Geosynthetics are widely used in hydraulic engineering and within coastal protection constructions at the Baltic Sea shore, such as walls, promenades, and gabions walls. Storms influence leads to deformation of some of the protection structures and cause the release of geotextiles onto the beach. Fragments of geotextile migrate along the shore, experiencing additional degradation and destruction down to macro-, meso-, and micro-particles. During October 2017 - March 2018, the Baltic Sea shore along the Sambia Peninsula (Kaliningrad Oblast of the Russian Federation) was monitored to establish the contamination of sandy beaches by geotextiles that had degraded. Several local sources of pollution of beaches by geosynthetic materials were established.
Rohstoffe sind knapp. Hinzu kommt, dass auf dem Weg vom Erz zum Metall viel Energie benötigt wird, mechanische Energie beim Zerkleinern, thermische Energie beim Schmelzen oder elektrische Energie bei der Elektrolyse. Ausgedrückt als Exergie kann man die Verbräuche gut vergleichen. Die meisten technischen Prozesse sind aber vom berechneten thermodynamischen Optimum weit entfernt.
Microplastics are increasingly entering marine, limnic and terrestrial ecosystems worldwide, where they sorb hydrophobic organic contaminants. Here, the sorption behavior of the fuel-related water contaminants benzene, toluene, ethyl benzene and xylene (BTEX) and four tertiary butyl ethers to virgin and via UV radiation aged polypropylene (PP) and polystyrene (PS) pellets was investigated. Changes in material properties due to aging were recorded using appropriate polymer characterization methods, such as differential scanning calorimetry, Fourier transform infrared spectroscopy, gel permeation chromatography, X-ray photoelectron spectroscopy, and microscopy.
Pellets were exposed to water containing BTEX and the ethers at 130-190 mg/L for up to two weeks.
Aqueous sorbate concentrations were determined by headspace gas chromatography. Sorption to the polymers was correlated with the sorbate's Kow and was significant for BTEX and marginal for the ethers.
Due to substantially lower glass transition temperatures, PP showed higher sorption than PS. Aging had no effect on the sorption behavior of PP. PS sorbed less BTEX after aging due to an oxidized surface layer.
Construction products are in contact with water (e.g., rain, seepage water) during their service lifetime and may release potentially harmful compounds by leaching processes. Monitoring studies showed that compounds attributed to construction products are found in storm water and the receiving bodies of water and that the release of biocides in urban areas can be comparable to the input of pesticides from agricultural uses. Therefore, a prospective risk assessment of such products is necessary. Laboratory leaching tests have been developed by the Technical Committee CEN/TC 351 and are ready to use. One major task in the future will be the evaluation of the leaching test results, as concentrations found in laboratory experiments are not directly comparable to the field situations. Another Task will be the selection of compounds to be considered for construction products, which are often a complex mixture and contain additives, pigments, stabilization agents, etc. The formulations of the products may serve as a starting point, but total content is a poor predictor for leachability, and analysis of the eluates is necessary. In some cases, nontargeted approaches might be required to identify compounds in the eluates. In the identification process, plausibility checks referring to available information should be included. Ecotoxicological tests are a complementary method to test eluates, and the combined effects of all compounds—including Degradation products—are included. A bio test battery has been applied in a round robin test and was published in a guidance document. Published studies on the ecotoxicity of construction products show the tests’ suitability to distinguish between products with small and larger effects on the environment.