Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (193)
- Beitrag zu einem Tagungsband (15)
Referierte Publikation
- ja (208) (entfernen)
Schlagworte
- Laser beam welding (43)
- Resistance spot welding (17)
- Welding simulation (13)
- Laser metal deposition (12)
- Microstructure (11)
- Additive manufacturing (9)
- Laser welding (9)
- Solidification cracking (9)
- Gas metal arc welding (8)
- Mechanical properties (8)
Organisationseinheit der BAM
A numerical framework for simulation of the steady-state thermal behaviour in keyhole mode welding has been developed. It is based on the equivalent heat source concept and consists of two parts: computational thermo-fluid dynamics and heat conduction. The solution of the thermo-fluid dynamics problem by the finite element method for a bounded domain results in a weld pool interface geometry being the input data for a subsequent heat conduction problem solved for a workpiece by a proposed boundary element method. The main physical phenomena, such as keyhole shape, thermo-capillary and natural convection and temperature-dependent material properties are taken into consideration. The developed technique is applied to complete-penetration keyhole laser beam welding of a 15 mm thick low-alloyed steel plate at a welding speed of 33 mm/s and a laser power of 18 kW. The fluid flow of the molten metal has a strong influence on the weld pool geometry. The thermo-capillary convection is responsible for an increase of the weld pool size near the plate surfaces and a bulge formation near the plate middle plane. The numerical and experimental molten pools, cross-sectional weld dimensions and thermal cycles of the heat affected zone are in close agreement.
In additive manufacturing (AM) directed energy deposition (DED), parts are built by welding layers of powder or wire feedstock onto a substrate with applications for steel powders in the fields of forging tools, spare parts, and structural components for various industries. For large and bulky parts, the choice of toolpaths influences the build rate, the mechanical performance, and the distortions in a highly geometry-dependent manner. With weld-path lengths in the range of hundreds of meters, a reliable, automated tool-path generation is essential for the usability of DED processes. This contribution presents automated tool-path generation approaches and discusses the results for arbitrary geometries. Socalled “zig-zag” and “contour-parallel” processing strategies are investigated and the tool-paths are automatically formatted into machine-readable g-code for experimental validation to build sample geometries. The results are discussed in regard to volume-fill, microstructure, and porosity in dependence of the path planning according to photographs and metallographic cross-sections.
The development within the offshore wind energy sector towards more powerful turbines combined with increasing water depth for new wind parks is challenging both, the designer as well as the manufacturer of support structures. Besides XL-monopiles the jacket support structure is a reasonable alternative due to the high rigidity combined with low material consumption. However, the effort for manufacturing of the hollow section joints reduces the economic potential of jacket structures significantly. Therefore, a changeover from an individual towards a serial production based on automated manufactured tubular joints combined with standardized pipes must be achieved. Hence, this paper addresses the welding process chain of automated manufactured tubular joints including digitization of the relevant manufacturing parameters such as laser scanning of the weld seam geometry. Additionally, a methodology for the computation of the notch radius as well as the weld seam angle is presented based on the scanned profiles of three analysis points of an automated manufactured tubular X-joint. Subsequently, these parameters are considered within the notch stress approach based fatigue design and their impact is quantified by a comparison with the structural stress approach using equivalent stress concentration factors.
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding Parameters on the formation of end crater defects such as pores, cracks, root excess weld metal and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp-down causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques.
A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of between 8 mm and 10 mm and then transferred on the 10 mm thick pipe sections made of high-strength pipeline steel API5L-X100Q.
Liquid metal embrittlement (LME) cracking can occur during resistance spot welding (RSW) in zinc-coated advanced high-strength steels (AHSS) for automotive production. In this study, a methodological variation of hold time is performed to investigate the process-related crack influence factors. A combination of numerical and experimental investigations confirms, that the extent of heat dissipation and re-heating of the sheet surface can be influenced and thus the degree of crack formation can be controlled in a targeted manner by the parameterisation of the hold time. The temperature and stress history of crack-free and crack-afflicted spot welds are analysed and a conclusion on the borders defining the LME active region is derived.
Laser metal deposition (LMD) has been applied as a coating technology for many years. Today, the technologies capacity to produce 3D depositions leads to a new field of application as additive manufacturing method. In this paper, 3D laser metal deposition of titanium alloy Ti-6Al-4V is studied with special regard to the demands of additive manufacturing. Therefore, only the coaxial LMD powder nozzle is used to create the shielding gas atmosphere, which ensures high geometric flexibility. Furthermore, specimen with high aspect ratio and hundreds of layers are manufactured, which represent typical features in additive manufacturing. The presented study contains the following steps: First, cylindrical specimens are manufactured with a standard shell-core build-up strategy and mechanical properties as well as fracture mechanisms are determined. Based on the results, experiments are conducted to improve the build-up strategy and new tensile test specimens are built with the improved strategy. The improved strategy incorporates variable track overlap ratios to achieve a constant growth in the shell and core area. As blanks, lean cylinders comprising more than 240 layers and a height of more than 120mm are manufactured. The specimens are analyzed by X-ray inspection for material defects. Fractured surfaces are observed via scanning electron microscopy and the composition of the surfaces is determined using energy dispersive X-ray spectroscopy. The tensile test results prove mechanical properties close to ASTM F1108 specification for wrought material.
Build-up strategies for temperature control using laser metal deposition for additive manufacturing
(2018)
The track geometry created with laser metal deposition (LMD) is influenced by various parameters. In this case, the laser power has an influence on the width of the track because of an increasing energy input. A larger melt pool is caused by a rising temperature. In the case of a longer welding process, there is also a rise in temperature, resulting in a change of the track geometry. This paper deals with the temperature profiles of different zigzag strategies and spiral strategies for additive manufacturing. A two-color pyrometer is used for temperature measurement on the component surface near the melt pool. Thermocouples measure the temperatures in deeper regions of a component. The welds are located in the center and in the edge area on a test part to investigate the temperature evolution under different boundary conditions. The experiments are carried out on substrates made from mild steel 1.0038 and with the filler material 316L. The investigations show an influence on the temperature evolution by the travel path strategy as well as the position on the part. This shows the necessity for the development and selection of build-up strategies for different part geometries in additive manufacturing by LMD.
Welding is one of the most widely used joining processes in structural applications, like in car body production in the automotive industry. It is well-known that distortions and residual stresses occur during and after the welding process. Many procedures exist to decrease these negative heat effects of welding, but are often coupled with highly cost intensive experiments. For several decades, simulation models have been developed to understand and predict the heat effects of welding and to reduce experimental effort. In the production planning of various Original Equipment Manufacturers (OEM), some simulation tools are already well established, e.g. for crash test, forming or casting simulations. For welding, the demand is high but the implementation of welding simulation software is still not established yet. Welding is a complex process and the development of a flexible simulation tool, which produces good simulation results without expert knowledge in simulation, is not an easy task. In this paper, a welded assembly from the automotive industry has been simulated and compared to experimental data. Temperature fields and transient distortion distributions have been measured with thermocouples and with an optical 3D deformations analysis tool, respectively. The simulation has been run with a commercially available welding simulation software. The simulated temperature fields match the numerical ones perfectly. The simulated distortions are also qualitatively in best agreement with the experimental ones. Quantitatively, a difference of approximately 20 % between the simulated and the measured distortions is visible; this is acceptable considering the simplifications and assumptions of the simulation model. The global time to solution to get these results without expert knowledge in welding simulation was between 4 and 6 weeks, which is a reasonable time frame for an industrial application of welding simulation.
The amount of absorbed energy in the keyhole as well as its spatial and temporal distribution is essential to model the laser beam welding process. The recoil pressure, which develops because of the evaporation process induced by the absorbed laser energy at the keyhole wall, is a key determining factor for the macroscopic flow of the molten metal in the weld pool during high-power laser beam welding. Consequently, a realistic implementation of the effect of laser radiation on the weld metal is crucial to obtain reliable and accurate simulation results. In this paper, we discuss manyfold different improvements on the laser-material interaction, namely, the ray tracing method, in the numerical simulation of the laser beam welding process. The first improvement relates to locating the exact reflection points in the ray tracing method using a so-called cosine condition in the determination algorithm for the intersection of reflected rays and the keyhole surface. A second correction refers to the numerical treatment of the Gaussian distribution of the laser beam, whose beam width is defined by a decay of the laser intensity by a factor of 1/e2, thus ignoring around 14% of the total laser beam energy. In the third step, the changes in the laser radiation distribution in the vertical direction were adapted by using different approximations for the converging and the diverging regions of the laser beam, thus mimicking the beam caustic. Finally, a virtual mesh refinement was adopted in the ray tracing routine. The obtained numerical results were validated with experimental measurements.
This paper investigates the numerical simulations of multi-kilowatt disk laser and fiber laser welding, ranging from 6 to 18 kW to study the behavior of molten pool in 20-mm-thick steel plate by using Volume-Of-Fluid (VOF) method and several mathematical models like Gaussian heat source, recoil pressure, Marangoni flow, buoyancy force, and additional shear stress and heat source due to the metallic vapor. Vortex flow pattern is observed for higher laser power except for 6-kW case, and the higher the laser power, the bigger the vortex flow pattern. Welding speed has an influence on molten pool in terms of depth of penetration and size of molten pool, but overall shape of molten pool remains the same. The reasons for the vortex flow pattern in high-power laser welding are the absorption of more energy at the bottom of keyhole, which promotes more liquid metal at the bottom, while for lower power with lower speed, the melt formation is more uniform in the thickness direction and most of the molten metal in the lower part of keyhole reaches the top of molten pool, and consequently, no vortex flow pattern is observed in the keyhole bottom.