5 Werkstofftechnik
Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (6)
- Vortrag (4)
- Buchkapitel (1)
- Posterpräsentation (1)
- Forschungsdatensatz (1)
Referierte Publikation
- nein (13) (entfernen)
Schlagworte
- Ferritic-martensitic steels (3)
- Creep-fatigue (2)
- EBSD (2)
- Low Cycle Fatigue (2)
- P92 (2)
- Tempered Martensite Ferritic Steels (2)
- Thermo-Mechanical Fatigue (2)
- 9–12%Cr steel (1)
- AISI 316L (1)
- Creep (1)
Organisationseinheit der BAM
- 5 Werkstofftechnik (13) (entfernen)
Eingeladener Vortrag
- nein (4)
Results of an extended TMF test program on grade P92 steel in the temperature range of 620 ◦C–300 ◦C, comprising in-phase (IP) and out-of-phase (OP) tests, partly performed with symmetric dwells at Tmax/Tmin, are presented. In contrast to previous studies, the low-strain regime is also illuminated, which approaches flexible operation in a power plant with start/stop cycles. At all strain amplitudes, the material performance is characterized by continuous cyclic softening, which is retarded in tests at lower strains but reaches similar magnitudes in the course of testing. In the investigated temperature range, the phase angle does not affect fatigue life in continuous experiments, whereas the IP condition is more detrimental in tests with dwells. Fractographic analyses indicate creep-dominated and fatigue-dominated damage for IP and OP, respectively. Analyses of the (micro)hardness distribution in the tested specimens suggest an enhanced microstructural softening in tests with dwell times for the low- but not for the high-strain regime. To rationalize the obtained fatigue data, the fracturemechanics-based DTMF concept, which was developed for TMF life assessment of ductile alloys, was applied. It is found that the DTMF parameter correlates well with the measured fatigue lives, suggesting that subcritical growth of cracks (with sizes from a few microns to a few millimeters) governs failure in the investigated range of strain amplitudes.
In our current view, reference datasets in the MSE domain represent specific material properties, e.g., structural, mechanical, … characteristics. A reference dataset must fulfill high-quality standards, not only in precision of measurement but also in a comprehensive documentation of material, processing, and testing history (metadata). This Infrastructure Use Case (IUC) aims to develop a framework for generating reference material datasets using creep data of a single crystal Ni-based superalloy as a best practice example. In a community-driven process, we aim to encourage the discussion and establish a framework for the creation and distribution of reference material datasets. In this poster presentation, we highlight our current vision and activities and intend to stimulate the discussion about the topic reference datasets and future collaborations and work.
In nickelbasierten Superlegierungen, die für Gasturbinenschaufeln verwendet werden, sind bei hohen Betriebstemperaturen und -belastungen Kriechschäden, Ermüdung, Korrosion und Oxi-dation zu beobachten. Die betroffenen Turbinenschaufeln müssen ersetzt oder repariert werden, um Effizienzverluste und ein eventuelles Bauteilversagen zu vermeiden. In letzter Zeit wurden additive Fertigungs- und Lötverfahren für die Reparatur und das Fügen von Nickelbasiswerk-stoffen entwickelt, um die Einschränkungen der traditionellen Reparaturverfahren zu überwinden. Für eine auslegungsrelevante Bewertung des Risswachstumsverhaltens in den Fügezonen, die durch diese neuen Technologien erzeugt werden, sind Rissfortschrittsuntersuchungen erfor-derlich. Entsprechende Untersuchungen an gefügten Proben werden in diesem Beitrag vorge-stellt. Die Rissfortschrittsversuche werden an gefügten SEN-Proben (Single Edge Notch) bei einem Spannungsverhältnis von 0,1 und einer Temperatur von 950 °C durchgeführt. Das Riss-wachstum wird mit der DCPD-Methode (Direct Current Potential Drop) überwacht, und die ge-messenen Potenzialsignale werden anhand der optisch vermessenen Risslänge und einer Finite-Elemente-Analyse kalibriert. Der Spannungsintensitätsfaktor (SIF) für die gefügte SEN-Geometrie wird mit Hilfe von Finite-Elemente-Analysen berechnet. Auf diese Weise können Rissfortschrittskurven aus den experimentellen Daten abgeleitet werden.
Das hochaktuelle Thema der Integration und Wiederverwendung von Wissen und Daten aus Herstellung, Bearbeitung und Charakterisierung von Materialien ('Digitalisierung von Materialien') wird in den Projekten Innovationsplattform MaterialDigital (PMD, materialdigital.de) und Materials-open-Lab (Mat-o-Lab, matolab.org) adressiert. In diesem Beitrag werden die Weiterentwicklungen in diesen Projekten hinsichtlich der Speicherung von Zugversuchsdaten gemäß einer normenkonformen (DIN EN ISO 6892-1:2019-11) ontologischen Repräsentation vorgestellt. Das umfasst den Weg von der Entwicklung einer Ontologie nach Norm, der Konvertierung von Daten aus Standardtests in das interoperable RDF-Format bis hin zur Verknüpfung von Ontologie und Daten. Letztendlich können die entsprechenden Daten in einem Triple Store abgelegt und abgefragt werden.
The dataset contains experimental mechanical data from complex service-like creep-fatigue experiments performed isothermally at 620 °C and a low strain amplitude of 0.2 % on tempered martensite-ferritic grade P92 steel. The data sets in text file format provide cyclic deformation (min. and max. stresses) and the total (hysteresis) data of all recorded fatigue cycles for three different creep-fatigue experiments: 1) a standard relaxation fatigue (RF) test with symmetrical dwell times of three minutes introduced at minimum and maximum strain, 2) a fully strain-controlled service-like relaxation (SLR) test combining these three-minute peak strain dwells with a 30-minute dwell in between at zero strain, and 3) a partly stress-controlled service-like creep (SLC) test combining the three-minute peak strain dwells with 30-minute dwells at constant stress.
Further information on data and data acquisition, analysis, and experimental details are given in “Experimental Data from Service-Like Creep-Fatigue Experiments on Grade P92 Steel”, submitted to Data in Brief. Additional analyses of these datasets, as well as experimental findings and discussions are presented in “Creep-Fatigue of P92 in Service-Like Tests with Combined Stress- and Strain-Controlled Dwell Times”, submitted to International Journal of Fatigue.
Charakterisierung von Hochtemperaturwerkstoffen durch Zug- und Ermüdungsversuche an Kleinproben
(2019)
Die Verwendung von miniaturisierten Probengeometrien in der mechanischen Prüfung ermöglicht die Entnahme des Probenmaterials direkt aus kritischen Bereichen wie Fügeverbindungen und ermöglicht die Prüfung von kleinen Bauteilen wie additiv gefertigten Strukturen. In der vorliegenden Arbeit werden exemplarisch die Ergebnisse von vergleichenden Zug- und niederzyklischen Schwing-versuchen (LCF) an dem austenitischen Stahl AISI 316L und der Nickelbasislegierung IN718 vorgestellt. Die Prüfergebnisse der Kleinproben aus AISI 316L weisen die charakteristischen Eigenschaften des Werkstoffs auf, und die Analyse der Zug- und Ermüdungsdaten führt zu Werten, die den Literaturdaten weitgehend entsprechen. Der direkte Vergleich mit Standardprobendaten zeigt jedoch systematische Abweichungen bei Zugfestigkeit, Dehngrenze und Gleichmaßdehnung, die in diesem Beitrag diskutiert werden.
The current competitive situation on electricity markets forces power plants into cyclic operation regimes with frequent load shifts and starts/shutdowns. In the present work, the cyclic mechanical behavior of ferritic-martensitic 9-12 % Cr steels under isothermal and thermomechanical loading was investigated for the example of grade P92 material. A continuous softening was observed under all loading conditions. The introduction of hold periods to the applied cycles reduced material lifetime, with most prominent effects at technologically relevant small strain levels. The microstructural characterization reveals a coarsening of the original “martensitic” lath-type microstructure to a structure with polygonal subgrains and reduced dislocation density. The microstructural data forms the input for a physically-based modelling approach, both of which are presented in “Part 2: Microstructural Evolution during Cyclic Loading and its Representation in a Physically-based Micromechanical Model“.
The current competitive situation on electricity markets forces conventional power plants into cyclic operation regimes with frequent load shifts and starts/shutdowns. In the present work, the cyclic mechanical behavior of ferritic-martensitic 9-12 % Cr steels under isothermal and thermomechanical loading was investigated for the example of grade P92 material. A continuous softening was observed under all loading conditions. The introduction of hold periods to the applied cycles reduced material lifetime, with most prominent effects at technologically relevant small strain levels. The microstructural characterization reveals a coarsening of the original “martensitic” lath-type microstructure to a structure with polygonal subgrains and reduced dislocation density. The microstructural data forms the input for a physically-based modelling approach.
Cyclic mechanical performance and microstructure evolution of P92 under LCF and TMF conditions
(2019)
9-12% Cr ferritic-martensitic stainless steels are widely used as high temperature construction materials in fossil fueled power plants due to their excellent creep and oxidation resistance, but changes in electricity markets during the last two decades have considerably changed the typical working conditions of these facilities. The growing contribution of renewable energy sources in power generation forces most of these plants into flexible operation with frequent load shifts or shutdowns. These cyclic operation profiles constitute a major lifetime issue, raising the question which fundamental processes govern the reaction of ferritic-martensitic steels to cyclic load and temperature variations.
The present contribution reports on current findings obtained in a multidisciplinary project funded by German Ministry of Education and Research (BMBF) which combines cyclic mechanical and cyclic oxidation testing of different 9-12% Cr grades with detailed microstructural analyses and related micromechanical modeling.
In this contribution, an overview will be given on the results obtained in the mechanical testing programme of the project. Mechanical analyses were carried out on P91 and (mainly) P92 steel grades, particularly looking at softening phenomena and lifetimes obtained in isothermal cyclic loading (low cycle fatigue, LCF), non-isothermal cyclic loading (thermo-mechanical fatigue, TMF), and service-like combinations of fatigue and creep/relaxation periods. For this purpose, cylindrical specimens were extracted from thick-walled steam pipes, orthogonal to the pipe axis, and subjected to strain controlled cyclic loading (± 0.2 to ±0.5 % mechanical strain). Temperature intervals of TMF tests were chosen as either 300-620°C or 500-620°C, resembling so-called warm or hot start conditions of a power plant.
The test results will be presented and discussed with a focus on the impact of hold periods during testing (combined creep/relaxation-fatigue conditions) on mechanical softening, lifetime and formation of cracks. The findings will be complemented by results on the modification of the hierarchical ferritic-martensitic microstructure under different loading scenarios.
The current competitive situation on electricity markets forces power plants into cyclic operation regimes with frequent load shifts and starts/shutdowns. In the present work, the cyclic mechanical behavior of ferritic-martensitic 9-12 % Cr steels under isothermal and thermomechanical loading was investigated for the example of grade P92 material. A continuous softening was observed under all loading conditions. The introduction of hold periods to the applied cycles reduced material lifetime, with most prominent effects at technologically relevant small strain levels. The microstructural characterization reveals a coarsening of the original “martensitic” lath-type microstructure to a structure with polygonal subgrains and reduced dislocation density. The microstructural data forms the input for a physically-based modelling approach.
9-12% Cr ferritic-martensitic stainless steels are widely used as high temperature construction materials in power plants due to their excellent creep and oxidation resistance. The growing share of renewable energy sources in power generation forces many of these plants into more flexible operation with frequent load shifts or shutdowns. These cyclic operation profiles constitute a major lifetime issue.
The present contribution reports on current findings obtained in a multidisciplinary project which combines cyclic mechanical and cyclic oxidation testing with detailed microstructural analyses. Mechanical analyses are carried out on P92 and P91 steel grades to give an overview of softening phenomena and lifetimes obtained in isothermal cyclic loading (low cycle fatigue, LCF), non-isothermal cyclic loading (thermo-mechanical fatigue, TMF), and service-like combinations of creep and fatigue periods (creep-fatigue interaction).
Oxidation testing focuses on the grades P92 and VM12 with the intention of clarifying the impact of frequent passes through intermediate temperature levels on the kinetics of steam-side oxidation and the characteristics of the evolving oxide scales. An attempt is made to evaluate their composition, strength, integrity and adhesion after up to 250 temperature cycles. Flat coupons as well as curved tube sections are tested to assess the mutual influence of geometry on oxide scale integrity.
Complementary microstructural investigations by scanning and transmission electron microscopy plus EBSD are used for phase identification and substrate/oxide interface characterisation. The evolutions of grain size and dislocation density under different test conditions are quantified.
9-12% Cr ferritic-martensitic stainless steels are widely used as high temperature construction materials in power plants due to their excellent creep and oxidation resistance. The growing share of renewable energy sources in power generation forces many of these plants into more flexible operation with frequent load shifts or shutdowns. These cyclic operation profiles constitute a major lifetime issue. The present contribution reports on current findings obtained in a multidisciplinary project which combines cyclic mechanical and cyclic oxidation testing of different 9-12% Cr grades with detailed microstructural analyses.
Mechanical analyses are carried out on P92 and P91 steel grades to give an overview of softening phenomena and lifetimes obtained in isothermal cyclic loading (low cycle fatigue, LCF), non-isothermal cyclic loading (thermo-mechanical fatigue, TMF), and service-like combinations of creep and fatigue periods.
Complementary microstructural investigations by scanning and transmission electron microscopy plus EBSD are used for phase identification, substrate/oxide interface characterization and quantification of the microstructure evolution under cyclic conditions.
Performing mechanical tests at high temperatures is a nontrivial issue: Compared to room temperature testing, additional phenomena like time-dependent Deformation processes and oxidation effects raise the complexity of the material’s response, while more sophisticated test setups and additional control parameters increase the number of potential sources of error. To a large extent, these complications can be overcome by carefully following all recommendations given in the respective high temperature testing standards, but more comprehensive background information helps to identify points of specific importance in particular test campaigns. In this chapter, an overview is given on general high temperature testing issues like the appropriate choice of experimental equipment and key aspects of temperature measurement. In subsequent sections, the major static and dynamic high temperature test methods are reviewed and their Special features, as compared to testing at room temperature, are highlighted based on example data sets. Influences of specimen size and environmental effects are shortly outlined in a concluding section. In the whole chapter, a focus is set on testing of “classical” metallic high temperature materials, but many considerations are equally valid for testing of intermetallics, composites, and high temperature ceramics.