4.4 Thermochemische Reststoffbehandlung und Wertstoffrückgewinnung
Filtern
Dokumenttyp
- Zeitschriftenartikel (56) (entfernen)
Schlagworte
- Phosphorus (10)
- Sewage sludge (8)
- Fertilizer (5)
- Phosphorus recovery (5)
- Klärschlamm (4)
- Wastewater (4)
- Circular economy (3)
- Diffusive gradients in thin films (DGT) (3)
- Fertilzer (3)
- Phosphat (3)
Organisationseinheit der BAM
- 4.4 Thermochemische Reststoffbehandlung und Wertstoffrückgewinnung (56) (entfernen)
Paper des Monats
- ja (4)
The use of highly water-soluble phosphorus (P) fertilizers can lead to P fixation in the soil, reducing fertilization efficiency. Waste-derived, low water-solubility sources can potentially increase sugarcane’s P uptake compared to triple superphosphate by reducing adsorption to the soil.
Aims:We aimed to test struvite, hazenite, and AshDec® for their agronomic potential as recycled fertilizers for sugarcane production in a typical tropical soil.We hypothesize that these sources can reduce P fixation in the soil, increasing its availability and sugarcane’s absorption.
Methods: In a greenhouse pot experiment, two consecutive sugarcane cycles, 90 days each, were conducted in a Ferralsol. The recovered sources struvite, hazenite, AshDec®, and the conventional triple superphosphate were mixed in the soil in three P doses (30, 60, and 90 mg kg–1), aside a control (nil-P). At both harvests, sugarcane number of sprouts, plant height, stem diameter, dry mass yield, shoot phosphorus, and soil P fractionation were investigated.
Results: At 90 days, struvite and hazenite performed better for dry mass yield (70.7 and 68.3 g pot–1, respectively) than AshDec® and triple superphosphate (59.8 and 57.4 g pot–1, respectively) and for shoot P, with 98.1, 91.6, 75.6, and 66.3 mg pot–1, respectively. At 180 days, struvite outperformed all treatments for dry mass yield (95.3 g pot–1) and AshDec® (75.5 mg pot–1) for shoot P. Struvite was 38% and hazenite 21% more efficient than triple superphosphate in P uptake, while AshDec® was 6% less efficient. Soil had higher labile P under struvite, hazenite, and AshDec® than triple superphosphate by the end of the first cycle, while only the later increased nonlabile P by the end of the experiment (180 days).
Conclusions:Waste-derived P sources were more efficient in supplying P for sugarcane and delivering labile P in 180 days than triple superphosphate.
Small-scale variations in mineral chemistry, textures, and platinum group element (PGE) mineralization were investigated in the Lower and Middle Group chromitite layers LG6, LG6a, MG1, MG2, and MG2 II from vertical drill core profiles at the Thaba mine in the northwestern limb of the Bushveld Complex. We present detailed geochemical profiles of chromite composition and chromite crystal size distribution curves to shed light on the processes of chromite accumulation and textural modification as well as mineralization. Multiple samples within each layer were assayed for PGE concentrations, and the respective platinum group mineral association was determined by mineral liberation analysis (MLA).
There is strong evidence for postcumulus changes in the chromitites. The crystal size distribution curves suggest that the primary chromite texture was coarsened by a combination of adcumulus growth and textural equilibration, while compaction of the crystal mush played only a minor role. Mineral compositions were also modified by postcumulus processes, but because of the very high modal amount of chromite and its local preservation in orthopyroxene oikocrysts, that phase retained much primary information. Vertical variations of chromite composition within chromitite layers and from one layer to another do not support the idea of chromite accumulation from crystal-rich slurries or crystal settling from a large magma chamber. Instead, we favor a successive buildup of chromitite layers by repeated injections of relatively thin layers of chromite-saturated magmas, with in situ crystallization occurring at the crystal mush-magma interface. The adcumulus growth of chromite grains to form massive chromitite required addition of Cr to the layers, which we attribute to downward percolation from the overlying magma.
The PGE concentrations are elevated in all chromitite layers compared to adjacent silicate rocks and show a systematic increase upward from LG6 (avg 807 ppb Ir + Ru + Rh + Pt + Pd + Au) to MG2 II (avg 2,062 ppb).
There are also significant internal variations in all layers, with enrichments at hanging and/or footwalls. The enriched nature of chromitites in PGEs compared to host pyroxenites is a General feature, independent of the layer thickness. The MLA results distinguish two principal groups of PGE mineral associations: the LG6, LG6, and MG1 are dominated by the malanite series, laurite, and PGE sulfarsenides, while the MG2 and MG2 II layers are characterized by laurite and PGE sulfides as well as Pt-Fe-Sn and PGE-Sb-Bi-Pb alloys. Differences in the PGE associations are attributed to postcumulus alteration of the MG2 and MG2 II layer, while the chromitites below, particularly LG6 and LG6a, contain a more pristine association.
Phosphorus (P) recovery is obligatory for all sewage sludges with more than 20 g P/kg dry matter (DM) from 2029 in Germany. Nine wastewater treatment plants (WWTPs) were chosen to investigate variations of phosphorus contents and other parameters in sewage sludge over the year. Monthly sewage sludge samples from each WWTP were analyzed for phosphorus and other matrix elements (C, N, H, Ca, Fe, Al, etc.), for several trace elements (As, Cr, Mo, Ni, Pb, Sn) and loss of ignition. Among the nine WWTPs, there are four which have phosphorus contents both above and below the recovery limit of 20 g/kg DM along the year. Considering the average phosphorus content over the year, only one of them is below the limit. Compared to other matrix elements and parameters, phosphorus fuctuations are low with an average of 7% over all nine WWTPs. In total, only hydrogen and carbon are more constant in the sludge.
In several WWTPs with chemical phosphorus elimination, phosphorus fuctuations showed similar courses like iron and/or aluminum. WWTPs with chamber flter presses rather showed dilution efects of calcium dosage. As result of this study, monthly phosphorus measurement is highly recommended to determine whether a WWTP is below the
20 g/kg DM limit.
More sustainable waste management practices are an important element in the Transformation towards a circular economy (CE). Activities in this area should be dedicated to all groups of waste, including those generated in the water and sewage sector. This paper presents the characteristics of sewage sludge ash (SSA) coming from Polish municipal waste incineration plants. Due to the high content of nutrients such as phosphorus (8.01% P2O5), calcium (5.11% CaO) and magnesium (2.75% MgO), the analyzed SSA may constitute a valuable source of raw materials for the fertilizer industry.
Despite the good fertilizing properties of the SSA, in some cases the presence of heavy metals such as cadmium (0.74–1.4 mg/kg dry matter), lead (49.8–99 mg/kg dry matter), mercury (3.93 mg/kg dry matter) and arsenic (4.23–4.43 mg/kg dry matter) and poor bioavailability of P from SSA disqualifies this waste from direct use as a fertilizer. Therefore, it is necessary to look for methods that will allow the municipal SSA to be processed, for example, technologies for the extraction of phosphorus and the production of phosphate fertilizer. This way of SSA management is in the line with the CE assumptions, in which waste becomes a valuable source of secondary raw materials. Fertilizer produced from waste meeting quality, safety and labelling requirements and limits of organic, microbiological and physical contaminants will be able to be traded freely within the European Union (EU) and receive the CE marking. The idea of use of SSA for fertilizer purposes is consistent not only with the objectives of the CE but also with the Polish National Waste Management Plan 2022 and the Municipal Sewage Sludge Strategy 2019–2022, which emphasizes the necessity to maximize the use of biogenic substances contained in wastewater. Therefore, sustainable management of SSA, in particular its storage in a way enabling the recovery of phosphorus, should be promoted.
Uranium and thorium species in phosphate rock and sewage sludge ash based phosphorus fertilizers
(2020)
Phosphorus (P) is an essential element for all forms of life and is thus often applied as phosphate rock-based P-fertilizers in agriculture to enable continuous farming. However, these P-fertilizers contain also hazardous uranium (U) and thorium (Th), up to 660 and 220 mg/kg, respectively. On the contrary, novel P-fertilizers made from sewage sludge (ash) contain only low mass fractions of U and Th. In addition to the total amount of U and Th in P-fertilizers, their mobility and bioavailability is important, which depends to a large extent on their chemical state, especially oxidation state and chemical bonding. Thus, we analyzed their chemical state in various P-fertilizers by U and Th L3-edge HERFD-XANES spectroscopy. Phosphate rocks and sewage sludge-based P-fertilizers contain mainly U(IV) compounds which have only a low bioavailability. In contrast, acidic treatment of phosphate rock to produce super phosphates lead to an oxidation to U(VI) compounds (including formation of uranium phosphates) with a strongly increased bioavailability. On the contrary, all analyzed P-fertilizers contain Th in form of strongly insoluble phosphates and oxides with a low bioavailability. Additionally performed water extractions and Diffusive Gradients in Thin-films (DGT) experiments support these findings.
The leaching behavior of scandium (Sc) from bauxite residues can differ significantly when residues of different geological backgrounds are compared. The mineralogy of the source rock and the physicochemical environment during bauxitization affect the association of Sc in the bauxite i.e., how Sc is distributed amongst different mineral phases and whether it is incorporated in and/or adsorbed onto those phases. The Sc association in the bauxite is in turn crucial for the resulting Sc association in the bauxite residue. In this study systematic leaching experiments were performed on three different bauxite residues using a statistical design of experiments approach. The three bauxite residues compared originated from processing of lateritic and karstic bauxites from
Germany, Hungary, and Russia. The recovery of Sc and Fe was determined by ICP-OES measurements. Mineralogical changes were analyzed by X-ray-diffraction and subsequent Rietveld refinement. The effects of various parameters including temperature, acid type, acid concentration, liquid-to-solid ratio and residence time were studied. A response surface model was calculated for the selected case of citric acid leaching of Hungarian bauxite residue. The investigations showed that the type of bauxite residue has a strong influence. The easily leachable fraction of Sc can vary considerably between the types, reaching ~20–25% in German Bauxite residue and ~50% in Russian bauxite residue. Mineralogical investigations revealed that a major part of this fraction was released from secondary phases such as cancrinite and katoite formed during Bayer processing of the bauxite.
The effect of temperature on Sc and Fe recovery is strong especially when citric acid is used. Based on the exponential relationship between temperature and Fe-recovery it was found to be particularly important for the selectivity of Sc over Fe. Optimization of the model for a maximum Sc recovery combined with a minimum Fe
recovery yielded results of ~28% Sc recovery at <2% Fe recovery at a temperature of 60 ◦C, a citric acid normality of 1.8, and a liquid-to-solid ratio of 16 ml/g. Our study has shown that detailed knowledge about the Sc association and distribution in bauxite and bauxite residue is key to an efficient and selective leaching of Sc
from bauxite residues.
Calcium alkali phosphates Ca(Na,K)PO4 are main constituents of bioceramics and thermochemically produced phosphorus fertilizers because of their bioavailability. Sparse thermodynamic data are available for the endmembers CaNaPO4 and CaKPO4. In this work, the missing data were determined for the low-temperature phase modifications of the endmembers CaNaPO4 and CaKPO4 and three intermediate Ca(Na,K)PO4 compositions. Standard enthalpy of formation ranges from - 2018.3 ± 2.2 kJ mol-1 to - 2030.5 ± 2.1 kJ mol-1 and standard entropy from 137.2 ± 1.0 J mol-1 K-1 to 148.6 ± 1.0 J mol-1 K-1 from sodium endmember b-CaNaPO4 to potassium endmember b0-CaKPO4.
Thermodynamic functions are calculated up to 1400 K for endmembers and the sodium-rich intermediate phase b-Ca(Na0.93K0.07)PO4. Functions above 640 K are extrapolated because of the phase transition from low- to high-temperature phase. Impurities in the synthesized intermediate phases c-Ca(Na0.4K0.6)PO4 and c-Ca Na0.35K0.65)PO4 and one additional phase transition around 500 K impeded the determination of high-temperature thermodynamic functions. In general, data for phase transition temperatures agree with the previously reported phase diagrams.
Phosphorus (P) recovery from sewage sludge ash (SSA) is one of the most promising approaches of phosphate rock substitution in mineral fertilizers and might be a sustainable way to secure supply of this raw material in the future. In the current investigation, the process of thermochemical treatment of SSA was applied to SSA coming from selected mono-incineration plants of municipal sewage sludge in Poland (Cracow, Gdansk, Gdynia, Lodz, Kielce and Szczecin).
The Polish SSA was thermochemically converted in the presence of sodium (Na) additives and a reducing agent (dried sewage sludge) to obtain secondary raw materials for the production of marketable P fertilizers. The process had a positive impact on the bioavailability of phosphorus and reduced the content of heavy metals in the obtained products. The P solubility in neutral Ammonium citrate, an indicator of its bioavailability, was significantly raised from 19.7–45.7% in the raw ashes and 76.5–100% in the thermochemically treated SSA. The content of nutrients in the recyclates was in the range of 15.7–19.2% P2O5, 10.8–14.2% CaO, 3.5–5.4% Na2O, 2.6–3.6% MgO and 0.9–1.3% K2O. The produced fertilizer raw materials meet the Polish norms for trace elements covered by the legislation: the content of lead was in the range 10.2–73.1 mg/kg, arsenic 4.8–22.7 mg/kg, Cadmium 0.9–2.8 mg/kg and mercury <0.05 mg/kg. Thus, these products could be potentially directly used for fertilizer production. This work also includes an analysis of the possibilities of using ashes for fertilizer purposes in Poland, based on the assumptions indicated in the adopted strategic and planning documents regarding waste management and fertilizer production.
Treatment and reusing of hazardous wastes have become significant issues of modern societies. Blast furnace sludge (BFS) and electric arc furnace dust (EAFD) are such typical wastes, because they usually contain high amounts of undesirable elements such as zinc (Zn) and lead (Pb).
These elements can cause operational problems in reusing of BFS and EAFD. In this study, the Ferro Duo GmbH and the Federal Institute for Materials Research and Testing have investigated a novel approach for eliminating and/or recovering Zn and Pb from both wastes. Applied was a selective chlorination and volatilization of Zn and Pb as chlorides at temperatures between 500 °C and 1100 °C. Both product obtained, Zn and Pb in the form of ZnCl2 and PbCl2 and the purified solid mineral compound are attractive materials for further use. Hydrochloric acid and iron(II) chloride were used as chlorination agents. Exceptionally high Zn and Pb removal efficiencies of >99.5 % could be achieved with both chlorination agents, whereby iron(II) chloride exhibited better performance.
Phosphorus (P) resource availability and quality is declining and recycling P-fertilizers from waste materials are becoming increasingly important. One important secondary P resource is sewage sludge (SSL) where P is often bound as aluminum phosphate (Al-P), iron phosphate (Fe-P) and polyphosphate (poly-P), respectively. Thermal treatment in different ways is a promising way in P recycling to produce highly plant-available P-fertilizers. To investigate mechanisms behind transformation of hardly available P-species toward plant-available P forms we treated a model SSL containing different kinds of defined P sources by low-temperature conversion (LTC) at 500 °C and subsequent thermochemical treatment of the LTC product with Na additives (TCT) at 950 °C, respectively. Pot experiments with ryegrass were carried out to determine the plant availability of P of the different treatments. The poly-P (here pyrophosphates) based fertilizers had a very high plant availability after both thermal treatments. During LTC treatment the plant availability of the Fe-P and Al-P variants increased because of the Formation of Fe(II) phosphates and/or pyro-/polyphosphates. Especially the formation of Al-polyphosphate shows a high plant availability. The subsequent TCT further increased strongly the plant availability of the Fe-P variants because of the formation of highly plant-available CaNaPO4. Thus, a direct TCT without prior LTC probably also produce CaNaPO4 and is recommended for Fe-P based SSL. However, a molar Ca/P ratio of 1 in the fertilizer is favorable for CaNaPO4 formation. Thus, the knowledge on the source of primary P in SSL is essential for choosing the accurate thermal treatment method to produce highly plant-available P-fertilizers from SSL.
Gegenstand dieser Arbeit ist die Untersuchung eines bestehenden pyrometallurgischen Prozesses zur Rückgewinnung von Tantal und Niob aus metallurgischen Reststoffen mit vorwiegend niedriger Wertstoffkonzentration.
Zur näheren Erforschung der im vorliegenden Stoffsystem ablaufenden Reduktionsprozesse wurden in einem Elektrolichtbogenofen Schmelzversuche im Pilotmaßstab durchgeführt. Als Reduktionsmittel diente Koks, welcher mithilfe einer Argon-gespülten Eisenlanze in die flüssige mineralische Schmelze eingebracht wurde. Während der Reduktionsbehandlung werden Refraktärmetalle wie Tantal und Niob in ihre Carbide überführt und anschließend in der erschmolzenen eisenbasierten Metallphase am Boden des Reaktors angereichert. Neben Tantal und Niob gelangt auch ein Teil des im Einsatzmaterial enthaltenen Titans als unerwünschtes Begleitelement in die Metallphase.
Sein Großteil verbleibt jedoch als Oxid in der Schlacke und wird dort hauptsächlich im Mineral Perowskit (CaTiO3) gebunden. Die erstarrten Schlackeproben wurden mit verschiedenen Methoden wie Röntgenfluoreszensanalyse, Röntgenbeugung und Rasterelektronenmikroskopie mit gekoppelter energiedispersiver Röntgenanalyse untersucht, um die Bildung tantalhaltiger Mineralphasen zu verschiedenen Stadien des Reduktionsprozesses zu verfolgen.
Die hier gewonnenen Erkenntnisse zeigen, dass weniger die durch das Einblasen von Koks verursachte Reduktionsreaktion, sondern das Absinken der tantalreichen Eisentröpfchen in der flüssigen mineralischen Schmelze, gefolgt von ihrer Anreicherung in die Metallphase, für die Kinetik ausschlaggebend ist.
Based on recently published research on leaching control mechanisms in electric arc furnace (EAF) slags, it is assumed that a FeO/SiO2 ratio of around one leads to low leached V and Cr concentrations. This ratio influences the mineral phase composition of the slag toward higher amounts of spinel and a lower solubility of calcium silicate phases by suppressing the formation of magnesiowuestite and highly soluble calcium silicate phases. To evaluate this hypothesis, laboratory and scaled up tests in an EAF pilot plant were performed on slag samples characterized by elevated V and Cr leaching and a high FeO/SiO2 ratio. Prior to the melting experiments, the optimum FeO/SiO2 ratio was calculated via FactSageTM. In the melting experiments, the ratio was adjusted by adding quartz sand, which also decreased the basicity (CaO/SiO2) of the slag. As a reference, remelting experiments without quartz sand addition were conducted and additionally, the influence of the cooling rate of the slag was examined. The remelted (without quartz sand) and the remelted modified slags (with quartz sand) were analyzed chemically and mineralogically and the leaching behavior was investigated. The modification of the slags yielded a minimized release of V and Cr, supporting the hypothesis that the FeO/SiO2 ratio influences the mineralogy and the leaching behavior.
Based on recently published research on leaching control mechanisms in electric arc furnace (EAF) slags, it is assumed that a FeO/SiO2 ratio of around one leads to low leached V and Cr concentrations. This ratio influences the mineral phase composition of the slag toward higher amounts of spinel and a lower solubility of calcium silicate phases by suppressing the formation of magnesiowuestite and highly soluble calcium silicate phases. To evaluate this hypothesis, laboratory and scaled up tests in an EAF pilot plant were performed on slag samples characterized by elevated V and Cr leaching and a high FeO/SiO2 ratio. Prior to the melting experiments, the optimum FeO/SiO2 ratio was calculated via FactSageTM. In the melting experiments, the ratio was adjusted by adding quartz sand, which also decreased the basicity (CaO/SiO2) of the slag. As a reference, remelting experiments without quartz sand addition were conducted and additionally, the influence of the cooling rate of the slag was examined. The remelted (without quartz sand) and the remelted modified slags (with quartz sand) were analyzed chemically and mineralogically and the leaching behavior was investigated. The modification of the slags yielded a minimized release of V and Cr, supporting the hypothesis that the FeO/SiO2 ratio influences the mineralogy and the leaching behavior.
Basic oxygen furnace slags (BOFS) are by-products of the steelmaking process. Several researchers have studied the production of Portland cement clinker and metallic iron from BOFS via a reductive treatment.
In this study, we applied a carbothermal reduction of BOFS in a technical-scale electric arc furnace and characterised the clinker-like products. Those clinker-like non-metallic products (NMPs) had a chemical and mineralogical composition comparable to clinker for ordinary Portland cement (OPC) and contained large elongated alite crystals as major component. The pure NMPs reacted more slowly and achieved a lower degree of hydration compared with commercial OPC.
If the reactivity of the products can be further increased by employing specific adaptations, it can be used as a full clinker substitute for OPC. Nevertheless, it is also an option to use the material without further modifications as a cement component or concrete addition, which contributes to the strength development in both cases.
Sugarcane bagasse is commonly combusted to generate energy. Unfortunately, recycling strategies rarely consider the resulting ash as a potential fertilizer. To evaluate this recycling strategy for a sustainable circular economy, we characterized bagasse ash as a fertilizer and measured the effects of co-gasification and co-combustion of bagasse with either chicken manure or sewage sludge: on the phosphorus (P) mass fraction, P-extractability, and mineral P phases. Furthermore, we investigated the ashes as fertilizer for soybeans under greenhouse conditions. All methods in combination are reliable indicators helping to assess and predict P availability from ashes to soybeans. The fertilizer efficiency of pure bagasse ash increased with the ash amount supplied to the substrate. Nevertheless, it was not as effective as fertilization with triple-superphosphate and K<sub>2</sub>SO<sub>4</sub>, which we attributed to lower P availability. Co-gasification and co-combustion increased the P mass fraction in all bagasse-based ashes, but its extractability and availability to soybeans increased only when co-processed with chicken manure, because it enabled the formation of readily available Ca-alkali phosphates. Therefore, we recommend co-combusting biomass with alkali-rich residues to increase the availability of P from the ash to plants.
The Brazilian sugarcane industry produced around 173 million tons (Mt) of bagasse in 2018. Bagasse is a by-product of juice extraction for ethanol and sugar production and is combusted in order to generate power, producing up to 10 Mt of ash per year. This ash contains various concentrations of plant nutrients, which allow the ash to be used as a crop fertilizer. However, the concentration and extractability of phosphorus (P), an essential plant nutrient, are low in bagasse ash. To increase the P content, we co-gasified and co-combusted bagasse with P-rich chicken manure. The resulting ash was thermochemically post-treated with alkali additives (Na2SO4 and K2SO4) to increase the availability of P to plants. We aimed to: (i) investigate the effect of thermochemical post-treatment of co-gasification residue and co-combustion ash on P availability to soybeans, (ii) explore the potential of chemical extraction methods (citric acid, neutral ammonium citrate, formic acid, and Mehlich-I) and diffusive gradients in thin films (DGT) to predict the availability of P to soybeans, and (iii) identify the responsible P-phases using X-ray diffraction . We evaluated P availability to soybeans growing in Brazilian Oxisol soil in two independent greenhouse pot experiments. The positive effect of thermochemical treatment on P availability from gasification residue was confirmed through the observation of increased P uptake and biomass in soybean plants. These findings were confirmed by chemical extraction methods and DGT. The gasification residue contained whitlockite as its main P-bearing phase. Thermochemical post-treatment converted whitlockite into highly soluble CaNaPO4. In contrast, co-combustion ash already contained highly soluble Ca(Na,K)PO4 as its main P-bearing phase, making thermochemical post-treatment unnecessary for increasing P availability. In conclusion, increased extractability and availability of P for soybeans were closely connected to the formation of calcium alkali phosphate. Our findings indicate that this combined methodology allows for the prediction of P-fertilization effects of ash.
Here, we show that calcium sulfate dihydrate (gypsum) can be directly, rapidly and reversibly converted to calcium sulfate hemihydrate (bassanite) in high salinity solutions (brines). The optimum conditions for the efficient production of bassanite in a short time (<5 min) involve the use of brines with c(NaCl) > 4 M and maintaining a temperature, T > 80 °C. When the solution containing bassanite crystals is cooled down to around room temperature, eventually gypsum is formed. When the temperature is raised again to T > 80 °C, bassanite is rapidly re-precipitated. This contrasts with the better-known behaviour of the bassanite phase in low-salt environments. In low-salinity aqueous solutions, bassanite is considered to be metastable with respect to gypsum and anhydrite, and therefore gypsum-to-bassanite conversion does not occur in pure water. Interestingly, the high-salinity transformation of gypsum-to-bassanite has been reported by many authors and used in practice for several decades, although its very occurrence actually contradicts numerical thermodynamic predictions regarding solubility of calcium sulfate phases. By following the evolution of crystalline phases with in situ and time-resolved X-ray diffraction/scattering and Raman spectroscopy, we demonstrated that the phase stability in brines at elevated temperatures was inaccurately represented in the thermodynamic databases. Most notably for c(NaCl) > 4 M, and T > 80 °C gypsum becomes readily more soluble than bassanite, which induces the direct precipitation of the latter from gypsum. The fact that these transformations are controlled by the solution provides extensive opportunities for precise manipulation of crystal formation. Our experiments confirmed that bassanite remained the sole crystalline phase for many hours before reverting into gypsum. This property is extremely advantageous for practical processing and efficient crystal extraction in industrial scenarios.
Re-melting of scrap in an electric arc furnace (EAF) results in the accumulation of filter dust from off-gas treatment that predominantly consists of iron and zinc oxides. Filter dust is classified as hazardous waste due to its high contents of potentially toxic or ecotoxic elements such as Pb, Cr, Cd, and As. A promising processing route for this waste is selective chlorination, in which the non-ferrous metal oxides are chlorinated and selectively evaporated in form of their respective chlorides from the remaining solids via the process gas flow. Here, we investigate stepwise thermochemical treatment of EAF dust with either waste iron(II) chloride solution or hydrochloric acid at 650, 800, and 1100 ◦C. The Zn and Pb contents of the thermochemically processed EAF dust could be lowered from 29.9% and 1.63% to 0.09% and 0.004%, respectively. Stepwise heating allowed high separation between zinc chloride at the 650 ◦C step and sodium-, potassium-, and lead-containing chlorides at higher temperatures. Furthermore, the lab-scale results were transferred to the use of an experimental rotary kiln highlighting the possibilities of upscaling the presented process. Selective chlorination of EAF dust with liquid chlorine donors is, therefore, suggested as a potential recycling method for Zn-enriched steelworks dusts.
The steel industry is an important engine for sustainable growth, added value, and high-quality employment within the European Union. It is committed to reducing its CO2 emissions due to production by up to 50% by 2030 compared to 1990′s level by developing and upscaling the technologies required to contribute to European initiatives, such as the Circular Economy Action Plan (CEAP) and the European Green Deal (EGD). The Clean Steel Partnership (CSP, a public–private partnership), which is led by the European Steel Association (EUROFER) and the European Steel Technology Platform (ESTEP), defined technological CO2 mitigation pathways comprising carbon direct avoidance (CDA), smart carbon usage SCU), and a circular economy (CE). CE ap-proaches ensure competitiveness through increased resource efficiency and sustainability and consist of different issues, such as the valorization of steelmaking residues (dusts, slags, sludge) for internal recycling in the steelmaking process, enhanced steel recycling (scrap use), the use of secondary carbon carriers from non-steel sectors as a reducing agent and energy source in the steelmaking process chain, and CE business models (supply chain analyses). The current paper gives an overview of different technological CE approaches as obtained in a dedicated workshop called “Resi4Future—Residue valorization in iron and steel industry: sustainable solutions for a cleaner and more competitive future Europe” that was organized by ESTEP to focus on future challenges toward the final goal of industrial deployment.
The present work demonstrates a sustainable approach of using relatively coarser iron ore particles for ironmaking. The motivation is to reduce the energy consumption in the milling of the iron ore by utilizing coarser iron ore particles (+0.05 mm) and to select a suitable binder for improving pellet properties. Iron ore fines in the range of 0.05–0.25 mm was selected and classified into three size ranges. Fluxed iron ore pellets were prepared using lime as a binder for the basicity of 0, 1, and 2. Reduction of these pellets with a packed bed of coal fines was performed in the temperature range of 900–1200 °C for a duration of 30–120 min. The direct reduction kinetics of the iron ore pellets were studied by employing diffusion and chemical reaction control models to the experimental data. The results show that pellets made with coarser iron ore particles have improved reduction behavior and kinetics. The reduction reaction is found to be a mixed control. The activation energy for the reduction reaction varies from 44.3 to 74.76 kJ mol−1 as iron ore particle size decreases from 0.25 to 0.05 mm and basicity increases from 0 to 2.