A European round robin test according to ISO 5725-2 was conceptually prepared, realised, and evaluated. The aim was to determine the inter-laboratory variability of the overall process for the ecotoxicological characterization of construction products in eluates and bioassays. To this end, two construction products BAM-G1 (granulate) and HSR-2 (roof sealing sheet), both made of EPDM polymers (rubber), were selected. The granular construction product was eluted in a one stage batch test, the planar product in the Dynamic Surface Leaching test (DSLT). A total of 17 laboratories from 5 countries participated in the round robin test: Germany (12), Austria (2), Belgium (1), Czech Republic (1) and France (1). A test battery of four standardised ecotoxicity tests with algae, daphnia, luminescent bacteria and zebrafish eggs was used. As toxicity measures, EC50 and LID values were calculated. All tests, except the fish egg test, were basically able to demonstrate toxic effects and the level of toxicity. The reproducibility of test results depended on the test specimens and the test organisms. Generally, the variability of the EC50 or LID values increased with the overall level of toxicity. For the very toxic BAM-G1 eluate a relative high variability of CV ¼ 73%e110% was observed for EC50 in all biotests, while for the less toxic HSR-2 eluate the reproducibility of EC50 varied with sensitivity: it was very good (CV ¼ 9.3%) for the daphnia test with the lowest sensitivity, followed by the algae test (CV ¼ 36.4%). The luminescent bacteria test, being the most sensitive bioassay for HSR-2 Eluate, showed the highest variability (CV ¼ 74.8%). When considering the complex overall process the reproducibility of bioassays with eluates from construction products was acceptable.
Nanocomposites of bisphenol A polycarbonate with 2, 4, 6, and 15 wt% multiwall carbon nanotubes (MWNT) and their use in fire retardancy are investigated. Their thermal behavior and pyrolysis are characterized using thermogravimetry, differential scanning calorimeter, oscillatory shear rheology, and dynamic mechanical analysis. The flammability is addressed using LOI and UL 94; the fire behavior, with a cone calorimeter using different irradiation. With increasing MWNT content the storage modulus is increased (10-20%) and melt viscosity increases by several orders of magnitude, particularly for low shear rates. The melt flow, dripping, and deformation during fire are hindered, which influences UL 94 and cone calorimeter results. The peak heat release rate is reduced up to 40-50% due to an improved barrier for small amounts (2 wt%) of MWNT and for low irradiation, whereas the effect is reduced for increasing irradiation and nearly vanishes for increasing filling. Adjuvant but also deleterious mechanisms result in the complex dependency on the MWNT content. Significant flame retardancy effects are specific and limited to only some fire properties. This study allows the materials' potential for implementation in different fire scenarios and tests to be assessed and provides insight into active mechanisms.
Nanocomposites of polyamide 6 with 5 wt.% multiwall carbon nanotubes are investigated to clarify their potential as regards the fire retardancy of polymers. The nanocomposites are investigated using SEM, electrical resistivity, and oscillatory shear rheology. The pyrolysis is characterized using thermal analysis. The fire behaviour is investigated with a cone calorimeter using different external heat fluxes, by means of the limiting oxygen index and the UL 94 classification. The fire residue is characterized using SEM. The comprehensive fire behaviour characterization not only allows the materials potential for implementation in different fire scenarios and fire tests to be assessed, but also provides detailed insight into the active mechanisms. The increased melt viscosity of the nanocomposites and the fibre-network character of the nanofiller are the dominant mechanisms influencing fire performance. The changes are found to be adjuvant with respect to forced flaming conditions in the cone calorimeter, but also deleterious in terms of flammability.