Filtern
Dokumenttyp
- Vortrag (12)
- Posterpräsentation (4)
- Zeitschriftenartikel (1)
- Beitrag zu einem Sammelband (1)
- Beitrag zu einem Tagungsband (1)
- Dissertation (1)
Referierte Publikation
- nein (20) (entfernen)
Schlagworte
- ToF-SIMS (9)
- Hydrogen assisted cracking (7)
- Data-fusion (5)
- Hydrogen Embrittlement (5)
- EBSD (4)
- Gaseous hydrogen (4)
- DSS (2)
- Data fusion (2)
- Duplex stainless steel (2)
- Hollow specimen (2)
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (12)
Influence of Hydrogen Uptake and Diffusion in Structural Components in the Field of Renewable Energy
(2021)
Great efforts are invested worldwide in the development of efficient electrolysis processes, fuel cells technologies and hydrogen transport and storage infrastructures. This includes the exploitation of existing gas-grid infrastructure for the injection of hydrogen. Considering transport and storage facilities, the utilization of gaseous hydrogen can be divided into two main groups which are differentiating in the pressure regime. Fueling stations are operating in high pressure (>800 bar) and high purity and therefore use austenitic stainless steels in their compression systems. On the other hand, existing gas infrastructure where the natural gas is transported across long distances is usually operating with up to 300 bar. In this case the pipe-systems consist of several steel classes, mainly low alloyed steels in which the surface quality and the gas mixture are strongly varying.
Even though ingress of hydrogen can lead to catastrophic failures in all steels, its exact impact on the mechanical properties, as well as its interaction with the surface, microstructure and lattice and the underlying mechanisms remain unclear. Therefore, research on the impact of gaseous hydrogen in pressure vessels and pipes has clearly an integral part on the path to safe and sustainable use of the different components along the different chains. This becomes even more relevant considering the influence of impurities in the gas, e.g. sulfur and with the introduction of new production technologies, such as additive manufacturing, into the market.
Determination of these interactions and impact that might lead to the degradation of the properties can allow a safe use of steels in present and future hydrogen-based energy applications.
The following contribution gives an overview of the problem and introduction to the conventional and innovative tools used and developed nowadays to analyze it. For this purpose, materials were loaded with hydrogen by electrochemical means and under high pressure and elevated temperatures. The results presented provide an invaluable insight into the impact of hydrogen on the integrity of selected steels used in the two mentioned above applications. This work is part of an ongoing research in which mechanical, chemical, structural, and microstructural analyses tools are combined in-situ and ex-situ.
Um die Absorption von Wasserstoff und dessen Verhalten in den Werkstoffen beim Einsatz unter Druck-H2 sowie die H- abhängigen Materialeigenschaften zu definieren, entwickelt die BAM mit ihrer langjährigen Erfahrung adäquate Prüfkonzepte, die einsatzrelevante Bedingungen und reale Beanspruchungen (Temperatur, Wasserstoff und mech. Beanspruchung) hierarchisch berücksichtigen. Der Vortrag gibt eine Einführung in das Thema von wasserstoffunterstützen Materialschäden durch die Problematik der Einspeisung von Wasserstoff in bestehende Erdgasnetze. Ferner wird auf die Hochdruck-Infrastruktur (sowie H2-Tankstellen) und die Entwicklung von Prüfkonzepten für die Gasinfrastruktur unter Druckwasserstoffbeaufschlagung eingegangen.
Increasing environmental problems with conventional energy technology are stimulating the demand for alternative energy solutions. With air quality reaching catastrophic levels in large cities worldwide, Fuel Cell Electric Vehicles offer the ideal combination of clean power with the amenities of electric drives. Hydrogen use on vehicles, nevertheless, also raises some issues about safe handling. As fuel cells and hydrogen applications, including vehicles, approach technological maturity, developing their business cases becomes crucial in introducing them to the consumer markets.
The Joint European Summer School JESS 2021 addresses these issues by offering high quality graduate level courses on selected topics of vehicle technology, innovation & business development, safe handling of hydrogen, and modelling. This series of summer schools has been ongoing since 2004 and targets an audience of university students (MSc and PhD levels) and post-doctoral researchers. We also welcome more experienced researchers and engineers wishing to expand their general knowledge, for instance, to suit a newly acquired position or collect credits for Continuous Professional Development (CPD). The course content is tailored to the needs of a diverse audience: newcomers to the field, experienced students, and young professionals working at the forefront of fuel cell and hydrogen applications.
As a chemical metrology tool time-of-flight secondary ion mass spectrometry (ToF-SIMS) has become a very popular technique to monitor the elemental, isotopic and molecular distribution in two or three dimensions. Its reduced sampling depth, high sensitivity, great structural specificity and the direct detection of hydrogen thereby increase the emergence of ToF-SIMS for material and analytical surface science, particularly due to recent instrumental developments improving mass, depth and lateral resolution. For basic surface science, adsorption processes and surface reactivity thus can be investigated in high detail on organic as well as inorganic samples. The use of multivariate data analysis in addition can effectively assist to identify trends in the complex SIMS raw data set and define key co-variances between certain samples or mass spectra. In this contribution the essence of ToF-SIMS is illustrated by discussing two highly relevant energy applications. First, for piezoelectric electroceramics oxygen exchange active zones have been visualized to determine the impact of external field-load to the oxygen vacancy distribution between anode and cathode. As a second case study the interaction of hydrogen species with the microstructure of a duplex stainless steel was investigated. It was concluded that ToF-SIMS has a valuable essence for detailing hydrogen related degradation mechanisms.
Deuterium permeation and cracking in duplex steels as viewed by ToF-SIMS and HR-SEM with data fusion
(2016)
Better understanding of hydrogen assisted degradation and trapping mecha-nisms requires sufficient imaging techniques for respective hydrogen-microstructure interaction studies, in particular with multi-phase metallic micro-structures [1]. The present work is focusing on the elucidation of deuterium be-havior in two austenitic-ferritic duplex stainless steels (DSS) under the assumption that deuterium behaves in many ways similarly to hydrogen [2]. For case studies standard 2205 and lean 2101 DSSs were chosen due to the extensive use of these steels in industry [3]. The analyses were conducted by using a novel in-situ permeation and Time-of-Flight secondary ion mass spectrometry (ToF-SIMS) imaging technique or by ex-situ ToF-SIMS imaging following electrochemical charging experiments. Another pioneering procedure was data fusion (including chemometry) of results of powerful laterally resolved chemical analysis and high resolution structural characterization techniques .
Results for the ex-situ observations showed a different influence of deuterium loading on the two steel grades as well as different damage mechanisms in each phase. Formation of sub-surface blisters between the ferrite and austenite were obtained in both the standard and the lean DSS. In both steels, an increased deuterium concentration was observed around deformed regions such as cracks, confirming that they originate from the presence of deuterium [4]. The formation of parallel cracks was obtained only in the austenite within the standard duplex whereas in the lean duplex the highest intensity of deuterium was obtained in the austenite along the ferrite-austenite interphase.
In comparison, application of the novel in-situ permeation technique enabled to register and record the deuterium permeation through the material and the respective saturation sequence of the two phases as well as the interfaces. Faster diffusion of the deuterium was observed in the ferrite and a direct proof for deuterium enrichment at the austenite-ferrite interface has been given [1]. The integration of the specified techniques gives a better insight into the processes leading to hydrogen induced failure. These two experimental techniques provide very valuable tools for elucidation of respective metallurgical failure mechanisms that can be used for the validation of respective numerical models for hydrogen assisted cracking (HAC).
For almost 150 years it is known that hydrogen has a deleterious effect on the mechanical properties of metallic components. Nowadays, the problem of hydrogen assisted degradation is highly relevant in energy related fields due to the massive use of steel as a structural component in these applications and its sensitivity to hydrogen. Since the discovery of hydrogen assisted cracking (HAC), researchers studied intensively and suggested possible explanations and mechanisms in order to define how hydrogen is affecting the material. In general, it is considered that hydrogen changes the mechanical properties more in terms of ductility (deformation capacities) than in strength (load capacities). Hydrogen concentration is one of three crucial factors in the degradation process, together with the microstructure of the material and the internal/external mechanical load. The relatively high concentration of hydrogen resulting in this loss of ductility can originate during production or before service (e.g. welding processes) and during service (i.e. catholically protected systems to eliminate corrosion processes in sour environments).
In parallel to the theoretical work, tremendous efforts were, and are still, invested in searching for a proper method to elucidate, map and quantify the hydrogen in the microstructure, which is the basis for this work. For steels, the focus is mainly on the observations of diffusion processes and the interaction of hydrogen with the microstructure
in regions with high local stresses/strains (for example around evolving cracks). The challenge for reaching this goal arises from the fact that accurate indication of hydrogen by means of position, unlike heavier atoms, can be made only by mass spectrometry or by interaction with another element (e.g. silver decoration, special coating and resonant nuclear reaction by nitrogen). In addition to this, the difficulty recording the hydrogen behavior while it rapidly diffuses through the material, leaving only the unpredicted failure, should be taken into account.
Although using powerful characterization methods, models and computational simulations, the key to defining the mechanisms behind HAC is still under debate and not fully understood. The relationship between material and hydrogen is determined by three factors, i.e., the material structure and microstructure – determining the physical properties, the mechanical load applied on the material and the hydrogen concentration. It is well known that in order to have a complete definition of HAC these three factors must be examined locally with the minimal scale and the maximal resolution reachable. The major gap is the lack in such a characterization method or a technique by which one has the ability to detect and observe the hydrogen in the metallic microstructure. The commonly used techniques nowadays are capable of characterization of the microstructure without the ability to observe the hydrogen distribution. Global hydrogen concentration and localized hydrogen observation are possible by some techniques which are incapable of indicating a change in the structure or microstructure therefore a comprehensive overview can be gained only by combining several methods.
In the presented research, secondary ion mass spectrometry (SIMS) was adopted as the main tool to detect and locally map the hydrogen distribution in two types of duplex stainless steel grades: EN 1.4462 (standard 2205 duplex stainless steel) and EN 1.4162 (2101 lean duplex stainless steel). The term duplex stainless steel (DSS) refers to the austenitic-ferritic microstructure of the steel where the combination of physical and mechanical properties of the two phases is achieved. The DSS was selected as a case study for this work due to the wide use of this grade in many energy and the lack of knowledge on hydrogen behavior in two-phase containing microstructures. ToFSIMS was exploited in-situ and ex-situ in three experimental approaches during or following
an electrochemical charging procedure. This type of hydrogen charging was selected as it simulated a procedure of cathodic protection of most sub-water oil and gas extraction and delivery systems. The experimental procedures were:
1. Ex-situ charging followed by ToF-SIMS imaging for basic understanding of hydrogen distribution.
2. Ex-situ charging followed by in-situ mechanical loading to obtain information on hydrogen behavior around a propagating crack.
3. In-situ permeation of hydrogen through a steel membrane inside the ToF-SIMS to obtain information on diffusion behavior of hydrogen in a two-phase microstructure.
The comprehensive view of the effect of hydrogen on steel was gained by using supplementary methods, such as high resolution scanning electron microscopy (HR-SEM), focused ion beam (FIB) and electron back-scattered diffraction (EBSD). The state of the art in this work lies in applying both: in-situ experimental approaches and data treatment of the ToF-SIMS raw data. The data treatment includes the combination of data from several sources (data fusion).
The results for the ex-situ charging followed by static sample imaging and data fusion showed that when the analyzed surface is directly exposed to the electrolyte the degradation is pronounced differently in the ferrite, austenite and interface. The degradation mechanisms in the ferrite and austenite were reflected by the formation of cracks on the surface of both, where a high concentration of hydrogen was obtained. This result supports the assumption that hydrogen is attracted to highly deformed regions. The advantage of using in-situ charging/permeation in comparison to ex-situ charging is that the effect of hydrogen on the ferrite and austenite phases when the hydrogen is evolving from within the microstructure is realized, in comparison to when the analyzed surface is initially exposed directly to the electrolyte. In both experiments the ferrite was observed as a fast diffusion path for the hydrogen. The faster diffusion of hydrogen through the ferrite is expected due to the higher diffusion coefficient, however, a direct proof for the diffusion sequence in this scale was never shown. Most significant results were achieved by the ‘core’ experiments of this research. These experiments included the design of a novel dynamic mechanical loading device to apply an external load during SIMS imaging of a hydrogen precharged-notched sample. For the first time it was shown that plastic deformation induced by applying a mechanical load is resulting in a redistribution of hydrogen locally around the notch.