5 Werkstofftechnik
Filtern
Dokumenttyp
- Vortrag (419) (entfernen)
Sprache
- Englisch (320)
- Deutsch (96)
- Mehrsprachig (3)
Referierte Publikation
- nein (419)
Schlagworte
- Additive Manufacturing (36)
- Additive manufacturing (23)
- Corrosion (20)
- Microstructure (18)
- Glass (15)
- Ontology (15)
- Ceramics (13)
- Fatigue (12)
- LCF (11)
- Additive Fertigung (10)
Organisationseinheit der BAM
- 5 Werkstofftechnik (419)
- 5.1 Mikrostruktur Design und Degradation (110)
- 5.2 Metallische Hochtemperaturwerkstoffe (106)
- 5.4 Multimateriale Fertigungsprozesse (102)
- 5.3 Polymere Verbundwerkstoffe (52)
- 5.6 Glas (47)
- 5.5 Materialmodellierung (44)
- 8 Zerstörungsfreie Prüfung (40)
- 9 Komponentensicherheit (38)
- 7 Bauwerkssicherheit (33)
Manipulating ceramic powder compacts and ceramic suspensions (slurries) within their volume with light requires a minimum transparency of the materials. Compared to polymers and metals, ceramic materials are unique as they offer a wide electronic band gap and thus a wide optical window of transparency. The optical window typically ranges from below 0.3 µm up to 5µm wavelength. Hence, to penetrate with laser light into the volume of a ceramic powder compound its light scattering properties need to be investigated and tailored. In the present study we introduce the physical background and material development strategies to apply two-photon-polymerization (2PP) for the additive manufacture of filigree structures within the volume of ceramic slurries.
Manipulating ceramic powder compacts and ceramic suspensions (slurries) within their volume with light requires a minimum transparency of the materials. Compared to polymers and metals, ceramic materials are unique as they offer a wide electronic band gap and thus a wide optical window of transparency. The optical window typically ranges from below 0.3 µm up to 5µm wavelength. Hence, to penetrate with laser light into the volume of a ceramic powder compound its light scattering properties need to be investigated and tailored. In the present study we introduce the physical background and material development strategies to apply two-photon-polymerization (2PP) for the additive manufacture of filigree structures within the volume of ceramic slurries.
Manipulating ceramic powder compacts and ceramic suspensions (slurries) within their volume with light requires a minimum transparency of the materials. Compared to polymers and metals, ceramic materials are unique as they offer a wide electronic band gap and thus a wide optical window of transparency. The optical window typically ranges from below 0.3 µm up to 5µm wavelength. Hence, to penetrate with light into the volume of a ceramic powder compound, its light scattering properties need to be investigated and tailored. In the present study we introduce the physical background and material development strategies to apply two-photon-polymerization (2PP), and other volumetric methods for the additive manufacture of filigree structures within the volume of ceramic slurries.
In order to be able to manipulate ceramic powder compacts and ceramic suspensions (slurries) within their volume with light, a minimum transparency of the materials is required. Compared to polymers and metals, ceramic materials are characterized by the fact that they have a wide electronic band gap and therefore a wide optical window of transparency. The optical window generally ranges from less than 0.3 µm to 5 µm wavelength. In order to focus light into the volume of a ceramic powder compact, its light scattering properties must therefore be tailored. In this study, we present the physical background and material development strategies for the application of two-photon polymerization (2PP) and selective volumetric sintering for the additive manufacturing of structures in the volume of ceramic slips and green compacts.
The Binder Jetting BJ process is one of the most versatile additive manufacturing technologies in use. In this process a binder is locally jetted into a powder bed for the consolidation of a 3D structure, layer by layer. Basically, all materials which can be provided as a flowable powder and, thus, spreadable to a thin layer, can be processed. Metals, ceramics and polymers are processable, but also materials from nature, such as sand, wood sawdust and insect frass. Moreover, the BJ technology is adapted to large building volumes of some cubic meters easily. Besides these striking advantages, the manufacture of ceramic parts by BJ is still challenging, as the packing density of the powder bed is generally too low and the particle size of a flowable powder too large for a successful densification of printed parts in a subsequent sintering step to an advanced ceramic product. After an introduction of binder jetting in general and highlighting some examples, strategies for obtaining dense ceramic parts by BJ will be introduced.
Regarding feedstocks for the additive manufacturing (AM) of ceramics, two features are most critical in classical powder based AM processes: a high particle packing density (typically >50% TD) must be achieved with very fine particles (typically submicron) in order to ensure sufficient sintering activity. Three innovative approaches will be introduced to overcome this problem:
1. Layer wise slurry deposition: The use of water based ceramic slurries as feedstock for the additive manufacture of ceramics has many advantages which are not fully exploit yet. In the layerwise slurry deposition (LSD) process a slurry with no or low organic content is repetitively spread as thin layers on each other by means of a doctor blade. During the deposition, the ceramic particles settle on the previously deposited and dried material to form thin layers with a high packing density (55-60%). The LSD therefore shares aspects both of tape casting and slip casting. The LSD differentiates from the classical powder-based AM layer deposition, which typically achieves with a flowable coarse grained powder a low packing density (35-50%) only, consequently hindering the ability of sintering ceramic parts to full density. The LSD is coupled with the principles of selective laser sintering (SLS) or binder jetting, to generate novel processes which take advantage of the possibility of achieving a highly dense powder-bed.
2. Laser induced slip casting: Contrary to the LSD process, which requires drying of each individual layer, the direct interaction of ceramic slurries with intense laser radiation, for the laser induced slip casting (LIS), is a promising approach for the additive manufacture of voluminous parts.
3. Gas flow assisted powder deposition: By the application of a vacuum pump a gas flow is realized throughout the powder bed. This gas flow stabilizes the powder bed and results into an enhanced flowability and packing density of the powder during layer deposition.
The presentation will provide a detailed discussion of potentialities and issues connected to the mentioned technologies and will describe the most recent developments in their application to technical ceramics.
Gas turbine components, made of nickel-based alloys, undergo material damage due to high temperatures and mechanical stresses. These components need periodic replacement to avoid efficiency loss and failure. Repair of these parts is more cost-effective than replacement. State-of-the-art repair technologies, including different additive manufacturing (AM) and brazing processes, are considered for efficient restoration. Materials properties mismatches and/or internal defects in repaired parts may expedite crack initiation and propagation, reducing fatigue life. To understand the crack growth behavior in joining zones and predict the remaining life of repaired components, fatigue crack growth (FCG) tests were conducted on specimens of nickel-based alloys joined via brazing, pre-sintered preforms and AM. The FCG experimental technique was successfully adapted for joined specimens and results indicate that the investigated braze material provides a lower resistance to crack growth. In AM-sandwich specimens, the crack growth rates are significantly reduced at the interface of AM and cast material.
Unlike conventional alloys, which typically consist of one main element, high-entropy alloys (HEAs) contain five or more principal elements, which broaden chemical complexity and with it a realm of synergistic mechanisms. The AlMo0.5NbTa0.5TiZr HEA initiated a subclass of Al-containing refractory (r)HEAs that has recently drawn attention [2]. The alloy has a superalloy-resembling B2/bcc nanostructure, which inspired its name refractory high entropy superalloy (RSA). With high-temperature (HT) compressive strengths beyond conventional Ni-based superalloys, this nanostructure could be used for improved HT structural applications. However, in the application-relevant HT regime the Al-Zr-rich B2 phase decomposes to form a hexagonal Al-Zr-based intermetallic (Al4-xZr5; x: 0..1) [3,4]. This work explores the fascinating yet fatal micromechanisms associated to this phase transformation, in the context of creep, annealing and oxidation experiments performed between 800 and 1200 °C.
The material was produced by arc-melting and heat treatment in argon, which lead to grain boundaries decorated with up to 7%. Interrupted constant-load creep tests were performed under vacuum (at 10-4 Pa), at 900–1100 °C with external tensile stresses of 30–120 MPa. Oxidation experiments were separately conducted for 24 hours at 800 and 1000 °C in both dry (21% O2 + 79% N2) and humid (8% O2 + 74% N2 + 18% H2O) air. After the experiments, the samples were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy to reveal degradation mechanisms. Crystallographic texture, orientation relationships and stabilization of an oxygen-containing iso structure (Al4-xZr5(Ox-y); y: 0..x) of the Al-Zr-rich intermetallic are found and discussed.
This contribution presents the results of an experimental study on the LCF behavior of an austenitic 316L stainless steel produced by laser powder bed fusion featuring a low defect population, which allows for an improved understanding of the role of other typical aspects of a PBF‑LB microstructure. The LCF tests were performed between room temperature and 600 °C. A hot‑rolled 316L variant was tested as a reference. The mechanical response is characterized by strain-life curves, a Coffin‑Manson‑Basquin fitting, and cyclic deformation curves. The damage and deformation mechanisms are studied with X-ray computed tomography, optical and electron microscopy. The PBF‑LB/M/316L exhibits lower fatigue lives at lower strain amplitudes. The crack propagation is mainly transgranular. The solidification cellular structure seems to be the most relevant underlying microstructural feature determining the cyclic deformation behavior.
Several studies have been shown that the electron beam can be used to create nanomaterials from microparticle targets in situ in a transmission electron microscope (TEM). Here, we show how this method has to be modified in order to synthesize plasmonic gold nanoparticles (NPs) on insulating silicon oxide substrate by employing a scanning electron microscope with a comparatively low acceleration voltage of 30 kV. The synthesized NPs exhibit a random distribution around the initial microparticle target: Their average size reduces from 150 nm to 3 nm with growing distance to the initial Au microparticle target. Similarly, their average distance increases. The synthesized NP assemblies therefore show distinctly different plasmonic behaviour with growing distance to the target, which allows to study consequences of random hybridization of surface plasmon in disordered system, such as Anderson localization. To reveal the surface plasmons and their localization behaviour we apply electron energy loss spectroscopy in the TEM.
Im Rahmen des 2. BAM-Akademie Info-Tages "Nano or not Nano" wurde die OECD TG 124 "Volume Specific Surface Area of Manufactured Nanomaterials" vorgestellt.
Der Vortrag beschreibt die Bestimmung der spezifischen Oberfläche von dispersen und/oder porösen Pulvern mittels Gasadsorption nach dem BET-Verfahren.
Es wird auf die Anwendbarkeit der Methode eingegangen und es werden praktische Hinweise zur Probenvorbereitung und Messung von Nanomaterialien gegeben.
Following the new paradigm of materials development, design, and optimization, digitalization is the main goal in materials sciences and engineering (MSE) which imposes a huge challenge. In this respect, the quality assurance of processes and output data as well as the interoperability between applications following FAIR principles are to be ensured. For storage, processing, and querying of data in contextualized form, Semantic Web technologies (SWT) are used since they allow for machine-actionable and human-readable knowledge representations needed for data management, retrieval, and (re)use.
The project ‘platform MaterialDigital’ (PMD, https://materialdigital.de) aims to bring together and support interested parties from both industrial and academic sectors in a sustainable manner in solving digitalization tasks and implementing digital solutions. Therefore, the establishment of a virtual material data space and the systematization of the handling of hierarchical, process-dependent material data are focused. Core points to be dealt with are the development of agreements on data structures and interfaces implemented in distinct software tools and to offer users specific support in their projects. Furthermore, the platform contributes to a standardized description of data processing methods in materials research. In this respect, selected MSE methods are semantically represented which are supposed to serve as best practice examples with respect to knowledge representation and the creation of knowledge graphs used for material data.
Accordingly, this presentation shows the efforts taken within the PMD project towards the digitalization in MSE such as the development of the mid-level PMD core ontology (PMDco, https://github.com/materialdigital/core-ontology). Furthermore, selected results of a PMD partner project use case addressing data and knowledge management from synthesis, production, and characterization of materials are shown.
Im Rahmen des 2. BAM-Akademie Info-Tages "Nano or not Nano" wurde die OECD TG 124 "Volume Specific Surface Area of Manufactured Nanomaterials" vorgestellt. Der Vortrag beschreibt detailliert das Messverfahren der He-Gaspyknometrie zur Bestimmung der Skelettdichte von Pulvern und geht auf Anwendbarkeit, Besonderheiten bei Nanopulvern und wichtige Einstellparameter für die Messung ein.
Einführungsvortrag im Rahmen der Veranstaltung der BAM-Akademie zur Anwendung der OECD TG 124 "Volume Specific Surface Area of Manufactured Nanomaterials" zu Herausforderungen bei der Granulometrie von Nanopulvern. Es werden die Einflüsse von Partikelform, Breite der Partikelgrößenverteilung und Agglomeration/ Aggregation auf das Messergebnis sowie die Vergleichbarkeit der Ergebnisse verschiedener Messverfahren dargelegt.
Highly unrelaxed structural states of metallic glasses have often advantageous mechanical properties. Since metallic glasses continuously relax with time (age) or inherently are well relaxed after processing, methods to uniformly rejuvenate the material are needed. One approach that has received attention is the so-called cryogenic-cycling method, during which a metallic glass is repeatedly immersed into liquid nitrogen. In some cases, cryogenic cycling is truly efficient in increasing the stored excess enthalpy of metallic glasses, but it does not seem to be universally applicable to all alloys and structural states. The origins for these differences remain unclear due to our limited understanding of the underlying structural evolution. In order to shed more light onto the fundamental structural processes of cryogenic cycling, we pursue in-situ x-ray photon correlation spectroscopy (XPCS) to trace the atomic-scale structural dynamics of a Zr-based metallic glass in two different structural states (ribbon and bulk metallic glass). This method allows calculating the relaxation times as a function of time throughout the thermal cycling. It is found that the investigated glasses exhibit heterogeneous structural dynamics at 300 K, which changes to monotonic aging at 78 K. Cryogenic cycling homogenizes the relaxation time distribution for both structural states. This effect is much more pronounced in the ribbon, which is the only structural state that rejuvenates upon cycling. We furthermore reveal how fast atomic-scale dynamics is correlated with long-time average structural relaxation times irrespective of the state, and that the ribbon exhibits unexpected additional fast atomic-scale relaxation in comparison to the plate material. Overall, a picture emerges that points towards heterogeneities in fictive temperature as a requirement for cryogenic energy storage.
Die Nutzung von Sensortechnologien, insbesondere im Bereich der Gasdetektion mit einem Schwerpunkt auf Wasserstoff, spielt eine entscheidende Rolle in verschiedenen Anwendungsbereichen der Wasserstofftechnologie. Sicherheitsüberwachung, Leckdetektion und Prozesskontrolle gehören zu den prominenten Anwendungsgebieten dieser Sensortechnologien. Ein zentrales Ziel ist die Erkennung von freigesetztem Wasserstoff sowie die genaue Bestimmung des Wasserstoff-Luftverhältnisses mithilfe von Gassensoren. Dies ist von entscheidender Bedeutung, um potenzielle Gefahren frühzeitig zu erkennen und angemessene Maßnahmen zu ergreifen.
Ein weiterer Schwerpunkt dieses Beitrags liegt auf der Analytik und der Verwendung zertifizierter Referenzmaterialien in Verbindung mit Metrologie für die Wasserstoffspeicherung. Dies gewährleistet eine präzise und zuverlässige Charakterisierung von Wasserstoff und unterstützt die Entwicklung sicherer Speichertechnologien. Im Rahmen des Euramet-Vorhabens Metrology for Advanced Hydrogen Storage Solutions (MefHySto) wird eine Kurzvorstellung präsentiert.
Der Vortrag stellt zwei zerstörungsfreie Prüfverfahren zum strukturellen Zustandsüberwachung (Structural Health Monitoring, SHM) für Wasserstofftechnologien vor. Insbesondere die Fehlstellenerkennung mittels geführter Ultraschallwellen spielt eine bedeutende Rolle bei der Lebensdauerüberwachung von Wasserstoffspeichern. Ein weiterer Aspekt ist die Anwendung faseroptischer Sensorik zur Schadensfrüherkennung von Wasserstoffspeichern. Diese zerstörungsfreien Prüfverfahren ermöglichen eine präzise und frühzeitige Identifizierung von Schäden, was die Sicherheit und Effizienz von Wasserstoffspeichersystemen entscheidend verbessert.
Gypsum (CaSO4∙2H2O), bassanite (CaSO4∙0.5H2O), and anhydrite (CaSO4) are essential evaporite minerals for the evolution of hyper-arid surface environments on Earth and Mars (Voigt et al. 2019; Vaniman et al. 2018). The formation mechanism of especially anhydrite has been a matter of scientific debate for more than a century (van’t Hoff et al. 1903). To date, there exists no model that can reliably predict anhydrite formation at earth’s surface conditions. While thermodynamics favor its formation, it is hardly achieved on laboratory time scales at conditions fitting either the Atacama Desert on Earth, or the surface of Mars (Wehmann et al. 2023). In light of most recent developments (e.g. Stawski et al. 2016), that advocate for a complex, non-classical nucleation mechanism for all calcium sulphates, we present an analysis of natural samples from the Atacama Desert to identify key features that promote the nucleation and growth of anhydrite under planetary surface conditions. Our analyses reveal at least three distinct anhydrite facies, with differing mineralogy and micro- to nano-structures. The facies are (1) aeolian deposits with sub-μm grain sizes, (2) (sub-)surface nodules that formed from aeolian deposits and (3) selenites with secondary anhydrite rims. Possible mechanisms of their formation will be discussed.
Several studies have shown that the electron beam (e-beam) can be used to create nanomaterials from microparticles in situ in a TEM. However, attempts to produce gold nanoparticles (NPs) on silicon oxide substrate remained to be accomplished. Here, we show that the production of gold NPs is possible by using the e-beam in a SEM, under a set of parameters. To understand the physical mechanisms leading to the gold NPs, the mechanisms of e-beam induced charging as well as e-beam induced heating of the MPs were discussed. Several hints point to heating as the driving mechanism.
Several studies have shown that the electron beam (e-beam) can be used to create nanomaterials from microparticles in situ in a TEM. However, attempts to produce gold nanoparticles (NPs) on silicon oxide substrate remained to be accomplished. Here, we show that the production of gold NPs is possible by using the e-beam in a SEM, under a set of parameters. The NPs produced present a size gradient along the radial direction. A parameter study shows that the microparticles may: 1) flicker away without producing NPs, 2) fragment to form NPs and/or 3) react with the silicon oxide substrate, depending on the applied current. A hypothesis regarding the driving physical phenomena that lead the microparticles to fragment into NPs is discussed. Fabrication of gold NPs in the SEM provides a more cost-effective option as compared to the established method in the TEM.