Filtern
Erscheinungsjahr
Dokumenttyp
Schlagworte
- Surface analysis (3)
- Calcium phosphate ceramics (2)
- Central venous access port (2)
- Complication (2)
- EDX (2)
- Kalzium-Phosphat (2)
- Abfallmaterialien (1)
- Additive Manufacturing (1)
- Alcium alkali phosphate (1)
- Areal density (1)
Organisationseinheit der BAM
Plasma Spreyed Coatings of Calcium Titanium Phosphate - A New Generation of Bioactive Coatings
(1995)
Bioresorbable carriers for subchondral anchoring of tissue-engineered cartilage in articular defects
(2000)
Amorphous calcium phosphate cements and their transformation into calcium deficient hydroxyapatite
(1996)
In the current study, the tribological properties of TiC-based coatings paired with polycrystalline alumina under unlubricated sliding conditions were investigated in order to demonstrate the technological and engineering potential of such coatings. (Ti,Mo)(C,N)-Co coatings were prepared from an agglomerated and sintered spray powder by HVOF spraying using JP-5000 equipment. Cr3C2-NiCr coatings were studied for comparison. Sliding wear tests were performed over the temperature range from 23°C to 800°C with sliding speeds in the range 0.3-3 m/s, a wear distance of 5000 m and a normal force of 10 N. Wear rates of coatings and sintered alumina counterparts were measured separately. Compared with Cr3C2-NiCr coatings, (Ti,Mo)(C,N)-Co coatings showed significantly lower total wear rates, corresponding to those found in the region of mixed/boundary lubrication. With few exceptions, the coefficients of friction were found to be lower for (Ti,Mo)(C,N)-Co coatings than for Cr3C2-NiCr coatings. After tests were performed, the coating microstructures were studied by optical microscopy and SEM. The oxide scales formed on the coating surfaces were investigated by SEM and X-ray diffraction. Comparison of the total wear rates of the couples consisting of sintered alumina and a (Ti,Mo)(C,N)-Co coating with those of other alumina-ceramic and hardmetal-hard metal tribological systems demonstrates the immense potential of TiC-based coatings for sliding wear applications.
Osteoclastic bioresorption of biomaterials: Two- and three-dimensional imaging and quantification
(2010)
Purpose: Bioresorbable materials have been developed in the hope that the body will replace them with newly formed tissue. The first step of this remodeling process in bone is the bioresorption of the material by osteoclasts. The aim of this study was to analyze osteoclastic resorption of biomaterials in vitro using the commonly used two-dimensional methods of light-microscopy (LM) and scanning electron microscopy (SEM) in comparison with infinite focus microscopy (IFM), a recently developed imaging method allowing for three-dimensional surface analysis. Methods: Human hematopoietic stem cells were cultivated in the presence of the cytokines M-CSF and RANK-L for 4 weeks directly on dentin and a calcium phosphate cement. Osteoclast development was surveyed with standard techniques. After removal of the cells, resorption was characterized and quantified by LM, SEM and IFM. Results: Osteoclast cultures on the biomaterials presented the typical osteoclast-specific markers. On dentin samples LM, SEM as well as IFM allowed for discrimination of resorption. Quantification of the resorbed area showed a linear correlation between the results (LM vs. SEM: r=0.996, p=0.004; SEM vs. IFM: r=0.989, p=0.011; IFM vs. LM: r=0.995). It was not possible to demarcate resorption pits on GB14 using LM or SEM. With IFM, resorption on GB14 could be visualized and quantified two- and three-dimensionally.
Commonly, to determine osteoclastic resorption of biomaterials only the resorbed area is measured. The depth of the resorption pit, however, may also be important for the performance of a material. To generate such data we used two calcium phosphate ceramics (Ca10 and Ca2). The solubility of the materials was determined according to DIN EN ISO 10993-14. They were scanned three-dimensionally using infinite focus microscopy and subsequently cultivated for 4 weeks in simulated body fluid without (control) or with human osteoclasts. After this cultivation period osteoclasts number was determined and surface changes were evaluated two- and three-dimensionally. Ca10 and Ca2 showed solubilities of 11.0 ± 0.5 and 23.0 ± 2.2 mg g-1, respectively. Both materials induced a significant increase in osteoclast number. While Ca10 did not show osteoclastic resorption, Ca2 showed an increased pit area and pit volume due to osteoclastic action. This was caused by an increased average pit depth and an increased number of pits, while the average area of single pits did not change significantly. The deduced volumetric osteoclastic resorption rate (vORR) of Ca2 (0.010.02 µm3 µm-2 day-1) was lower than the remodelling speed observed in vivo (0.08 µm3 µm-2 day-1), which is in line with the observation that implanted resorbable materials remain in the body longer than originally expected. Determination of volumetric indices of osteoclastic resorption might be valuable in obtaining additional information about cellular resorption of bone substitute materials. This may help facilitate the development of novel materials for bone substitution.
Polyurethane versus silicone catheters for central venous port devices implanted at the forearm
(2016)
Purpose: We aimed to analyse short and long-term complications of polyurethane (PU) versus silicone catheters used in totally implantable venous-access ports (TIVAPs) implanted at the forearm.
Methods: Retrospective analysis of 698 consecutively implanted TIVAPs was performed. Primary end-points were defined as rates of major complications associated with either type of central venous port catheter. Technical success rate, device service interval as well as minor complications not requiring port explantation were defined as secondary end-points.
Results: A total of 698 port devices were implanted in 681 patients, 396 equipped with a PU catheter, 302 with a silicone catheter. The technical success rate was 99.9% with no major periprocedural complications. During follow-up a total of 211 complications in 146 patients were observed (1.0/1000 catheter days), 183 occurred associated with PU catheters (1.8/100 catheter days), 28 (0.3/1000 catheter days) with silicone catheters (log rank test p < 0.0001). Catheter-related bloodstream infections as well as thrombotic complications occurred significantly more frequently with PU catheters, while silicone catheters exhibited a trend towards a higher rate of mechanical failure such as disconnection or catheter rupture. Major complications requiring explantation of the device occurred more frequently with PU-based catheters (10.6%) compared to silicone catheter carrying ports (4.6%, log rank test p < 0.001).
One of the crucial characteristics of functionalized thin films is their porosity (i.e., the ratio between the pore volume and the volume of the whole film). Due to the very low amount of material per coated area corresponding to thin films, it is a challenge for analytics to measure the film porosity. In this work, we present an Approach to determine the porosity of thin films by means of electron probe microanalysis (EPMA) either by wavelength-dispersive X-ray spectrometry (WDX) or by energy-dispersive X-ray spectrometry (EDX) with a scanning electron microscope (SEM). The procedure is based on the calculation of the film mass deposition from electron-excited X-ray spectra. The
mass deposition is converted into film density by division of measured film thickness.
Finally, the film porosity is calculated from the measured film density and the density of bulk, nonporous film material. The general applicability of the procedure to determine the
porosity is demonstrated on thin templated mesoporous TiO₂
films, dip-coated on silicon
wafer, with controlled porosity in the range of 15 to 50%. The high accuracy of the mass deposition as determined from X-ray spectra was validated with independent methods (ICP-OES and weighing). Furthermore, for the validation of the porosity results, ellipsometry, interference fringes method (IFM), and focused ion beam (FIB) cross sectioning were employed as independent techniques. Hence, the approach proposed
in the present study is proven to be suited as a new analytical tool for accurate and relatively fast determination of the porosity of thin films.
Polycapillary halflenses are widely used to focus X-ray radiation onto a small spot. Additionally they can reduce the field of view of a semiconductor detector when placed in front of one. In 3D micro X-ray fluorescence spectroscopy (3D Micro-XRF) with synchrotron radiation, two polycapillary halflenses are used in a confocal geometry. Up until now, characterization measurements in the focal plane have only been performed in the case of the lens focusing parallel radiation. Assumptions have been made, that in the other case, when isotropic radiation from a spot source is transported to a detector, the acceptance distribution in the focal plane is also Gaussian. We performed measurements with an electron beam as well as a proton beam which confirm this assumption. In addition, a comparison between measurements in collecting and focusing mode show differences in spot size and transmission. These differences exemplify the fact that there is not one global spot size or transmission function of a polycapillary halflens. Illumination and divergence effects can alter both characteristic lens parameters.
A method is proposed to determine the effective detector area for energy-dispersive X-ray spectrometers (EDS). Nowadays, detectors are available for a wide range of nominal areas ranging from 10 up to 150mm2. However, it remains in most cases unknown whether this nominal area coincides with the “net active sensor area” that should be given according to the related standard ISO 15632, or with any other area of the detector device. Moreover, the specific geometry of EDS installation may further reduce a given detector area. The proposed method can be applied to most scanning electron microscope/EDS configurations. The basic idea consists in a comparison of the measured count rate with the count rate resulting from known X-ray yields of copper, titanium, or silicon. The method was successfully tested on three detectors with known effective area and applied further to seven spectrometers from different manufacturers. In most cases the method gave an effective area smaller than the area given in the detector description.
Over the last decade there have been increasing efforts to develop three-dimensional (3D) scaffolds for bone tissue Engineering from bioactive ceramics with 3D printing emerging as a promising technology. The overall objective of the present study was to generate a tissue engineered synthetic bone graft with homogenously distributed osteoblasts and mineralizing bone Matrix in vitro, thereby mimicking the advantageous properties of autogenous bone grafts and facilitating usage for reconstructing segmental discontinuity defects in vivo . To this end, 3D scaffolds were developed from a silica-containing calcium alkali orthophosphate, using, fi rst, a replica technique – the Schwartzwalder – Somers method – and, second, 3D printing, (i.e. rapid prototyping). The mechanical and physical scaffold properties and their potential to facilitate homogenous colonization by osteogenic cells and extracellular bone matrix formation throughout the porous scaffold architecture were examined.
Osteoblastic cells were dynamically cultured for 7 days on both scaffold types with two different concentrations of 1.5 and 3 × 10⁹ cells/l. The amount of cells and bone matrix formed and osteogenic marker expression were evaluated using hard tissue histology, immunohistochemical and histomorphometric analysis. 3D-printed scaffolds (RPS) exhibited more micropores, greater compressive strength and silica release. RPS seeded with 3 × 10⁹ cells/l displayed greatest cell and extracellular Matrix formation, mineralization and osteocalcin expression. In conclusion, RPS displayed superior mechanical and biological properties and facilitated generating a tissue engineered synthetic bone graft in vitro, which mimics the advantageous properties of autogenous bone grafts, by containing homogenously distributed terminally differentiated osteoblasts and mineralizing bone matrix and therefore is suitable for subsequent in vivo implantation for regenerating segmental discontinuity bone defects.
A thin-layer reference material for surface and near-surface analytical methods was produced and certified. The surface density of the implanted Sb layer was determined by Rutherford backscattering spectrometry (RBS), instrumental neutron activation analysis (INAA), and inductively coupled plasma isotope dilution mass spectrometry (ICP-IDMS) equipped with a multi-collector. The isotopic abundances of Sb (121Sb and 123Sb) were determined by multi-collector ICP-MS and INAA. ICP-IDMS measurements are discussed in detail in this paper. All methods produced values traceable to the SI and are accompanied by a complete uncertainty budget. The homogeneity of the material was measured with RBS. From these measurements the standard uncertainty due to possible inhomogeneities was estimated to be less than 0.78% for fractions of the area increments down to 0.75 mm2 in size. Excellent agreement between the results of the three different methods was found. For the surface density of implanted Sb atoms the unweighted mean value of the means of four data sets is 4.8121016 cm-2 with an expanded uncertainty (coverage factor k=2) of 0.0921016 cm-2. For the isotope amount ratio R (121Sb/123Sb) the unweighted mean value of the means of two data sets is 1.435 with an expanded uncertainty (coverage factor k=2) of 0.006.
Recently, efforts towards the development of patient-specific 3D printed scaffolds for bone tissue engineering from bioactive ceramics have continuously intensified. For reconstruction of segmental defects after subtotal mandibulectomy a suitable tissue engineered bioceramic bone graft needs to be endowed with homogenously distributed osteoblasts in order to mimic the advantageous features of vascularized autologous fibula grafts, which represent the standard of care, contain osteogenic cells and are transplanted with the respective blood vessel. Consequently, inducing vascularization early on is pivotal for bone tissue engineering. The current study explored an advanced bone tissue engineering approach combining an advanced 3D printing technique for bioactive resorbable ceramic scaffolds with a perfusion cell culture technique for pre-colonization with mesenchymal stem cells, and with an intrinsic angiogenesis technique for regenerating critical size, segmental discontinuity defects in vivo applying a rat model. To this end, the effect of differing Si-CAOP (silica containing calcium alkali orthophosphate) scaffold microarchitecture arising from 3D powder bed printing (RP) or the Schwarzwalder Somers (SSM) replica fabrication technique on vascularization and bone regeneration was analyzed in vivo. In 80 rats 6-mm segmental discontinuity defects were created in the left femur.