Filtern
Dokumenttyp
Sprache
- Englisch (8)
Schlagworte
- Aqueous polymer solution (2)
- LCST (2)
- POF (2)
- Temperature sensor (2)
- Thermoresponsive polymer (2)
- Bi-modal size distribution characterization (1)
- Biodegradation (1)
- Biomaterial (1)
- Biphasic reactions (1)
- Calcium phosphate (1)
Organisationseinheit der BAM
- 8 Zerstörungsfreie Prüfung (3)
- 8.6 Faseroptische Sensorik (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.3 Instrumentelle Analytik (1)
- 3 Gefahrgutumschließungen; Energiespeicher (1)
- 3.3 Sicherheit von Transportbehältern (1)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
- 5.2 Metallische Hochtemperaturwerkstoffe (1)
- 7 Bauwerkssicherheit (1)
Short diffusion paths and high specific interfacial areas in microstructured devices can increase mass transfer rates and thus accelerate multiphase reactions. This effect can be intensified by the application of ultrasound. Herein, we report on the design and testing of a novel versatile setup for a continuous ultrasound-supported multiphase process in microstructured devices on a preparative scale. The ultrasonic energy is introduced indirectly into the microstructured device through pressurized water as transfer medium. First, we monitored the influence of ultrasound on the slug flow of a liquid/liquid two-phase system in a channel with a high-speed camera. To quantify the influence of ultrasound, the hydrolysis of p-nitrophenyl acetate was utilized as a model reaction. Microstructured devices with varying channel diameter, shape, and material were applied with and without ultrasonication at flow rates in the mL min-1 range. The continuous procedures were then compared and evaluated by performing a simplified life cycle assessment.
In accordance with IAEA SSR-6 para 306 a management system shall be established and implemented to ensure compliance with the relevant provisions of the IAEA regulations. BAM has issued an update of the guideline: the BAM-GGR 011. The new revision describes necessary quality assurance measures for design, manufacture, testing, documentation, use, maintenance and inspection of packagings for package designs requiring competent authority approval for the transport of radioactive material.
The measures can be categorised as system-related and design-related. They are independently approved and monitored by the German competent authority BAM and its authorised expert (BAM/T). The qualification of the organisation applying for the design approval certificate is reviewed in the context of the design approval procedure. The quality assurance measures for manufacture consist of three main steps. Pre-assessment of manufacturing documents such as quality plans, specifications etc., Manufacturing inspections according the pre-assessed documents and inspection before commissioning including documentation review. Periodic inspections during operation as well as relevant specifications for use and maintenance ensure that the properties specified in the approval certificate are preserved over the package life time. Special provisions for the return on
experience regarding operational feedback for design, manufacture, use, maintenance and inspection are given. Special focus shall be given here to the rearranged and meanwhile established system of manufacturing inspections. This includes more transparent roles for a) the Producers authorised inspection 11282 representative, b) the independent inspection expert (S), acting on behalf of the manufacturer with acceptance of BAM, and c) BAM or its authorised expert (BAM/T). Additional attention shall be drawn to the management of deviations during manufacturing and provisions for maintenance and periodic inspections.
Particle size modality in bi-modal iron oxide suspensions was resolved by exploiting complex ac-susceptibility (ACS), small angle X-ray scattering (SAXS) and photon cross-correlation spectroscopy. To explain dynamic magnetic response of bi-modal suspensions, the Debye model was expanded to a linear superposition form allowing for the contribution of both particle fractions. This modified and adopted model is able to resolve the bi-modal particle size distributions. The SAXS curves of mono- and bi-modal suspensions were fitted well using a Monte Carlo simulation scheme, allowing the detection of bi-modal particle size distributions with high precision.
The amount of data generated worldwide is constantly increasing. These data come from a wide variety of sources and systems, are processed differently, have a multitude of formats, and are stored in an untraceable and unstructured manner, predominantly in natural language in data silos. This problem can be equally applied to the heterogeneous research data from materials science and engineering. In this domain, ways and solutions are increasingly being generated to smartly link material data together with their contextual information in a uniform and well-structured manner on platforms, thus making them discoverable, retrievable, and reusable for research and industry. Ontologies play a key role in this context. They enable the sustainable representation of expert knowledge and the semantically structured filling of databases with computer-processable data triples.
In this perspective article, we present the project initiative Materials-open-Laboratory (Mat-o-Lab) that aims to provide a collaborative environment for domain experts to digitize their research results and processes and make them fit for data-driven materials research and development. The overarching challenge is to generate connection points to further link data from other domains to harness the promised potential of big materials data and harvest new knowledge.
We present a temperature sensor based on a polymer exhibiting a Lower Critical Solution Temperature (LCST) in aqueous solution encapsulated in a capillary. Parameters are chosen such that the solution exhibits a cloud point in a temperature range of 30° C to 39°C. The characteristic of thermoresponsive polymers with an LCST, is that above that temperature phase separation of the polymer takes place which leads to a temperature-dependent formation of a cloudy suspension. An optical intensity measurement over the desired temperature range is established by an increase of optical attenuation inside the polymer solution caused by a rising temperature. For our purpose, the polymer capillary is connected to transmitter and receiver via a Polymer Optical Fibre (POF). Our intensity measurement is, to the best of our knowledge, a novel method and can be considered simple when compared to existing fibre-based temperature measurement techniques. Due to the lack of electrical components at the probe, this sensor is suitable for measurements in strong electromagnetic fields and environments for which flying sparks are hazardous, i.e., inflammable fluids or gases. Furthermore, all manufactured sensors share the same temperature dependence and, therefore, are well-suited for comparative measurement, e.g., flow measurement systems. With the given temperature range, a body temperature measurement is also suitable.
We present a high-precision fiber-optic temperature sensor based on a polymer possessing a Lower Critical Solution Temperature (LCST) in aqueous solution encapsulated in a capillary. For a temperature higher than the LCST the transparent homogenous polymer solution changes into a suspension which forms an opaque fluid. The resulting temperature-dependent turbidity influences the transmission characteristics measured using a simple fiber-optic system.
The presented development provides a small-sized, robust temperature sensor, patented by the BAM (patent nr.: EP 3 043 161 B1), easy to integrate in many application fields, especially for process monitoring.
Osteoclastic bioresorption of biomaterials: Two- and three-dimensional imaging and quantification
(2010)
Purpose: Bioresorbable materials have been developed in the hope that the body will replace them with newly formed tissue. The first step of this remodeling process in bone is the bioresorption of the material by osteoclasts. The aim of this study was to analyze osteoclastic resorption of biomaterials in vitro using the commonly used two-dimensional methods of light-microscopy (LM) and scanning electron microscopy (SEM) in comparison with infinite focus microscopy (IFM), a recently developed imaging method allowing for three-dimensional surface analysis. Methods: Human hematopoietic stem cells were cultivated in the presence of the cytokines M-CSF and RANK-L for 4 weeks directly on dentin and a calcium phosphate cement. Osteoclast development was surveyed with standard techniques. After removal of the cells, resorption was characterized and quantified by LM, SEM and IFM. Results: Osteoclast cultures on the biomaterials presented the typical osteoclast-specific markers. On dentin samples LM, SEM as well as IFM allowed for discrimination of resorption. Quantification of the resorbed area showed a linear correlation between the results (LM vs. SEM: r=0.996, p=0.004; SEM vs. IFM: r=0.989, p=0.011; IFM vs. LM: r=0.995). It was not possible to demarcate resorption pits on GB14 using LM or SEM. With IFM, resorption on GB14 could be visualized and quantified two- and three-dimensionally.
Commonly, to determine osteoclastic resorption of biomaterials only the resorbed area is measured. The depth of the resorption pit, however, may also be important for the performance of a material. To generate such data we used two calcium phosphate ceramics (Ca10 and Ca2). The solubility of the materials was determined according to DIN EN ISO 10993-14. They were scanned three-dimensionally using infinite focus microscopy and subsequently cultivated for 4 weeks in simulated body fluid without (control) or with human osteoclasts. After this cultivation period osteoclasts number was determined and surface changes were evaluated two- and three-dimensionally. Ca10 and Ca2 showed solubilities of 11.0 ± 0.5 and 23.0 ± 2.2 mg g-1, respectively. Both materials induced a significant increase in osteoclast number. While Ca10 did not show osteoclastic resorption, Ca2 showed an increased pit area and pit volume due to osteoclastic action. This was caused by an increased average pit depth and an increased number of pits, while the average area of single pits did not change significantly. The deduced volumetric osteoclastic resorption rate (vORR) of Ca2 (0.010.02 µm3 µm-2 day-1) was lower than the remodelling speed observed in vivo (0.08 µm3 µm-2 day-1), which is in line with the observation that implanted resorbable materials remain in the body longer than originally expected. Determination of volumetric indices of osteoclastic resorption might be valuable in obtaining additional information about cellular resorption of bone substitute materials. This may help facilitate the development of novel materials for bone substitution.