5 Werkstofftechnik
Filtern
Dokumenttyp
- Vortrag (420)
- Zeitschriftenartikel (389)
- Posterpräsentation (109)
- Beitrag zu einem Tagungsband (76)
- Forschungsdatensatz (22)
- Buchkapitel (11)
- Dissertation (9)
- Forschungsbericht (7)
- Sonstiges (6)
- Sammelband (Herausgeberschaft für den kompletten Band) (3)
Sprache
- Englisch (889)
- Deutsch (157)
- Mehrsprachig (8)
- Französisch (2)
- Russisch (1)
Schlagworte
- Additive Manufacturing (59)
- Additive manufacturing (57)
- Corrosion (56)
- Microstructure (38)
- Glass (34)
- Creep (32)
- Transmission electron microscopy (30)
- Fatigue (29)
- EBSD (26)
- Ontology (25)
Organisationseinheit der BAM
- 5 Werkstofftechnik (1057) (entfernen)
Paper des Monats
- ja (9)
A constitutive model for the mechanical behaviour of single crystal Ni-base superalloys under high temperature conditions has been developed in the framework of a Cooretec project in cooperation with Siemens AG, MTU Aero Engines AG and University Bayreuth. In addition to the conventional material properties e.g. elastic constants, the model requires the parameters of the initial microstructure as an input. Thus, the γ’-precipitate size and the channel width of the γ-matrix were obtained from SEM micrographs. The model uses the slip system theory and describes the movement, multiplication and annihilation of dislocations in the channels. Furthermore, the cutting of precipitates is another mechanism contributing to the plastic flow. The evolution of the morphology due to rafting and its effects on the deformation have been implemented according to. The kinematic hardening is introduced as a stress tensor to realistically represent the strain hardening of arbitrary oriented single crystals.
The mechanical behaviour of single crystal specimens has been experimentally investigated in tension tests at different strain rates and in creep tests under various loads. The constitutive model has been calibrated based on the experimental data for temperatures of 950°C and 850°C and the [001] and [111] crystallographic orientations.
Finally, a micromechanical model was created to simulate the creep response of additive manufactured polycrystalline structures. An EBSD image is taken to obtain the grain geometry and their respective orientation. The grain boundaries are discretised using cohesive elements, whereas the single crystal model was applied to each grain in the representative volume. The polycrystal model is generated using Dream3D, NetGen and other software previously developed at the BAM.
The methods of computational damage mechanics are well-established for the description of degradation of materials under monotone loading. An extension to structural damage induced by cyclic loading is however significantly limited. This is due to enormous computational costs required to resolve each load cycle by conventional temporal incremental integration schemes while a typical fatigue loading history comprises between thousands and millions of cycles. Despite the permanent increase of computational resources and algorithmic performance, a successful approach is rather based on the development of novel multiscale in time integration schemes.
A Fourier transformation-based temporal integration (FTTI) is represented, which takes advantage of temporal scale separation incorporated into the cycle jump method. The response fields are approximated by a Fourier series whose coefficients undergo the evolution on a long-time scale. This is correlated with the evolution of the history variables, including damage, by means of the adaptive cycle jump method of various orders. The necessary extrapolation rates are obtained from the underlying solution of a short-time scale problem, which results from the oscillatory boundary condition and fulfills the global equilibrium of the Fourier coefficients. In this way, a remarkable speedup is achieved because the number of cycles to be fully integrated dramatically decreases.
The key idea behind the FTTI method is that the global in space equilibrium problem is linear since it is decoupled from the evolution equations. The latter are solved in the quadrature points under response fields prescribed throughout the whole load cycle. Consequently, integration of a single load cycle is much more efficient than the conventional single scale integration where the global equilibrium iteration and the local iteration of the evolution equations are coupled. This results in an additional speedup of the FTTI method.
The performance of the FTTI technique is demonstrated for two different constitutive behaviors: a viscoplastic model with a damage variable governed by the local equivalent viscoplastic strain; a quasi-brittle response where the damage variable is driven by a non-local equivalent strain. The latter is implicitly introduced as proposed by Peerlings. Both, the explicit and implicit extrapolation schemes are validated. The FTTI solutions agree very well with the reference cycle-by -cycle solutions, while significantly reducing the computational costs. The adaptive determination of the jump length can properly recognize the particular responses throughout the fatigue loading history (stationary fatigue, acceleration of fatigue damage when approaching failure) as well as stress redistribution phenomena.
Environmental conditions are known to influence sub-critical crack growth (SCCG) that are released from microscopic flaws at the glass surface, leading to stress corrosion phenomena at the crack tip. The processes at the crack-tip are complex and water has been identified as a key component governing SCCG at low crack velocities (region I). In particular, the influence of humidity accelerating crack propagation is well studied for industrial soda-lime silicate glasses, which are practically free (< 1000 ppm) of dissolved water. To shed light on the corrosion process, the situation at the crack-tip is reversed in the present study as dissolved water in larger fractions is present in the glass and crack propagation is triggered in dry environment. For this purpose, water-bearing silicate glasses of up to 8 wt% total water were synthesized in an internally heated pressure vessel at 0.5 GPa and compared to dry glasses of standard glass manufacturing. SCCG was measured using the double cantilever beam technique and by Vickers indentation. For dry glasses, three trends in the crack growth velocity versus stress intensity curve were found. The slope in region I limited by environmental corrosion increases in the order sodium aluminosilicate < sodium borosilicate ≲ sodium lead silicate. The velocity range of region II reflecting the transition between corrosion affected and inert crack growth (region III), varies within one order of magnitude among the glasses. The KI region of inert crack growth strongly scatters between 0.4 and 0.9 MPam1/2. For hydrous glasses, it is found that those of low Tg are more prone to SCCG. As water strongly decreases Tg, it promotes SCCG. First results indicate that molecular water has a dominating influence on SCCG.
Effective hydrogen storage capacities are prerequisite for an efficient energy provision using fuel cells. Since glass has low intrinsic hydrogen permeability, it is a promising material for hydrogen storage containers as well as hydrogen diffusion barriers. Previous studies on oxidic glasses suggest a correlation between the glass composition and hydrogen permeation that was derived mainly from silica glass. In the present study, we concentrate on the relationship between thermodynamic (i.e., configurational entropy) and topologic (i.e., free volume, network polymerization) parameters. Experimental data were gathered well below the glass transition temperature, excluding significant effects caused by structural relaxation and chemical dissolution of hydrogen. The results of seven analysed glasses on the SiO2-NaAlO2 joint showed that the hydrogen permeability in fully polymerized glasses cannot solely be derived from the total free volume of the glass structure. Hence, evidence is provided that the size distribution of free volume contributes to hydrogen solubility and diffusion. Additionally, the results indicate that the configurational heat capacity ΔCp at Tg affects the hydrogen permeability of the investigated glasses.
Glass-fibre-reinforced plastics (GFRP) are commonly used for the construction of pressure vessels and tanks for example in automotive and aerospace industries. Especially for pressure vessels used for the storage of natural gas or hydrogen with operation pressures up to 700 bar, an early material fatigue detection is of great interest. Measuring the distributed strain profile of GFRP structures helps to understand and detect material fatigue. In this article, we demonstrate the great potential of swept wavelength interferometry (SWI) based distributed strain sensing for the monitoring of pressure vessels made from GFRP. A resin transfer molding (RTM) process was used to manufacture GFRP-tube specimens. Commercial optical fibres with polyimid coating were glued to the surface externally in circumferential and axial direction. A cyclic load of up to 150 bar was applied to the samples using a servo-hydraulic test bench. Comparing the loaded and unloaded test conditions, we determined up to 2 % elongation in circumferential direction. We demonstrate reliable distributed strain measurements with sub-centimetre spatial resolution. By monitoring these high-resolution strain profiles, we were able to detect local material degradation that manifested itself as localized strain changes. Crucially, the material Degradation could be detected already after 75 % of dat the fatigue life before a crack appeared that led to leakage.
The first documentation of fuel biodeterioration dates back to the late 19th century. However, extensive studies concerning the microbial fuel contamination started in 1980’s. Polymeric fuel storage tanks containing diesel and biodiesel provide environmental conditions for microbial growth. Several studies demonstrated that bacteria, which were found in contaminated fuel systems, can use fuels as macronutrient; but such bacteria can also cause microbiologically influenced corrosion and fouling.
The aim of this study is to investigate the initial attachment behavior of bacteria, isolated from a diesel contamination, on neat and photooxidized high-density polyethylene (PE-HD). Two common PE-HD’s, less- and biodiesel-stabilized, were radiated to UV light representing a tank exposed to sunlight. The effect of photooxidiation on PE-HD’s surface were characterized chemically by Fourier-transform infrared spectroscopy (FTIR). The attached bacteria Pseudomonas aeruginosa and Bacillus subtilis on the polymer surface were evaluated by fluorescence microscopy and colony-forming unit tests (CFU).
PE-HD as a polymeric fuel storage tank material: Photooxidation, fuel sorption and long-term storage
(2018)
High-density polyethylene (PE-HD) is a commodity thermoplastic polymer which is typically used for packing of dangerous goods. Its good resistance against photooxidation, fuels, chemicals and other environmental factors in addition to low production costs makes PE-HD attractive for fuel storage applications. Typical engine fuels stored in polymer tanks are petrol, diesel and biodiesel that receives increasing attention as proper alternative to fossil fuels. One of the major problems with biodiesel is its susceptibility to oxidize due to its chemical composition of unsaturated fatty acids which also can cause polymer degradation.
The aim of this study is to investigate the influence of different environmental factors, UV radiation and commonly stored fuels, on the mechanical, physical and chemical properties of two types of PE-HD polymers (stabilized and non-stabilized). The influence on the mechanical properties was tested by Charpy and tensile tests, chemical and physical properties were evaluated by Fourier-transform infrared spectroscopy (FTIR) and by dynamical mechanical analysis (DMA) tests. Samples were characterized after varying exposure time of UV radiation and after fully and partially immersion in biodiesel. In addition, similar experiments were conducted using diesel for comparison.
We invented the first non-metallic, self-adhesive and dry biosignalling electrode. The PEDOT polymer electrode changes its aggregate state and conductivity by a light curing procedure. The electrode can be applied as a gel underneath hair without shaving. With the aid of blue light, the electrode can be hardened within a few seconds at the desired location on the scalp. The cured polymer electrode is highly conductive and can be applied on a very small location. Unlike other EEG electrodes, our electrode does not lose conductivity upon drying. Furthermore, our electrode strongly bonds to Skin and does not require any additional adhesive. Short circuits due to an outflow of gel are prevented with this technique. Therefore, the PEDOT polymer electrode is extremely well suited for applications that, up to now, have been challenging, such as non-invasive EEG recordings from awake and freely moving animals, EEG recordings from preterm babies in the neonatal intensive care unit or long-term recordings in the case of sleep monitoring or epilepsy diagnostics. We addressed two technical questions in this work. First, is the EEG recorded with polymer electrodes comparable to a standard EEG? Second, is it possible to record full-band EEGs with our electrodes?
Additive Manufacturing (AM) through the Selective Laser Melting (SLM) route offers ample scope for producing geometrically complex parts compared to the conventional subtractive manufacturing strategies. Nevertheless, the residual stresses which develop during the fabrication can limit application of the SLM components by reducing the load bearing capacity and by inducing unwanted distortion, depending on the boundary conditions specified during manufacturing. The present study aims at characterizing the residual stress states in the SLM parts using different diffraction methods. The material used is the nickel based superalloy Inconel 718. Microstructure as well as the surface and bulk residual stresses were characterized. For the residual stress analysis, X-ray, synchrotron and neutron diffraction methods were used. The measurements were performed at BAM, at the EDDI beamline of -BESSY II synchrotronand the E3 line -BER II neutron reactor- of the Helmholtz-Zentrum für Materialien und Energie (HZB) Berlin. The results reveal significant differences in the residual stress states for the different characterization techniques employed, which indicates the dependence of the residual state on the penetration depth in the sample. For the surface residual stresses, longitudinal and transverse stress components from X-ray and synchrotron agree well and the obtained values were around the yield strength of the material. Furthermore, synchrotron mapping disclosed gradients along the width and length of the sample for the longitudinal and transverse stress components. On the other hand, lower residual stresses were found in the bulk of the material measured using neutron diffraction. The longitudinal component was tensile and decreased towards the boundary of the sample. In contrast, the normal component was nearly constant and compressive in nature. The transversal component was almost negligible. The results indicate that a stress re-distribution takes place during the deposition of the consecutive layers. Further investigations are planned to study the phenomenon in detail.
The creep behavior of single-crystals of the nickel-base superalloy CMSX-4 was investigated at 1288°C, which is the temperature of the hot isostatic pressing (HIP) treatment applied to this superalloy in the industry. It was found that at this super-solvus temperature, where no Gamma’-strengthening occurs, the superalloy is very soft and rapidly deforms under stresses between 4 and 16 MPa. The creep resistance was found to be very anisotropic, e.g. the creep rate of [001] crystals was about 11 times higher than that of a [111] crystal. The specimens of different orientations also showed a very different necking behavior. The reduction of the cross-section area psi of [001] crystals reached nearly 100%, while for a [111] crystal psi=62%. The EBSD analysis of deformed specimens showed that despite such a large local strain the [001] crystals didn’t not recrystallize, while a less deformed [111] crystal totally recrystallized within the necking zone. From the shape of deformed specimens and TEM investigations it was concluded that the main strain contribution resulted from <011> {111} octahedral slip.
Efficient energy provision using fuel cells requires effective hydrogen storage capacities. Glass is a material of low intrinsic hydrogen permeability and is therefore a promising material for hydrogen storage containers or diffusion barriers. Pioneer work on oxidic glasses seems to indicate a correlation between glass composition and hydrogen permeation, which was mainly derived from the behavior of silica glass. In this study, we focus on the relationship between topologic (free volume; network polymerization) and thermodynamic (configurational entropy) glass parameters. Experiments were performed well below the glass transition temperature, which excludes significant structural relaxation and chemical dissolution of hydrogen. The compositional dependence of seven glasses on the SiO2-NaAlO2 join pointed out that in fully polymerized glasses the H2 permeability cannot be solely derived from the total free volume of the glass structure. Hence, evidence is provided that the size distribution of free volume contributes to hydrogen diffusion and solubility. Additionally, results indicate that hydrogen permeability of the glasses is affected by the configurational heat capacity ΔCp at Tg.
Glass-ceramics are noted for their unusual combination of properties and manifold commercialized products for consumer and specialized markets. Evolution of novel glass and ceramic processing routes, a plethora of new compositions, and unique exotic nano- and microstructures over the past 60 years led us to review the Definition of glass-ceramics. Well-established and emerging processing methods, such as co-firing, additive manufacturing, and laser patterning are analyzed concerning the core requirements of processing glass-ceramics and the Performance of the final products. In this communication, we propose a revised, updated definition of glass-ceramics, which reads “Glass-ceramics are inorganic, non-metallic materials prepared by controlled crystallization of glasses via different processing methods. They contain at least one type of functional crystalline phase and a residual glass. The volume fraction crystallized may vary from ppm to almost 100%”.
Glasses with compositions of 21Gd2O3-63MoO3-(16-x)B2O3-xTeO2 (mol%) (x= 0, 2, 4, 8) were prepared using a conventional melt quenching technique, and the crystallization behavior of ferroelastic β′-Gd2 MoO4)3 Crystals was examined to clarify the mechanism of self-powdering phenomenon and to design bulk crystallized glasses. It was found that the self-powdering phenomenon appeared significantly during the crystallization at temperatures near the crystallization peak temperature, but the phenomenon is suppressed in the crystallization at temperatures much higher than the glass transition temperature. It was also found that the substitution of TeO2 for B2O3 in the base glasses suppresses the self-powdering phenomenon and consequently bulk crystallized glasses were obtained in the glass with x=8 mol%. The densities at room temperature of the base glasses are d =4.755–4.906 g/cm3, being much higher than the value of d=4.555 g/cm3 for β′-Gd2(MoO4)3 crystal. It is proposed that the stresses in the inside of crystals induced by large density differences (i.e., large molar volume differences) between the glassy phase and crystals might be relaxed effectively in the glasses containing TeO2 with weak TeeO bonds and fragile character.
Glass powders are promising candidates for manufacturing a broad diversity of sintered materials like sintered glass-ceramics, glass matrix composites or glass bonded ceramics with properties and complex shape. Powder processing, however, can substantially affect sinterability, e.g. by promoting surface crystallization. On the other hand, densification can be hindered by gas bubble formation for slow crystallizing glass powders. Against this background, we studied sintering and foaming of silicate glass powders with different crystallization tendency for wet milling and dry milling in air, Ar, N2, and CO2 by means of heating microscopy, DTA, Vacuum Hot Extraction (VHE), SEM, IR spectroscopy, XPS, and ToF-SIMS. In any case, foaming activity increased significantly with progressive milling. For moderately milled glass powders, subsequent storage in air could also promote foaming. Contrarily, foaming could be substantially reduced by milling in water and 10 wt% HCl. Although all powder compacts were uniaxially pressed and sintered in air, foaming was significantly affected by different milling atmosphere and was found most pronounced for milling in CO2 atmosphere. Conformingly, VHE studies revealed that foaming is mainly driven by carbonaceous species, even for powders milled in other gases. Current results of this study thus indicate that foaming is caused by carbonaceous species trapped on the glass powder surface.
The sound numerical prediction of welding-induced thermal stresses, residual stresses, and distortions strongly depends on the accurate description of a welded material’s thermomechanical deformation behaviour. In this work, we provide experimental data on the viscoplastic deformation behaviour of a grade-s960ql steel up to a temperature of 1000 ◦C. In addition, a multi-phase viscoplastic material model is proposed, which accounts for the experimentally observed isothermal deformation behaviour of grade-s960ql steel base and austenitised material, as well as for athermal contributions that originate from solid-state phase transformations. The multi-phase viscoplastic and a classic rateindependent isotropic hardening material model were applied in the numerical simulations of both-ends-fixed bar Satoh tests and a single-pass gas metal arc weld. The influence of material modelling choices on the agreement between numerical simulation and experimental results is discussed, and recommendations for further work are given.
In Germany spent nuclear fuel (SNF) and high level radioactive waste (HLW) are stored in interim storage containers with double lid systems. Those lids are equipped with metal seals (e.g. Helicoflex®) that ensure the safe enclosure of the inventory. Being licensed for up to 40 years of interim storage the evaluation of the long-term behavior of the seals is necessary, taking into account storage conditions, decay heat and possible mechanical loads.
Der Vortrag zeigt zwei Möglichkeiten zur Verbesserung der VSSA-Screening-Methode zur Identifizierung von Nanopulvern auf. Bisher ist das Verfahren nur für monodisperse Partikel mit idealer Kugelform valide. Die Verteilungsbreite der Partikelgröße soll durch die Nutzung des Modells einer logarithmischen Normalverteilung implementiert werden. Die Abweichung der gemessenen Partikel von einer idealen Kugel in Sphärizität, Rundheit und Rauigkeit sind über einen Morphologiefaktor MF zu berücksichtigen. An einem konkreten Beispiel werden Auswirkungen der Implementierungen rechnerisch dargestellt und mit dem bisherigen Verfahren verglichen.
Effects of various geometrical and physical factors, as well as the method of data reduction (analysis of
experimental forceedisplacement curves) on the values of local interfacial strength parameters (local IFSS, td, and critical energy release rate, Gic) determined by means of a single fiber pull-out test are discussed. Experimental results of our pull-out tests on several fiberepolymer matrix systems showed that td and Gic weakly depended on geometrical factors. However, the pull-out test appeared to be sensitive to the conditions of specimen formation and testing, such as changing the nature of the contacting surfaces (fiber sizing) and the fiber pull-out rate. Of several methods of td and Gic Determination from a forceedisplacement curve, the most reliable and reproducible one is the approach based on the values of the maximum force recorded in a pull-out test and the interfacial frictional force immediately after fiber debonding.
Hochleistungsverbundwerkstoffe, bzw. Glasfaser-Kunststoff-Verbunde (GFK), haben sich als Leichtbauwerkstoffe für Leichtflugzeuge und Rotorblätter von Windkraftanlagen etabliert. Die hohe spezifische Festigkeit und Steifigkeit qualifizieren sie besonders für diese Anwendung. Während der Fertigung werden Imperfektionen häufig in die Blattschalen eingebracht. Durch Witterungseinflüsse kommt es zum Schadensfortschritt. Infolgedessen treten Schäden in der Blattschale, die den sicheren Betrieb gefährden können, weit vor der projektierten Lebensdauer von 20 Jahren auf. Da der Austausch von ganzen Blättern sehr kostintensiv ist, ist eine lokale Reparatur des geschädigten Bereichs zur Wiederherstellung der strukturellen Integrität, viel preisgünstiger. Die Reparatur von Rotorblättern ist in den letzten Jahren zu einem wichtigen Thema geworden. Derzeit werden verschiedenste Reparaturkonzepte angewendet. Eine einheitliche Reparaturvorgabe gibt es bisher nicht. Die Auswirkungen der angewendeten Reparaturkonzepte auf die Betriebsfestigkeit der Reparaturstelle sind weitestgehend unbekannt und sollen deshalb in diesem Projekt untersucht werden. Gekrümmte Voll-Laminat sowie Sandwich Prüfkörper werden mit dem Vacuum-Assisted-Resin-Infusion-Prozess (VARI) produziert. Um einen Teil einer Rotorblattschale darzustellen, sind sie als GFK aufgebaut, beziehungsweise die Sandwich Strukturen mit einem Polyvinylchlorid-Schaumkern (PVC) Kern, wie im Original. Schalenreparaturen in verschiedenen Layup-Techniken und Geometrie werden eingebracht und die Materialeigenschaften mit zyklischen Ermüdungstests untersucht. Im Projekt werden ideal im Labor erzeugte Reparaturstellen mit in der Praxis angewendeten Ausführungstechniken eines Industriepartners experimentell verglichen. Für die in-situ Detektion der Schadensentwicklung während des Ermüdungsversuches kommt ein kombiniertes Felddehnungs- und Thermografie-Kamerasystem zum Einsatz. Das mechanische Verhalten und die Schadensentwicklung in den verschiedenen reparierten Prüfkörper wird miteinander sowie mit den Referenzproben ohne Reparaturstellen verglichen. Zudem wird in numerischen Modellen für die verschiedenen Reparaturtechniken eine Spannungsanalyse durchgeführt um hinsichtlich der Betriebsbeanspruchung eine Bewertung angeben zu können.
Werkstoffe im Hochtemperatureinsatz verändern mit der Zeit ihre Mikrostruktur. Mit diesem Alterungsprozess einher geht eine Veränderung der mechanischen Eigenschaften ebenso wie eine Veränderung des Schädigungsverhaltens. Im Rahmen des FVV Vorhabens „Alterung und Lebensdauer“ haben das Fraunhofer IWM in Freiburg und die BAM in Berlin die weit verbreitete warmfeste Aluminiumlegierung EN AW-2618A in verschiedenen Alterungszuständen experimentell charakterisiert und darauf aufbauend Modelle für die Lebensdauerbewertung mit der Finite-Elemente- Methode implementiert.
Materials subjected to high-temperature service conditions will change their microstructure with time. Associated with this aging process is a change of mechanical properties as well as a change of damage mechanisms. Within the scope of the FVV project Aging and Lifetime, Fraunhofer IWM in Freiburg and BAM in Berlin (both Germany) experimentally characterized the widespread high-temperature aluminum alloy EN AW-2618A in different overaging states. Based on the experimental findings, models for numerical lifetime assessment with the finite-element method were implemented.
High-performance composites, including glass-fiber reinforced plastic (GFRP) materials, are favored as a construction material for wind turbine rotor blades due to their high specific strength and stiffness properties. During the manufacturing process, however, imperfections are often introduced, then further propagated due to harsh environmental conditions and a variety of loads. This leads to failure significantly before their projected 20-year lifespan. As replacement of entire blades can be a costly potential outcome, localized repair of the damaged region to restore structural integrity and thus lengthen its lifespan has become an important issue in recent years. Rotor blades are often repaired using a common technique for composite laminates: adhesively bonded structural repair patches. These methods involve replacing the lost load path with a new material that is joined to the parent structure, and include scarf or plug repairs. However, there currently do not exist any standardized repair procedures for wind turbine rotor blades, as comparisons of blade properties repaired with the existing methods have not been studied in depth. Namely, there is a lack of understanding about the effects of various repair methods on the fatigue life of the shells of rotor blades. This study therefore aims to begin to fill this knowledge gap by testing the influence of different repair patches on the blades’ mechanical properties. Manufactured with the vacuum-assisted resin infusion process, the test specimens are produced as a curved structure with GFRP sandwiching a polyvinyl chloride foam core to best represent a portion of a rotor blade shell. Scarf repairs are then introduced with varying layup techniques, and material properties are examined with cyclical fatigue tests. Crack growth and development is monitored during fatigue testing by various non-destructive testing methods, including passive thermography with an infrared camera system, and a 3D deformation analysis system with ARAMIS. Large deformation fields and detection of in- and out-of-plane deformations is thus possible in-situ. The mechanical behavior and development of defects in the various repaired specimens is compared to each other as well as to reference test specimens with no repair patches. In-situ test data is combined with further non-destructive testing methods, including laminography, and active thermography, to develop a robust understanding of the effects of repair concepts.
Biomaterials for bone replacement and grafting should possess sufficient strength, be bioresorbable and demonstrate osteoconductivity/osteoinductivity. Nowadays, hydroxyapatite (HA) and tricalcium phosphate (TCP) are the most widespread ceramics for bone grafting at the market, however, their resorption is reported, in some cases, to be not enough. This is why the search for more soluble ceramics compared to HA and TCP looks rather viable.
A possible way to increase ceramics solubility leads to partial substitution of Ca2+-ions in Ca3(PO4)2 by alkali castions, like Na+ or/and K+. Improvement of solubility stems from decreasing lattice energy of a substituted phase, as well as increase in hydration energy of the ions releasing from the phase to ambient solution. From this viewpoint, bioceramics based on compositions from Ca3(PO4)2 - CaKPO4 - CaNaPO4 ternary system seems to be prospective for bone replacement and grafting in sense of resorption properties. At the same time, one should bear in mind that solubility level (resorbability) is governed not only by reduction of lattice energy, but also by microstructure features. Grain sizes and porosity contribute much to dissolution rate making study of sintering of aforementioned ceramics highly important.
With the introduction of a mass transport mechanism the entire problem is subjected to a time frame that dictates the time-dependent action of soluted species on mechanical properties. A numerical framework within the phase-field approach is presented with an embrittlement-based coupling mechanism. The underlying functionals are expressed in terms of the displacement, mass concentration and crack phase-field. Within the phase-field approach the modelling of sharp crack discontinuities is replaced by a diffusive crack model facilitating crack initiation and complex crack topologies without the requirement of a predefined crack path. The isotropic hardening of the elasto-plastic deformation model and the local fracture criterion are affected by the species concentration. This allows for embrittlement and leads to an accelerated crack propagation. An extended mass transport equation for hydrogen embrittlement, accounting for mechanical stresses and deformations, is implemented. For stabilisation purposes a staggered scheme is applied to solve the system of partial differential equations by a multi-field finite-element method. A thermodynamically consistent coupling relation that accommodates the required mechanisms is presented.
Powder bed -based technologies are amongst the most successful Additive Manufacturing (AM) techniques. "Selective laser sintering/melting" (SLS/SLM) and "binder jetting 3D printing" (3DP) especially are leading AM technologies for metals and polymers, thanks to their high productivity and scalability. In this context, the "layerwise slurry deposition" (LSD) has been developed as a layer deposition method which enables the use of SLS/SLM and 3DP technologies for advanced ceramic materials. LSD consists in the layer-by-layer deposition of a ceramic slurry by means of a doctor blade. Each layer is deposited and dried to achieve a highly packed powder layer, which can be used for SLM or for 3DP. This technique offers high flexibility in the ceramic feedstock used, especially concerning material and particle size, and is capable of producing parts with physical and mechanical properties comparable to traditionally shaped parts. In this presentation, the LSD technique will be introduced and several examples of application to porcelain, SiC and alumina products will be reported.
In powder-based Additive Manufacturing (AM) processes, an object is produced by successively depositing thin layers of a powder material and by inscribing the cross section of the object in each layer. The main methods to inscribe a layer are by binder jetting (also known as powder 3D printing) or by selective laser sintering/melting (SLS/SLM).
Powder-based AM processes have found wide application for several metallic, polymeric and also ceramic materials, due to their advantages in combining flexibility, easy upscaling and (often) good material properties of their products.
The deposition of homogeneous layers is key to the reproducibility of these processes and has a direct influence on the quality of the final parts. Accordingly, powder properties such as particle size distribution, shape, roughness and process related properties such as powder flowability and packing density need to be carefully evaluated.
Due to these requirements, these processes have been so far precluded to find commercial use for certain applications. In the following, two outstanding cases will be presented.
A first example is that powder-based AM processes are widely used for many metallic and polymeric materials, but they find no commercial application for most technical ceramics.
This seemingly contradicting observation is explained by the fact that in powder based AM, a dry flowable powder needs to be used. The processing of technical ceramics in fact typically requires very fine and poorly flowable powder, which makes them not suitable for the standard processes. There have been several approaches to adapt the raw materials to the process (e.g. by granulation), but in order to maintain the superior properties of technical ceramics it seems necessary to follow the opposite approach and adapt the process to the raw materials instead.
This was the motivation for developing the Layerwise Slurry Deposition (LSD), an innovative process for the deposition of powder layers with a high packing density. In the LSD process, a ceramic slurry is deposited to form thin powder layers, rather than using a dry powder. This allows achieving high packing density (55-60%) in the layers after drying. It is also important, that standard ceramic raw materials can be used. When coupled with a printing head or with a laser source, the LSD enables novel AM technologies which are similar to 3D printing or selective laser sintering, but taking advantage of having a highly dense powder bed.
The LSD -3D printing, in particular, offers the potential of producing large (> 100 mm) and high quality ceramic parts, with microstructure and properties similar to traditional processing. Moreover, due to the compact powder bed, no support structures are required for fixation of the part in the printing process.
Figure 1 shows the schematics of the working principle of the LSD-3D print and illustrates some examples of the resolution and features achievable.
The second outstanding case here described is the application of powder-based AM in environments with reduced or zero gravity. The vision is to be able to produce repair parts, tools and other objects during a space mission, such as on the International Space Station (ISS), without the need of delivering such parts from Earth or carrying them during the mission. AM technologies are also envisioned to play an important role even for future missions to bring mankind to colonize other planets, be it on Mars or on the Moon. In this situation, reduced gravity is also experienced (the gravitational acceleration is 0.16 g on the Moon and 0.38 g on Mars).
These environments cause the use of AM powder technologies to be very problematic: the powder layers need to be stabilized in order to avoid dispersion of the particles in the chamber. This is impossible for standard AM powder deposition systems, which rely on gravitation to spread the powder.
Also in this case, an innovative approach has been implemented to face this technological challenge. The application of a gas flow through a powder has a very strong effect on its flowability, by generating a force on each particle, which is following the gas flow field. This principle can be applied in a simple setup such as the one shown in Figure 2.
In this setup, the gas flow causes an average pressure on the powder bed in direction of the arrows, generating a stabilizing effect which acts in the same direction of the gravitational force. This effect can be used in addition to normal gravity on Earth to achieve a better stabilization of 3D printed parts in the powder bed. In this case, even a significant increase of packing density of the powder was measured, compared to the same experimental setup without gas flow. This is due to the fact that the force on each single particle follows the gas flow field, which is guiding the particles to settle between the pores of the powder bed, thus achieving an efficient packing.
The same principle can be applied in absence of gravitation, where the gas flow acts to stabilize the powder layers. It has been shown that ceramic powder could be deposited in layers and laser sintered in µ-gravity conditions during a DLR (Deutsches Zentrum für Luft- und Raumfahrt) campaign of parabolic flights, as shown in Figure 2. A follow-up campaign is dedicated to the deposition of metallic (stainless steel) powder in inert atmosphere and to study the effects of laser melting in µ-gravity.
In conclusion, the description of these two example cases shows how the development of novel technological processes can address some of the limitations of standard powder-based AM, in order to enable the use of new materials, such as technical ceramics, or to tackle the challenges of AM in space.
Additive Manufacturing (AM) through the Selective Laser Melting (SLM) route offers ample scope for producing geometrically complex parts compared to the conventional subtractive manufacturing strategies. Nevertheless, the residual stresses which develop during the fabrication can limit application of the SLM components by reducing the load bearing capacity and by inducing unwanted distortion, depending on the boundary conditions specified during manufacturing.
The present study aims at characterizing the residual stress states in the SLM parts using different diffraction methods. The material used is the nickel based superalloy Inconel 718. Microstructure as well as the surface and bulk residual stresses were characterized. For the residual stress analysis, X-ray, synchrotron and neutron diffraction methods were used. The measurements were performed at BAM, at the EDDI beamline of -BESSY II synchrotron- and the E3 line -BER II neutron reactor- of the Helmholtz-Zentrum für Materialien und Energie (HZB) Berlin.
The results reveal significant differences in the residual stress states for the different characterization techniques employed, which indicates a dependence of the residual state on the penetration depth in the sample. For the surface residual stresses, longitudinal and transverse stress components from both X-ray and synchrotron agree well and the obtained values were around the yield strength of the material. Furthermore, synchrotron mapping disclosed gradients along the width and length of the sample for the longitudinal and transverse stress components. On the other hand, lower residual stresses were found in the bulk of the material measured using neutron diffraction. The longitudinal component was tensile and decreased towards the boundary of the sample. In contrast, the normal component was nearly constant and compressive in nature. The transversal component was almost negligible. The results indicate that a stress re-distribution takes place during the deposition of the consecutive layers. Further investigations are planned to study the phenomenon in detail.
Virtual-lab-based determination of a macroscopic yield function for additively manufactured parts
(2018)
This work presents a method for the yield function determination of additively manufactured parts of S316L steel. A crystal plasticity model is calibrated with test results and used afterwards to perform so-called virtual experiments, that account for the specific process-related microstructure including crystallographic and morphological textures. These simulations are undertaken on a representative volume element (RVE), that is generated from EBSD/CT-Scans on in-house additively manufactured specimen, considering grain structure and crystal orientations. The results of the virtual experiments are used to determine an anisotropic Barlat yield function, that can be used in a macroscopical continuum-sense afterwards. This scale-bridging approach enables the calculation of large-scale parts, that would be numerically too expensive to be simulated by a crystal plasticity model.
Sandwich-Schalenstrukturen in situ charakterisiert mit Thermographie und Felddehnungsmessungen
(2018)
An der BAM wurde ein Schalenprüfstand entwickelt, mit dem typische Sandwichschalenstrukturen unter simulierter Betriebsbeanspruchung belastet werden können. Im mechanischen Ermüdungsversuch wurden in situ die Entstehung von Schäden in Schalenprüfkörpern mit Test-Imperfektionen mittels der passiven Thermographie und Felddehnungsmessungen verfolgt. Damit konnten der Zeitpunkt, der Schadensursprung und der Schadensfortschritt zerstörungsfrei bestimmt werden. Zudem wurden vergleichend Schalenprüfkörper mit Luftultraschall und der Röntgen-Laminographie untersucht. Im Rahmen eines BMWi-Forschungsvorhabens wurden die Schädigungsmechanismen evaluiert und Empfehlungen für die Praxis der Fertigung von Rotorblättern abgeleitet. In diesem Beitrag wird sich auf die Darstellung der ZfP-Verfahren und der ZfP-Ergebnisse konzentriert.
Tunable microwave devices will play an important role in future wireless systems, in which high-frequency bands, e.g. millimeter waves, will become promising, due to its huge spectrum availability. At such frequency bands, liquid crystals (LCs) exhibit low microwave loss, which is excellent compared with the other tuning elements. In this paper, LC-based microwave components are fabricated by using low temperature co-fired ceramic technology, allowing the integration of the LC into microwave structures. The first component, the Amplitude tuner, controls the signal’s amplitude by using the interference concept, which exhibits a tunable attenuation range from 11 dB to 30 dB at 30 GHz. The second component is a 3-pole tunable bandpass filter, which is realized by using a substrate integrated waveguide topology, enabling a device with comparatively high-quality factors (Q-factors). The measurement results show Q-factors in the range of 68 to 100 for a frequency tuning of 29.4–30.1 GHz, i.e. a tuning range of 700 MHz, accompanied by an insertion loss 2 dB to 4 dB.
Most additive manufacturing processes which produce dense ceramics are nowadays limited in size because of inevitable post-processing steps like for example binder removal in stereolithography. The additive manufacturing of voluminous ceramic parts is realized by powder bed based processes which, however, generate parts with residual porosity. Via infiltration these parts can be processed to dense parts like for example SiC but this is not possible for all ceramics like for example Si3N4. There is a lack of methods for the additive manufacturing of dense voluminous parts for most ceramics.
We have developed a new additive manufacturing technology, the Laser Induced Slip casting (LIS), based on the layerwise deposition of slurries and their local drying by laser radiation. Laser Induced Slip casting generates ceramic green bodies which can be sintered to dense ceramic components like traditional formed ceramic powder compacts. We will introduce the LIS technology, green bodies and sintered parts will be shown and their microstructure and mechanical properties will be discussed.
Most additive manufacturing processes which produce dense ceramics are nowadays limited in size because of inevitable post-processing steps like for example binder removal in stereolithography. The additive manufacturing of voluminous ceramic parts is realized by powder bed based processes which, however, generate parts with residual porosity. Via infiltration these parts can be processed to dense parts like for example SiC but this is not possible for all ceramics like for example Si3N4. There is a lack of methods for the additive manufacturing of dense voluminous parts for most ceramics.
We have developed a new additive manufacturing technology, the Laser Induced Slip casting (LIS), based on the layerwise deposition of slurries and their local drying by laser radiation. Laser Induced Slip casting generates ceramic green bodies which can be sintered to dense ceramic components like traditional formed ceramic powder compacts. We will introduce the LIS technology, green bodies and sintered parts will be shown and their microstructure and mechanical properties will be discussed.
It is widely accepted that the magnetic state of a ferromagnetic material may be irreversibly altered by mechanical loading due to magnetoelastic effects. A novel standardized nondestructive testing (NDT) technique uses weak magnetic stray fields, which are assumed to arise from inhomogeneous deformation, for structural health monitoring (i.e., for detection and assessment of damage). However, the mechanical and microstructural complexity of damage has hitherto only been insufficiently considered. The aim of this study is to discuss the phenomenon of inhomogeneous “self-magnetization” of a polycrystalline ferromagnetic material under inhomogeneous deformation experimentally and with stronger material-mechanical focus. To this end, notched specimens were elastically and plastically deformed. Surface magnetic states were measured by a three-axis giant magnetoresistant (GMR) sensor and were compared with strain field (digital image correlation) and optical topography measurements. It is demonstrated that the stray fields do not solely form due to magnetoelastic effects. Instead, inhomogeneous plastic deformation causes topography, which is one of the main origins for the magnetic stray field formation. Additionally, if not considered, topography may falsify the magnetic signals due to variable lift-off values. The correlation of magnetic vector components with mechanical tensors, particularly for multiaxial stress/strain states and inhomogeneous elastic-plastic deformations remains an issue.
The influence of heat treatment and creep loading on the microstructure of an Al-Cu-Li alloy was investigated. Especially the formation of different precipitates (T1 and Theta') were characterized and the microstructural changes under different ageing conditions (with and without external strain) were investigated to determine the effect od stress on the ageing process.
The influence of heat treatment and creep loading on the microstructure of an Al-Cu-Li alloy was investigated. Especially the formation of different precipitates (T1 and Theta') were characterized and the microstructural changes under different ageing conditions (with and without external strain) were investigated to determine the effect od stress on the ageing process.
A wide range of solid-state synthesis routes for calcium manganate is reported in the literature, but there is no systematic study about the influence of the solid-state synthesis conditions on thermoelectric properties. Therefore, this study examined the influence of calcination temperature and calcination cycles on the Seebeck coefficient, electrical conductivity, and thermal conductivity. Higher calcination temperatures and repeated calcination cycles minimized the driving force for sintering of the synthesized powder, leading to smaller shrinkage and lower densities of the sintered specimens. As the electrical conductivity increased monotonously with increasing density, a higher energy input during calcination caused deterioration of electrical conductivity. Phase composition and Seebeck coefficient of sintered calcium manganate were not influenced by the calcination procedure. The highest thermoelectric properties with the highest power factors and figures of merit were obtained by means of reaction-sintering of uncalcined powder.
The granules commonly yielded by spray drying procedures exhibit a hard shell and an irregular, dimpled shape, which is often described as donut-like morphology. Sintered parts produced from such granules suffer from microstructural defects and reduced mechanical properties resulting from these disadvantageous granule properties.
Using the example of alumina, zirconia and zirconia-toughened alumina (ZTA) batches, this paper shows that the morphology of the granules can be tuned by adjusting slurry stability. High zeta potential is essential to optimally disperse the particles. But to achieve spherical and soft granules the electrostatic repulsion forces between the particles should be reduced before spray granulation. Electrostatic repulsion forces were changed with the addition of nitric acid. Measurements of zeta potential and viscosity, as well as sedimentation investigations with an optical centrifuge were used for precise slurry assessment as a major precondition for optimal and reproducible adjustment of slurries before spray drying. Sedimentation analysis using an optical centrifuge was performed to investigate different influences like that of additive composition, solids content or pH-value on the sedimentation behavior. Adequately flocculated slurries lead to homogeneous, soft granules that can be easily deformed and pressed. The fraction of donut-shaped particles and the rigidity of granules were reduced. Consequently, the sintered parts produced from these granulates show improvements regarding porosity, pore size distribution, sintered density and biaxial strength.
Entwickelt wurde eine mehrstufige Fertigungstechnologie (Schruppen, Schlichten, Trennschnitt) zur Herstellung keramischer Federn aus gesinterten Hohlzylindern. Durch Optimierung von Maschinenparametern, Schleifscheiben sowie Werkstück- und Werkzeugaufnahmen ist es gelungen, Federn aus Hochleistungskeramik (Aluminiumoxid und Zirkonoxid) mit hoher Kanten- und Oberflächenqualität reproduzierbar herzustellen. Eine hohe Variabilität bezüglich Außen- und Innendurchmesser, Steigung, Windungsquerschnitt und Abstand zwischen den Windungen ermöglicht es, die Federkonstante über drei Größenordnungen zu variieren.
Untersucht wurden Federstabilität und Spannungs-Dehnungs-Verhalten unter konstanter und zyklischer Druckbelastung sowie die thermomechanische Stabilität der Keramikfedern. Aluminiumoxid-Federn können bis etwa 800°C, Zirkonoxid-Federn bis etwa 600°C ohne bleibende geometrische Verformung eingesetzt werden.
Unter konstanter Spannung zeigen Federn aus Y-stabilisiertem TZP (Zirkonoxid)-Werkstoffen, von anderen Keramikwerkstoffen abweichend, bei Raumtemperatur eine zeitabhängige, elastische, Verformung (Superelastizität), die nach Entlastung über einen Zeitraum von mehreren Stunden reversibel verläuft. Als Ursache wird eine spannungsinduzierte reversible Phasenumwandlung zwischen austenitischer (tetragonales ZrO2) und martensitischer (monoklines ZrO2) Phase postuliert.
Diskutiert wird das Anwendungspotenzial der entwickelten Federn für kapazitive keramische Federsensoren für Gravimeter und Wägetechnik.
In der vorliegenden Arbeit wurden verschiedene Epoxidharzsysteme charakterisiert. Zwei Systeme mit großen bruchmechanischen Unterschieden wurden zur Fertigung äquivalenter GFK- und CFK-Laminate mit Faserausrichtungen in 0/90° und ±45° ausgewählt. In quasi-statischen Zugversuchen und Einstufenschwingversuchen mit einem Beanspruchungsverhältnis von R= 0,1 wurden diese Laminate hinsichtlich ihres Schädigungsbeginns und ihrer Schädigungsentwicklung untersucht. Die Detektion der Schädigungen sowie die Dokumentation der Schädigungsentwicklung wurde anhand der Lichtabsorptionsanalyse an GFK-Laminaten und anhand der Röntgenrefraktionsanalyse an CFK-Laminaten umgesetzt. Auf diese Weise konnten Einflüsse der bruchmechanischen Eigenschaften der Matrix auf die Schädigungsentwicklung im Verbund aufgezeigt werden. Zudem wurden für die untersuchten Laminate die Schädigungsgrenzen bei schwingender Beanspruchung ermittelt. Anhand durchgeführter Schwingversuche an CFK-Laminaten im Very High Cycle Fatigue-(VHCF)-Lastwechselbereich bis 108 konnten Rückschlüsse vom Schädigungsverhalten im High Cycle Fatigue-(HCF)-Lastwechselbereich bis 106 auf die Dauerfestigkeit im VHCF-Bereich gezogen werden und damit VHCF-Dauerfestigkeitsgrenzen bestimmt werden. Mit dem Ziel die Ermüdung der Laminate auf die Beanspruchung der Matrix zurückzuführen, wurden die Erweiterte Inverse Laminattheorie, mikromechanikbasierte Mischungsregeln sowie eine Vergleichsspannungshypothese auf die untersuchten Laminate angewendet. Die Schädigungsgrenzen konnten damit in Form der Matrixbeanspruchung wiedergegeben werden. Die Abbildung der Ermüdung verschiedener Laminate anhand einer matrixspezifischen normierten Masterschädigungslinie ist für die behandelten CFK- und GFK-Laminate gelungen.
The residual stress distribution in IN718 elongated prisms produced by Selective Laser Melting was studied by means of neutron (bulk) and laboratory X-ray (surface) diffraction.
Two deposition hatch lengths were considered. A horizontal plane near the top surface (perpendicular to the building direction) and a vertical plane near the lateral surface (parallel to the building direction) were investigated. Samples both in as-built (AB) condition and removed (RE) from the base plate were characterized.
While surface stress fields seem constant for AB condition, X-ray diffraction shows stress gradients along the hatch direction in the RE condition. The stress profiles correlate with the distortion maps obtained by tactile probe measurements.
Neutron diffraction shows bulk stress gradients for all principal components along the main sample directions. We correlate the observed stress patterns with the hatch length, i.e. with its effect on temperature gradients and heat flow. The bulk stress gradients partially disappear after removal from the baseplate.
All in all, practicing professionals as well as researchers can read this book with pleasure and great benefit. It presents a comprehensive collection of data and practical examples manifested in about 100 graphs, 80 schemes of processes and devices, a manifold of images showing the microstructure of alloys or details of components and several phase diagrams. Tables containing data on commercially available coatings, alloys, compositions of corrosive salts, function of constituents of coatings add further important pieces of information. Thus, this book is a valuable source of information for anyone engaged in work with or research on high temperature coatings.
Up to now, the mechanisms of surface nucleation and surface-induced texture formation are far from being understood. Very few observations of crystal orientation were focused on separately growing surface crystals. In conclusion, no systematic studies on initially oriented crystal growth or nucleation from defined active surface nucleation sites exists. Therefore, the main objective of this just is to advance the basic understanding of the mechanisms of surface-induced microstructure formation in glass ceramics. As a first attempt, we focus on reorientation of separately growing surface crystals during their early growth.
For the additive manufacturing of large components typically powder-based methods are used. A powder is deposited layer by layer by means of a recoater, then, the component structure is printed into each individual layer. We introduce here the new method of local laser drying, which is a suspension-based method specially developed for the manufacturing of large voluminous ceramic parts. The structure information is directly written into the freshly deposited layer of suspension by laser drying. Initially, the technology was developed for ceramic suspensions, however, first experiments with geopolymers reveal a high potential for this class of materials. Metakaolin, fly ash and lithium aluminate-based one-part geopolymers were used in first experiments. The local annealing of the geopolymer slurry results in a drying and crosslinking reaction and, thus, in a local consolidation of the material. First parts made are introduced and their properties are discussed.
Lifetime aspects including fatigue failure of concrete structures were traditionally only of minor importance. Because of the growing interest in maxing out the capacities of concrete, its fatigue failure under compression has become an issue. A variety of interacting phenomena such as e.g. loss of prestress, degradation due to chemical reactions or creep and shrinkage influence the fatigue resistance. Failure due to cyclic loads is generally not instantaneous, but characterized by a steady damage accumulation. Therefore, a reliable numerical model to predict the performance of concrete over its lifetime is required, which accurately captures order effects and full three-dimensional stress states.
Many constitutive models for concrete are currently available, which are applicable for specific loading regimes, different time scales and different resolution scales.
However, a key limitation of those models is that they generally do not address issues related to fatigue on a structural level. Very few models can be found in the literature that reproduce deterioration of concrete under repeated loading-unloading cycles. This is due to the computational effort necessary to explicitly resolve every cycle which exceeds the currently available computational resources. The limitation can only be overcome by the application of multiscale methods in time.
The objective of the paper is the development of numerical methods for the simulation of concrete under fatigue loading using temporal multiscale methods.
First, a continuum damage model for concrete is developed with a focus on fatigue under compressive stresses [1]. This includes the possibility to model stress redistributions and capture size effects. In contrast to cycle based approaches, where damage is accumulated based on the number of full stress cycles, a strain based approach is developed that can capture cyclic degradation under variable loading cycles including different amplitudes and loading frequencies. The model is designed to represent failure under static loading as a particular case of fatigue failure after a single loading cycle. As a consequence, most of the material parameters can be deduced from static tests. Only a limit set of additional constitutive parameters is required to accurately describe the evolution under fatigue loading. Another advantage of the proposed model is the possibility to directly incorporate other multi-physics effects such as creep and shrinkage or thermal loading on the constitutive level.
Second, a multiscale approach in time is presented to enable structural computations of fatigue failure with a reduced computational effort. The damage rate within the short time scale corresponding to a single cycle is computed based on a Fourier based approach [2]. This evolution equation is then solved on the long time scale using different implicit and explicit time integration schemes. Their performance and some limitations for specific loading regimes is discussed.
Finally, the developed methods will be validated and compared to experimental data.
[1] Vitaliy Kindrachuk, Marc Thiele, Jörg F. Unger. Constitutive modeling of creep-fatigue interaction for normal strength concrete under compression, International Journal of Fatigue, 78:81-94, 2015
[2] Vitaliy Kindrachuk, Jörg F. Unger. A Fourier transformation-based temporal integration scheme for viscoplastic solids subjected to fatigue deterioration, International Journal of Fatigue, 100:215-228, 2017
Lifetime aspects including fatigue failure of concrete structures were traditionally only of minor importance. Because of the growing interest in maxing out the capacities of concrete, its fatigue failure under compression has become an issue. A variety of interacting phenomena such as e.g. loss of prestress, degradation due to chemical reactions or creep and shrinkage influence the fatigue resistance. Failure due to cyclic loads is generally not instantaneous, but characterized by a steady damage accumulation. Therefore, a reliable numerical model to predict the performance of concrete over its lifetime is required, which accurately captures order effects and full three-dimensional stress states.
Many constitutive models for concrete are currently available, which are applicable for specific loading regimes, different time scales and different resolution scales.
However, a key limitation of those models is that they generally do not address issues related to fatigue on a structural level. Very few models can be found in the literature that reproduce deterioration of concrete under repeated loading-unloading cycles. This is due to the computational effort necessary to explicitly resolve every cycle which exceeds the currently available computational resources. The limitation can only be overcome by the application of multiscale methods in time.
The objective of the paper is the development of numerical methods for the simulation of concrete under fatigue loading using temporal multiscale methods.
First, a continuum damage model for concrete is developed with a focus on fatigue under compressive stresses. This includes the possibility to model stress redistributions and capture size effects. In contrast to cycle based approaches, where damage is accumulated based on the number of full stress cycles, a strain based approach is developed that can capture cyclic degradation under variable loading cycles including different amplitudes and loading frequencies. The model is designed to represent failure under static loading as a particular case of fatigue failure after a single loading cycle. As a consequence, most of the material parameters can be deduced from static tests. Only a limit set of additional constitutive parameters is required to accurately describe the evolution under fatigue loading. Another advantage of the proposed model is the possibility to directly incorporate other multi-physics effects such as creep and shrinkage or thermal loading on the constitutive level.
Second, a multiscale approach in time is presented to enable structural computations of fatigue failure with a reduced computational effort. The damage rate within the short time scale corresponding to a single cycle is computed based on a Fourier based approach. This evolution equation is then solved on the long time scale using different implicit and explicit time integration schemes. Their performance and some limitations for specific loading regimes is discussed.
Finally, the developed methods will be validated and compared to experimental data.
Morphology and structure of TixOy nanoparticles generated by femtosecond laser ablation in water
(2018)
In this work femto-second pulsed laser ablation in liquid (PLAL) procedure for the generation of titanium oxide nanoparticles (NP) is reported with the purpose of understanding morphology and structure of the newly generated NPs. Ablation duration was varied for optimization of NP generation processes between 10 and 90 min. Surface morphology of NPs as well as their size and shape (distribution) were analysed by various complementary electron microscopy techniques, i.e. SEM, TSEM and TEM. The crystalline structure of titanium oxide particles was investigated byXRD(two instruments operated in different geometries) and HR-TEM. Concentration of generated titanium oxide NPs in liquid was analysed by ICP-MS. A mix of crystalline (mainly anatase), partly crystalline and amorphous spherical titanium oxide NPs can be reported having a mean size between 10 and 20 nm, which is rather independent of the laser ablation (LA) duration. A second component consisting of irregularly shaped, but crystalline titanium oxide nanostructures is co-generated in the LA water, with more pronounced occurrence at longer LA times. The provenance of this component is assigned to those spherical particles generated in suspension and passing through the converging laser beam, being hence subject to secondary irradiation effects, e. g. fragmentation.
The alloying system Co-Al-W-Ta is comprehensively investigated in the vicinity of the compositional point Co-9Al-10W-2Ta, at. pct. These investigations provided a large amount of quantitative information, which can be used for alloy development, namely, the compositional dependences of the The alloying system Co-Al-W-Ta is comprehensively investigated in the vicinity of the compositional point Co-9Al-10W-2Ta, at. pct. These investigations provided a large amount of quantitative information, which can be used for alloy development, namely, the compositional dependences of the γ‘-solvus, solidus, and liquidus temperatures; fraction of the extrinsic phases after casting; the compositional dependence of the γ/γ‘-lattice misfit; the element partitioning between γ- and γ‘-phases; and the two Phase compositional area γ/γ‘ in the Co-rich part of the Co-Al-W-Ta phase diagram at 900°C. It is shown that additions of Ta elevate the γ‘-solvus temperature and increase the γ/γ‘-lattice misfit, but adding more than about 3 at. pct Ta results in a large amount of undissolvable extrinsic phases. Additionally, two Co-Al-W-Ta alloys with lower content of W were developed and solidified as [001] single crystals for mechanical testing in a temperature range between 20 and 1200°C. These tests included measurement of the Young modulus, tensile tests with constant strain rate, and stress rupture tests. It was found that at temperatures up to about 750°C the ultimate tensile strength of Co-Al-Ta-W alloys can be at the same level or even higher than of Ni-based superalloys.
To increase efficiency, modern steam plants are pushing their operational regime from super-critical (600 °C/300 bar) to ultra-super-critical (740/760 °C/350 bar) stretching existing turbine materials to their limits. The focus is on new generation functional materials and technologies which complement the inherent properties of existing materials.
Current work proposes a novel High Power Impulse Magnetron Sputtering (HIPIMS) Deposition technology, for the first time, for deposition of a ceramic based CrN/NbN coating with a nanoscale multilayer structure (bi-layer thickness Δ = 1.9 nm) with superior adhesion (LC2 = 80 N) to protect low Chromium P92 steel widely used in steam power plants. Thermodynamic calculations predict the equilibrium phases and aggressive gaseous compounds generated by the interaction of steam with the coating. CrN/NbN coated P92 steel samples oxidised at 600 °C in a high pressure (50 bar) 100% steam atmosphere for up to 1000 h reveal the coating's superior oxidation resistance and protective mechanisms, especially against the detrimental effect of Hydrogen. High temperature (650 °C) Tensile Strength, Low Cycle Fatigue and Creep tests confirm that, unlike other state-of-the-art PVD technologies, HIPIMS is not detrimental to the mechanical properties of the substrate material. Water droplet erosion tests confirm no measurable weight loss after 2.4 X 10⁶ impacts.
Comprehensive insights into the early stages of corrosion mechanisms provide fundamental knowledge to further understand and model long time material behaviour. The present work studies the early stages of combined oxidation and sulphidation of ferritic model alloys for time scales up to 250 h at 650 °C to observe the influence of chromium during the corrosion under SO2. Model alloys were used to focus on the reaction of the intended elements: Fe, Cr, S, and O. Pure iron simultaneously forms magnetite and iron sulphide in an early stage of corrosion, covered by a pure oxide layer after 100 h. Iron with 13 wt% Cr shows hematite and mixed Fe-Cr-oxides first, before sulphides nucleate in the inner corrosion zone. With increasing ageing time a magnetite layer is observed below the hematite layer. Quantitative phase fractions of all corrosion products observed were determined from cross section images. Characterization of the Fe13Cr corrosion scale by FIB revealed a highly porous structure in the inner corrosion zone where Cr-rich (Fe, Cr)-sulphides are present, and caused the scale to spall easily.
The sliding behavior of an amorphous silica sample between two rigid surfaces is in the focus of the present paper. Molecular Dynamics using a classical Tersoff’s potential and a recently developed ReaxFF potential was applied for simulating sliding within a thin film corresponding to a tribofilm formed from silica nanoparticles. The simulations were performed at different temperatures corresponding to moderate and severe tribological stressing conditions. Simulations with both potentials revealed the need of considering different temperatures in order to obtain a sound interpretation of experimental findings. The results show the striking differences between the two potentials not only in terms of magnitude of the resistance stress (about one order of magnitude) but also in terms of friction mechanisms. The expected smooth sliding regime under high temperature conditions was predicted by both simulations, although with Tersoff’s potential smooth sliding was obtained only at the highest temperature. On the other hand, at room temperature Tersoff-style calculations demonstrate stick-slip behavior, which corresponds qualitatively with our experimental findings. Nevertheless, comparison with a macroscopic coefficient of friction is not possible because simulated resistance stresses do not depend on the applied normal pressure.
Thin Sol-Gel Alumina Coating as Protection of a 9% Cr Steel Against Flue Gas Corrosion at 650 °C
(2018)
Samples of sol-gel alumina coated and uncoated P92 steel were exposed to flue gas at 650 °C for 300 h. As result of this treatment a 50 µm thick bi-layered oxide scale had formed on the surface of the uncoated sample. Below the scale a 40 µm thick inner oxidation zone was detected. In contrast, the porous, micron thick alumina coating enabled the formation of a chromium oxide scale with a thickness of some nanometers at the interface between steel substrate and coating. In this case high temperature corrosion of the steel was prevented so far.
Due to the increasing global demand for pure silver, native wire silver aggregates in very high purities are gaining more industrial attention. Up to the present, no substantial metallurgical Investigation of natural wire silver exists in the accessible literature. To convey urgently needed cross-disciplinary fundamental knowledge for geoscientists and metallurgical engineers, twenty natural wire silver specimens from eight different ore deposits have been investigated in detail for the first time by EBSD (Electron Back Scattering Diffraction), supported by light microscopy and micro-probe analyses. The improved understanding of the natural silver wire microstructure provides additional Information regarding the growth of natural silver aggregates in comparison to undesired artificial growth on electronic devices. Clear evidence is provided that natural silver curls and hairs exhibit a polycrystalline face-centered cubic microstructure associated with significant twinning. Although the investigated natural wire silver samples have relatively high purity (Ag > 99.7 wt.-%), they contain a variety of trace elements such as, S, Cu, Mn, Ni, Zn, Co and Bi, As and Sb. Additionally, Vickers micro-hardness measurements are provided for the first time which revealed that natural silver wires and curls are softer than it might be expected from conversion of the general Mohs hardness of 2.7.
Interdiffusion in the Face-Centered Cubic Phase of the Co-Al-W-Ta System Between 1090 and 1240 °C
(2018)
Interdiffusion of Al, W, Ta and Co in a Co-base alloy at temperatures between 1090 and 1240 °C has been investigated. The interdiffusion coefficients were found to be close to those reported for these elements in Ni-base alloys. Combining the diffusion simulation software DICTRA with the Ni-base diffusion databases TCNi5 and MobNi3, the interdiffusion profiles of Co, Al W, and Ta were modeled for Co9Al8W2Ta/Co diffusion couples annealed at different temperatures and for different times. The results show that interdiffusion in the Co-Al-W-Ta alloys can be modeled reasonably well using the available commercial databases for thermodynamics and kinetics of Ni-base systems.
Technically relevant P92 steel (9% Cr) was coated with a micron-thick porous alumina layer prepared by sol-gel technique and treated with flue gas (60 CO2-30 H2O-2 O2-1 SO2-7 N2 (mole fraction in %)) at 650 ° to mimic an oxyfuelcombustion process. Local defects in the coating were marked using focused ion beam (FIB) technique and were inspected after exposition to hot flue gas atmosphere at 300, 800, and 1300 h, respectively. Local defects like agglomerated alumina sol particles tend to spall off from the coating uncovering the underlying dense chromia scale. Re-coating was found to restore the protection ability from oxidation when repeatedly treated with hot flue gas. Cracks and voids did not promote the local oxidation due to the formation of crystalline Mn/S/O species within and on top of the coating. The protective character of the steel-coating system is a result of (i) the fast formation of a dense chromia scale at the surface of sol-gel alumina-coated P92 steel bars in combination with (ii) the porous alumina coating acting as diffusion barrier, but also as diffusion partner in addition with (iii) fast Mn outward diffusion capturing the S species from flue gas.
Metal sulfide grain boundary precipitates of a ferrous model alloy with 13 wt.% chromium formed at 650°C under a gas atmosphere containing 0.5% SO2 and 99.5% Ar were investigated after ageing for 3 h, 6 h, and 12 h. The precipitates formed along grain boundaries were identified as Cr5S6 using energy-dispersive x-ray spectroscopy in transmission electron microscopy and electron backscatter diffraction analysis. Serial focused ion beam slicing was conducted followed by three-dimensional reconstruction to determine the number, size, and penetration depth of the precipitates evolved at the different time steps. There was a linear increase in the number of precipitates with time, while their average size increased only for the initial aging time but became constant after 6 h. Based on these results, a model for grain boundary sulfidation of ferritic alloys is discussed.
In this work, the focus was set on the corrosion process of condensate as drops on the surface of carbon steels (X52, X70), martensitic steel UNS S41500, and superaustenite UNS N08031 in CO2 atmosphere with impurities at 278 K (to simulate the transportation condition in a buried pipeline). Exposure tests were performed at both normal pressure and high pressure where CO2 is supercritical or in dense phase. The drop, 1 ‑ 10 μL in volume, was prepared by dropping CO2 saturated ultra-pure water onto the surface of steel coupons in a one-liter-autoclave. The CO2 gas stream, simulating the oxyfuel flue gas with varying concentration of impurities (SO2 and O2 ), was then pumped into the autoclave to observe the condensation and corrosion impacts of impurities. Comparable exposure tests were carried out with the same gas mixture and the same volume of water as vapor to observe the drop formation and the corrosion process that follows. The wettability and stability of drops on the surface of steel coupons in CO2 supercritical/dense phase environment was evaluated additionally by contact angle measurement.
In CCS environment (carbon capture and storage) pipes are loaded statically and/or cyclically and at the same time exposed constantly to the highly corrosive hot thermal water. Experimental procedures such as ambient pressure immersions tests, in-situ corrosion fatigue experiments using a flexibly designed corrosion chamber at ambient pressure and a specially designed corrosion chamber at high pressure. Experimental set-ups for push/pull and rotation bending load are introduced. The corrosion behavior and lifetime reduction of high alloyed steels (X46Cr13, 1.4043), (X5CrNiCuNb16-4, 1.4542) and (X2CrNiMoN22-5-3, 1.4462) is demonstrated (T=60 °C, geothermal brine: Stuttgart Aquifer flow rate: 9 l/h, CO2 ).
The commercial usage of latent thermal energy storages primarily depends on the development of a suitable phase change material (PCM). For industrial high temperature applications above 400 °C multicomponent chloride eutectics are promising and therefore discussed seriously. The profound thermodynamic investigation of such eutectics requires a much greater amount of specimen material than conventional calorimeter can handle. Therefore, a special adiabatic calorimeter was developed and designed. With a specimen mass of > 100 g the typical thermodynamic measurements with a commercial calorimeter can be extended by cycle stability measurements, which are often decisive for practical application of PCM. Furthermore, by implementing corrosion specimens inside the calorimeter high temperature corrosion experiments according to ISO 21608 can be performed inside the calorimeter. Adiabatic measuring conditions can be provided by using two separate heating systems. Therefore, the outer “protective system” follows the temperature curve of the inner “measuring system” minimizing the temperature difference between the heating systems and simultaneously preventing heat losses from the measuring systems.
The work presents the microstructure, chemical composition and mechanical properties of Inconel 686 coatings after high - temperature corrosion in environment of aggressive gases and ashes. To produce the Ni - based coatings the QS Nd:YAG laser cladding process was carried out. As the substrate used 13CrMo4-5 boilers plate steel. Ni - base alloys characterize the excellent high-temperature corrosion resistance, good strength and ability to work in aggressive environments. Formed clad were characterized by high quality of metallurgical bonding with the substrate material and sufficiently low amount of the iron close to the clad layer surface. After corrosion experiment the oxide scale on the substrate and clad created. The scale on 13CrMo4-5 steel had 70 μm thickness while the scale of the clad had less than 10 μm. The microstructure, chemical composition of the obtained clad and scales were investigated by scanning electron microscope (SEM) and electron probe microanalyzer (EPMA) equipped with the EDS detectors.
Carbon Capture and Storage (CCS) is identified as an excellent technology to reach the target of CO2 reduction. However, the safety issue and cost effectiveness hinder the future of CCS. For the reliability and safety issues of injection wells the corrosion resistance of the materials used needs to be determined.
In this study, representative low cost materials including carbon steel 1.8977 and low alloyed steel 1.7225 were embedded in cement to mimic the realistic casing-cement interface. Electrochemical studies were carried out using these metal-cement specimens in comparison with those made of metal only in CO2 saturated synthetic aquifer fluid, at 333 K, to reveal the effect of cement on the steel performance. The results showed the protective effect of cement on the performance of pipeline metals during polarisation process. However, the corrosion current density was high in all cases, with and without cement, indicating that the corrosion resistance of these materials is low. This conclusion was supported by the surface analysis of the polarized specimens, which revealed both homogenous and pitting corrosions.
Pipe steels suitable for carbon capture and storage technology (CCS) require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products are FeCO3 and FeOOH. Corrosion rates obtained at 100 bar are generally much lower than those measured at ambient pressure. Highest surface corrosion rates are 0.8 mm/year for 42CrMo4 and lowest 0.01 mm/year for X5CrNiCuNb16-4 in the vapour phase at ambient pressure. At 100 bar the highest corrosion rates are 0.01 mm/year for 42CrMo4, X20Cr13 (liquid phase), X46Cr13 and less than 0.01 mm/year for X35CrMo4 and X5CrNiCuNb16-4 after 8000 h of exposure with no regard to atmosphere. Martensitic microstructure offers good corrosion resistance.
The current competitive situation on electricity markets forces power plants into cyclic operation regimes with frequent load shifts and starts/shutdowns. In the present work, the cyclic mechanical behavior of ferritic-martensitic 9-12 % Cr steels under isothermal and thermomechanical loading was investigated for the example of grade P92 material. A continuous softening was observed under all loading conditions. The introduction of hold periods to the applied cycles reduced material lifetime, with most prominent effects at technologically relevant small strain levels. The microstructural characterization reveals a coarsening of the original “martensitic” lath-type microstructure to a structure with polygonal subgrains and reduced dislocation density. The microstructural data forms the input for a physically-based modelling approach.
This work presents the microstructure and chemical composition of oxide scales created on Ni – base coating after corrosion experiments in aggressive gases and ashes. The Inconel 686 coating applied on the low carbon steel 13CrMo4-5 was performed by a CO2 laser cladding process. The experiments were carried out in oxidizing gas atmospheres containing O2, COx, SOx. The second Variation of corrosion experiments were performed in a reducing atmosphere with ashes containing elements such as: Na, Cl, Ca, Si, C, Fe, Al etc. After 240 h and 1.000 h corrosion experiments the oxide scales on the substrate and overlay were created in both cases.
The sulfur compounds were found on the top of the coating surface (EPMA) and also higher contents of silica compounds were revealed on specimens covered by ashes during the experiments. The microstructure and chemical composition of the clad and scales were investigated by means of a light microscope and an electron microscope (SEM)equipped with an EDS detector.
Our research focused on Inconel 625 weld overlays on 16Mo3 steel boiler pipes. The Investigation focused on the characterization of changes in the microstructure and chemical composition after annealing. The annealing was performed for ten hours at temperatures from 600 to 1000°C. Changes in the microstructure were observed with a scanning and transmission electron microscope (SEM and TEM). The investigation was supplemented by hardness measurements.
This study examines the relationship between the magnetic mesostructure with the microstructure of low carbon steel tungsten inert gas welds. Optical microscopy revealed variation in the microstructure of the parent material, in the heat affected and fusion zones, correlating with distinctive changes in the local magnetic stray fields measured with high spatial resolution giant magneto resistance sensors. In the vicinity of the heat affected zone high residual stresses were found using neutron diffraction.
Notably, the gradients of von Mises stress and triaxial magnetic stray field modulus follow the same tendency transverse to the weld. In contrast, micro-X-ray fluorescence characterization indicated that local changes in element composition had no independent effect on magnetic stray fields.
Shear testing can contribute to a better understanding of the plastic deformation of Ni-base superalloy single crystals. In the present study, shear testing is discussed with special emphasis placed on its strengths and weaknesses. Key mechanical and microstructural results which were obtained for the high-temperature (T ≈ 1000 °C) and low-stress (τ ≈ 200 MPa) creep regime are briefly reviewed. New 3D stereo STEM images of dislocation substructures which form during shear creep deformation in this regime are presented. It is then shown which new aspects need to be considered when performing double shear creep testing at lower temperatures (T < 800 °C) and higher stresses (τ > 600 MPa). In this creep regime, the macroscopic crystallographic [11−2](111) shear system deforms significantly faster than the [01−1](111) system. This represents direct mechanical evidence for a new planar fault nucleation scenario, which was recently suggested (Wu et al. in Acta Mater 144:642–655, 2018). The double shear creep specimen geometry inspired a micro-mechanical in-situ shear test specimen. Moreover, the in-situ SEM shear specimen can be FIB micro-machined from prior dendritic and interdendritic regions. Dendritic regions, which have a lower γ′ volume fraction, show a lower critical resolved shear stress.
We describe a lattice-based crystallographic approximation for the analysis of distorted crystal structures via Electron Backscatter Diffraction (EBSD) in the scanning electron microscope. EBSD patterns are closely linked to local lattice parameter ratios via Kikuchi bands that indicate geometrical lattice plane projections. Based on the transformation properties of points and lines in the real projective plane, we can obtain continuous estimations of the local lattice distortion based on projectively transformed Kikuchi diffraction simulations for a reference structure. By quantitative image matching to a projective transformation model of the lattice distortion in the full solid angle of possible scattering directions, we enforce a crystallographically consistent approximation in the fitting procedure of distorted simulations to the experimentally observed diffraction patterns. As an application example, we map the locally varying tetragonality in martensite grains of steel.
Carbon Capture and Storage (CCS) is well acknowledged to mitigate climate change. Therefore, pipe Steels suitable for CCS technology require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe Steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products analysed on pits are FeCO3 and FeOOH. The carbon content does not show significant influence on the pitting behaviour. Generally, higher chromium Content results in better corrosion resistance. Although X35CrMo17-1 and X5CrNiCuNb16-4 show low surface corrosion rates, their resistance against local corrosion in CCS environment is not significantly better compared to the much less costly Steels X20Cr13 and X46Cr13.
Subsurface characterization of high-strength high-interstitial austenitic steels after impact wear
(2018)
The microstructure of the subsurface after impact wear of three high-strength high interstitial austenitic steels has been analysed using transmission electron microscopy (TEM) in alloys with C and N as interstitial elements. In all cases, a nanocrystalline region followed by a transition zone and a cold-worked area are present. Additionally, microhardness and nano-scratching tests were conducted to study the wear-related properties of the impact subsurface and the base material. The results of the microstructural analysis reveal that the following mechanisms are involved during impact wear: abrasion (ploughing), microcrack formation associated with contact fatigue, entrapment and adhesion of SiO2 particles. The analysis of the wear-related properties indicates that the subsurface acts as a self-protective layer that prevents the deterioration of the substrate.
Commercial grade-1 titanium samples (Ti, 99.6%) were treated using three alternative methods, (i) femtosecond laser processing, (ii) thermal heat treatment, and (iii) electrochemical anodization, respectively, resulting in the formation of differently conditioned superficial titanium oxide layers. The laser processing (i) was carried out by a Ti:sapphire laser (pulse duration 30 fs, central wavelength 790 nm, pulse repetition rate 1 kHz) in a regime of generating laser-induced periodic surface structures (LIPSS). The experimental conditions (laser fluence, spatial spot overlap) were optimized in a sample-scanning setup for the processing of several square-millimeters large surface areas covered homogeneously by these nanostructures. The differently oxidized titanium surfaces were characterized by optical microscopy, micro Raman spectroscopy, variable angle spectroscopic ellipsometry, and instrumented indentation testing. The tribological performance was characterized in the regime of mixed friction by reciprocating sliding tests against a sphere of hardened steel in fully formulated engine oil as lubricant. The specific tribological performance of the differently treated surfaces is discussed with respect to possible physical and chemical mechanisms.
Insights into early damage mechanisms during high-temperature gas corrosion provide important aspects for the prediction of the long-term stability of hightemperature materials exposed to a hot and corrosive environment. The current work presents a real time study concerning the combined oxidation and sulfidation of ferritic model alloys in a hot SO2 containing atmosphere using energy dispersive X-ray diffraction. The applied high temperature reactor allows the transmittance of high energetic X-rays in order to collect X-ray diffraction pattern of the sample surface in situ during the reaction with the reactive environment. The results revealed that the first phases crystallizing on iron with 2 wt% chromium and with 9 wt% chromium are oxides. The aging experiments at T = 650° C with 0.5% SO2 and 99.5% Ar were followed in situ and caused an external mixed oxide-sulfide layer on top of iron with 2 wt% chromium. On the higher alloyed material the external scale consists of iron oxides and the inner scale of mixed (Fe,Cr)-oxides and chromium-sulfides. The oxide content continuously increases parallel to an increase of the sulfide amount. Thus, the initially formed (Fe,Cr)-oxides do not have a protective character and support the transport of sulfur through the growing oxide scale.
Wood treated with nano metal fluorides is found to resist fungal decay. Sol−gel synthesis was used to synthesize MgF2 and CaF2 nanoparticles. Electron microscopy images confirmed the localization of MgF2 and CaF2 nanoparticles in wood. Efficacy of nano metal fluoride-treated wood was tested against brown-rot fungi Coniophora puteana and Rhodonia placenta. Untreated wood specimens had higher
mass losses (∼30%) compared to treated specimens, which had average mass loss of 2% against C. puteana and 14% against R. placenta, respectively. Nano metal fluorides provide a viable alternative to current wood preservatives.
A great amount of material properties is strongly influenced by dislocations, the carriers of plastic deformation. It is therefore paramount to have appropriate tools to quantify dislocation substructures with regard to their features, e.g., dislocation density, Burgers vectors or line direction. While the transmission electron microscope (TEM) has been the most widely-used equipment implemented to investigate dislocations, it usually is limited to the two-dimensional (2D) observation of three-dimensional (3D) structures. We reconstruct, visualize and quantify 3D dislocation substructure models from only two TEM images (stereo pairs) and assess the results. The reconstruction is based on the manual interactive tracing of filiform objects on both images of the stereo pair. The reconstruction and quantification method are demonstrated on dark field (DF) scanning (S)TEM micrographs of dislocation substructures imaged under diffraction contrast conditions. For this purpose, thick regions (> 300 nm) of TEM foils are analyzed, which are extracted from a Ni-base superalloy single crystal after high temperature creep deformation. It is shown how the method allows 3D quantification from stereo pairs in a wide range of tilt conditions, achieving line length and orientation uncertainties of 3% and 7°, respectively. Parameters that affect the quality of such reconstructions are discussed.
We use pattern matching of experimental and dynamically simulated backscattered Kikuchi diffraction (BKD) patterns to increase the orientation precision of electron backscatter diffraction (EBSD) measurements. In order to quantify the improvement in orientation precision, we analyze the experimental distribution of the kernel average misorientation (KAM) angles. We find that for the same raw data, i.e. the same EBSD data acquisition time budget, the pattern matching approach improves the KAM resolution by an order of magnitude compared to orientation data delivered from the conventional Hough-transform based data analysis. This quantitative improvement enables us to interpret small orientation changes in plastically deformed materials which are hidden in noisy orientation data delivered from the reference EBSD system.
As an application example, we analyze a ferritic-martensitic steel (P92) sample before and after low-cycle fatigue (LCF) loading (±0.3% strain) at 620 °C. Whereas the low precision of the EBSD orientation data from the manufacturer software does not allow a reliable discrimination of the gradually changing microstructure, we find very clear systematic differences of the local microstructure after the pattern matching orientation refinement of the initial, raw pattern data. For the investigated P92 sample, the KAM-angle histograms are well described by two log-normal distributions indicating the already tempered and the remaining and mostly untempered martensite.
The Bravais lattices and their lattice parameters are blindly determined using electron backscatter diffraction (EBSD) patterns of materials with cubic or tetragonal crystal structures. Since the geometric relationships in a single EBSD pattern are overdetermined, the relative errors of determining the lattice parameters as well as the axial ratios are confined to about 0.7 ± 0.4% and 0.07 ± 0.03%, respectively, for ideal simulated EBSD patterns. The accuracy of the crystal orientation determination reaches about 0.06 ± 0.03°. With careful manual band detection, the accuracy of determining lattice parameters from experimental patterns can be as good as from simulated patterns, although the results from simulated patterns are often better than expermental patterns, which are lower quality and contain uncertain systematic errors. The reasonably high accuracy is obtained primarily because the detection of the diffracting-plane traces and zone axes is relatively accurate. The results here demonstrate that the developed procedure based on the EBSD technique presents a reliable tool for crystallographic characterization of the Bravais lattices of unknown phases.
A femto-second pulsed laser ablation in liquid (PLAL) procedure for the generation of titanium oxide nanoparticles (NP) is reported with the purpose of understanding morphology and structure of the newly generated NPs. Ablation duration was varied for optimization of NP generation processes between 10 and 90 min. Surface morphology of NPs as well as their size and shape (distribution) were analysed by various complementary electron microscopy techniques, i.e. SEM, TSEM and TEM. The crystalline structure of titanium oxide particles was investigated by XRD(two instruments operated in different geometries) and HR-TEM. Concentration of generated titanium oxide NPs in liquid was analysed by ICP-MS. A mix of crystalline (mainly anatase), partly crystalline and amorphous spherical titanium oxide NPs can be reported having a mean size between 10 and 20 nm, which is rather independent of the laser ablation (LA) duration. A second component consisting of irregularly shaped, but crystalline titanium oxide nanostructures is co-generated in the LA water, with more pronounced occurrence at longer LA times. The provenance of this component is assigned to those spherical particles generated in suspension and passing through the converging laser beam, being hence subject to secondary irradiation effects, e. g. fragmentation.
(Bio)geochemical cycling of gold (Au) has been demonstrated in present-day (semi)-arid, (sub)-tropical and temperate environment. Hereby biofilms on Au-bearing mineral- and Au-particle surfaces drive Au dispersion and reconcentration, thereby (trans)forming the particles. However, it is unknown if biogeochemical cycling of Au occurs in polar environments, where air temperatures can reach −40 °C and soils remain frozen for much of the year. Therefore, placer Au-particles, soils and waters were collected at two placer mining districts in arctic Finland, i.e., the Ivalojoki and Lemmenjoki goldfields. Sites were chosen based on contrasting settings ((glacio)-fluvial vs. glacial-till deposits) and depths (surface to 5m below current surface). Gold particles were studied using a combination of tagged 16S rRNA gene next generation sequencing and electron microscopic/microanalytical techniques. Across all sites a range of Au-particle morphologies were observed, including morphotypes indicative of Au dissolution and aggregation. Elevated Au concentrations indicative of Au mobility were detected in placer particle bearing soils at both districts. Typically Au-particles were coated by polymorphic biofilm layers composed of living and dead cells embedded in extracellular polymeric substances. Intermixed were biominerals, clays and iron-sulfides/oxides and abundant secondary Au morphotypes, i.e., nano-particles, microcrystals, sheet-like Au, branched Au networks and overgrowths and secondary rims. Biofilms communities were composed of Acidobacteria (18.3%), Bacteroidetes (15.1%) and Proteobacteria (47.1%), with β-Proteobacteria (19.5%) being the most abundant proteobacterial group. Functionally, biofilms were composed of taxa contributing to biofilm establishment, exopolymer production and nutrient cycling, abundant taxa capable of Au mobilization, detoxification and biomineralization, among them Cupriavidus metallidurans, Acinetobacter spp. and Pseudomonas spp., were detected. In conclusion, these results demonstrate that placer Au-particle transformation and Au dispersion occur in cold, arctic environments. This corroborates the existence of biogeochemical Au cycling in present-day cold environments.
Degradation of AISI 630 exposed to CO2-saturated saline aquifer at ambient pressure and 100 bar
(2018)
In general high alloyed steels are suitable as pipe steels for carbon capture and storage technology (CCS), because they provide sufficient resistance against the corrosive environment of CO2-saturated saline aquifer which serves as potential CCS-site in Germany. High alloyed martensitic steel AISI 630 has been proven to be sufficient resistant in corrosive environments, e.g. regarding heat, pressure, salinity of the aquifer, CO2-partial pressure), but reveals a distinct corrosion pattern in CCS environment. Therefore coupons of AISI 630 heat treated using usual protocols were kept at T=60 °C and ambient pressure as well as p=100 bar up to 8000 h in an a) water saturated supercritical CO2 and b) CO2-saturated synthetic aquifer environment similar to on-shore CCS-sites in the Northern German Basin. AISI 630 precipitates a discontinuous ellipsoidal corrosion layer after being exposed for more than 4000 hours. Best corrosion resistance in the CO2-saturated synthetic aquifer environment phase is achieved via normalizing prior to exposure. In water saturated supercritical CO2 tempering at medium temperatures after hardening gives lowest corrosion rates. Corrosion fatigue via push-pull tests with a series of 30 specimens was evaluated at stress amplitudes between 150 MPa and 500 MPa (sinusoidal dynamic test loads, R=-1; resonant frequency ~ 30 Hz). The endurance limit of AISI 630 is reduced by more than 50% when exposed to CCS environment (maximum number of cycles (10 x 106) at a stress amplitude of 150 MPa).
The research focus of this study was set on the corrosion process of condensate as droplets on the surface of carbon steels (X52, X70) martensitic steel UNS S41500, and super austenite UNS N08031 in CO2 atmosphere with impurities at 278 K (to simulate the offshore transportation condition in a buried pipeline). The possibility of dew/droplet formation on the steel surface and wetting behavior of corresponding materials were evaluated by contact angle measurement in dense CO2 at 278 K. To observe the effect of impurities (SO2 and O2) on droplet corrosion process, exposure tests were carried out in the mixed atmosphere with a drop, 1 ‑ 10 µL in volume, of CO2 saturated ultra-pure water on steel surface. Comparable exposure tests were carried out with the same gas mixture and the same volume of water, as vapor, to observe the droplet formation and the corrosion process that follows. Effects of surface roughness on the droplet formation and its corrosion process were further studied and showed no significant role upon long time exposure. The results from droplet experiments were compared to those from the bulk electrolyte for the further recommendation on the quality control of gas stream along with the use of carbon steels as transport pipelines in CCS - Carbon Capture and Storage system.
A gray cast iron disc, which had been submitted to a heavy duty automotive brake test, was examined with energy filtered transmission electron microscopy. A graphite flake in a convenient angular position showed the shear interaction of graphite layers with the iron matrix in nano-scale resolution. Atomic layers of graphite were wedged into the ferritic bulk, allowing the entrance of oxygen and the subsequent formation of magnetite. The exfoliated few-layer graphene batches deformed heavily when forced into the matrix. When Raman spectra from the disc surface, which show distinctive carbonaceous bands, were compared with Raman spectra from graphite subjected to deformation in a shaker mill with different milling times, it could be seen that the shear stress on the brake surface was much more effective to induce disorder than the milling, where compressive and impact forces had been additionally exerted on the sample. During shear load the high anisotropy of elastic modulus in the graphite crystalline structure and the low adhesion between graphite basal planes allowed the exfoliation of wrinkled few-layer grapheme batches, causing the formation of more defect related Raman bands than the mechanical stress during high-energy milling.
The Ni-Cr-Mo-W alloy is characterized by the excellent high-temperature corrosion resistance, good strength and ability to work in aggressive environments. To protect the surface of the substrate 13CrMo4-5 steel against aggressive environments the Inconel 686 as clad layer was used. The corrosion process was performed in oxidizing mixture of gases like O2, COx, SOx. The second part of corrosion Experiment concerned the corrosion test of the coating in reducing atmosphere of the specified gases with ashes, which contained e.g. Na, Cl, Ca, Si, C, Fe, Al.
The Ni-Cr-Mo-W alloy is characterized by the excellent high-temperature corrosion resistance, good strength and ability to work in aggressive environments. To protect the surface of the substrate 13CrMo4-5 steel against aggressive environments the Inconel 686 as clad layer was used. The corrosion process was performed in oxidizing mixture of gases like O2, COx, SOx. The second part of corrosion Experiment concerned the corrosion test of the coating in reducing atmosphere of the specified gases with ashes, which contained e.g. Na, Cl, Ca, Si, C, Fe, Al.
A femto-second pulsed laser ablation in liquid (PLAL) procedure for the generation of titanium oxide nanoparticles (NP) is reported with the purpose of understanding morphology and structure of the newly generated NPs. Ablation duration was varied for optimization of NP generation processes between 10 and 90 min. Surface morphology of NPs as well as their size and shape (distribution) were analysed by various complementary electron microscopy techniques, i.e. SEM, TSEM and TEM. The crystalline structure of titanium oxide particles was investigated by XRD and HR-TEM. Concentration of generated titanium oxide NPs in liquid was analysed by ICP-MS. A mix of crystalline (mainly anatase), partly crystalline and amorphous spherical titanium oxide NPs can be reported having a mean size between 10 and 20 nm, which is rather independent of the laser ablation (LA) duration. A second component consisting of irregularly shaped, but crystalline titanium oxide nanostructures is co-generated in the LA water, with more pronounced occurrence at longer LA times. The provenance of this component is assigned to those spherical particles generated in suspension and passing through the converging laser beam, being hence subject to secondary irradiation effects, e. g. fragmentation.
Dislocations are the carriers of plastic deformation. As such, their characterization offers important information on the properties they affect. In this contribution, a new tool is presented, which is incorporated in Amira ZIB Edition and allows for three-dimensional (3D) imaging and quantification of dislocations substructures from thick regions an electron-transparent specimen. In the tool, the dislocation segments are traced on diffraction contrast images that are obtained in the transmission electron microscope (TEM). The uncertainties related to the experimental setup and to the proposed method are discussed on the base of a tilt series.
The Topic of the presentationis a discussion on defects which can cause failure in cyclically loaded metallic components. Although also touching Features such as material defects such as pores or micro-shrinkages, etc. and geometric defects such as surface roughness and secondary notches (which are not considered in the design process) which origin in manufacturing, and others the presentation concentrates on non-metallic inclusions. It is prefaced by an introduction to the life cycle of a fatigue crack from initiation up to fracture. Special emphasis is put on the fact that only cracks which are not arrested during one of their distinct Propagation stages can grow to a critical size.
Impact of acid condensation on wetting and corrosion behavior of CO2 transport-pipeline steel
(2018)
Es ist allgemein akzeptiert, das Korrosion in CO2-Transport-Pipelines vernach¬lässigbar ist, solange der Wassergehalt des CO2-Stroms deutlich unter der maximal löslichen Menge liegt. Bisher gibt es keinen allgemeinen Konsens darüber, welcher maximale Wassergehalt in zu transportierendem CO2 zugelassen werden sollte. Bei einem Druck von 100 bar und im Temperaturbereich von 277 K bis 298 K beträgt die Löslichkeit von Wasser in CO2 ca. 1.900 bis 3.200 ppmv, aber die Korrosionsrate von Stählen steigt schon ab einem Wassergehalt von 500 ppmv deutlich an. Bei Anwesenheit von Begleitstoffen wie SO2, NO2 und O2, können sich HNO3, H2SO3 und H2SO4 bilden. Menge und Zusammensetzung von kondensierter Säure sind von der Gaszusammensetzung abhängig, und der Korrosionsmechanismus und die Korrosionsform sind vom Kondensationsverhalten abhängig.
Carbon Capture and Storage (CCS) is identified as an excellent technology to reach the target of CO2 reduction. However, the safety issue and cost effectiveness hinder the future of CCS. For the reliability and safety issues of injection wells the corrosion resistance of the materials used needs to be determined.
In this study, representative low cost materials including carbon steel 1.8977 and low alloyed steel 1.7225 were embedded in cement to mimic the realistic casing-cement interface. Electrochemical studies were carried out using these metal-cement specimens in comparison with those made of metal only in CO2 saturated synthetic aquifer fluid, at 333 K, to reveal the effect of cement on the steel performance. The results showed the protective effect of cement on the performance of pipeline metals during polarisation process. However, the corrosion current density was high in all cases, with and without cement, indicating that the corrosion resistance of these materials is low. This conclusion was supported by the surface analysis of the polarized specimens, which revealed both homogenous and pitting corrosions. Furthermore, to reveal the possible protective performance of FeCO3, the pipeline steels were pre-carbonated and then tested in the same condition as freshly polished specimens.
Among the very few techniques to localize hydrogen (H) at the microscale in steels, Time-of-flight secondary ion mass spectrometry (ToF-SIMS) was proven to be a reliable tool. The necessity to detect hydrogen stems from its deleterious effects in metals, that are often used as structural components and to obtain better understanding of the underlying metallurgical mechanisms of hydrogen embrittlement (HE) which are still unclear.
Austenitic stainless steels are nowadays commonly used in a wide variety of application, from hydrogen transport and storage facilities to petrochemical and offshore applications where they are exposed to aggressive environments and therefore prone to HE. One of the greater risks in the austenitic class is the embrittlement of the material due to the instability of the γ austenite and its transformation into a brittle α martensitic phase. This transformation takes place due to the local stresses that are induced by the uptake of hydrogen during service. Nonetheless, it was shown that this transformation can occur as an artefact during SIMS analysis itself where Cs-sputtering is necessary not only to remove surface contaminations but mainly to enhance H/D secondary ion yield.
In the following contribution we show the influence of different sputtering conditions on AISI 304L austenitic stainless steel in order to distinguish the artefact from the hydrogen induced transformation. The material was charged electrochemically in a deuterium based electrolyte. Deuterium (D) must be in these experiments as a replacement for hydrogen which cannot be used because adsorbed hydrogen superimposes hydrogen originating from charging the sample in the SIMS images. ToF-SIMS analyses were conducted by ToF SIMS IV (IONTOF GmbH, Münster, Germany). The experiments were carried out on deuterium charged and non-charged samples. The structural characterization was carried out by SEM and EBSD examinations before and after charging, both with a Leo Gemeni 1530VP field-emission scanning electron microscope and a Zeiss Supra 40 instrument (Carl Zeiss Microscopy GmbH, Oberkochen, Germany). The results showed that the use of 1keV Cs+ beam induces stacking faults while higher sputter beam energies results in γ→α transformation.
In context of CLUSTER project, impacts of impurities (SO2, NO2, O2, CO, H2S, H2, N2, Ar and H2O) in CO2 streams captured from different sources in a regional cluster on transport, injection and storage were investigated. Corrosion studies of oxidizing, reductive or mixed atmospheres towards transport pipeline steel X70 were carried out applying high pressure (10 MPa) at low temperatures (278 K or 313 K).
The fundamental impact of sulfur and water on corrosion rates and potential failure of the exposed material is well known. However, the access to the related corrosion mechanism causing material degradation is often a problem to solve. This study investigates the effect of SO2 and water vapor in the initial stages of corrosion of an Fe9Cr0.5Mn model alloy at 650 °C in situ. The analysis was carried out under laboratory conditions using energy-dispersive X-ray diffraction (EDXRD).
We investigated the effect of water vapor in the initial stages of SO2 corrosion of an Fe-9Cr-0.5Mn model alloy at 650 °C. Two separate experiments were run, one with 99.5%-Ar + 0.5%-SO2 and one with 69.5%-Ar + 0.5%-SO2 with 30%-H2O atmosphere. During the experiment the scale growth was observed in-situ, using energy dispersive X-ray diffraction (EDXRD). Our results confirm an increased speed of oxygen transport into the material, with the addition of water, while the transport of sulfur appears to be less affected.
In this work, the focus was set on the corrosion process of condensate as drops on the surface of carbon steels (X52, X70), martensitic steel UNS S41500, and superaustenite UNS 08031 in CO2 atmosphere with impurities at 278 K (to simulate the transportation condition in a buried pipeline). Exposure tests were performed at both normal pressure and high pressure where CO2 is supercritical or in dense phase. The drop, 1 ‑ 10 µL in volume, was prepared by dropping CO2 saturated ultra-pure water onto the surface of steel coupons in a one-liter-autoclave. The CO2 gas stream, simulating the oxyfuel flue gas with varying concentration of impurities (SO2 and O2), was then pumped into the autoclave to observe the condensation and corrosion impacts of impurities. Comparable exposure tests were carried out with the same gas mixture and the same volume of water as vapor to observe the drop formation and the corrosion process that follows. The wettability and stability of drops on the surface of steel coupons in CO2 supercritical/dense phase environment was evaluated additionally by contact angle measurement.