4.4 Thermochemische Reststoffbehandlung und Wertstoffrückgewinnung
Filtern
Dokumenttyp
- Vortrag (95)
- Zeitschriftenartikel (56)
- Beitrag zu einem Tagungsband (15)
- Posterpräsentation (14)
- Buchkapitel (5)
- Tagungsband (Herausgeberschaft für den kompletten Band) (1)
- Dissertation (1)
- Forschungsbericht (1)
Schlagworte
- Recycling (26)
- Phosphor (20)
- Klärschlamm (17)
- Phosphorus (15)
- Phosphorrückgewinnung (14)
- Phosphorus recovery (14)
- Sewage sludge (12)
- Fertilizer (9)
- Klärschlammverordnung (9)
- CFK (8)
Organisationseinheit der BAM
- 4.4 Thermochemische Reststoffbehandlung und Wertstoffrückgewinnung (188) (entfernen)
Paper des Monats
- ja (4)
Phosphorus (P) recycling from sewage sludge for agricultural needs has to meet requirements for agricultural implementation, such as short and long-term P-plant-availability under field conditions. Field experiments often bring no evaluable results, because agricultural soils got a high potential of P-supply even if they are classified as low in P-supply according to the CAL extraction method. The present study presents a possible way to investigate the P-plant-availability of P-recycling-fertilizers under field-like conditions. The plant experiments are firstly performed in small Mitscherlich pots in growth chambers and subsequently in containers with a high soil volume of 170 kg under greenhouse conditions, in which plants can grow until ripening. The tested P-recycling fertilizers were produced from sewage sludge in a large-scale thermal process. It was a two-step treatment process performed with a pyrolysis of sewage sludge at 550°C (SSC-550) and a subsequent thermochemical post-treatment at 950°C with Na2SO4 (SSA-Na) and HCl + Na2SO4 (SSA-HCl/Na) as additives. The results show, that the P-recycling-products from pyrolysis got an adequate long-term but a 65% lower short-term P-plant-availability compared to triple superphosphate. SSA-Na and SSA-HCl/Na show both a high short and longterm P-plant-availability comparable to triple-superphosphate. This can be explained by their highly plant-available P-compound CaNaPO4.
Solid wastewater-based fertilizers were screened for per- and polyfluoroalkyl substances (PFAS) by the extractable organic fluorine (EOF) sum parameter method. The EOF values for ten sewage sludges from Germany and Switzerland range from 154 to 7209 mg kg−1. For thermal treated sewage sludge and struvite the EOF were lower with values up to 121 mg kg−1. Moreover, the application of PFAS targeted
and suspect screening analysis of selected sewage sludge samples showed that only a small part of the EOF sum parameter values can be explained by the usually screened legacy PFAS. The hitherto unknown part of EOF sum parameter contains also fluorinated pesticides, pharmaceutical and aromatic compounds. Because these partly fluorinated compounds can degrade to (ultra-)short PFAS in wastewater treatment plants they should be considered as significant sources of organic fluorine in the environment. The combined results of sum parameter analysis and suspect screening reveal the need to update current regulations, such as the German fertilizer ordinance, to focus not solely on a few selected PFAS such as perfluorooctane sulfonic acid (PFOS) and perfluorooctanoic acid (PFOA) but
consider an additional sum parameter approach as a more holistic alternative. Moreover, diffusion gradient in thin-films (DGT) passive samplers were utilized as an alternative simplified extraction method for PFAS in solid wastewater-based fertilizers and subsequently quantified via combustion ion chromatography. However, the DGT method was less sensitive and only comparable to the EOF values
of the fertilizers in samples with >150 mg kg−1, because of different diffusion properties for various PFAS, but also kinetic exchange limitations.
New developments in legislation and technology development for P-recovery were presented with focus on the situation in Germany.
Die Zementindustrie und weitere energieintensive Industrien wie etwa die Stahlindustrie stehen vor dem Hintergrund der Transformation unserer Gesellschaft zur Klimaneutralität vor erheblichen Herausforderungen. Ziel dieser Branchen ist perspektivisch die vollständige Vermeidung klimaschädlicher Emissionen – mit besonderem Fokus auf Kohlendioxid. Neben der Umstellung auf regenerative Energieträger, sind im Speziellen für die Zementindustrie die erheblichen Anteile an CO2-Emissionen durch die Entsäuerung von Kalkstein zukünftig zu vermeiden. Da die hervorragenden Bindemitteleigenschaften des bisher hauptsächlich in Zementen eingesetzten Portlandklinkers jedoch auf Calciumverbindungen wie Tri- und Di-calciumsilikaten basieren, stellt die Substitution des Kalks derzeit für die Zementindustrie die größte Herausforderung dar. Neben vollständig neuen Bindemittelsystemen ohne Verwendung von Kalk und CCS/CCU-Technologien zur Vermeidung der CO2-Emissionen bei Verwendung von Kalk, können Abfälle und Nebenprodukte wie etwa Betonbrechsand, verschiedene Schlacken und weitere Massenreststoffe sinnvoll zur Einsparung von Rohstoffen und zur Vermeidung von CO2-Emissionen eingesetzt werden. Es gilt diese Potentiale von Sekundärrohstoffen branchenübergreifend zu identifizieren und Synergien zwischen den Branchen nutzbar zu machen. Hierbei werden neben der chemischen Zusammensetzung der Abfälle und Nebenprodukte auch die Verfügbarkeit und der Massenstrom relevante Kriterien sein. Die potenziellen Sekundärrohstoffe und deren Gemische mit chemisch ähnlicher Zusammensetzung wie die bisher verwendeten Bindemittel, können durch verschiedene technische Ansätze wieder in reaktive Bindemittel umgewandelt und damit nutzbar gemacht werden. Eine gezielte Umwandlung der nicht reaktiven mineralischen Phasen in neue mineralische Phasen mit guten Bindemitteleigenschaften, kann u. a. durch Schmelzprozesse erzielt werden. In Schmelzen können bei hohen Temperaturen die bestehenden, nicht reaktiven mineralischen Phasen zerstört und neue mineralische Phasen mit guten Bindemitteleigenschaften erzeugt werden. Hohe Freiheitsgrade durch gezielte Einstellung der stofflichen Zusammensetzung der Schmelze, durch Stoffseparationen und durch geregelte Abkühlregimes können eine maßgeschneiderte Erzeugung neuer Bindemitteltypen ermöglichen. Aufgrund der hohen erforderlichen Temperaturen von Schmelzprozessen ist die Umsetzung dieser neuen Verfahren nach Möglichkeit in bestehenden pyrometallurgischen Produktionsrouten wie etwa der Stahlproduktion vorzunehmen. So kann etwa der Einsatz von Betonbrechsand als Schlackebildner in der Stahlproduktion zielführend sein, wenn die Schlacke wieder zu einem Bindemittel prozessiert wird und in Zementen Verwendung findet. Eine stoffliche Kreislaufführung wäre hiermit gegeben, wobei der Einsatz von Kalkstein als Schlackebildner oder Rohstoff für die Zementproduktion, und damit die entsprechenden CO2-Emissionen, vermieden werden. Die Entwicklung neuartiger Bindemittelsysteme auf Basis von Sekundärrohstoffen sollte von erforderlichen Anpassungen und neuen Entwicklungen in der Regelsetzung und Normung begleitet werden. Vor allem muss gewährleistet sein, dass die mit neuen Bindemitteln hergestellten Betone den hohen Anforderungen an Dauerhaftigkeit und Umweltverträglichkeit genügen. Des Weiteren sollte mit den etablierten Methoden, wie etwa der Lebenszyklusanalyse, untersucht werden, inwiefern und in welchem Umfang die neuen technischen Entwicklungen zu Nachhaltigkeit und Klimaschutz beitragen.
Microbially induced carbonate precipitation (MICP), a widespread phenomenon in nature, is gaining attention as a low-carbon alternative to ordinary Portland cement (OPC) in geotechnical engineering and the construction industry for sustainable development. In the Philippines, however, very few works have been conducted to isolate and identify indigenous, urease-producing (ureolytic) bacteria suitable for MICP. In this study, we isolated seven, ureolytic and potentially useful bacteria for MICP from marine sediments in Iligan City. DNA barcoding using 16s rDNA identified six of them as Pseudomonas stutzeri, Pseudomonas pseudoalcaligenes, Bacillus paralicheniformis, Bacillus altitudinis, Bacillus aryabhattai, and Stutzerimonas stutzeri but the seventh was not identified since it was a bacterial consortium. Bio-cementation assay experiments showed negligible precipitation in the control (without bacteria) at pH 7, 8, and 9. However, precipitates were formed in all seven bacterial isolates, especially between pH 7 and 8 (0.7–4 g). Among the six identified bacterial species, more extensive precipitation (2.3–4 g) and higher final pH were observed in S. stutzeri, and B. aryabhattai, which indicate better urease production and decomposition, higher CO2 generation, and more favorable CaCO3 formation. Characterization of the precipitates by scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDS) and attenuated total reflectance Fourier transform spectroscopy (ATR-FTIR) confirmed the formation of three carbonate minerals: calcite, aragonite, and vaterite. Based on these results, all six identified indigenous, ureolytic bacterial species from Iligan City are suitable for MICP provided that the pH is controlled between 7 and 8. To the best of our knowledge, this is the first report of the urease-producing ability and potential for MICP of P. stutzeri, P. pseudoalcaligenes, S. stutzeri, and B. aryabhattai.
This paper focuses on the scandium speciation in bauxite residues of different origin. Insights into mineralchemical similarities and differences of these materials will be presented and links to their natural geological background discussed. The presented research should provide fundamental knowledge for the future development of efficient and viable technologies for Sc-recovery from bauxite residues derived from different bauxites and accumulating at different localities. In total, five bauxite residues were investigated which originated from Greece, Germany, Hungary and Russia (North Ural & North Timan) using a combination of different analytical tools. Those included: laser ablation inductively coupled plasma mass spectrometry, X-ray absorption near Edge structure (XANES) spectroscopy, μ-Raman spectroscopy as well as scanning electron microscopy and electron microprobe analyses. X-ray fluorescence and inductively coupled plasma mass spectrometry were used to determine the overall chemical composition. The investigated samples were found to exhibit a relatively homogenous distribution of Sc between the larger mineral particles and the fine-grained matrix except for Al-phases like diaspore, boehmite and gibbsite. These phases were found to be particularly low in Sc. The only sample where Sc mass fractions in Al-phases exceeded 50 mg/kg was the Russian sample from North Ural. Fe-phases such as goethite, hematite and chamosite (for Russian samples) were more enriched in Sc than the Al-phases.
In fact, in Greek samples goethite showed a higher capacity to incorporate or adsorb Sc than hematite. Accessory minerals like zircon, rutile/anatase and ilmenite were found to incorporate higher mass fractions of Sc (>150 mg/kg), however, those minerals are only present in small amounts and do not represent major host phases for Sc. In Russian samples from North Ural an additional Ca–Mg rich phase was found to contain significant mass fractions of Sc (>500 mg/kg). μ-XANES spectroscopy was able to show that Sc in bauxite residue occurs adsorbed onto mineral surfaces as well as incorporated into the crystal lattice of certain Fe-phases. According to our observations the bauxite type, i.e. karstic or lateritic, the atmospheric conditions during bauxitization, i.e. oxidizing or reducing, and consequently the dominant Sc-bearing species in the primary Bauxite influence the occurrence of Sc in bauxite residues. In karstic bauxites, underlying carbonate rocks can work as a pH-barrier and stabilize Sc. This prevents the Sc from being mobilized and removed during bauxitization. Hence, karstic bauxites are more prone to show a Sc enrichment than lateritic bauxites. Reducing conditions during bauxitization support the incorporation of Sc into clay minerals such as chamosite, which can dissolve and reprecipitate during Bayer processing causing Sc to be redistributed and primarily adsorb onto mineral surfaces in the bauxite residue. Oxidizing conditions support the incorporation of Sc into the crystal lattice of Fe-oxides and hydroxides, which are not affected in the Bayer process. The genetic history of the bauxite is therefore the major influential factor for the Sc occurrence in bauxite residues.
In recent times, as the need for new high-tech materials is growing steadily to fulfil future sustainability goals, more and more looks turn towards industrial waste streams as potential sources of valuable metals. Bauxite residue (BR), accumulating during alumina production, is one of the major waste streams in the metal industry. Suitable re-use possibilities for BR are intensively investigated including approaches for the recovery of scandium (Sc). This transition metal, even though rarely recognized by the broader audience yet, has recently gained the interest of e.g. aerospace industries and SOFC-producers since its use is strongly improving the performance and durability of the respective materials.
Even though many sources classify Sc as one of the REE, there are many aspects, such as its ionic radius, which significantly differentiate Sc from the REE and cause its behaviour to be distinct as well. The large ionic potential (radius/charge) causes Sc to be incompatible in most rock forming minerals, which results in generally low concentrations in the earth’s crust and rare occurrences of natural Sc-deposits.
The general occurrence of enriched concentrations of Sc in some BRs compared to the earth’s crust is known for some time now and has especially been investigated for Greek materials. However, the (geo)chemical and mineralogical behaviour, the Sc speciation, the association and the variation of Sc occurrences in BRs of different origin is still not fully understood. This study aims to gain better knowledge on the different kinds of Sc-occurrences and their possible impact on future recovery schemes. We therefore apply a diverse set of analytical methods including novel measurement techniques such as X-ray absorption near edge structure (XANES) spectroscopy as well as standard techniques such as electron microprobe analyses, and Raman spectroscopy on BRs from Germany, Hungary and Greece. Information on the local distribution of Sc is determined by high-resolution laser ablation – inductively coupled plasma – mass spectrometry (LA-ICP-MS) mappings.
Sc in Greek BR seems to have an affinity towards Fe-Phases such as Goethite and Hematite. However, whereas some of these phases show distinct enrichment of Sc, others are particularly barren, which might be a result of the different input materials. By means of XANES measurements it was possible to show that Sc in the Greek samples occurs adsorbed on the surface of those Fe-Phases, likely in the form of amorphous Sc-hydroxide or -oxyhydroxide or can be incorporated into the crystal lattice as well. The general affinity of Sc to those kinds of phases has been reported for natural rocks such as laterites before, where similar investigations were made using the XANES method [8]. Likewise, the Fe-association has been observed for Greek BR by Vind et al. [7]. Hungarian BRs show similar results as the Greek samples and LA-ICP-MS mappings show distinct Sc enrichment rims surrounding mineral particles. In German BR, Fe as well as Ti-phases occur to be partially enriched in Sc. Depending on the original primary bauxite, the source rock of the bauxite and the bauxite processing route, it is likely that many different parameters influence the occurrence and species of Sc in the BR. Theoretically, it either can therefore remain within its original carrier or can be partially or fully redistributed within the BR. Since the processing of the bauxite involves elevated temperatures, pressure and dissolving reagents, it is however very likely that some of the Sc will be redistributed and adsorb on mineral surfaces of smaller and larger particles, making beneficiation steps rather ineffective.
The study shows that there is no general rule defining how Sc is associated mineralogically or chemically within BRs. Therefore, the effective development of a recovery method needs a case specific background knowledge on the Sc-species present in the BR of interest. This research has received funding from the European Community’s Horizon 2020 Programme SCALE (H2020/2014-2020) under grant agreement n° 730105.
This paper presents an inventory of sewage sludge ashes (SSA) generated in the mono-incineration plants for municipal sewage sludge in Poland. This research focused on the detailed study of mass flows, chemical composition, and phosphorus recovery potential. There are currently 11 sludge mono-incineration plants operated with a total capacity of 160,300 Mg dry weight (d.w.) of sludge annually. Recently, a significant increase in the amount of SSA generated in these plants has been observed, reaching 26,756 Mg in 2018. Chemical composition of SSA showed significant amounts of the main nutrients: calcium (~14%), phosphorus (~13%), magnesium (~3%), and potassium (~1%). Additional main elements were iron (~14.5%), silicon (~13%), and aluminium (~6%). The main trace elements in the SSA were zinc (~3750 mg/kg) and copper (~899 mg/kg). Pollutants, according to fertilizer regulations of different countries, present in Polish SSA were chromium(~703 mg/kg), nickel (~260 mg/kg), lead (~94 mg/kg), and Cadmium (~9 mg/kg). The radionuclides, uranium, and thorium often present in higher amounts in commercial phosphate rock-based fertilizers, were only detected in SSA t low levels of 4–9 mg/kg and 2–3 mg/kg, respectively. Theoretical phosphorus recovery potential from the SSA (from plants in Cracow, Lodz, Gdansk, Gdynia, Szczecin, and Kielce) was estimated at 1613.8 Mg, of which 33.9% is bioavailable. Currently, in Poland, the recommended approach is the production of fertilizers as a result of the extraction of phosphorus from the SSA with its use in the production of secondary mineral fertilizers.
Further research in this area is required considering Polish conditions and legislation.
In Denmark, increasing amounts of woody biomass are being used for the production of renewable energy, resulting in more wood ashes being generated. While these materials have been mainly landfilled, wood ashes may also be utilised for fertilizing and liming purposes on top of soils. Pre-treatments involving hardening or granulation may be carried out prior to soil application. In this study, two Danish wood ash samples were hardened and/or granulated. Lab-hardening induced rapid changes in the shape of the acid neutralisation capacity curve of the ashes. Up-flow column tests, assuming local equilibrium conditions, were employed to investigate the leaching from pre-treated ashes. Granules and loose ashes demonstrated similar leaching behaviours, indicating that similar geochemical processes were governing their leaching. In comparison with untreated fresh ashes, the hardened ashes demonstrated reduced leaching of Ca, Ba, Pb and Zn with concentration levels generally below or close to the analytical limits of quantification; to the contrary, the leaching of As, P, Sb, Si, V and Mg was enhanced in the hardened ashes. The release of alkalinity was reduced by hardening. In general, all granules were barely breakable by finger-pinching and they could withstand one month of continuous leaching, preserving their overall shape. The solubility of phosphorous in neutral ammonium citrate indicated that about 30–51% of the total P content in the ash samples was released, suggesting that the ashes could be potentially valuable as P-fertiliser if applied onto soil.
An existing pyrometallurgical process for tantalum and niobium recovery, mainly from low grade pyrometallurgical residues, was investigated. Series of melting experiments were carried out in a pilot-scale electric arc furnace to study how the amount, the grain size and the way of feeding affect the activity of carbon as a reducing agent. During the pyrometallurgical treatment refractory metals such as tantalum and niobium are reduced to their carbide form and enriched in the molten iron-based metal phase. The cooled down slag and metal phase were analysed to investigate thermodynamic and kinetic conditions of the carbide formation. FACT Sage simulations were also used to investigate the material system in state of thermodynamic equilibrium. Results show that mass transfer and kinetics may play an important role if compared to equilibrium analyses using FACT Sage.
An existing pyrometallurgical process for tantalum and niobium recovery, mainly from low grade pyrometallurgical residues, was investigated. Series of melting experiments were carried out in a pilot-scale electric arc furnace to study how the amount, the grain size and the way of feeding affect the activity of carbon as a reducing agent. During the pyrometallurgical treatment refractory metals such as tantalum and niobium are reduced to their carbide form and enriched in the molten iron-based metal phase. The cooled down slag and metal phase were analysed to investigate thermodynamic and kinetic conditions of the carbide formation. FACT Sage simulations were also used to investigate the material system in state of thermodynamic equilibrium. Results show that mass transfer and kinetics may play an important role if compared to equilibrium analyses using FACT Sage.
Phase formation and evolution was investigated in the CaO–SiO2 system in the range of 70–80 mol% CaO. The samples were container-less processed in an aerodynamic levitation system and crystallization was followed in situ by synchrotron x-ray diffraction at the beamline P21.1 at the German electron synchrotron (DESY). Modification changes of di- and tricalcium silicate were observed and occurred at lower temperatures than under equilibrium conditions. Despite deep sample undercooling, no metastable phase formation was observed within the measurement timescale of 1 s. For the given cooling rates ranging from 300 K s−1 to about 1 K s−1, no decomposition of tricalcium silicate was observed. No differences in phase evolution were observed between reducing and oxidizing conditions imposed by the levitation gas (Ar and Ar + O2). We demonstrate that this setup has great potential to follow crystallization in refractory oxide liquids in situ. For sub-second primary phase formation faster detection and for polymorph detection adjustments in resolution have to be implemented.
Basic oxygen furnace slags (BOFS) are a by-product of steel production. In 2016, 10.4 Mt of BOFS were produced in the European Union (EU). The main part of BOFS is used in road construction, earthwork and hydraulic engineering. A smaller part is returned to the metallurgical circle, used as fertilizer or landfilled. However, it is also possible to produce higher value products from BOFS. For example, many researchers have investigated the possibility of producing Portland cement clinker and crude iron from BOFS by a carbothermal post-treatment.
In this study, German BOFS was reduced in a small-scale electric arc furnace using petrol coke as reducing agent. The carbothermal treatment reduces the iron oxides in the BOFS to metallic iron, which accumulates at the bottom of the furnace by density separation. In addition to metallic iron, the process generates a mineral product rich in the tricalcium silicate solid solution alite. As the main constituent of Portland cement clinker, the hydraulic reactive mineral alite is of high economic importance.
In previous studies, the hydraulic reactivity of the mineral product was investigated by testing the compressive strength of blends with 70 wt.% ordinary Portland cement (OPC). Recent investigations focused on the hydraulic properties of the pure mineral product from the reduced BOFS. The heat of hydration of the mineral product was measured by isothermal calorimetry and compared with the heat of hydration of a synthetic low-iron slag and OPC. In addition, the formation of hydration products was investigated with differential scanning calorimetry (DSC) and x-ray diffraction analysis (XRD) on freeze-dried samples after defined curing times. The results of the calorimetric measurements indicate that the mineral product produced less heat of hydration and its reaction was delayed compared to the synthetic low-iron slag and OPC. Hydration products such as portlandite and calcium silicate hydrates (C-S-H) formed later and in lower amounts.
The production of a hydraulic material from BOFS by reductive treatment is of great interest to both the cement and steel industries. The substitution of cement clinker in OPC with a hydraulic material such as reduced BOFS leads to a reduction in greenhouse gas emissions from cement production. The steel industry benefits from an application for its by-products that avoids cost expensive landfilling and may even bring economic advantages. Furthermore, it may be possible to return the recovered crude iron to production.
Herstellung neuer Düngemittelausgangsstoffe durch thermochemische Behandlung von Klärschlammaschen
(2018)
Der Fachbereich 4.4 hat zusammen mit der Firma Outotec ein thermochemisches Verfahren im Drehrohrofen entwickelt, um die Phosphorphasen in Klärschlammasche umzuwandeln, damit die behandelten Aschen als Dünger eingesetzt werden können. In dem Vortrag wird das Verfahren erklärt, die Düngewirkung dargestellt und Pilotversuche vorgestellt.
Herstellung neuer Düngemittelausgangsstoffe durch thermochemische Behandlung von Klärschlammaschen
(2018)
Klärschlammasche kann viel Phosphor enthalten (bis zu 12%). Aus diesem Grund ist diese Asche ein gutes Ausgangsmaterial für Phosphordünger. Aufgrund der geringen Pflanzenverfügbarkeit des Phosphors in der Asche ist eine Aufbereitung notwendig.
In diesem Buchbeitrag wird das thermochemische Verfahren AshDec vorgestellt, welches von dem Fachbereich 4.4 mit der Firma Outotec entwickelt worden ist. Es werden die Hintergründe diskutiert, die Phasenreaktionen bei diesem Prozess besprochen, Pflanzenversuche ausgewertet, verschiedene Extraktionen diskutiert und ein Konzept für eine mögliche Pilotanlage dargestellt.
Gypsum (calcium sulfate dihydrate) has excellent building material properties and has been widely used in constructions in the last decades in many countries. Accordingly, an increase of waste gypsum in C&D waste is expected in the upcoming years. On one hand, sulfates are unwanted in other secondary building materials (particularly in recycled concrete aggregates) and should be minimized for quality reasons. On the other hand, used gypsum from CDW can also be used in gypsum production if the high quality requirements for the recycled gypsum – especially regarding the sorting accuracy - are met.
A large percentage of the gypsum from buildings was installed as gypsum plasterboards in interior fittings so far. Gypsum plasterboards are comparatively simple to remove and to separate during selective dismantling. Therefore, a high sorting purity can be achieved. In addition, techniques for the recycling of gypsum plasterboards already exist and high quality standards can be achieved. Also, the reuse in gypsum production has been improved in the last decade. Furthermore, an environmental evaluation of the whole process of gypsum plasterboard recycling and reuse showed that this approach can be environmentally advantageous. Therefore, a closed-loop recycling of gypsum plasterboards is feasible.
This poster will show the development of gypsum consumption in different countries as well as a prognosis for the upcoming of gypsum in CDW in the future decades in Germany. Furthermore, a simplified scheme of the recycling process and selected results from an environmental evaluation will be presented.
The use of secondary building materials can meet the requirements of sustainability in several ways: the extended time availability of primary raw materials and, thereby, the protection of natural ressources as well as the conservation of landfill sites. Regarding the predicted decrease of gypsum supply in Germany, particularly the recycling of gypsum (calcium sulfate) is of growing importance. Currently, the gypsum demand is fulfilled (at least 60%) by gypsum as side product from coal-fired power plants (FGD Gypsum). Germany’s natural gypsum deposits fulfil the remaining gypsum demand. Due to national climate protection goals the gypsum supply from coal power plants will decrease significantly in the future.
In addition, the content of sulfates in other secondary building materials, in particular in recycled concrete aggregates, should be minimized for quality reasons. Separated gypsum can be used in gypsum production if the high quality requirements for recycled gypsum are met. Accordingly, there have been significant advancements in the processing of gypsum residues in the last years. Since almost all processing steps in the recycling process are associated with environmental impacts, an evironmental evaluation of the use of recycled gypsum as a substitute in gypsum production has to be carefully conducted.
The presentation focusses on the techniques for generating recycled gypsum from gypsum plaster boards, the related quality requirements and a comprehensive environmental evaluation of the complete process.