5 Werkstofftechnik
Filtern
Dokumenttyp
- Zeitschriftenartikel (12)
- Vortrag (9)
- Buchkapitel (1)
Schlagworte
- Oxidation (7)
- High temperature corrosion (6)
- Diffraction (5)
- Corrosion (4)
- In situ (4)
- Sulfidation (4)
- Iron (3)
- SEM (3)
- SIMS (3)
- Spectroscopy (3)
- High entropy alloys (2)
- High temperature (2)
- Steel (2)
- Sulphidation (2)
- X-ray absorption spectroscopy (2)
- XANES (2)
- XRD (2)
- Chalcogenides (1)
- Copper vacancies (1)
- CrCoNi (1)
- CrMnFeCoNi (1)
- EDXRD (1)
- Early oxidation (1)
- Early stages (1)
- Early sulfidation (1)
- FIB Tomography (1)
- Ferritic Alloys (1)
- Ferritic steels (1)
- Grain Boundary Corrosion (1)
- Heißgaskorrosion (1)
- High Entropy Alloys (1)
- High Temperature Corrosion (1)
- High temperature oxidation (1)
- High-temperature corrosion (1)
- High‐temperature corrosion (1)
- Hochentropielegierungen (1)
- In situ diffraction (1)
- In-situ (1)
- Internal Sulfidation (1)
- KCl (1)
- Medium Entropy Alloys (1)
- Medium entropy alloys (1)
- Microstructure (1)
- Mixed conductors (1)
- Mn-oxides (1)
- Neutron diffraction (1)
- Oxides (1)
- Powder diffraction (1)
- SO2 (1)
- Steel alloy (1)
- TEM (1)
Organisationseinheit der BAM
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (9)
Comprehensive insights into the early stages of corrosion mechanisms provide fundamental knowledge to further understand and model long time material behaviour. The present work studies the early stages of combined oxidation and sulphidation of ferritic model alloys for time scales up to 250 h at 650 °C to observe the influence of chromium during the corrosion under SO2. Model alloys were used to focus on the reaction of the intended elements: Fe, Cr, S, and O. Pure iron simultaneously forms magnetite and iron sulphide in an early stage of corrosion, covered by a pure oxide layer after 100 h. Iron with 13 wt% Cr shows hematite and mixed Fe-Cr-oxides first, before sulphides nucleate in the inner corrosion zone. With increasing ageing time a magnetite layer is observed below the hematite layer. Quantitative phase fractions of all corrosion products observed were determined from cross section images. Characterization of the Fe13Cr corrosion scale by FIB revealed a highly porous structure in the inner corrosion zone where Cr-rich (Fe, Cr)-sulphides are present, and caused the scale to spall easily.
Metal sulfide grain boundary precipitates of a ferrous model alloy with 13 wt.% chromium formed at 650°C under a gas atmosphere containing 0.5% SO2 and 99.5% Ar were investigated after ageing for 3 h, 6 h, and 12 h. The precipitates formed along grain boundaries were identified as Cr5S6 using energy-dispersive x-ray spectroscopy in transmission electron microscopy and electron backscatter diffraction analysis. Serial focused ion beam slicing was conducted followed by three-dimensional reconstruction to determine the number, size, and penetration depth of the precipitates evolved at the different time steps. There was a linear increase in the number of precipitates with time, while their average size increased only for the initial aging time but became constant after 6 h. Based on these results, a model for grain boundary sulfidation of ferritic alloys is discussed.
Insights into early damage mechanisms during high-temperature gas corrosion provide important aspects for the prediction of the long-term stability of hightemperature materials exposed to a hot and corrosive environment. The current work presents a real time study concerning the combined oxidation and sulfidation of ferritic model alloys in a hot SO2 containing atmosphere using energy dispersive X-ray diffraction. The applied high temperature reactor allows the transmittance of high energetic X-rays in order to collect X-ray diffraction pattern of the sample surface in situ during the reaction with the reactive environment. The results revealed that the first phases crystallizing on iron with 2 wt% chromium and with 9 wt% chromium are oxides. The aging experiments at T = 650° C with 0.5% SO2 and 99.5% Ar were followed in situ and caused an external mixed oxide-sulfide layer on top of iron with 2 wt% chromium. On the higher alloyed material the external scale consists of iron oxides and the inner scale of mixed (Fe,Cr)-oxides and chromium-sulfides. The oxide content continuously increases parallel to an increase of the sulfide amount. Thus, the initially formed (Fe,Cr)-oxides do not have a protective character and support the transport of sulfur through the growing oxide scale.
Ferritic high temperature alloys are widely used as boiler tube and heat exchanger materials in coal, biomass and co-fired power plants. All technologies have in common that the applied materials are exposed to different temperatures, process pressures and reactive atmospheres that lead to a change of the material properties and a further degradation of the material. Material changes caused by aging in highly corrosive and toxic gases such as SO2 are mainly studied ex situ after the reaction is finished. The solid material is deposited in the atmosphere for a certain period of time, and material changes are then examined by various microscopic techniques such as optical microscopy (OM), electron microprobe analysis (EMPA), scanning electron microscopy (SEM and TEM) and X-ray diffraction (XRD). Nevertheless, extensive efforts were made to study material changes of high temperature alloys under oxidizing and reducing atmospheres by environmental scanning electron microscopy or in situ TEM techniques However, the possibilities of microscopic in situ techniques are very limited for the use of highly corrosive and toxic gases such as SO2. Since Sulfur induced corrosion at temperatures relevant for coal and biomass fired power plants, which is causing breakaway oxidation and sulfide precipitation at grain boundaries, is still of scientific interest, the current work focuses on the effect of SO2 in an initial stage of corrosion of ferritic alloys. For the analysis of early stages of combined oxidation and sulphidation processes of Fe-Cr model alloys the usage of a light furnace to conduct a rapid reactive annealing experiment is feasible. Previous studies presented distinct results of the influence of chromium on early high temperature corrosion by SO2 by this technique and subsequent classical metallographic analyses. However, it is still not possible to trace the corrosion mechanism in real time by conducting single aging experiments. The current work introduces two different approaches to study the initial stages of high temperature oxidation processes by applying above state of the art X-ray diffraction and spectroscopy methods. One part focuses on the real time observation of the formation of corrosion products such as oxides and sulfides by energy dispersive X-ray diffraction (EDXRD). The potential of this technique to study crystallization and growth processes of thin films in a reactive environment in real time was previously shown for different compound semiconductors. This approach was now applied to follow oxidation and sulphidation processes of ferritic model alloys in SO2 and SO2/H2O environments. The diffraction signals of the X-rays were detected during the corrosion process and the peak area and positions were analyzed as a function of time. This procedure enables monitoring external oxide growth and material loss in real time in an early stage of corrosion.
The other part of the current work presents the possibilities of X-ray absorption near edge structure spectroscopy (XANES) to characterize oxide scales and their growth mechanisms. Precise phase identification and quantification of corrosion products in a multi-phase oxide/sulfide scale is a pre-requisite to understand diffusion paths of metal ions and gas components. It is a challenging task to distinguish structurally similar reaction products such as Fe3O4 and FeCr2O4 especially in thin films with texture effects by diffraction. To illustrate for example Cr-out diffusion of an alloy throughout an inner and external oxide scale the differentiation of Fe3O4 and FeCr2O4 is indispensable. XANES uses the photoionization effect at the metal absorption edge in an aging product and accesses by this structural and chemical information. The current work uses XANES at the Fe-K and Cr-K absorption edge to identify various aging products grown as thin layers on alloys after short time aging experiments. A reaction chamber for combining high temperature oxidation experiments with surface sensitive X-ray absorption near edge structure spectroscopy will be introduced and first results of XANES on scales at high temperatures will be presented.
Ferritic-martensitic alloys with 12-16 % Cr in weight are subject to devices for various energy systems, such as coal power plants and waste incineration plants. These materials are exposed to a highly corrosive environment which lead to a degradation of the material. Especially the simultaneous oxidation and sulfidation is thereby of special interest. Proper spatially resolved measurements that determine not only chemical compositions but phases are rare. However, precise phase identification and quantification of corrosion products within the multi-phase corrosion scales is a key aspect to understand diffusion paths of metal ions and gas ions/molecules. This study investigated Fe-Cr model alloys with Cr contents from 0 to 13 % in weight in 0.5 % SO2 and 99.5 % Ar atmosphere to aim in a fundamental and systematic analysis. Samples were aged at 650 °C for time scales from 12 h to 250 h. The results presented here correspond to depth dependent phase identification of oxide and sulphide phases in the corrosion scales by using X-ray absorption near edge spectroscopy (XANES). Per sample a series of ca. 20 spots (1-5 µm spot size) from scale-gas to scale-metal interface were measured. XANES spectroscopy was performed at the Fe-K edge (7.11 keV) on polished cross sections. The collected spectra were fitted to a combination of reference materials to quantify the present phases at different positions within the scale.The phase distribution differs with Cr content and the Cr diffusion through pure Fe-oxide and mixed Fe-Cr-oxide phases is discussed.
Konventionelle und innovative Hochtemperaturwerkstoffe sind im technischen Betrieb einer Vielzahl an Belastungen ausgesetzt. Neben mechanischen Beanspruchungen stellt die chemische Belastung durch das Vorhandensein von aggressiven und korrosiven Medien (SO2, CO2, O2, H2O…) bei hoher Temperatur einen Schlüsselfaktor dar, der die Langlebigkeit der Materialien im Einsatz beeinflusst. Neben konventionellen, mikroskopischen Analyseverfahren bieten röntgenbasierte Techniken Möglichkeiten, die Grenzflächenreaktionen zwischen dem Werkstoff und den Medien während der chemischen Belastung (in situ) zu untersuchen. Neuartige Einblicke in die zugrunde liegenden Prozesse der Schädigungsmechanismen werden anhand von klassischen ferritischen Legierungen beschrieben. Das Verständnis von Schlüsselfaktoren zur Induzierung eines Schutzmechanismus ist insbesondere für die Entwicklung von neuartigen Materialklassen wie Hochentropie- und chemisch komplexe Legierungen notwendig. Erste Einblicke in Schädigungsmechanismen durch Gaskorrosion dieser innovativen Materialsysteme werden vorgestellt.
The prediction of structural parameters and optoelectronic properties of compound semiconductors is very important. However, calculations often neglect chemical variability and structural defects. In chalcopyrite type semiconductors one of the major defects are copper vacancies (V Cu). The four cation neighbors of the anion determine its position in the chalcopyrite type structure expressed by the Wyckoff position 8d (x, 1/4, 1/8). Intrinsic point defects like V
Cu and anti-sites may cause variations of the Anion position in the middle of the cation tetrahedron, especially in the Anion position Parameter x. For stoichiometric chalcopyrite type compounds a formalism according to the principle of conservation of tetrahedral bonds (CTB) can be applied to calculate the anion position parameter, but it fails in the case of off-stoichiometric chalcopyrites. This case study of chalcopyrite type CuGaS 2 and Mn-substituted GuGaS 2
shows that the experimentally determined anion position Parameter x
deviate from values calculated by CTB approach. The systematic investigation of off-stoichiometric CuGaS 2 and Mn-substituted GuGaS
2 demonstrates the effect of copper vacancies on the average radii of the cation sites (Wyckoff positions 4a and 4b) as well as on the anion position Parameter x. By applying an elaborated CTB Approach implementing copper vacancies an agreement between experimental and calculated anion position Parameter x can be obtained.
Real-time observation of high- temperature gas corrosion in dry and wet SO2-containing atmosphere
(2019)
Sulfur and water have a fundamental impact on the corrosion rate and potential failure of materials. It is therefore necessary to understand the mechanisms, rates, and potential means of transport, as well as the reactions of these elements with an alloy. This paper investigates the effect of water vapor in the initial stages of SO2 corrosion of an Fe-9Cr-0.5Mn model alloy at 650°C in situ under laboratory conditions using energy-dispersive x-ray diffraction analysis. Two separate experiments were run, one with a 99.5% Ar + 0.5% SO2 atmosphere and one with a 69.5% Ar + 0.5% SO2 + 30% H2O atmosphere. With a wet atmosphere, the alloy formed a scale with decreasing oxygen content towards the scale–alloy interface. Sulfides were identified above and below a (Fe, Cr)3O4 layer in the inner corrosion zone. In contrast to this, the overall scale growth was slower in a dry SO2 atmosphere.
The precise analysis of cation diffusion profiles through corrosion scales is an important aspect to evaluate corrosion phenomena under multicomponent chemical load, as during high‐temperature corrosion under deposits and salts. The present study shows a comprehensive analysis of cation diffusion profiles by electron microprobe analysis and microbeam X‐ray absorption near edge structure (µ‐XANES) spectroscopy in mixed oxide/sulfide scales grown on Fe–Cr model alloys after exposing them to 0.5% SO2. The results presented here correspond to depth‐dependent phase identification of oxides and sulfides in the corrosion scales by µ‐XANES and the description of oxidation‐state‐dependent diffusion profiles. Scales grown on low‐ and high‐alloyed materials show both a well‐pronounced diffusion profile with a high concentration of Fe3+ at the gas and a high concentration of Fe2+ at the alloy interface. The distribution of the cations within a close‐packed oxide lattice is strongly influencing the lattice diffusion phenomena due to their different oxidation states and therefore different crystal‐field preference energies. This issue is discussed based on the results obtained by µ‐XANES analysis.