3.1 Sicherheit von Gefahrgutverpackungen und Batterien
Filtern
Dokumenttyp
- Zeitschriftenartikel (27)
- Vortrag (26)
- Posterpräsentation (11)
- Beitrag zu einem Tagungsband (5)
Sprache
- Englisch (69) (entfernen)
Schlagworte
- Dangerous goods packagings (19)
- Sift-proofness (11)
- Drop test (9)
- Lithium Ion Batteries (9)
- Bags (6)
- Structural dynamics (5)
- Thermal Runaway (5)
- Ageing (4)
- Angle of repose (4)
- Bubble test (4)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (69)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (69)
- 8 Zerstörungsfreie Prüfung (11)
- 7 Bauwerkssicherheit (10)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (8)
- 1 Analytische Chemie; Referenzmaterialien (7)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (7)
- 1.6 Anorganische Referenzmaterialien (6)
- 5 Werkstofftechnik (6)
- 5.1 Mikrostruktur Design und Degradation (5)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (26)
Exploring the electrochemical and physical stability of lithium-ion cells exposed to liquid nitrogen
(2024)
The transport and storage of lithium-ion (Li-ion) batteries — damaged or in an undefined state — is a major safety concern for regulatory institutions, transportation companies, and manufacturers. Since (electro)chemical reactivity is exponentially temperature-dependent, cooling such batteries is an obvious measure for increasing their safety.
The present study explores the effect of cryogenic freezing on the electrochemical and physical stability of Li-ion cells. For this purpose, three different types of cells were repeatedly exposed to liquid nitrogen (LN2).
Before and after each cooling cycle, electrical and electrochemical measurements were conducted to assess the impact of the individual freezing steps. While the electrochemical behavior of the cells did not change significantly upon exposure to LN2 , it became apparent that a non-negligible number of cells suffered from physical changes (swelling) and functional failures. The latter defect was found to be caused by the current interrupt device of the cylindrical cells. This safety mechanism is triggered by the overpressure of expanding nitrogen which enters the cells at cryogenic temperatures.
This study underlines that the widely accepted reversibility of LN2 -cooling on a material scale does not allow for a direct extrapolation toward the physical integrity of full cells. Since nitrogen enters the cell at cryogenic temperatures and expands upon rethermalization, it can cause an internal overpressure. This can, in turn, lead to mechanical damage to the cell. Consequently, a more appropriate temperature condition — less extreme than direct LN2 exposure — needs to be found
A high precision nail‐penetration (NP) tool for characterizing the mechanically induced thermal‐runaway (TR) of lithium‐ion battery (LIB) cells in a defined range of temperatures down to −140 °C was developed. To understand the cell specific behavior at low temperatures aiming at the determination of safe handling conditions, different scenarios are analyzed. First, accuracy tests of the NP‐tool regarding motion and penetration depth are conducted with cylindrical cells at different temperatures. Thus, postmortem computer tomographic (CT) images are compared to the data measured with the newly integrated 3‐axis force sensor which is further combined with a high‐resolution position sensor. The herein developed setup allows evaluation of the NP‐metrics at an accuracy of ±1 pierced electrode layer without CT‐scans. Further NP examinations at 20 °C of fully charged cylindrical lithium nickel manganese cobalt oxide cells reveal a reproducible minimum damage as a reliable TR‐trigger. Moreover, NP‐tests at low temperature disclose a relation of the short circuit conductivity and TR‐reactions during subsequent rethermalization to room temperature. Finally, the implementation of a novel fixture for a controlled very fast cooling of LIB‐cells during critical damage opens the way to investigate the individual steps during a TR and, thus, to gain important information of the specific TR‐mechanism of different LIB‐cells.
Lithium-ion batteries usually consist of numerous individual cells. There is ongoing discussion about enhancing sustainability by considering the replacement of heavily aged or damaged cells. Nevertheless, the planned replacement of individual cells poses significant challenges in ensuring the required reliability and safety of the refurbished device.
AbstractLithium‐ion cells connected in series are prone to an electrical safety risk called overdischarge. This paper presents a comprehensive investigation of the overdischarge phenomenon in lithium‐ion cells using operando nondestructive imaging. The study focuses on understanding the behavior of copper dissolution and deposition during overdischarge, which can lead to irreversible capacity loss and internal short‐circuits. By utilizing synchrotron X‐ray computed tomography (SXCT), the concentration of dissolved and deposited copper per surface area is quantified as a function of depth of discharge, confirming previous findings. The results also highlight for the first time a nonuniform distribution pattern for copper deposition on the cathode. This research provides insights for safer battery cell design.
Due to their increasing energy density, lithium-ion-batteries (LIBs) play a key role in the traffic energy transition. Regarding their safety behavior, the main challenge of LIB-cells remains the thermal runaway (TR) process. In situ/operando investigations of the TR on commercial cells is possible with radiographic and computer tomographic measurements. Nonetheless, high resolution visualization of the TR persists as a challenge due to the high progression speed of the TR-process itself. Generally, performing abuse tests at cryogenic temperatures allows to slow down or even prevent the TR. Nevertheless, not all abuse methods are suitable for TR investigations at low temperatures. Nail penetration is an appropriate option, however, contains numerous unknown parameters and therefore suffers regarding reproducibility.
Herein, a self-developed high precision nail-penetration-setup is introduced, approaching the necessary mechanically reproducibility with controlled temperatures down to -190°C. The setup allows the preparation of critically abused, however, at cryogenic temperatures stable LIB-cells. These cells were controlled rethermalized to room temperature during synchrotron x-ray computer tomography (SXCT) with a pixel size up to 0.7 μm. During this measurement, the temperature and voltage of the cell is monitored allowing the visualization of the initial internal cell reactions. This study reveals the relation between internal reactions and cell voltage. Finally, the developed set-up enables in-depth analysis of thermal runaway behavior down to material level for various commercial battery cells in the future.
Next to performance features, safety aspects of lithium-ion batteries (LIBs) are a crucial research field. The abuse/misuse of a LIB can trigger a chain of exothermic reactions on cell level. Hence, the cell temperature increases dramatically, causing the so-called thermal runaway (TR). Moreover, the TR of one cell can initiate the TR of adjacent cells leading to a TR-propagation. Due to the risk of a TR, special measures need to be applied while handling, storing, and transporting batteries. According to current transport regulations, all different types of lithium-ion and lithium metal cells/batteries (by means of cell format, cathode chemistry, etc.) require the same transport conditions regardless of the intensity of their reaction during abuse tests. To allow more differentiated transport requirements, the United Nations (UN) Subcommittee Transport of Dangerous Goods created an Informal Working Group (IWG) on the topic of a hazard-based classification of LIBs. BAM is one of nine laboratories working on the development of a respective classification scheme including appendant test protocols.
Herein, we discuss the latest results of our safety tests on commercial LIB-cells employing the test protocols developed in the UN-IWG. Single cell tests are analysed regarding different hazardous features during the TR, e.g., cell temperature, flame occurrence, and gas amount. Next to the general occurrence of a propagation, the propagation speed is analysed by propagation tests. In total, the presented results are gathered from over 200 tests. Next to the classification of the tested cells, the data set obtained is analysed in respect to the cells’ key features, such as cell energy, state of charge and cathode type. Generally, the presented results can increase the overall understanding of the TR-mechanism supporting the design of advanced safety measures on cell level in the future.
Lithium-ion batteries (LIBs) are essential for the electrification of vehicles and play an important role for stationary storage units needed for grid-balancing. Research groups all over the world work on the improvement of LIBs regarding an increase in energy density as well as cycle-life and a decrease in costs. Next to these research topics, a continuously uprising and crucial field is safety features of LIBs, which can be implemented at different levels, such as material, cell, battery and system level.
The abuse/misuse of a LIB can cause an internal release of heat which can trigger a chain of exothermic reactions on cell level. Hence, the cell temperature increases dramatically, causing the so-called thermal runaway (TR), possibly leading to flames and/or explosion of the cell. Moreover, the TR of one cell can initiate the TR of adjacent cells leading to a so-called propagation, possibly, causing the TR of the whole battery. Ideally, easily obtainable key features of a certain cell – such as cathode type, cell format, cell energy and state of charge (SOC) - could allow the prediction of its behaviour under abuse conditions. In the present study, we will discuss the latest result of our safety tests on cell level employing an external heater as TR-trigger. Single cell tests will be analysed regarding different hazardous features during the TR, e.g., cell temperature, occurrence of flames, peak pressure, gas amount and gas composition. Moreover, the possibility of a TR-propagation and the respective propagation speed will be gained from propagation tests utilizing six cells with identical SOC. In total, the study comprises over 200 tests on cell level. The gained data set is analysed in respect to the cell parameters, such as cell format, cell energy, SOC and the cathode type as well as the atmosphere (air vs. N2) present during the test. A special focus is put on the discussion of general conclusions linking cell parameters to TR-effects and propagation behaviour.
The findings regarding common conclusions between key features and TR-effects can enable a rather facile selection process of cells/batteries for certain applications according to specific safety targets. Moreover, it allows to choose cell-specific safety measures, suitable during operation. In further works, the study will be extended to end-of-first life cells yielding important conclusions regarding crucial safety aspects for the implementation of those cells in 2nd-life application. Generally, the presented results can increase the overall understanding of the TR mechanism supporting the design of advanced measures to enhance the safety on cell level in the future.
Lithium-ion battery (LIB) powered devices, such as laptops, mobile phones and power tools are ubiquitous in our daily lives. Moreover, LIBs are essential for the electrification of vehicles, and play an important role for stationary storage units needed for grid-balancing. The improvement of LIBs, in terms of increasing energy density as well as cycle-life and decreasing costs, is tackled by numerous research groups all over the world. In the last years, research regarding safety aspects has steadily gained more interest. The safety of LIBs can be implemented at different levels, such as material, cell, battery and system level.
The abuse/misuse of an LIB can lead to an internal increase in heat which can trigger a chain of exothermic reactions on cell level. Thus, the cell temperature increases dramatically causing the so-called thermal runaway (TR). This process can lead to flames and/or explosion of the cell. Furthermore, the TR of one cell can initiate the TR of adjacent cells causing the so-called propagation, possibly, leading to the TR of the whole battery.
Herein, we will show the latest result of our safety tests on cell level employing an external heater as TR-trigger. Regarding single cell tests, we will compare different hazardous features during the TR, e.g., cell temperature, occurrence of flames, peak pressure, and toxic gases, depending on the cell format, cell energy and the cathode type. The same cell parameters will be used to discuss the results of the propagation tests. Moreover, the influence of the state of charge (SOC) and the present atmosphere (air vs. N2) as well as the repeatability will be discussed. Overall, the study comprises over 180 tests on cell level.
The findings regarding the TR behaviour can be used to create a hazard-classification scheme of LIBs, e.g., allowing the definition of (cell type specific) conditions for a safe transport. Furthermore, the results can increase the general understanding of the TR mechanism promoting the development of advanced measures to enhance the safety on cell level in the future.