Two methods were employed to prepare hyperbranched polyamine ester (HPAE)/kaolinite (Ka) nanocomposites resulting in different morphologies. In the case of the in situ polymerization, diethanolamine is inserted as monomer between the Ka layers and polymerized with methyl acrylate to prepare HPAE/Ka–DEA nanocomposites. For the ex situ method, Ka is modified with dodecylamine and solution-blended with HPAE. The former method leads to an intercalated morphology where the latter approach results in an exfoliated structure, as proofed by SAXS and TEM. A complementary combination of methods like differential scanning calorimetry (DSC), broadband dielectric relaxation (BDS), and specific heat spectroscopy (SHS) was used to investigate both kinds of nanocomposites in detail. Above Tg, the dielectric spectra are dominated by the conductivity contribution while the segmental dynamics is retrieved by SHS. A comparison of the temperature dependencies reveals a decoupling of segmental dynamics and conductivity, which becomes weaker with decreasing fragility.
Particle size modality in bi-modal iron oxide suspensions was resolved by exploiting complex ac-susceptibility (ACS), small angle X-ray scattering (SAXS) and photon cross-correlation spectroscopy. To explain dynamic magnetic response of bi-modal suspensions, the Debye model was expanded to a linear superposition form allowing for the contribution of both particle fractions. This modified and adopted model is able to resolve the bi-modal particle size distributions. The SAXS curves of mono- and bi-modal suspensions were fitted well using a Monte Carlo simulation scheme, allowing the detection of bi-modal particle size distributions with high precision.
Because of the rising application of nanoparticles in food and food-related products, we investigated the influence of the digestion process on the toxicity and cellular uptake of silver nanoparticles for intestinal cells. The main food components – carbohydrates, proteins and fatty acids – were implemented in an in vitro digestion process to simulate realistic conditions. Digested and undigested silver nanoparticle suspensions were used for uptake studies in the well-established Caco-2 model. Small-angle X-ray scattering was used to estimate particle core size, size distribution and stability in cell culture medium. Particles proved to be stable and showed radii from 3.6 to 16.0 nm. Undigested particles and particles digested in the presence of food components were comparably taken up by Caco-2 cells, whereas the uptake of particles digested without food components was decreased by 60%. Overall, these findings suggest that in vivo ingested poly (acrylic acid)-coated silver nanoparticles may reach the intestine in a nanoscaled form even if enclosed in a food matrix. While appropriate for studies on the uptake into intestinal cells, the Caco-2 model might be less suited for translocation studies. Moreover, we show that nanoparticle digestion protocols lacking food components may lead to misinterpretation of uptake studies and inconclusive results.
Resovist® originally developed as a clinical liver contrast agent for Magnetic Resonance Imaging exhibits also an outstanding performance as a tracer in Magnetic Particle Imaging (MPI). In order to study the physical mechanism of the high MPI performance of Resovist®, we applied asymmetric flow fieldflow fractionation (A4F) and static magnetic fractionation (SMF) to separate Resovist® into a set of fractions with defined size classes. As A4F based on an elution method separates MNP according to their hydrodynamic size, SMF fractionates a particle distribution by its magnetic moment. The obtained fractions of both separation techniques were then magnetically characterized by magnetorelaxometry measurements to extract the corresponding effective magnetic anisotropy and hydrodynamic size distribution parameters. Additionally, the MPI performance of each fraction was assessed using magnetic particle spectroscopy. With both separation techniques fractions (normalized to their iron amount) an MPI signal gain of a factor of two could be obtained, even though the distribution of effective anisotropy and hydrodynamic size were significantly different. Relating these findings to the results from magnetic characterization allows for a better understanding of the underlying mechanisms of MPI performance of Resovist®. This knowledge may help to improve the design of novel MPI tracers and development of separation methods.
We report on the formation of polymer-stabilized superparamagnetic single-core and multi-core maghemite nanoparticles. The particle formation was carried out by coprecipitation of Fe(II) and Fe(III) sulfate in a continuous aqueous process using a micromixer system. Aggregates containing 50 primary particles with sizes of 2 nm were formed at a reaction temperature of 30 °C. These particles aggregated further with time and were not stable. In contrast, stable single-core particles with a diameter of 7 nm were formed at 80 °C as revealed by small-angle X-ray scattering (SAXS) coupled in-line with the micromixer for particle characterization. X-ray diffraction and TEM confirmed the SAXS results. X-ray absorption near-edge structure spectroscopy (XANES) identified the iron oxide phase as maghemite.
The development of novel dendrimers containing oligospiroketal (OSK) rods as building blocks is described. The linkage between the core unit (CU), branching units (BU), and OSK rods relies on the CuAAC reaction between terminal alkynes and azides. Two different strategies of dendrimer synthesis were investigated and it was found that the convergent approach is clearly superior to the divergent one. SAXS measurements and MD simulations indicate that the obtained dendrimer features a globular structure with very low density. Obviously, the OSK rods stabilize a rather loose mass-fractal structure.
We studied the magnetic resonance imaging liver contrast agent Resovist by a variety of magnetic measurement techniques, in order to understand the physical mechanism of their high magnetic particle imaging (MPI) performance, wirh a focus on the size-dependent contributions of the MPI signal. To this end, we used asymmetric flow field-flow fractionation to separate Resovist into a set of fractions with defined hydrodynamic diameters. The individual fractions were magnetically characterized by static magnetization and magnetorelaxometry measurements to obtain the corresponding effective magnetic anisotropy and effective size distribution parameters. In addition, the MPI performance of each fraction was assessed by magnetic particle spectroscopy. We observed an MPI signal gain of about 100% with respect to their iron amount for the best fraction. Relating these finding to the results from magnetic characterization provides more insight into mechanisms of MPI performance of Resovist. This knowledge may help to improve the design of novel MPI tracers.