Filtern
Dokumenttyp
Schlagworte
- Automated analysis (1)
- Bacterial adhesion (1)
- Biofilm (1)
- Biofilm quantification (1)
- Built environment (1)
- Computed tomography (1)
- Conservation of wooden artwork (1)
- Construction products (1)
- Ecotoxicity tests (1)
- Eluates (1)
Organisationseinheit der BAM
Recent DNA-based studies have shown that the built environment is surprisingly rich in fungi. These indoor fungi – whether transient visitors or more persistent residents – may hold clues to the rising levels of human allergies and other medical and building-related health problems observed globally. The taxo¬nomic identity of these fungi is crucial in such pursuits. Molecular identification of the built mycobiome is no trivial undertaking, however, given the large number of unidentified, misidentified, and technically compromised fungal sequences in public sequence databases. In addition, the sequence metadata required to make informed taxonomic decisions – such as country and host/substrate of collection – are often lacking even from reference and ex-type sequences. Here we report on a taxonomic annotation workshop (April 10–11, 2017) organized at the James Hutton Institute/University of Aberdeen (UK) to facilitate reproducible studies of the built mycobiome. The 32 participants went through public fungal ITS bar¬code sequences related to the built mycobiome for taxonomic and nomenclatural correctness, technical quality, and metadata availability. A total of 19,508 changes – including 4,783 name changes, 14,121 metadata annotations, and the removal of 99 technically compromised sequences – were implemented in the UNITE database for molecular identification of fungi (https://unite.ut.ee/) and shared with a range of other databases and downstream resources. Among the genera that saw the largest number of changes were Penicillium, Talaromyces, Cladosporium, Acremonium, and Alternaria, all of them of significant importance in both culture-based and culture-independent surveys of the built environment.
A European round robin test according to ISO 5725-2 was conceptually prepared, realised, and evaluated. The aim was to determine the inter-laboratory variability of the overall process for the ecotoxicological characterization of construction products in eluates and bioassays. To this end, two construction products BAM-G1 (granulate) and HSR-2 (roof sealing sheet), both made of EPDM polymers (rubber), were selected. The granular construction product was eluted in a one stage batch test, the planar product in the Dynamic Surface Leaching test (DSLT). A total of 17 laboratories from 5 countries participated in the round robin test: Germany (12), Austria (2), Belgium (1), Czech Republic (1) and France (1). A test battery of four standardised ecotoxicity tests with algae, daphnia, luminescent bacteria and zebrafish eggs was used. As toxicity measures, EC50 and LID values were calculated. All tests, except the fish egg test, were basically able to demonstrate toxic effects and the level of toxicity. The reproducibility of test results depended on the test specimens and the test organisms. Generally, the variability of the EC50 or LID values increased with the overall level of toxicity. For the very toxic BAM-G1 eluate a relative high variability of CV ¼ 73%e110% was observed for EC50 in all biotests, while for the less toxic HSR-2 eluate the reproducibility of EC50 varied with sensitivity: it was very good (CV ¼ 9.3%) for the daphnia test with the lowest sensitivity, followed by the algae test (CV ¼ 36.4%). The luminescent bacteria test, being the most sensitive bioassay for HSR-2 Eluate, showed the highest variability (CV ¼ 74.8%). When considering the complex overall process the reproducibility of bioassays with eluates from construction products was acceptable.
Während in einem konventionellen Ultraschallprüfkopf ein Kunststoffdämpfungskörper mit Kleber oder Öl an einen Piezoschwinger angekoppelt ist, werden als Hochtemperaturlösung feinporöse sintermetallische Dämpfungsmaterialien mit einer Flüssigglasankopplung eingesetzt. Um dabei das Sintermetall vor dem korrosiven Angriff der Glasschmelze zu schützten, wird am Dämpfungskörper gegenwärtig Gold- oder Platinfolie zeit- und kostenaufwendig appliziert.
In der aktuellen Arbeit wurde eine Methode zum Korrosionsschutz der sintermetallischen Oberfläche aus rostfreiem Stahl mittels Laser-Pulverauftragschweißen entwickelt. Im Laufe einer Schweißparameterstudie auf dem Substratmaterial aus massivem rostfreiem Stahl wurde die Eignung unterschiedlicher Auftragsmaterialien auf Nickel- und Kobaltbasis untersucht. Dabei wurde zunächst der Einfluss verschiedener Schweißparameter wie Laserleistung, Vorschubgeschwindigkeit und Pulvermenge auf die Auftragsqualität (Nahtform, Vermischungsgrad, Porosität) metallografisch bewertet. Anschließend wurden die aufgetragenen Schichten hinsichtlich ihrer Korrosionsbeständigkeit getestet. Der Kontakt mit einer flüssigen Glasmischung bei 500 °C hat bei keiner der beschichteten Proben sichtbare Korrosionswirkung gezeigt. Als Resultat der Schweißparameterstudie haben sich besonders die nickelbasierten Pulver als gut geeignete Materialien für den Prozess gezeigt. Die identifizierten Schweißparameter wurden im nächsten Schritt erfolgreich an das sintermetallische Substrat angepasst.
The objects of this investigation were sculptures taken from a ca. three hundred years old baroque epitaph of a church in Tonning, a town in Northern Germany. Around 1900 it was found in a disastrous state heavily damaged by wood-worm. At that time, the whole artwork was treated with the tar extract carbolineum as a remedy. Nowadays, this substance has been identified as carcinogenic, and its presence can be perceived by its stench and visually at certain spots on the surface where it has penetrated the covering paint.
A gold-painted sculpture of a massive wooden skull was interrogated with X-rays and fast neutrons to investigate the internal distribution of the carbolineum. The X-ray tomography, with its excellent spatial resolution revealed galleries left over from the worm infestation in the outer areas and cracks in the central region. The golden color coating appeared as a thick and dense layer. In comparison the tomography with fast neutrons, though being of lower resolution and yet unresolved artefacts revealed sections of slightly different densities in the bulk of the wood. These differences we attribute to the differences in the distribution of the impregnant in the wood, visible due to its higher hydrogen content making it less transparent for neutrons.
Biofilms cause complications and high costs in both industry and medicine. Of particular interest are bacterial infections of prosthetic materials, which usually cannot be eliminated due to the high antibiotic resistance known for bacteria forming biofilms. The search for new materials and coatings with lower colonization potential and antibacterial activity is of great importance to reduce biofilm formation. However, there is no standardized procedure to examine the colonization characteristics of bacteria in the Biofilm state in situ. Here, we describe an automated epifluorescence microscopy system for the semi-quantitative analysis of three-dimensional (3D) biofilms on various surfaces. To analyze adherent bacteria, three materials (glass, steel and titanium) were incubated with bacteria in a flow chamber system. After fluorescence staining of the bacteria, automated image capturing, quantification of the bacteria, measurement of the colonized area and determination of the 3D biofilm height were carried out by using novel software.
Furthermore, the materials were examined for their surface topography using white light scanning interferometry. Titanium compared to glass showed a significantly higher number of adherent bacteria.
We argue that this was due to the higher microroughness of titanium. The colonized area was in accordance with the number of adherent bacteria and was also significantly larger on titanium coupons compared to glass. Maximum 3D biofilm height on glass coupons was significantly lower compared to the ones on steel and titanium. This novel method enables the standardized, automated investigation of the colonization with bacteria on different materials. This approach can considerably support the characterization of new material surfaces and their innovative coatings by analyzing the amount of attached Bacteria and thickness of biofilms in situ and eliminates the need of conventional cultivation.
Layered silicate epoxy nanocomposites: formation of the inorganic-carbonaceous fire protection layer
(2011)
The layered silicate (LS) modification and processing parameters applied control the morphology of the LS/polymer composites. Here, increasing the surface area of the LS particles by using alternative drying processes increases dispersion towards a more typical nanocomposite morphology, which is a basic requirement for promising flame retardancy. Nevertheless, the morphology at room temperature does not act itself with respect to flame retardancy, but serves as a prerequisite for the formation of an efficient surface protection layer during pyrolysis. The formation of this residue layer was addressed experimentally for the actual pyrolysis region of a burning nanocomposite and thus our results are valid without any assumptions or compromises on the time period, dimension, surrounding atmosphere or temperature. The formation of the inorganic-carbonaceous residue is influenced by bubbling, migration, reorientation, agglomeration, ablation, and perhaps also delamination induced thermally and by decomposition, whereas true sintering of the inorganic particles was ruled out as an important mechanism. Multiple, quite different mechanisms are relevant during the formation of the residue, and the importance of each mechanism probably differs from one nanocomposite system to another. The main fire protection effect of the surface layer in polymer nanocomposites based on non-charring or nearly non-charring polymers is the increase in surface temperature, resulting in a substantial increase in reradiated heat flux (heat shielding).