4 Material und Umwelt
Filtern
Dokumenttyp
- Vortrag (37) (entfernen)
Sprache
- Englisch (37) (entfernen)
Referierte Publikation
- nein (37)
Schlagworte
- PFAS (7)
- Per- and Polyfluoroalkyl substances (PFAS) (6)
- Soil (6)
- Sewage sludge (5)
- XANES spectroscopy (5)
- Ecotoxicity (4)
- Leaching (4)
- Phosphorus (4)
- X-ray absorption near-edge structure (XANES) spectroscopy (4)
- Combustion ion chromatography (3)
Organisationseinheit der BAM
- 4.3 Schadstofftransfer und Umwelttechnologien (37) (entfernen)
Eingeladener Vortrag
- nein (37)
In Europe, nearly 19 Mt/y of bottom ash (BA) are produced. Of this quota, only 46 %wt. was treated, often in poorly performing plants, leaving behind 10 Mt of untreated and unrecovered BA, destined to landfill. The resulting 2.14 Mt loss of valuable materials included 1 Mt mineral fraction and 0.97 Mt ferrous metals, mostly from untreated BA, and 0.18 Mt non-ferrous metals, mostly from unrecovered BA. For the coarser fractions, the main obstacle to BA being used as recycling aggregate is the content of salts and potential toxic elements (PTEs), concentrated in a layer that coats BA particles. For the fine BA fractions, usually underexploited and landfilled, it is estimated that up to 0.95 Mt/y of ferrous and non-ferrous metals are not recovered in Europe.
During the workshop, the key results of BASH Treat project will be presented: the results of 2 industrial tests performed in BA treatment plants in Germany and Sweden; a novel dry treatment for the removal of salts and PTEs from BA coarse particles; a wet process for the recovery of heavy metal compounds from the fine fraction; a technical-economic assessment of the EU potential for the optimization of BA management.
Transformation of carbendazim, diuron, octylisothiazolinone and terbutryn was investigated in two paints containing either white titanium dioxide or a red iron oxide pigment.
Test specimens of these coatings on glass were exposed to water contact and UVA-radiation under laboratory conditions. Panels of birch plywood were coated and exposed to natural weather conditions in a field experiment. Concentrations of biocides and transformation products were analysed in leachates from laboratory tests, runoff samples and remaining coatings. Water contact, UVA radiation as well as pigments in the paints affected the pattern and amount of transformation products.
Tools for the characterization of secondary raw materials - status of leaching test application
(2018)
Leaching tests are used as tools for the assessment of environmental compatibility of granular waste materials with potential for reuse. The presentation gives an overview on available leaching tests, their field of application and relation to legislation. Furthermore robustness testing to elaborate optimized test conditions as well as performance characteristics from validation studies by BAM are addressed.
Tools for the characterization of secondary raw materials - status of leaching test application
(2018)
Leaching tests are used as tools for the assessment of environmental compatibility of granular waste materials with potential for reuse. The presentation gives an overview on available leaching tests, their field of application and relation to legislation. Furthermore robustness testing to elaborate optimized test conditions as well as performance characteristics from validation studies by BAM are addressed.
Thermal Destruction of PFAS
(2023)
Thermal treatment processes are currently the only full-scale option for thedestruction of per- and polyfluoroalkyl substances (PFAS) in large waste streams. While all organic molecules including PFAS are susceptible to thermal destruction, their decomposition rates are controlled by process variables such as temperature, reaction atmosphere, and residence time. Concerns exist about the formation of products of incomplete destruction and their emission from hazardous waste incinerators. This talk will summarize the current stateof-the-art of thermal PFAS destruction, identify research needs, and showcase future research designed to address critical knowledge gaps.
Designing the performance of geogrids in reinforce soil constructions usually does not consider long-term behavior and possible failure modes of junctions between longitudinal and transverse ribs. How could behavior of junctions be included? To which extend is it necessary? On the conference Geo-Chicago 2016, Swan and Yuan presented an ultimate limit state equation for the short-term material resistance of junctions. We discuss limitations and suggest improvements to include long-term behavior of junctions. Nevertheless, the approach applies only to a specific mode of shear-tensile failure of junctions and only to strictly rigid geogrids. A new design concept presented in the same year by Jacobs on the conference GeoAmerica for the special case of the anchorage of geogrids, which reinforce capping system on long and steep slopes of landfills, tried to overcome these drawbacks. We discuss the aspects of this concept related to the long-term behavior of junctions and the interplay between the load applied to junctions and the flexibility of longitudinal ribs. This interplay and the long-term junction strength determine the long-term behavior of geogrids.
Aim. The European biocidal products regulation requires environmental risk assessments for biocidal products under service conditions. This is only possible, if processes that lead to biocide emissions into the environment are understood and can be reasonably predicted.
Actual emissions due to leaching result from different processes that are affected by material properties and environmental conditions. Transformation of biocides can affect emissions considerably.
Leaching and possible transformation of the film preservatives carbendazim, diuron, OIT and terbutryn in paints was observed under laboratory and field conditons in order to investigate the influence of different factors, e.g. water contact and radiation on biocide emissions. The paints contained either white titanium dioxide or a red iron oxide pigment to check whether pigments affect leaching processes.
Methods. Test specimens of a water-based styrene acrylic dispersion paint on glass were exposed to UVA-radiation in a UV weathering device and/or exposed to water contact by immersion events on the basis of the European standard EN 16105. Plywood panels were coated and exposed to natural weather conditions in a semi-field experiment. Concentrations of biocides and transformation products were analysed in leachates from laboratory tests, runoff samples and remaining coatings.
Results. The impact of weathering conditions on transformation processes differs for the investigated active substances. Water contact, radiation as well as pigments in the paints determine the pattern and amount of transformation products on coatings, leachates and runoff water. Observations from laboratory and field experiments were compared. It proved that results from laboratory tests support understanding of data from field experiments.
Detailed knowledge on the fate of active substances under environmental conditions supports manufacturers to develop safe applications of film preservatives and authorities to evaluate its environmental impact.
Half of the global material consumption is mineral material. The circularity is still low so that enhanced use of secondary building material is required to close loops. Three different secondary building materials are discussed based on exemplary research results: construction and demolition waste (C&D waste), soil-like material and incineration bottom ash (IBA). Focus was laid on the environmental compatibility of the materials examined mainly by standardized leaching tests. C&D waste was investigated after a wet treatment using a jigging machine, soil-like material and IBA were characterized with respect to their material composition. The environmental compatibility in particular was studied using standard leaching tests (batch tests and column tests). It was concluded that soil-like material can mostly be utilized even when the precautionary limit values set are exceeded by a factor of less than 2. For C&D waste the fine fraction below 2 mm and the content of brick material is problematic. IBA fulfills quality level HMVA-2 following German regulation. Higher quality levels of utilization might be achievable with better treatment technologies.
The production of secondary materials from waste materials requires, in most cases, significantly lower energy amounts than the primary material production of raw materials. Along with lower energy demand, the greenhouse gas emissions produced are also lower. The duty of a modern waste management system should therefore be to collect and sort the waste materials in a way that the highest amounts of single material fractions with the highest qualities can be generated. In this contribution, the greenhouse gas balances of the theoretical treatment of the household waste, if collected as mixed waste in sanitary landfills, in waste incineration plants, or in mechanical-biological treatment plants, are compared to the existing separate waste collection and treatment in Germany in 2014.
Geosynthetic materials are applied in measures for coastal protection. Weathering or any damage of constructions, as shown by a field study in Kaliningrad Oblast (Russia), could lead to the littering of the beach or the sea (marine littering) and the discharge of possibly harmful additives into the marine environment. The ageing behavior of a widely used geotextile made of polypropylene was studied by artificial accelerated ageing in water-filled autoclaves at temperatures of 30 to 80° C
and pressures of 10 to 50 bar. Tensile strength tests were used to evaluate the progress of ageing, concluding that temperature rather than pressure was the main factor influencing the ageing of geotextiles. Using a modified Arrhenius equation, it was possible to calculate the half-life for the loss of 50% of the strain, which corresponds to approximately 330 years.