The multi-phase approach has proven to widen the application properties of high entropy alloys. After a decade of testing different alloys in the Al-Co-Cr-Cu-Fe-Ni-Ti family the Al10Co25Cr8Fe15Ni36Ti6 was found to be a solid base for more fine-tuned microstructural optimization. Following the example of superalloys, the Al10Co25Cr8Fe15Ni36Ti6 alloy aims for a γ/γ' microstructures in order to guarantee a good microstructural stability at high temperatures. The shape and volume fraction of the γ' particles is known to influence the mechanical properties of superalloys, and they do so in the high entropy family as well [1]. Shape, misfit and creep properties of several modified versions of the Al10Co25Cr8Fe15Ni36Ti6 alloy are compared and discussed in this talk.
Trace elements W and Hf have different influence on the microstructure and the mechanical properties when added to the Al10Co25Cr8Fe15Ni36Ti6 compositionally complex alloy. The addition of both can thus merge both element’s beneficial influences when combined with the appropriate heat treatment: Hf enhances the cubicity of the γ’ particles in the γ matrix while the W reduces the negative influence of the Heusler phase: this phase can be completely dissolved when W is present in the alloy.
The high-temperature corrosion behaviors of the equimolar CrCoNi medium- and CrMnFeCoNi high-entropy alloy were studied in a gas atmosphere consisting of a volumetric mixture of 10% H2O, 2% O2, 0.5% SO2, and 87.5% Ar at 800 °C for up to 96 h. Both alloys were initially single-phase fcc structured and showed a mean grain size of ~50 µm and a homogeneous chemical composition. The oxide layer thickness of the Cantor alloy CrMnFeCoNi increased linearly with exposure time while it remained constant at ~1 µm for CrCoNi. A Cr2O3 layer and minor amounts of (Co,Ni)Cr2O4 developed on CrCoNi while three layers were detected on the Cantor alloy. These layers were a thin and continuous chromium rich oxide layer at the oxide/alloy interface, a dense (Mn,Cr)3O4 layer in the center and a thick and porous layer of Mn3O4 and MnSO4 at the gas/oxide interface. Additionally, a few metal sulfides were observed in the CrMnFeCoNi matrix. These results were found to be in reasonable agreement with thermodynamic calculations.
A new race for high performance structural materials has started since the discovery of high entropy alloys at the beginning of the 21st century. The possible combination of several elements in an, until then, unknown composition space opened the ground for discovering new materials. Solid solution strengthening remains the most prominent mechanisms that is active in this family of materials, but it is supported by all other strengthening mechanism on the path to better and better performing materials. Chemical, thermal and mechanical approaches are combined to optimize these alloys. Optimum performances can be reached by using a high number of different strengthening mechanisms, induced both by composition and processing. The most prominent with composition induced mechanism is precipitation hardening, and on the processing side it is cold working such as cold-rolling, torsion or extrusion. The contribution uses tensile test data at room temperature solely for comparison – high temperature and cryogenic data are omitted because it would lead beyond the scope of this manuscript.
The main deference between high entropy alloys and conventional alloys is the solid solution strengthening effect, which moves from a single element to a multi-element matrix. Little is known about the effectiveness of this effect at high temperatures. Investigation of temperature dependent solid solution strengthening in single phase multicomponent alloys with medium and high entropy using creep testing was performed. Creep tests carried out on single phase SX CrCoNi , CrMnFeCoNi and pure Ni from 700 to 1200 °C excluding oxidation, grain boundaries and multiphase effects. It was found that the influence of solid solution strengthening of CrCoNi and CrMnFeCoNi increases by decreasing temperature (1200 to 700 °C), and dislocation forests occur in CrCoNi and CrMnFeCoNi in comparison to pure Ni.
The discovery of the high entropy concept at the beginning of the 3rd millennium lead to a worldwide increase in metallurgical research, as the possible element combinations seemed nearly endless and the range of applications wide. In the early years of research, one of the main goals was the discovery of a single-phase high entropy alloy. As research evolved, it was found that properties could be enhanced by opening the HE-concept towards multiphase alloys, and from the wide area of possibilities our group chose a tuning of the properties towards high temperature application.
Compositionally complex Al10Co25Cr8Fe15Ni36Ti6 alloy, which is single-phase at high temperature, around 1200°C, shows a three phase morphology at intermediate temperatures, around 800°C. A high temperature homogenization procedure has to be applied in order to decrease the segregation induced by the dendritic growth. Subsequent annealing promotes the formation of the strengthening γ' precipitates. The alloy shows a positive lattice misfit between the γ and the γ' phase, which can be an indicator for good creep properties.
The microstructure can be optimized by adding trace elements such as Mo and Hf, known as γ and γ' strengtheners in Ni-based superalloys, respectively. Atom probe measurements show that Mo segregates into the γ matrix, and Hf prefers the γ' precipitates, where it increases the lattice parameter and thus also the lattice misfit, by about 50%. The alloy family shows interesting mechanical properties, especially the Al9.5Co25Cr8Fe15Ni36Ti6Hf0,5 alloy – its tensile properties are better than those of commercial Alloy 800H and IN617 at temperatures up to 700°C.