We report on ultrasmall zinc oxide single-crystalline nanoparticles of narrow size distribution and long-term colloidal stability. These oleate-stabilized nanoparticles were synthesized using microwave-assisted synthesis for 5 min, corresponding to a 99% decrease in synthesis time, when compared to the conventional synthesis method. It was observed that the average particle radius increases from 2.6 ± 0.1 to 3.8 ± 0.1 nm upon increasing synthesis temperature from 125 to 200 °C. This change also corresponded to observed changes in the optical band gap and the fluorescence energy of the particles, from 3.44 ± 0.01 to 3.36 ± 0.01 eV and from 2.20 ± 0.01 to 2.04 ± 0.01 eV, respectively. Small-angle X-ray scattering, dynamic light scattering, and UV–vis and fluorescence spectroscopy were employed for particle characterization. Debye–Scherrer analysis of the X-ray diffraction (XRD) pattern reveals a linear increase of the crystallite size with synthesis temperature. The consideration of the convolution of a Lorentz function with a Gaussian function for data correction of the instrumental peak broadening has a considerable influence on the values for the crystallite size. Williamson–Hall XRD analyses in the form of the uniform deformation model, uniform stress deformation model, and uniform deformation energy density model revealed a substantial increase of strain, stress, and deformation energy density of the crystallites with decreasing size. Exponential and power law models were utilized for quantification of strain, stress, and deformation energy density.
ZnO nanoparticles are found in different food and consumer products, and their toxicological effects are still under investigation. It is therefore important to understand their behavior in the gastrointestinal tract. Here, we used an in vitro model to assess the physicochemical fate of ZnO nanoparticles during the digestive process in artificial saliva, stomach juice, and intestinal juice. Atomic absorption spectrometry and small-angle X-ray scattering were employed to investigate two ZnO nanomaterials, one intensively characterized reference material and soluble ZnCl2 in a broad range of concentrations between 25 and 1000 μg/mL in the intestinal fluid. Because food components may influence the behavior of nanomaterials in the gastrointestinal tract, starch, milk powder, and olive oil were used to mimic carbohydrates, protein, and fat, respectively. Additionally, ion release of all Zn species was assessed in cell culture media and compared to artificial intestinal juice to investigate relevance of typical cell culture conditions in ZnO nanotoxicology. ZnCl2 as well as the ZnO species were present as particles in artificial saliva but were solubilized completely in the acidic stomach juice. Interestingly, in the intestinal fluid a concentration-independent de novo formation of particles in the nanoscale range was shown. This was the case for all particles as well as for ZnCl2, regardless of the concentration used. Neither of the food components affected the behavior of any Zn species. On the contrary, all Zn species showed a Zn-concentration-dependent ion release in common cell culture medium. This questions the suitability of cell culture studies to investigate the effect of ZnO nanoparticles on intestinal cells. Our results show that Zn-containing nanoparticles reach the intestine. This underlines the importance of determining the influence of the test environment on nanoparticle fate.
Particle size modality in bi-modal iron oxide suspensions was resolved by exploiting complex ac-susceptibility (ACS), small angle X-ray scattering (SAXS) and photon cross-correlation spectroscopy. To explain dynamic magnetic response of bi-modal suspensions, the Debye model was expanded to a linear superposition form allowing for the contribution of both particle fractions. This modified and adopted model is able to resolve the bi-modal particle size distributions. The SAXS curves of mono- and bi-modal suspensions were fitted well using a Monte Carlo simulation scheme, allowing the detection of bi-modal particle size distributions with high precision.
Resovist® originally developed as a clinical liver contrast agent for Magnetic Resonance Imaging exhibits also an outstanding performance as a tracer in Magnetic Particle Imaging (MPI). In order to study the physical mechanism of the high MPI performance of Resovist®, we applied asymmetric flow fieldflow fractionation (A4F) and static magnetic fractionation (SMF) to separate Resovist® into a set of fractions with defined size classes. As A4F based on an elution method separates MNP according to their hydrodynamic size, SMF fractionates a particle distribution by its magnetic moment. The obtained fractions of both separation techniques were then magnetically characterized by magnetorelaxometry measurements to extract the corresponding effective magnetic anisotropy and hydrodynamic size distribution parameters. Additionally, the MPI performance of each fraction was assessed using magnetic particle spectroscopy. With both separation techniques fractions (normalized to their iron amount) an MPI signal gain of a factor of two could be obtained, even though the distribution of effective anisotropy and hydrodynamic size were significantly different. Relating these findings to the results from magnetic characterization allows for a better understanding of the underlying mechanisms of MPI performance of Resovist®. This knowledge may help to improve the design of novel MPI tracers and development of separation methods.
We studied the magnetic resonance imaging liver contrast agent Resovist by a variety of magnetic measurement techniques, in order to understand the physical mechanism of their high magnetic particle imaging (MPI) performance, wirh a focus on the size-dependent contributions of the MPI signal. To this end, we used asymmetric flow field-flow fractionation to separate Resovist into a set of fractions with defined hydrodynamic diameters. The individual fractions were magnetically characterized by static magnetization and magnetorelaxometry measurements to obtain the corresponding effective magnetic anisotropy and effective size distribution parameters. In addition, the MPI performance of each fraction was assessed by magnetic particle spectroscopy. We observed an MPI signal gain of about 100% with respect to their iron amount for the best fraction. Relating these finding to the results from magnetic characterization provides more insight into mechanisms of MPI performance of Resovist. This knowledge may help to improve the design of novel MPI tracers.
Today there are hundreds of products available containing silver in form of nanoparticles, so-called nanosilver. This situation and the foreseeable future growing market of nanosilver will supposedly cause an increased release of silver into the environment. In this way, silver can be also incorporated into the human body and accumulated in different organs, which can be toxic or at least an unknown risk to human health. For these reasons, it is important to constantly study materials containing silver nanoparticles, their production, application in products and technical processes, dissemination of silver nanoparticles in the environment, and effects on humans and nature. The state-of-the-art nanoparticle size and concentration characterization are illustrated in an extensive interlaboratory comparison. To guarantee the traceability of measurements and to secure the comparison of results of different analytical methods, reference materials (RM) and certified reference materials (CRM) are essential. As a case study, the objective of the presented project was to provide an aqueous suspension of silver nanoparticles as a reference material with a nominal diameter below 10 nm for application in the determination of the size and concentration of nanoparticles in an aqueous surrounding. Measurands are the particles’ diameter D, size distribution width σ, number density N, and concentration c. Target uncertainties, defined as one sigma of the measurand values, are 5% for D, 10% for σ, 20% for N, and 20% for c. The certification was carried out based on ISO 17867 and the relevant ISO-Guides to produce reference material. The process of using SAXS as a reliable method for testing homogeneity and short-term and long-term stability of the material is reported. The particle preparation is described in detail so that the user can carry out the steps of synthesis and characterization in his own laboratory if required. Optionally, one can also contact the author for the provision of the silver nanoparticles. Detailed information can be found elsewhere (BAM Certification Reports, BAM-N008 (2022)).
SI Files for "Towards automation of the polyol process for the synthesis of silver nanoparticles"
(2022)
The graphml file: reaction_graph_AgNP.graphml is included. It contains topological information (Fig. 1 in the main text) about the reaction setup and metadata with reaction condtions. It used by the Python API used to control the Chemputer.
SAXS reports. The complete report sheets generated by McSAS are included. They contain extended information characterising the size distributions and the fitting parameters.
NP3_I: saxs_report_NP3_I.pdf
NP3_II: saxs_report_NP3_II.pdf
NP3_III: saxs_report_NP3_III.pdf
NP3_IV: saxs_report_NP3_IV.pdf
NP5_I: saxs_report_NP5_I.pdf
NP5_II: saxs_report_NP5_II.pdf
NP5_III: saxs_report_NP5_III.pdf
The spherical gold nanoparticle reference materials RM 8011, RM 8012, and RM 8013, with a nominal radius of 5, 15, and 30 nm, respectively, have been available since 2008 from NIST. These materials are recommended as standards for nanoparticle size measurements and for the study of the biological effects of nanoparticles, e.g., in pre-clinical biomedical research. We report on determination of the size distributions of these gold nanoparticles using different small-angle X-ray scattering (SAXS) instruments. Measurements with a classical Kratky type SAXS instrument are compared with a synchrotron SAXS technique. Samples were investigated in situ, positioned in capillaries and in levitated droplets. The number-weighted size distributions were determined applying model scattering functions based on (a) Gaussian, (b) log-normal, and (c) Schulz distributions. The mean radii are 4.36 ± 0.04 nm (RM 8011), 12.20 ± 0.03 nm (RM 8012), and 25.74 ± 0.27 nm (RM 8013). Low polydispersities, defined as relative width of the distributions, were detected with values of 0.067 ± 0.006 (RM 8011), 0.103 ± 0.003, (RM 8012), and 0.10 ± 0.01 (RM 8013). The results are in agreement with integral values determined from classical evaluation procedures, such as the radius of gyration (Guinier) and particle volume (Kratky). No indications of particle aggregation and particle interactions-repulsive or attractive-were found. We recommend SAXS as a standard method for a fast and precise determination of size distributions of nanoparticles.