependencies. In analogy to mechanical strength, the Weibull distribution is commonly used to evaluate dielectric strength data. This works well for a given group of specimens with constant geometry. But unlike mechanical strength, dielectric strength scales with the inverse square root of sample thickness. This cannot be explained by the classic Weibull concept. The Griffith type energy release rate model of dielectric breakdown proposed by Schneider is based on space charge injection and conducting filaments from the sample surface. This model incorporates the distinct thickness dependence and the pronounced influence of surface defects. Based on this model and the classic Weibull probability of failure, Schneider’s group theoretically derived a probability of breakdown that predicts an increase of failure probability with increasing electrode area. In our study we tested this model with dielectric strength data measured on dense alumina samples using different electrode areas. Weibull modulus and characteristic dielectric strength (scale parameter) were determined for a set of measurements using small electrodes. These values were used to calculate the failure probability under large electrodes according to the model. The calculated data excellently fits the measured values. Thus, our experiments substantiate the assumptions made in the breakdown model and the significance of surface defects for dielectric failure.
The ProboStat is a multi-purpose measurement cell suitable for various electrical and physical measurements under different atmospheres and at high temperatures. Disc and bar shaped samples are sandwiched between platinum electrodes at the top of the tubular cell. The gas tight assembly can be inserted into a furnace. Different gases can be flushed through the tube. For this study, a ProboStat was adapted to measure volume resistivity of ceramic insulators at high temperatures according to standards.
The standardized measurement of volume resistivity of ceramic insulators requires the consideration of many specifications including sample diameter, thickness, electrode design, and the proportion of these characteristics. Measurements are ideally performed in a state of dielectric equilibrium. The time-related slope of resistivity of a specific sample follows a power function. Thus, care must be taken when choosing a charge time or defining the duration of a measurement. As fringing of the guarded electrode occurs under high voltage, the effective electrode area for evaluation of the results should be corrected with respect to sample thickness and electrode design. The demands of effective standards on sample geometry and electrode design are stricter for room temperature measurements than for high temperature measurements.
To perform high temperature measurements on ceramic samples that also fulfill the demands on room temperature measurements, a ProboStat was equipped with a dedicated large sample setup for discs with diameters of up to 60 mm. The volume resistivity of different alumina samples was first measured at room temperature in a standard test fixture and then compared to results obtained with the ProboStat. All measurements were performed for at least 100 min using a 26 mm guarded electrode. High temperature measurements at 500 °C were performed using the same samples. Room temperature values obtained with the standard test fixture are in the order of 10^17 Ohm·cm. The quantitative effect of electrode area correction is presented. Practical issues related to the use of the multi-purpose cell are addressed. These include electrode material selection, application of electrodes, and compensation of leakage currents. High temperature results of volume resistivity of the different alumina samples are presented. The validity is discussed with respect to the suitability of the multi-purpose cell for such measurements.
The precise analysis of cation diffusion profiles through corrosion scales is an important aspect to evaluate corrosion phenomena under multicomponent chemical load, as during high‐temperature corrosion under deposits and salts. The present study shows a comprehensive analysis of cation diffusion profiles by electron microprobe analysis and microbeam X‐ray absorption near edge structure (µ‐XANES) spectroscopy in mixed oxide/sulfide scales grown on Fe–Cr model alloys after exposing them to 0.5% SO2. The results presented here correspond to depth‐dependent phase identification of oxides and sulfides in the corrosion scales by µ‐XANES and the description of oxidation‐state‐dependent diffusion profiles. Scales grown on low‐ and high‐alloyed materials show both a well‐pronounced diffusion profile with a high concentration of Fe3+ at the gas and a high concentration of Fe2+ at the alloy interface. The distribution of the cations within a close‐packed oxide lattice is strongly influencing the lattice diffusion phenomena due to their different oxidation states and therefore different crystal‐field preference energies. This issue is discussed based on the results obtained by µ‐XANES analysis.
The current competitive situation on electricity markets forces power plants into cyclic operation regimes with frequent load shifts and starts/shutdowns. In the present work, the cyclic mechanical behavior of ferritic-martensitic 9-12 % Cr steels under isothermal and thermomechanical loading was investigated for the example of grade P92 material. A continuous softening was observed under all loading conditions. The introduction of hold periods to the applied cycles reduced material lifetime, with most prominent effects at technologically relevant small strain levels. The microstructural characterization reveals a coarsening of the original “martensitic” lath-type microstructure to a structure with polygonal subgrains and reduced dislocation density. The microstructural data forms the input for a physically-based modelling approach, both of which are presented in “Part 2: Microstructural Evolution during Cyclic Loading and its Representation in a Physically-based Micromechanical Model“.
An overview of the BAM funed Focus Area Materials Project "AGIL" will be presented. AGIL focussed on the stdiy of the ageing characteristics of additively manufactured austenitic stainless steel with a "powder to mechanical failure" Approach. Recent Highlights are presented and a perspective for future studies.
9-12% Cr ferritic-martensitic stainless steels are widely used as high temperature construction materials in fossil fueled power plants due to their excellent creep and oxidation resistance, but changes in electricity markets during the last two decades have considerably changed the typical working conditions of these facilities. The growing share of renewable energy sources in power generation forces most of these plants into flexible operation with frequent load shifts or shutdowns. These cyclic operation profiles constitute a major lifetime issue, raising the question which fundamental processes govern the reaction of ferritic-martensitic steels to cyclic load and temperature variations.
The present contribution reports on current findings obtained in a multidisciplinary project funded by German Ministry of Education and Research (BMBF) which combines cyclic mechanical and cyclic oxidation testing of different 9-12% Cr grades with detailed microstructural analyses and related micromechanical modeling.
In the present first part of our contribution, an overview will be given on the results obtained in the mechanical testing programme of the project. Mechanical analyses were carried out on P91 and (mainly) P92 steel grades, particularly looking at softening phenomena and lifetimes obtained in isothermal cyclic loading (low cycle fatigue, LCF), non-isothermal cyclic loading (thermo-mechanical fatigue, TMF), and service-like combinations of creep and fatigue periods. For this purpose, cylindrical specimens were extracted from thick-walled steam pipes, orthogonal to the pipe axis, and subjected to strain controlled cyclic loading (± 0.2 to ±0.5 % mechanical strain) to different degrees of softening at temperatures up to 620 °C.
The test results will be presented and discussed with a focus on the impact of hold periods (i.e. combined creep-fatigue conditions) on mechanical softening, lifetime and crack formation. Details on the microstructural evolution and their representation in a micromechanical model will be given in a second, complementary contribution to this conference.
Die Metal Magnetic Memory (MMM) Methode ist ein standardisiertes, zerstörungsfreies Prüfverfahren, das für die Detektion von lokal geschädigten Materialbereichen in ferromagnetischen Bauteilen oder Proben verwendet wird. Es basiert auf der Annahme lokaler magnetoelastischer Wechselwirkungen an Spannungskonzentrationsstellen, die schwache magnetische Streufelder an den geschädigten Prüfkörperoberflächen hervorrufen. Die MMM-Methode überträgt dabei die für einachsige und elastische Verformungen entwickelten magnetoelastischen Modellvorstellungen ohne weitere Anpassungen in den Schädigungskontext, der jedoch mehrachsige Beanspruchungen und elastisch-plastische Deformationsprozesse erwarten lässt. Das Ziel der Arbeit ist es daher, die gängigen MMM-Hypothesen zur Signalentstehung fach- und skalenübergreifend und unter stärkerer Berücksichtigung mechanischer und mikrostruktureller Aspekte zu überprüfen.
Zu diesem Zweck wurden zum einen gekerbte Flachzugproben aus einem unlegierten Baustahl inhomogen elastisch-plastisch verformt und die entstehenden magnetischen Streufelder an deren Oberflächen mit einem Drei-Achsen-GMR-Magnetometer detektiert. Die so ermittelten Magnetfeld-verteilungen wurden für unterschiedliche Verformungszustände ortsaufgelöst und richtungsabhängig mit gemessenen Dehnungsverteilungen (digitale Bildkorrelation) und mit simulierten Lastspannungs-verteilungen korreliert. Die eingeschnürten Probenbereiche wurden zusätzlich topographisch mittels Streifenlichtprojektion und Weißlichtinterferenzmikroskopie vermessen, um den Magnetisierungs-prozess ebenfalls vor dem Hintergrund geometrischer Effekte diskutieren zu können.
Um systematische, verformungsinduzierte Veränderungen der magnetischen Mikrostruktur (magnetischer Domänen) im polykristallinen, quasi-isotropen Material nachzuweisen, wurde zum anderen ein in dieser Arbeit entwickelter statistischer Ansatz der Domänenanalyse angewandt. Hierfür wurde das Material zunächst durch Härteeindrücke mehrachsig elastisch-plastisch verformt, und die verformten Probenbereiche wurden anschließend mit Hilfe der Bitterstreifentechnik hauptsächlich bei niedriger Vergrößerung lichtmikroskopisch untersucht. Die beobachteten makroskopischen Domänen-kontraste wurden über ein analytisches, kontaktmechanisches (ECM-) Modell und über Makro-Eigen-spannungsmessungen (energiedispersive Synchrotron-Beugungsuntersuchungen) charakteristischen Verformungszonen unter den Härteeindrücken zugeordnet.
Die Ergebnisse dieser Untersuchungen belegen, dass die Entstehung der Streufelder – entgegen bisheriger Annahmen – nicht allein auf mechanische Spannungs- und Verformungsgradienten im Material zurückzuführen, sondern auch topographisch bedingt ist. Die Vernachlässigung überlagerter geometrischer Effekte kann zu sicherheitsrelevanten Fehlinterpretationen der magnetischen Signale führen. Einachsige magnetoelastische Modellvorstellungen sollten zudem nicht ohne Anpassungen auf komplexe Beanspruchungen übertragen werden, da u. a. sowohl mechanische Größen (wie Spannungen oder Dehnungen) als auch mikrostrukturelle Parameter (wie z. B. Versetzungsdichten) bei komplexen Belastungen als ortsabhängige Variablen behandelt werden müssen. Die in dieser Arbeit beobachteten Domänenkontraste lassen sich zweifelsfrei charakteristischen Verformungszonen zuordnen, mikro-strukturell jedoch nicht allein mit anzunehmenden Gradienten der Versetzungsdichte erklären. Statt-dessen entstehen beispielsweise lokale Verformungstexturen, die zusätzliche magnetische Anisotropien bewirken könnten. Da bisher weder die makroskopischen noch die mikrostrukturellen Ursachen der Streufeldentstehung hinreichend verstanden sind, scheint die MMM-Methode für die quantitative Bewertung des Schädigungszustands derzeit ungeeignet.
As humanity contemplates manned missions to Mars, strategies need to be developed for the design and operation of hospitable environments to safely work in space for years. The supply of spare parts for repair and replacement of lost equipment will be one key need, but in-space manufacturing remains the only option for a timely supply. With high flexibility in design and the ability to manufacture ready-to-use components directly from a computeraided model, additive manufacturing (AM) technologies appear extremely attractive. For the manufacturing of metal parts, laser-beam melting is the most widely used AM process. However, the handling of metal powders in the absence of gravity is one prerequisite for its successful application in space. A gas flow throughout the powder bed is successfully applied to compensate for missing gravitational forces in microgravity experiments. This so-called gas-flow-assisted powder deposition is based on a porous Building platform acting as a filter for the fixation of metal particles in a gas flow driven by a pressure difference maintained by a vacuum pump.
The project ProMoAM is presented. The goal of the project is to evaluate which NDT techniques or combination of techniques is suited for in-situ quality assurance in additive manufacturing of metals. To this end, also 3d-data fusion and visualization techniques are applied. Additional ex-situ NDT-techniques are used as references for defect detection and quantification. Feasability studies for NDT-techniques that are presently not applicable for in-situ use are performed as well.
The presentation gives a brief overview of the whole project and the different involved NDT-techniques.
Der Aufbau der Werkstoffe wird durch Merkmale wie Bindungsart, atomare Strukturen, Kristallstrukturen einschließlich ihrer Gitterbaufehler, Körner und Phasen bestimmt. Die Mikrostruktur (Gefüge) stellt den Verbund der Kristalle, Phasen und Gitterbaufehler auf mikroskopischer und nanoskopischer Skala dar. Die Grundlagen der Phasenumwandlungen werden behandelt und die Bedeutung von Diffusionsprozessen erläutert. Werkstoffe sind bedeutend für Kultur, Wirtschaft, Technik und Umwelt. Ihre Herstellung benötigt Ressourcen und Energie. Recycling ist eine Möglichkeit zur Erhöhung der Ressourcenproduktivität.
Cyclic mechanical performance and microstructure evolution of P92 under LCF and TMF conditions
(2019)
9-12% Cr ferritic-martensitic stainless steels are widely used as high temperature construction materials in fossil fueled power plants due to their excellent creep and oxidation resistance, but changes in electricity markets during the last two decades have considerably changed the typical working conditions of these facilities. The growing contribution of renewable energy sources in power generation forces most of these plants into flexible operation with frequent load shifts or shutdowns. These cyclic operation profiles constitute a major lifetime issue, raising the question which fundamental processes govern the reaction of ferritic-martensitic steels to cyclic load and temperature variations.
The present contribution reports on current findings obtained in a multidisciplinary project funded by German Ministry of Education and Research (BMBF) which combines cyclic mechanical and cyclic oxidation testing of different 9-12% Cr grades with detailed microstructural analyses and related micromechanical modeling.
In this contribution, an overview will be given on the results obtained in the mechanical testing programme of the project. Mechanical analyses were carried out on P91 and (mainly) P92 steel grades, particularly looking at softening phenomena and lifetimes obtained in isothermal cyclic loading (low cycle fatigue, LCF), non-isothermal cyclic loading (thermo-mechanical fatigue, TMF), and service-like combinations of fatigue and creep/relaxation periods. For this purpose, cylindrical specimens were extracted from thick-walled steam pipes, orthogonal to the pipe axis, and subjected to strain controlled cyclic loading (± 0.2 to ±0.5 % mechanical strain). Temperature intervals of TMF tests were chosen as either 300-620°C or 500-620°C, resembling so-called warm or hot start conditions of a power plant.
The test results will be presented and discussed with a focus on the impact of hold periods during testing (combined creep/relaxation-fatigue conditions) on mechanical softening, lifetime and formation of cracks. The findings will be complemented by results on the modification of the hierarchical ferritic-martensitic microstructure under different loading scenarios.
Dielectric strength testing of ceramics can be performed with various setups and parameters. Comparisons of results from different sources are often not meaningful, because the results are strongly dependent on the actual testing procedure. The aim of this study is to quantify the influence of voltage ramp rate, electrode size, electrode conditioning, and sample thickness on the measured AC dielectric strength of a commercial alumina. Mean values, Weibull moduli, and failure probabilities determined in standardized short time tests are evaluated and related to withstand voltage tests. Dielectric strength values in the range from 21.6 to 33.2 kV/mm were obtained for the same material using different testing procedures. Short time tests resulted in small standard deviations (< 2 kV/mm) and high Weibull moduli around 30, while withstand tests at voltage levels with low and virtual zero failure probability in short time tests resulted in large scatter of withstand time and Weibull moduli < 1. The strong decrease in Weibull moduli is attributed to progressive damage from partial discharge and depolarization during AC testing. These findings emphasize the necessity of a thorough documentation of testing procedure and highlight the importance of withstand voltage tests for a comprehensive material characterization.