5 Werkstofftechnik
Filtern
Dokumenttyp
- Posterpräsentation (94) (entfernen)
Sprache
- Englisch (94) (entfernen)
Referierte Publikation
- nein (94)
Schlagworte
- Glass (6)
- Additive manufacturing (5)
- Degradation (5)
- Microstructure (5)
- Additive Manufacturing (4)
- Coarsening (4)
- Corrosion (4)
- Crack growth (4)
- Creep (4)
- FAIR (4)
- Transmission electron microscopy (4)
- 316L (3)
- Ab-initio (3)
- Alloy 2618A (3)
- Fatigue (3)
- Hydrogen (3)
- NTE (3)
- Nanoparticles (3)
- Soda-lime silicate glass (3)
- Sol-gel (3)
- Solid-state (3)
- TDEP (3)
- VSSA (3)
- Vickers (3)
- Crack Propagation (2)
- Crystal orientation (2)
- Crystallization (2)
- DCB (2)
- Dark-field transmission electron microscopy (DFTEM) (2)
- Depth-profiling (2)
- Deuterium (2)
- Electron beam induced modification (2)
- Electron microscopy (2)
- Environmental stress cracking (ESC) (2)
- FIB (2)
- GD-OES (2)
- Gold nanoparticles (2)
- High temperature corrosion (2)
- Imaging techniques (2)
- Inconel 686 (2)
- Iron oxide nanoparticles (2)
- LTCC (2)
- Lithium Ion Batteries (2)
- Low Cycle Fatigue (2)
- Machine Learning (2)
- Metadata schema (2)
- NFDI (2)
- Ontology (2)
- Oxidation (2)
- Polymer (2)
- Reference data (2)
- Referenzdaten (2)
- Sample preparation (2)
- Sandwich (2)
- Selective laser melting (2)
- Semantic Web Technologies (2)
- Sintering (2)
- Syngle Crystal alloy (2)
- Ti-6Al-4V (2)
- ToF-SIMS (2)
- Water content (2)
- Water speciation (2)
- 3D imaging (1)
- 5G (1)
- AFM (1)
- AISI 304L (1)
- AM (1)
- Aggressive environement (1)
- Aggressive environment (1)
- Aging mechanisms (1)
- Al-Cu-Li alloys (1)
- Alkali ions (1)
- Aluminium (1)
- Analysis (1)
- Anhydrite (1)
- Anisotropy (1)
- Artefact (1)
- Atacama Desert (1)
- Atmospheric Plasma Spraying (1)
- Atomic packing factor (1)
- Atomization (1)
- Austenitic stainless steel (1)
- Austenitic steel (1)
- Automation (1)
- BTS (1)
- Bio Ceramics (1)
- Bioactive glass (1)
- Biofilm (1)
- Bioresorbable (1)
- Borate glasses (1)
- Brittle / ductile fracture behavior (1)
- Brittle fracture (1)
- CALPHAD (1)
- CALPHAD databases analysis (1)
- CCS (1)
- Calcium cobaltite (1)
- Carbon Fiber Reinforced Plastics (1)
- Carbon capture (1)
- Carbon dioxide (1)
- Ceramic (1)
- Chemically Complex Alloy (1)
- Chromium oxide (1)
- Co-axial monitoring (1)
- Complex concentrated alloy (CCA) (1)
- Composite (1)
- Computed Tomography (1)
- Corrosion resistance (1)
- Crack evolution (1)
- Crack healing (1)
- Crack propagation analysis (1)
- Crystal plasticity (1)
- DED-L (1)
- Dark-field transmission electron microscopy (1)
- Data Interoperability (1)
- Data fusion (1)
- Density (1)
- Destabilization (1)
- Dielectric Spectroscopy (1)
- Diffraction Enhanced Imaging (1)
- Diffusion coefficient (1)
- Digital material representation (1)
- Digitalization (1)
- Diopside (1)
- Distributed fiber optic sensors (1)
- EBSD (1)
- EDX (1)
- Electromicroscopy (1)
- Electron Backscatter Diffraction (1)
- Environmental stress cracking (1)
- FeCr- alloys (1)
- Film depositition (1)
- Focussed ion beam growth (1)
- Fracture Toughness (1)
- Fracture surface analysis (1)
- Fresnoit (1)
- Full Notch Creep Test (1)
- Full Notch Creep Test (FNCT) (1)
- Full-Notch Creep Test (FNCT) (1)
- GFRP (1)
- Glas (1)
- Glass ceramic (1)
- Glass composition (1)
- Glass fiber reinforced polymers (1)
- Glass matrix composite (1)
- Glass melt (1)
- Glass structure (1)
- Glass transformation temperature (1)
- Glass-ceramic (1)
- Gypsum (1)
- HV-Insulation (1)
- Hardness (1)
- Heat Treatment (1)
- High Cycle Fatigue (1)
- High Temperature Testing (1)
- High Voltage Insulation (1)
- High entropy alloy (1)
- High temperature (1)
- High-density polyethylene (1)
- High-entropy alloys (1)
- High-temperature corrosion (1)
- Hot stage microscopy (1)
- Hydrogen permeability (1)
- IR (1)
- In situ (1)
- In situ tensile test (1)
- In-situ tomography (1)
- In718 (1)
- Internal friction (1)
- Knowledge Representation (1)
- LMD (1)
- LTCC multilayer (1)
- Laser Beam Melting (1)
- Laser Cladding (1)
- Laser Powder Bed Fusion (1)
- Laser ablation in liquid (1)
- Laser cladding (1)
- Lightweight materials (1)
- Lithium-ion batteries (1)
- Local landscape evolution (1)
- Long-term behavior (1)
- Low cycle fatigue (1)
- Manganese oxide (1)
- Material characterization (1)
- Material oxidation (1)
- Mechanical Behavior (1)
- Metal powder characterization (1)
- Metal seal (1)
- Metformin (1)
- Metrology (1)
- Micro computed tomography (1)
- Micromanipulation (1)
- Microplastics (1)
- Microstructure analysis (1)
- Modeling (1)
- NFDI-MatWerk (1)
- NMR (1)
- Nano-landscape (1)
- Nano-powder characterization (1)
- Nanomaterial screening (1)
- Optical criterion (1)
- Orientation (1)
- Orientation-dependent microstructure (1)
- Oxide Glasses (1)
- Oxidglas (1)
- PE-HD (1)
- PMD Core Ontology (1)
- PMDco (1)
- Particle size (1)
- Photocatalysis (1)
- Plattform MaterialDigital (1)
- Polyethylene, PE-HD (1)
- Polymer-Ceramic-Composite (1)
- Porosity (1)
- Precipitation (1)
- Process Monitoring (1)
- Property simulation (1)
- Reference Data (1)
- Reference Dataset (1)
- Reference material (1)
- Reference nanomaterials (1)
- Reliable characterization (1)
- Research Data Management (1)
- Residual stress (1)
- Risswachstum (1)
- Robot-assisted galss melting (1)
- Robotische Glasschmelzanlage (1)
- S-phase (1)
- SEM (1)
- SIMS (1)
- SLM (1)
- Salt melt (1)
- Scale-bridging (1)
- Scanning electron microscopy (SEM) (1)
- Scarf joint repairs (1)
- Semantic Interoperability (1)
- Silver (1)
- Silver glass paste (1)
- Silver nanoparticle (1)
- Size and size distribution (1)
- Slurry (1)
- Small angle x-ray scattering (1)
- Sodium zinc borate glass (1)
- Sodiumborosilicate glasses (1)
- Soil sample (1)
- Starch (1)
- Starch nanoparticle (1)
- Sulfidation (1)
- Sulfiding (1)
- Surface Energy (1)
- Surface crystallization (1)
- Surface energy (1)
- Synchrotron Tomography (1)
- Synchrotron tomography (1)
- Synthetic air (1)
- TED-GC-MS (1)
- TEM (1)
- Tensile Properties (1)
- Thermal Spray (1)
- Thermodynamic analysis (1)
- Thermoelectric generator design (1)
- Thermoelectric oxides (1)
- Thermomechanics (1)
- Titanium (1)
- Titanium oxide (1)
- Transmission electron microscope (TEM) (1)
- Ultrasound (1)
- VM12 SHC (1)
- Vickers indentation (1)
- Virtual experiments (1)
- Viscosity (1)
- Wind turbine blade shells (1)
- Wind turbine blades (1)
- X-Ray Diffraction (1)
- X-ray refraction (1)
- XRD (1)
- Young´s Modulus (1)
Organisationseinheit der BAM
- 5 Werkstofftechnik (94)
- 5.1 Mikrostruktur Design und Degradation (27)
- 5.4 Multimateriale Fertigungsprozesse (20)
- 5.6 Glas (20)
- 5.2 Metallische Hochtemperaturwerkstoffe (16)
- 6 Materialchemie (15)
- 5.3 Polymere Verbundwerkstoffe (10)
- 6.1 Oberflächen- und Dünnschichtanalyse (9)
- 8 Zerstörungsfreie Prüfung (9)
- 8.5 Röntgenbildgebung (8)
Despite of the significant advances in additive manufacturing (AM) process optimization there is still a lack of experimental results and understanding regarding the mechanical behavior and its relationship with the microstructural features of AM-parts, especially in loading conditions typical for safety-relevant applications. Within the scope of the presented ongoing investigations, a basic microstructural characterization, tensile tests at room and elevated temperature (400°C) as well as a characterization of the fatigue behavior of additively manufactured Ti-6Al-4V in the low cycle fatigue regime are carried out in the as-built state. After failure, different techniques are used to describe the failure mechanisms of the specimens. The AM-Specimens are provided by the Fraunhofer institute for production systems and design technology and investigated at the BAM following the philosophy of the TF-Project AGIL.
Within the perspective of increasing reliability of AM processes, real-time monitoring allows part inspection while it is built and simultaneous defect detection. Further developments of real-time monitoring can also bring to self-regulating process controls. Key points to reach such a goal are the extensive research and knowledge of correlations between sensor signals and their causes in the process.
This poster presents the focused ion beam preparation methodologies developed within the framework of the EU funded EURAMET project ADVENT (Advanced Energy-Saving Technology).
It summarises the key breakthroughs achieved for various in situ investigation techniques, e.g. in situ experiments at the Synchrotron facility BESSY II (IR-SNOM and XRS), TEM and SMM instrumentation.
The created experimental devices from diverse thin-film semiconductor materials paved the way to dynamic structural studies bearing the potential to determine nanoscale correlations between strain and electric fields and, moreover, for the fundamental development of new in situ capabilities.
The PMD Core Ontology (PMDco) is a comprehensive set of building blocks produced via consensus building. The ontological building blocks provide a framework representing knowledge about fundamental concepts used in Materials Science and Engineering (MSE) today. The PMDco is a mid-level ontology that establishes connections between narrower MSE application ontologies and domain neutral concepts used in already established broader (top-level) ontologies. The primary goal of the PMDco design is to enable interoperability between various other MSE-related ontologies and other common ontologies.
PMDco’s class structure is both comprehensive and extensible, rendering it an efficient tool to structure MSE knowledge. The PMDco serves as a semantic middle-layer unifying common MSE concepts via semantic mapping to other semantic representations using well-known key terms used in the MSE domain. The PMDco enables straight-forward documentation and tracking of science data generation and in consequence enables high-quality FAIR data that allows for precise reproducibility of scientific experiments.
The design of PMDco is based on the W3C Provenance Ontology (PROV-O), which provides a standard framework for capturing the production, derivation, and attribution of resources. Via this foundation, the PMDco enables the integration of data from various data origins and the representation of complex workflows.
In summary, the PMDco is a valuable advancement for researchers and practitioners in MSE domains. It provides a common MSE vocabulary to represent and share knowledge, allowing for efficient collaboration and promoting interoperability between diverse domains. Its design allows for the systematic integration of data and metadata, enabling seamless tracing of science data. Overall, the PMDco is a crucial step towards a unified and comprehensive understanding of the MSE domain in general.
Sintered bioactive glass scaffolds of defined shape and porosity, e.g. made via additive manufacturing, must provide sufficient bioactivity and sinterability. As higher bioactivity is often linked to high corrosion and crystallization tendency, a certain compromise between sintering ability and bioactivity is therefore required. Groh et al. developed a fluoride-containing bioactive glass (F3), which allows fiber drawing and shows a bioactivity well comparable to that of Bioglass®45S5.
To study whether and to what extent the sinterability of F3 glass powder is controlled by particle size, coarse and fine F3 glass powders (300-310µm and 0-32µm) were prepared by crushing, sieving and milling. Sintering, degassing and phase transformation during heating were studied with heating microscopy, vacuum hot extraction (VHE), DTA, XRD, and SEM.
For the coarse glass powder, sintering proceeds slowly and is limited by surface crystallization of primary Na2CaSi2O6 crystals. Although the crystallization onset of Na2CaSi2O6 is shifted to lower temperature, full densification is attained for the fine powder. This finding indicate that certain porosity might be tuned via particle size variation. Above 900°C, intensive foaming is evident for the fine powder. VHE studies revealed that carbon species are the main foaming source.
Crack healing in glass ceramic solid oxide fuel cell (SOFC) sealants is of utmost importance as cracks caused by thermal cycling remain a bottleneck in developing durable SOFC. Whereas no or low crystal volume fraction seems most favorable for viscous crack healing, it does not for load bearing and undesired diffusion. On the other hand, crystals or filler particles can make the sealant less prone to these disadvantages but it could increase the effective composite viscosity and retard crack healing.
Against this background, the influence of crystal volume fraction, phi, on viscous crack healing in glass matrix composites prepared from soda lime silicate glass and zirconia filler particles was studied. Vickers indention induced radial cracks were healed isothermally during interrupted annealing steps and monitored with optical microscopy. Due to the slow crystallization of the glass under study, phi could be kept constant during crack healing.
For bulk glass samples (phi = =), the decrease in radial crack length was retarded by an initial increase in crack width due to crack rounding. Up to phi = 0.15 the increase in effective viscosity retarded this crack broadening thereby yielding faster crack healing. For phi > 0.15, crack broadening was progressively suppressed but the same was true for crack healing, which was fully prevented above phi = 0.3. Results indicate that optimum micro structures can prevent crack broadening limited by the global effective composite viscosity and this way promote crack healing limited by local glass viscosity.
Influence of deposition hatch length on residual stress in selective laser melted Inconel 718
(2018)
The present study aims to evaluate the bulk residual stresses in SLM parts by using neutron diffraction measurements performed at E3 line -BER II neutron reactor- of Helmholtz-Zentrum für Materialien und Energie (HZB) Berlin. Together with microstructure characterization and distortion measurements, it is possible to describe the stress state throughout the whole sample. The sample was measured in as-build condition (on a build plate) and after releasing from the build plate. The used material is the nickel based superalloy 718. This alloy is widely used in aerospace and chemical industries due to its superior corrosion and heat resistant properties.
Obtained results indicated different residual stress states for each of the transversal, longitudinal and normal component. The normal and transversal component exhibits a rather compressive behavior while the longitudinal was tensile in the center part of the sample and became compressive towards the tip. As expected, the absolute values of all stress components decreased after releasing the sample from the building plate. A surface scan utilizing a coordinate-measuring machine (CMM) allowed us to present top surface distortion before and after releasing. The top surface showed a distortion around ±80µm after releasing. Microstructure evolution in the scanning-building cross-section is largely dominated by columnar grains. In addition, many small random orientated grains are prominent in the regions of a laser overlap during SLM.
In summary, for the sample of superalloy 718 manufactured by SLM, a small distortion occurred when removing the sample from the build plate whereby the residual stress state decreases. Moreover, the observed columnar grains in the building direction could give a reason for the lowest stress values in that normal direction. However, the most important parameter controlling the residual stresses is the temperature gradient. Hence, future investigations are planned for a different scan strategy to distribute the laser impact in a more homogenous manner.
Characterization of early crystallization stages in surface-crystallized diopside glass-ceramics
(2019)
Structure formation in glass-ceramics by means of surface crystallization is a challenging open question and remains elusive to definite answers. In several glass-ceramic systems, oriented crystal layers have been observed at the immediate surface, including diopside and some fresnoite systems. However, it is still open to debate, whether oriented surface crystallization is the result of oriented nucleation or growth selection effects. In the same vein, there is still discussion whether surface nucleation is governed by surface chemistry effects or by defects serving as active nucleation sites.
In order to help answer these questions, annealing experiments at 850°C have been performed on a MgO·CaO·2SiO2 glass, leading to the crystallization of diopside at the surface. Different annealing durations and surface treatment protocols (i.a. lapping with diamond slurries between 16 µm and 1 µm grain size) have been applied. Particular focus has been put on earliest crystallization stages, with crystal sizes down to about 200 nm. The resultant microstructure has been analyzed by electron backscatter diffraction (EBSD) and two different kinds of textures have been observed, with the a- or b-axis being perpendicular to the sample surface and the c-axis lying in the sample plane. Even at shortest annealing durations, a clear texture was present in the samples. Additionally, selected samples have been investigated with energy-dispersive x-ray spectroscopy in the scanning transmission electron microscope (STEM-EDX). The diopside crystals have been found to exhibit distinguished submicron structure variations and the glass around the crystals was shown to be depleted of Mg.