While artificial weathering is a long-established tool to investigate long-term behaviour of polymers at outdoor conditions, the use of chemiluminescence as a highly sensitive and broadly applicable sensor for the effected change is a recent addition. This combination of artificial weathering with chemiluminescence could already be successfully applied to differentiate and evaluate long-term stability of various real use polymeric building materials relatively to each other and promises to be a useful tool for a variety of other polymeric materials as well.
Degradation effects of automotive coatings after weathering as detected by thermoluminescence
(2004)
To determine a polymer’s spectral response of photo degradation, two main methods have been established. The so-called “filter technique” uses polychromatic radiation, which is filtered by a set of various sharp cut-on filters. This procedure provides separated reading points of an activation spectrum of the investigated material. With the "spectrographic technique” a specimen is irradiated with pectrally dispersed radiation, locally quasi monochromatically, and the local property changes.are related to the radiant exposure at the respective wavelengths. A third method, the irradiation of specimens with quasi monochromatic radiation behind interference filters, is rarely used.
These methods have advantages and disadvantages and therefore, there are limits for conclusions from these spectral data. Concerning the quasi monochromatic Irradiation of specimens the development of new UV radiation sources looks promising.
With the rapid development of inexpensive UV Light-emitting diodes (LEDs), new : sources of nearly monochromatic radiation in the UV ränge are available, even down to about 250 nm. To determine the spectral response, the use of such UV-LEDs in TO-18 ) and TO-39 metal cases combines the advantages of low cost and energy efficiency, stable spectral irradiance, temperature.and humidity control, larger specimen areas, and an easy and stable analysis.
Combinations of different UV LEDs are also discussed as replacement for xenon arc ' radiation sources, see patent application EP01528388A1.
Chemiluminescence (CL) is a sensitive method of investigating the thermo-oxidative stability of polymers in the early stages of degradation. Therefore, CL measurements were applied to different automotive coatings to evaluate their degradation behavior during artificial weathering. In this work, CL measurements were carried out for different automotive coatings to follow their degradation behavior during artificial weathering. The CL emission depends on sample-specific parameters like stabilizer, matrix, or hardener; experimental parameters like the oxygen partial pressure; and exposure parameters like the duration of weathering. The potential of CL could be demonstrated by classifying materials into categories of good, medium, and low degradation performance at a much earlier stage of weathering exposure than in combination with the usual visual detection of weathering effects.
Combined impact of ultraviolet and chemical fluids on high-density polyethylene packaging material
(2012)
To investigate the ageing behaviour of filled plastic containers outdoors, square cuts of the wall of two high-density polyethylene (HDPE) types were exposed to ultraviolet (UV) radiation at their front side and to specific liquid chemicals (de-ionized water, surfactant or White Spirit) at their back. The UV radiant exposure at the front side was 80 MJ/m².
To compare the actions of the different exposures, separate dark backside fluid exposures were performed, in parallel. Besides, UV weathering was carried out until a UV radiant exposure of 325 MJ/m², being roughly comparable to outdoor exposure of one year in Northern Australia.
An unpigmented HDPE included in the investigation gave no sufficient protection for the White Spirit. In addition, it showed clear degradation after several of these exposures. In combination with the White Spirit, an increase of carbonyl bonds was measured, presumably assignable to degradation products of the White Spirit.
For a pigmented HDPE material, with the implemented combined exposures, no relevant damage was observed, within applied the exposure period.
Scrap tyres are widely reused in the form of granules as infill materials or component of sub-base layers in construction of sporting grounds such as synthetic turf areas and athletic track surfaces. The recycled rubber may contain organic and inorganic pollutants due to the presence of vulcanisation catalysts, stabilisers and other additives which can be released into soil and groundwater in the case of outdoor sports facilities. In order to evaluate the amount of potentially mobile pollutants, leaching tests can be employed. This study aimed particularly at the investigation of the feasibility of column tests using complete synthetic surface flooring or turf system assemblies. The release of zinc and polycyclic aromatic hydrocarbons (PAH) leached from components of sports surfaces containing recycled rubber granules was considered. Additionally, batch tests on coated and uncoated styrene butadiene rubber (SBR) granules aged by artificial weathering were performed to indicate its possible influence on the leaching behaviour of zinc and PAH. The chosen approach of column tests simulating typical complete synthetic sports surface installations has been proven to be feasible and robust. The time-dependent leaching behaviour and interactions between single components can be evaluated by column tests. Zinc was the most relevant contaminant in the eluates and its leachability was enhanced after accelerated ageing by artificial weathering. Leachable PAH were found in relatively low but well detectable amounts which increase by ageing as well.
Jerrycans made from three different types of high-density polyethylene (HDPE) were exposed outdoors, for one Berlin summer season. They were filled with a 55 percent nitric acid solution (HN03), pure water, or air, and half of them were protected from sunlight by an UV absorbing canvas. Thus, the separate effects of UV radiation and nitric acid could be compared to the combined impact. Combined impact was mainly affected by decomposition of nitric acid, resulting in presence of reactive nitrogen oxides, increased oxygen partial pressure, and UV radiation energy, simultaneously in vapour phase.
To investigate the degradation effects after the outdoor exposure, jerrycans were exposed to a so called hydraulic internal pressure test, similar to an approval test for dangerous goods packaging. After combined impact of UV radiation and nitric acid, internal pressure tests showed very fast failures, whereas after separate impacts no remarkable deteriorations were observed, compared to unaged jerrycans.