Small grain sizes of municipal solid waste incineration (MSWI) bottom ash (BA) contain elemental and chemically bonded metals in appreciable amounts, especially copper. As different copper species have in general a higher density compared to the prevalent minerals, processes for density separation seemed to be favorable for the recovery of copper. Investigations with a centrifugal classifier were therefore carried out with BA from MWSI which have been used for a few years as the covering material for a landfill. The results show an appreciable enrichment of the precious copper. The concentrates contained up to 60 mg/kg copper in the dry weight (DW) (in general about 30 – 40 mg/kg DW) with enrichment factors of around 20 and a copper recovery of up to 50 % (in general around 20 %). A test series in order to evaluate the potential benefit for sequential processing illustrate the low efficiency for a further processing of the tailings.
Bottom ash from municipal solid waste incineration (MSWI) consists of elemental metals in considerable amounts. The fine fraction < 4 mm additionally contains chemically bound metals (oxides, carbonates, silicates). Separation prospects with techniques as in ore processing (flotation, density separation, bioleaching, hydrothermal solution) are discussed. During alteration after wet extraction mineral material with hydraulic properties form coatings on almost all particles of the bottom ash and complicate separation procedures. In addition bottom ash from MSWI is a heterogeneous material. For sufficient enrichment different concerted treatment steps seemed to be essential associated with an uncertainty of economic viability. The utilisation of metal compounds present in bottom ash as secondary raw material depends on the energy- and resource-efficiency of the enrichment processes. Therefore energy and material flow considerations are presented.
The fine fraction of bottom ash from municipal solid waste incineration is characterized of both a high pollution and relevant resource potential. Methods for studying the environmental behaviour of solid residues are leaching tests. Various leaching test are adopted all over Europe with liquid to solid ratio of 2 or 10 l/kg. In Germany three different leaching Tests are valid with the commencement of the draft of the ordinance of reuse of mineral waste as alternative building ordinance. Comparing two batch tests, only the concentration for chloride is comparable. To evaluate the metal resource potential in the sand fraction wet chemical Methods have been applied. Methodical problems were caused mainly by the material heterogeneity and especially for precious metals due to their low concentration around 1 mg/kg. Other Methods have been available, but hardly applicable.
Improving resource efficiency at the end-of-life stage is illustrated in this paper by the example of materials recovery from waste, here from residues out of municipal solid waste incineration (MSWI). With mechanical treatment valuable materials like ferrous and non-ferrous metals and secondary construction material can be extracted from MSWI bottom ash. The potential contribution on the resource efficiency will be discussed.
The industrial sector of bottom ash (BA) treatment from municipal solid waste incineration (MSWI) in Germany is currently changing. In order to increase the recovery rates of metals or to achieve a higher quality of mineral aggregates derived from BA, new procedures have been either implemented to existing plants or completely new treatment plants have been built recently. Three treatment trains, which are designated as entire sequences of selected processing techniques of BA, are introduced and compared. One treatment train is mainly characterized by usage of a high speed rotation accelerator whereas another is operating completely without crushing. In the third treatment train the BA is processed wet directly after incineration. The consequences for recovered metal fractions and the constitution of remaining mineral aggregates are discussed in the context of legislative and economical frameworks. Today the recycling or disposal options of mineral residues still have a high influence on the configuration and the operation mode of the treatment trains of BA despite of the high value of recovered metals.
In Germany, the direct material input (DMI) was 1727 million tons in the year 2014. This figure would be even higher by more than 14 % if no secondary materials were already used in industrial production. For example, production of secondary Cu is advantageous due to lower energy consumption and conservation of scarce natural resources. The presentation will discuss pathways to increase the use of secondary raw materials to foster a circular economy with a focus on waste treatment processes.