A new method for the evaluation of the low temperature properties of rubber materials is presented. The method emulates the standardized compression set measurement, which is frequently used for sealing materials, but can be performed within a considerably shorter time. The results are compared with the standard test and found to be qualitatively the same. Slight differences are discussed on the basis of the differences in the measurement procedures. Further data evaluation is done by fitting functions to describe the material behaviour.
The method for the determination of compression set values with a Dynamic Mechanical Analysis (DMA) setup at low temperatures, which was presented previously, allows a much faster and readily automated procedure than the standardized compression set test according to ISO 815-2. This method is applied to a series of different elastomeric materials that are commonly used for sealing applications. The results of the compression set test are compared with results from thermal analysis to allow an in depth comparison of the material behaviour at low temperatures.
Furthermore, a comparison between two EPDM materials is presented. These materials show very similar properties determined by thermo analytical methods such as Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) but differ clearly in their compression set behaviour. This comparison shows the importance and value of information of the compression set test in addition to thermal analysis to judge the behaviour of sealing materials and confirms the relevance of the new compression set test method for the investigation of low temperature properties of elastomers.
Der Druckverformungsrest (DVR) stellt insbesondere für Dichtungsanwendungen eine wichtige Kenngröße zur Beurteilung der Eignung eines Elastomers dar. Er ermöglicht die Einschätzung des zeitabhängigen Rückstellverhaltens eines Werkstoffs nach Deformation. Neben der Prüfung bei erhöhten Temperaturen, zur Beurteilung des Alterungsverhaltens, lässt sich bei der Durchführung bei tiefen Temperaturen die limitierende Einsatztemperatur bestimmen. Die Versuchsdurchführung unterscheidet sich je nach angewandter Norm und kann einen deutlichen Einfluss auf den DVR-Wert haben. Um bei tiefen Temperaturen eine schnelle Aussage zu gestatten, ist eine im Vergleich zu genormten Methoden deutlich schneller durchzuführende, automatisierte Methode entwickelt und mit Standardmethoden verglichen worden. Durch kontinuierliche Messung des Druckverformungsrests kann die Kinetik der Materialrückstellung betrachtet und dadurch ein effizienter Materialvergleich und eine effiziente Materialauswahl ermöglicht werden. Compression set (CS) is especially for sealing applications an important parameter for material selection. It allows an assessment of the time dependent recovery after deformation.
In addition to testing at elevated temperatures which aims at the evaluation of the ageing behaviour, testing at low temperatures permits the determination of the low working temperature limit. The test procedure varies depending on the applied standard and can show a significant effect on the CS value. In order to allow a quick statement regarding low temperatures an automated procedure being significantly faster realisable in relation to the standardised methods has been developed and compared with standard procedures. Continuous measurement of the compression set allows evaluating the recovery kinetics and therefore an efficient comparison and selection of materials.
Rubber is widely used as sealing material in various applications. In many fields the sealing function at low temperatures is necessary. Therefore the understanding of failure mechanisms is of high importance. Rubbers are normally used above their glass-rubber transition region but the minimum working temperature limit is not defined precisely. Therefore the lower operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with the results of the standardized compression set according to ISO 815 respectively a modified test using the DMA equipment.
Rubbers are widely used as sealing material in various applications. In many fieldsthefunction of seal materials at lowtemperatures is required. Therefore the understanding of faiiure mechanisms that lead to leakage at low temperatures is of high importance. Therefore the lower Operation temperature limit of rubber seals should be determined in dependence of the material properties.
The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the Standard tests a faster and more efficient technique was developed and applied. In addition the breakdown temperature of the sealing function of O-ring seals at lowtemperatures is measured in a component test Setup in dependence of the material and the degree of compression.
Elastomers are widely used as the main sealing materials for containers for low and intermediate level radioactive waste and as an additional component to metal seals in spent fuel and high active waste containers. The safe encapsulation of the radioactive container inventory has to be guaranteed according to regulation and appropriate guidelines for long term storage periods as well as for temperatures as low as -40°C during transport. Therefore, the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. It is known that the material properties of elastomers are strongly temperature dependent. At low temperatures, this is caused by the rubber-glass transition (abbreviated: glass transition). During continuous cooling, the material changes from a rubber-like entropy elastic to a stiff energy elastic behaviour, which allows nearly no strain or retraction. Hence, rubbers are normally used above their glass transition, but the minimum working temperature limit is not defined precisely; this can cause problems during the above noted applications. Therefore, the lower operation temperature limit of elastomer seals must be determined in dependence of the material properties. Differential scanning calorimetry (DSC) and dynamic mechanical analysis (DMA) are combined with standardised measurements to determine the compression set according to ISO 815. To reduce the test time of the standard tests, a faster technique than normally used was developed. Additionally, the breakdown temperature of the sealing function of complete O ring seals was measured in a component test set-up to compare it with the results of the other tests. The experimental set-up is capable of measuring the leakage rate at low temperatures by the pressure rise method. A fluorocarbon rubber (FKM) was selected for this investigation as it is often used for radioactive waste containers. The materials (seals and test sheets) were purchased from a commercial seal producer.