4 Material und Umwelt
Filtern
Dokumenttyp
Referierte Publikation
- ja (57) (entfernen)
Schlagworte
- Leaching (12)
- Bottom ash (6)
- Construction products (5)
- Biocides (4)
- Circular economy (4)
- Degradation (4)
- Geosynthetics (4)
- Geotextiles (3)
- PFAS (3)
- Phosphorus (3)
Organisationseinheit der BAM
- 4.3 Schadstofftransfer und Umwelttechnologien (57) (entfernen)
Paper des Monats
- ja (4)
For the first time, fluorine K-edge X-ray absorption near-edge structure (XANES) spectroscopy was applied to detect per- and polyfluoroalkyl substances (PFAS) in various soil and sewage sludge samples. The method can be used to determine the speciation of inorganic and organic fluorides, without pre-treatment of solid samples. Therefore, XANES spectra of several inorganic fluorides as well as selected fluorinated organic compounds were recorded. While inorganic fluorides partially exhibit a variety of sharp spectral features in the XANES spectrum, almost all inspected organofluorine compounds show two distinct broad features at 688.5 and 692.0 eV. Moreover, the peak intensity ratio 688.5 eV/692.0 eV in the PFAS XANES spectrum can be inversely correlated to the chain length of the perfluoro sulfonic acid group. The detection of targeted PFAS by bulk-XANES spectroscopy in combination with linear combination fitting in soils and sewage sludges was not applicable due to the low organic fluorine to total fluorine ratio of the samples (0.01–1.84%). Nonetheless, direct analysis of pure PFAS revealed that analysis of organofluorine species might be achieved in higher concentrated samples. Furthermore, quantitative measurements by combustion ion chromatography (CIC) evaluated as sum parameters extractable organically bound fluorine (EOF) and total fluorine (TF) emphasize that besides soils, sewage sludges are a significant source of organic fluorine in agriculture (154–7209 μg/kg).
Here, we report a comparative study of different sum parameter analysis methods for the extraction of per- and polyfluoroalkyl substances (PFAS) from manufactured consumer products, which can be measured by combustion ion chromatography (CIC). Therefore, a hydrolysis-based extraction method was further developed, which accounts for the addition of hydrolyzable covalently bound polyfluoroalkylated side-chain polymers (SFPs) to the extractable organic fluorine portion of the mass balance proposed as "hydrolyzable organically bound fluorine" (HOF). To test this hypothesis, the method was applied to 39 different consumer products containing fluoropolymers or monomeric PFAS taken from four different categories: outdoor textiles, paper packaging, carpeting, and permanent baking sheets. We also evaluated the method's efficiency by extracting four synthesized fluorotelomer polyacrylate reference compounds. The total fluorine (TF) and extractable organically bound fluorine (EOF) values were measured through CIC using established protocols. The TF values ranged from sub-ppb to %-levels, depending on the compound class. All samples showed results for hydrolyzed organofluorine (HOF) between 0.03 and 76.3 μg/g, while most EOF values were lower (<LOD to 58.1 μg/g). Moreover, the methods were contrasted with the "total hydrolyzable precursor" (THP) assay analyzed using gas-chromatography coupled mass spectrometry (GC-MS), which yielded concentrations of 6:2–10:2 fluorotelomer alcohols (<LOD-568 μg/g) for textile and paper samples. Furthermore, targeted analytical investigation of 25 compounds via liquid chromatography coupled tandem mass spectrometry (LC-MS/MS) was conducted and accounted for significantly lower sum amounts (<LOD-0.98 μg PFAS/g). To estimate the fluorine mass balance of all methods, the fluorine levels of target analytical data were calculated and compared to the sum parameter values and evaluated. Finally, the efficiency of the extraction method was approximated by the recovery analysis of four selected SFP model compounds compared to their TF values, yielding 36.7–74.0% after extraction and 3.8–36.3% after processing the extract for the HOF sum parameter.
This paper focuses on the scandium speciation in bauxite residues of different origin. Insights into mineralchemical similarities and differences of these materials will be presented and links to their natural geological background discussed. The presented research should provide fundamental knowledge for the future development of efficient and viable technologies for Sc-recovery from bauxite residues derived from different bauxites and accumulating at different localities. In total, five bauxite residues were investigated which originated from Greece, Germany, Hungary and Russia (North Ural & North Timan) using a combination of different analytical tools. Those included: laser ablation inductively coupled plasma mass spectrometry, X-ray absorption near Edge structure (XANES) spectroscopy, μ-Raman spectroscopy as well as scanning electron microscopy and electron microprobe analyses. X-ray fluorescence and inductively coupled plasma mass spectrometry were used to determine the overall chemical composition. The investigated samples were found to exhibit a relatively homogenous distribution of Sc between the larger mineral particles and the fine-grained matrix except for Al-phases like diaspore, boehmite and gibbsite. These phases were found to be particularly low in Sc. The only sample where Sc mass fractions in Al-phases exceeded 50 mg/kg was the Russian sample from North Ural. Fe-phases such as goethite, hematite and chamosite (for Russian samples) were more enriched in Sc than the Al-phases.
In fact, in Greek samples goethite showed a higher capacity to incorporate or adsorb Sc than hematite. Accessory minerals like zircon, rutile/anatase and ilmenite were found to incorporate higher mass fractions of Sc (>150 mg/kg), however, those minerals are only present in small amounts and do not represent major host phases for Sc. In Russian samples from North Ural an additional Ca–Mg rich phase was found to contain significant mass fractions of Sc (>500 mg/kg). μ-XANES spectroscopy was able to show that Sc in bauxite residue occurs adsorbed onto mineral surfaces as well as incorporated into the crystal lattice of certain Fe-phases. According to our observations the bauxite type, i.e. karstic or lateritic, the atmospheric conditions during bauxitization, i.e. oxidizing or reducing, and consequently the dominant Sc-bearing species in the primary Bauxite influence the occurrence of Sc in bauxite residues. In karstic bauxites, underlying carbonate rocks can work as a pH-barrier and stabilize Sc. This prevents the Sc from being mobilized and removed during bauxitization. Hence, karstic bauxites are more prone to show a Sc enrichment than lateritic bauxites. Reducing conditions during bauxitization support the incorporation of Sc into clay minerals such as chamosite, which can dissolve and reprecipitate during Bayer processing causing Sc to be redistributed and primarily adsorb onto mineral surfaces in the bauxite residue. Oxidizing conditions support the incorporation of Sc into the crystal lattice of Fe-oxides and hydroxides, which are not affected in the Bayer process. The genetic history of the bauxite is therefore the major influential factor for the Sc occurrence in bauxite residues.
Stormwater from urban areas can transport biocidally active substances and related transformation products from buildings into the environment. The occurrence of these substances in urban runoff depends on the availability of water, and on ultraviolet radiation exposure that causes photolytic reactions. In a systematic laboratory study, painted test specimens were exposed to either ultraviolet radiation, water contact, or a combination of both. Leaching of the biocidally active substances carbendazim, diuron, octylisothiazolinone, terbutryn, and selected transformation products of terbutryn and diuron were observed under various exposure conditions. Remaining concentrations of these substances in the paint were quantified. It was demonstrated that the distribution of active substances and transformation products in eluates and in the coatings themselves differs with exposure conditions. Strategies for environmental monitoring of biocide emissions need to consider the most relevant transformation products. However, environmental concentrations of biocidally active substances and transformation products depend on earlier exposure conditions. As a consequence, monitoring data cannot describe emission processes and predict expected leaching of biocidally active substances from buildings if the data are collected only occasionally.
Almost 500 municipal solid waste incineration plants in the EU, Norway and Switzerland generate about 17.6 Mt/a of incinerator bottom ash (IBA). IBA contains minerals and metals. Metals are mostly separated and sold to the scrap market and minerals are either disposed of in landfills or utilised in the construction sector. Since there is no uniform regulation for IBA utilisation at EU level, countries developed own rules with varying requirements for utilisation. As a result from a cooperation network between European experts an up-to-date overview of documents regulating IBA utilisation is presented. Furthermore, this work highlights the different requirements that have to be considered. Overall, 51 different parameters for the total content and 36 different parameters for the emission by leaching are defined. An analysis of the defined parameter reveals that leaching parameters are significantly more to be considered compared to total content parameters. In order to assess the leaching behaviour nine different leaching tests, including batch tests, up-flow percolation tests and one diffusion test (monolithic materials) are in place.
A further discussion of leaching parameters showed that certain countries took over limit values initially defined for landfills for inert waste and adopted them for IBA utilisation. The overall utilisation rate of IBA in construction works is approximately 54 wt%. It is revealed that the rate of utilisation does not necessarily depend on how well regulated IBA utilisation is, but rather seems to be a result of political commitment for IBA recycling and economically interesting circumstances.
Solid wastewater-based fertilizers were screened for per- and polyfluoroalkyl substances (PFAS) by the extractable organic fluorine (EOF) sum parameter method. The EOF values for ten sewage sludges from Germany and Switzerland range from 154 to 7209 mg kg−1. For thermal treated sewage sludge and struvite the EOF were lower with values up to 121 mg kg−1. Moreover, the application of PFAS targeted
and suspect screening analysis of selected sewage sludge samples showed that only a small part of the EOF sum parameter values can be explained by the usually screened legacy PFAS. The hitherto unknown part of EOF sum parameter contains also fluorinated pesticides, pharmaceutical and aromatic compounds. Because these partly fluorinated compounds can degrade to (ultra-)short PFAS in wastewater treatment plants they should be considered as significant sources of organic fluorine in the environment. The combined results of sum parameter analysis and suspect screening reveal the need to update current regulations, such as the German fertilizer ordinance, to focus not solely on a few selected PFAS such as perfluorooctane sulfonic acid (PFOS) and perfluorooctanoic acid (PFOA) but
consider an additional sum parameter approach as a more holistic alternative. Moreover, diffusion gradient in thin-films (DGT) passive samplers were utilized as an alternative simplified extraction method for PFAS in solid wastewater-based fertilizers and subsequently quantified via combustion ion chromatography. However, the DGT method was less sensitive and only comparable to the EOF values
of the fertilizers in samples with >150 mg kg−1, because of different diffusion properties for various PFAS, but also kinetic exchange limitations.
In 2018 municipal solid waste (MSW) incineration in Europe produced nearly 19 Mt of bottom ash (BA); only 46 %-wt. was treated, often in poorly performing plants, leaving behind 10 Mt of untreated and unrecovered BA, destined to landfill. This work was based on the inventory of BA across Europe, and on the hypothesis to achieve complete BA valorisation through two assumptions: treating 100% BA and minimizing the loss of valuable fractions due to technical limitations of state-of-the-art processes in comparison to advanced innovative processes. The research involved three phases: characterization of potential secondary raw materials (metals and mineral fraction) currently lost from untreated (the surplus compared to treatment capacity) and unrecovered BA (the fine fraction) through material flow analysis; environmental assessment (energy balance and net GHG emissions) of complete BA valorisation; investigation of the economic feasibility of complete BA Valorisation through state-of-the-art technologies. The resulting 2.14 Mt loss of valuable materials included 1 Mt Mineral fraction and 0.97 Mt ferrous metals, mostly from untreated BA, and 0.18 Mt non-ferrous metals, mostly from unrecovered BA. The energy balance and GHGs emissions required by the treatment of the currently untreated and unrecovered fractions of BA resulted in energy and GHGs emissions savings. Economic profitability was driven by iron and copper recycling and avoided landfill fees. Profitability was achieved by two thirds of considered countries (average values: NPV 83 M€, ROI 20%, payback time 11 years) with BA mass flow exceeding 0.02 Mt.
This Special Issue, ‘Measurement of the Environmental Impact of Materials’, is focused on the impact that materials have on the environmental compartments of soil, water and air. Leaching and emission processes, including underlying mechanisms, are a recurring topic in most published articles in the present Special Issue. Contributions have come from three continents and numerous countries (USA, Germany, France, Latvia, Poland, Russia, Japan, Korea and Thailand) indicating the global dimension of the subject.
Municipal solid waste incineration (MSWI) is one of the leading technologies for municipal solid waste (MSW) treatment in Europe. Incineration bottom ash (IBA) is the main solid residue from MSWI, and its annual European production is about 20 million tons. The composition of IBA depends on the composition of the incinerated waste; therefore, it may contain significant amounts of ferrous and non-ferrous (NFe) metals as well as glass that can be recovered. Technologies for NFe metals recovery have emerged in IBA treatment since the 1990s and became common practice in many developed countries. Although the principles and used apparatus are nearly the same in all treatment trains, the differences in technological approaches to recovery of valuable components from IBA – with a special focus on NFe metals recovery – are summarized in this paper.
Microspectroscopy reveals dust-derived apatite grains in acidic, highly-weathered Hawaiian soils
(2021)
Dust deposition is an important source of phosphorus (P) to many ecosystems. However, there is little evidence of dust-derived P-containing minerals in soils. Here we studied P forms along a well-described climatic Gradient on Hawaii, which is also a dust deposition gradient. Soil mineralogy and soil P forms from six sites along the climatic gradient were analyzed with bulk (X-ray diffraction and P K-edge X-ray absorption near edge structure) and microscale (X-ray fluorescence, P K-edge X-ray absorption near edge structure, and Raman) analysis methods. In the wettest soils, apatite grains ranging from 5 to 30 μm in size were co-located at the micro-scale with quartz, a known continental dust indicator suggesting recent atmospheric deposition. In addition to co-location with quartz, further evidence of dust-derived P included backward trajectory modeling indicating that dust particles could be brought to Hawaii from the major global dust-loading areas in central Asia and northern Africa. Although it is not certain whether the individual observed apatite grains were derived from long-distance transport of dust, or from local dust sources such as volcanic ash or windblown fertilizer, these observations offer direct evidence that P-containing minerals have reached surface layers of highly-weathered grassland soils through atmospheric deposition.