Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (77) (entfernen)
Referierte Publikation
- nein (77)
Schlagworte
- Welding (23)
- Hydrogen (21)
- Wasserstoff (11)
- Schweißen (8)
- Fügetechnik (7)
- Diffusion (6)
- Mechanical properties (6)
- Forschung (5)
- High-entropy alloy (5)
- Microstructure (5)
- Pipelines (5)
- Research (5)
- Creep-resistant steel (4)
- Hydrogen assisted cracking (4)
- Review (4)
- Studie (4)
- Thermal desorption analysis (4)
- Additive manufacturing (3)
- Carrier gas hot extraction (3)
- Degradation (3)
- High-strength steel (3)
- ISO 3690 (3)
- Wasserstofftechnologien (3)
- Electrochemical permeation (2)
- Experimental design (2)
- High Entropy Alloy (2)
- MAG Welding (2)
- Offshore (2)
- Pipeline (2)
- Post weld heat treatment (2)
- Steel (2)
- Stress relief cracking (2)
- Submerged arc welding (2)
- TIG welding (2)
- Weld metal (2)
- Wärmenachbehandlung (2)
- Activation energy (1)
- Additive Fertigung (1)
- Alloy concept (1)
- Arc melting technique (1)
- Austenitic stainless steel (1)
- Bauteilversuch (1)
- Bedeutung (1)
- Betrieb (1)
- Carrier gas hot extraction (CGHE) (1)
- Component (1)
- Component Test (1)
- Component manufatcturing (1)
- Comprehensive study (1)
- Constitution diagram (1)
- Cr-Mo-V steel (1)
- Cracking (1)
- Creep resisting materials (1)
- Creep-resisting materials (1)
- Creep-resisting steel (1)
- Cross-weld tensile sample (1)
- Digital Image Correlation (DIC) (1)
- Dissimilar metal weld (1)
- Dissimilar metal weld (DMW) joint (1)
- Dissimilar weld joints (1)
- Eigenspannungen (1)
- Embrittlement (1)
- Energieerzeugung (1)
- Friction stir welding (1)
- Gas analytic (1)
- Heat control (1)
- Heat treatment condition (1)
- High manganese steel (1)
- High strength steels (1)
- High-pressure (1)
- High-strength (1)
- High-strength Steel (1)
- High-strength steels (1)
- Hochdruck (1)
- Hochfest (1)
- Hochfester Feinkornbaustahl (1)
- Hochfester Stahl (1)
- Hollow tensile specimen (1)
- Hydrogen concentration (1)
- Hydrogen diffusion (1)
- Hydrogen embrittlement (1)
- Hydrogen trapping (1)
- I-girder (1)
- Imperfektion (1)
- In-service (1)
- Infractstructure (1)
- Joining (1)
- Joining process (1)
- Kaltrissbildung (1)
- Kaltrissprüfung (1)
- Komponenten (1)
- Measurement (1)
- Messung (1)
- Metallurgie (1)
- Metals (1)
- Mikrolegierungseinfluss (1)
- Mock-up (1)
- Modifizierter Sprühlichtbogen (1)
- Multi-principal element alloys (1)
- Multiple-principal element alloy (1)
- Normung (1)
- Numerical simulation (1)
- Overview (1)
- PWHT (1)
- Process parameters (1)
- Processing (1)
- Prüfverfahren (1)
- Repair Welding (1)
- Repair welding (1)
- Reparatur (1)
- Reparaturschweißen (1)
- Research and Development (1)
- Residual Stress (1)
- Riss (1)
- Scanning kelvin probe force microscopy (1)
- Schallemissionsanalyse (1)
- Schweißverbindung (1)
- Sectioning method (1)
- Spannungsrelaxationsriss (1)
- Spannungsrelaxationsrisse (1)
- Stahl (1)
- Standardization (1)
- Stress corrosion cracking (1)
- Study (1)
- Surface integrity (1)
- T24 / 7CrMoVTiB10-10 (1)
- Technologie (1)
- Technologies (1)
- Temperature (1)
- Testing (1)
- Thermal desorption analysis (TDA) (1)
- Thermodynamische Simulation (1)
- Thoughness (1)
- Trapping and diffusion (1)
- Trägergasheißextraktion (1)
- UP Schweißen (1)
- UP-Schweißen (1)
- Ultrasonic-assisted milling (1)
- WEZ-Erweichung (1)
- Warmfeste Stähle (1)
- Weld heat input (1)
- Weld joint (1)
- Weld residual stresses (1)
- Welding parameters (1)
Organisationseinheit der BAM
- 9 Komponentensicherheit (52)
- 9.0 Abteilungsleitung und andere (40)
- 9.4 Integrität von Schweißverbindungen (36)
- 9.2 Versuchsanlagen und Prüftechnik (9)
- 8 Zerstörungsfreie Prüfung (2)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
- 6 Materialchemie (1)
- 6.2 Material- und Oberflächentechnologien (1)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (1)
As energy carrier of the future, green hydrogen can make a decisive contribution to a sustainable energy supply. Particularly important is the decarbonization of heavy industry. Therefore, a reliable supply of hydrogen must be guaranteed. A hydrogen pipeline grid can achieve this purpose. In Europe concrete plans for a hydrogen pipeline grid already exist, as the so called “European Hydrogen backbone”. As building a completely new pipeline grid is economically not justifiable, a dual-way strategy of repurposing natural gas (NG) pipelines and newly built pipelines is intended. Long distance pipeline grids require regular maintenance and repairs. For natural gas (NG) pipelines in-service welding is state of the art. Concepts such as hot-tapping (drilling into pressurized pipelines) and “stoppling” (sealing off pipeline sections after installing bypasses or pressure relieves) allow the repair of damaged pipeline sections or the installation of new branches without shutting the pipeline down, which in most cases isn’t possible from an economic standpoint. The EIGA 121/14 guideline already pointed out in 2014 that “a hydrogen hot-tap shall not be considered a routine procedure”. This shows that the determination of the transferability of these repair concepts to hydrogen pipelines is of utmost importance. Due to the degrading effects of hydrogen on mechanical proper-ties, commonly referred to as “hydrogen embrittlement” it is necessary to understand and investigate the occurring effects. In the special case of repair welding on in-service hydrogen pipelines an increased hydro-gen uptake due to a large heat input and microstructural changes in the material needs to be considered. Therefore, material degradation must be investigated to determine whether modifications of repair procedures are necessary to ensure a reliable and safe hydrogen transportation via pipelines. For this reason, this paper gives an overview on existing weld repair concepts and its risks and limitations in terms of hydrogen absorption and possible embrittlement effects when transferred to hydrogen pipelines. The complexity lies in a large variety of materials (low alloyed steels), pipeline diameters and corresponding welded joints. The material compatibility of materials in used (repurposed NG-pipelines) and new condition must be investigated. Particularly for repurposed/used pipelines the effect of a pre-matured/corroded inner surface and sometimes insufficient documentation of the material “history” needs to be considered. An overview on ongoing and completed R&D-projects with respect to repair concepts for hydrogen pipelines and hydrogen effects on pipeline materials is given. The focus hereby lies on possible methods of material testing and modeling. Its current difficulties, limits and possible solution will be discussed.
Contemporary steels creep-resistant steels like the 13CrMoV9-10 are used as thick plates e.g., for applications in hydrocrackers. The large plate thickness requires high efficiency welding processes like submerged arc welding (SAW) and a mandatory post weld heat treatment (PWHT). The PWHT-parameters stem from a combination of empirical knowledge and traditional experiments on free shrinking (FS) welds. In that connection, the formation of so-called stress-relief cracking (SRC) must be anticipated. The SRC susceptibility of a welded component is a complex combination and interaction of com-ponent specific, thermal, and metallurgical factors. Many of which have to date not been conclusively researched. For example, it is well known that SRCs develop during PWHT due to formation and growth of carbides on prior austenite grain boundaries, resulting in a significant hardness increase (secondary hardening) and toughness decrease. This leads to a high SRC susceptibility of the coarse grain heat-affected zone (CGHAZ) of the last weld bead during PWHT. This is intensified in case of high residual stresses from the component-specific, structurally induced stiffness. In combination with multi-layer welding this leads to a multiaxial stress distribution. Nonetheless, the combined effect of PWHT and high-residual stresses on the SRC formation is merely unknown. For that reason, this study presents the effect of different heating rates in conjunction with a certain component stiffness. For that reason, SAW joints of 13CrMoV9-10 steel were investigated under FS and defined external restraint condition.
Microalloying elements such as Nb and Ti play a decisive function in achieving the desired mechanical strength of quenched and tempered, high-strength fine-grain structural steels with a nominal yield strength ≥ 690 MPa. The current specifications for the chemical composition only provide manufacturers with upper limits. However, even minor deviations in the alloy concept can have a significant impact on the mechanical properties. Consequently, accurate prediction of weldability and the integrity of welded joints becomes difficult or even impossible due to differences in composition and the resulting microstructures. Undesirable consequences include a possible softening of the heat-affected zone (HAZ) or, conversely, hardening effects. In view of these challenges, various microalloying strategies with different Ti and Nb contents are being systematically investigated for the first time using specially developed laboratory casting alloys. Each alloying route is based on the common S690QL, maintaining both the chemical composition and the heat treatment parameters. To analyse the weldability, three-layer welds were performed using gas metal arc welding (GMAW) and critical microstructures, such as areas of the heat-affected zone (HAZ) that exhibit significant softening or hardening, were identified. The effect of the softened HAZ region on failure was evaluated using transverse tensile specimens. Digital image correlation (DIC) is used to image changes in local strains in different HAZ regions in situ. Using a specially developed mirror system, the local strains of the microstructure zones on the top and bottom of the weld are recorded simultaneously. This makes it possible to analyse how the weld seam geometry (e.g., V-seam) influences the strain gradients. In addition, the analysis of the local deformation helps to understand the effects of the softened HAZ on the global strain, the fracture constriction, the fracture position, and the overall fracture behavior.
Joining and welding technologies are of high importance for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport. In that connection, offshore and on-shore installed wind turbines are of high interest for the generation of electrical energy as well as photo-voltaic systems (solar cells). The electricity can be either directly transported or conversed via power-to-gas e.g., to hydrogen. In that scope, electrolyzer up to MW-range are of interest as well as the conver-sion back to electricity via fuel cells. In addition, hydrogen is a key element of the decarburization of in-dustries as well as the mobility sector encompassing sea, air and land transportation driven by hydrogen or its derivates. Well-known examples cover the direct reduction of iron ore to replace the conventional blast furnace process up to gas turbines or fuel cells for home-end use. All mentioned technologies re-quire reliable components, which are to a high extend dependent on joining and especially welding pro-cessing of materials. Especially, the (petro-) chemical industry has many years of experience with both materials used in hydrogen applications. The challenge is e.g., the transition to mass production of sys-tem components of electrolyzers/fuel cells and for distribution grids. At this point, the scalability of cur-rently applied joining processes often limits the economic efficiency, whereas especially laser welding or additive manufacturing will be of high interest. In that connection, it is very important to provide answers by joint research of universities, institutes, and industrial companies. Very often, solutions are already available and “just” have to be investigated and adapted for the new application, like repair welding of NG pipelines. For that reason, we want to set up a series of comprehensive papers with the aforementioned title. The idea is to get an in-depth but manageable overview of the importance of joining technologies in sustaina-ble energy generation, conversion, and transport encompassing current processes, limitations, and fur-ther perspectives. In that connection, the additive manufacturing is gaining more and more attention. If applicable, current challenges in the adaption or creation of new standards/regulations shall be addressed.
Die Umstellung der Wirtschaft auf wasserstoffbasierte Energieversorgung soll in Deutschland vor allem auf Basis der Umstellung des bestehenden Erdgasnetzes erfolgen. Dabei sollen ca. 90 % dieser Fernleitungsnetze auf dem bestehenden Erdgasnetz basieren. Die Beimischung von Wasserstoff zum Erdgas als auch der reine Wasserstofftransport werfen jedoch die Frage auf, ob und wie kompatibel die eingesetzten Materialien sind. Die Reparatur- und Erweiterungsfähigkeit von Erdgas-Bestandspipelines ist zu klären, wenn diese auf Wasserstoff umgestellt werden. Denn gerade Gashochdruckleitungen müssen regelmäßig gewartet und erweitert werden, um einen ordnungsgemäßen Betrieb sicherzustellen. Insbesondere das Schweißen unter Betriebsdruck bzw. an in Betrieb befindlichen Gasleitungen ist eine der wichtigsten Instandhaltungstechnologien, unabhängig von der Zusammensetzung des geförderten Mediums. Es ist daher dringend notwendig, eine geeignete Teststrategie zu erarbeiten, welche die nötigen Vorrausetzungen für sicheres Schweißen an in Betrieb befindlichen Druckwasserstoffleitungen schafft und entsprechende Kriterien für die Praxis liefert. Im Projekt H2-SuD - Einfluss des Schweißens auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2-Ferngasleitungen - soll geklärt werden, ob und wie stark mit einer Eigenschaftsdegradation geschweißter Rohrstähle in Gasnetzen in Folge einer Wasserstoffaufnahme zu rechnen ist. Die Präsentation gibt dazu einen kurzen Überblick über den aktuellen Status des Projektes. Die Förderung erfolgt im Rahmen der DVGW-Innovationsprogammes Wasserstoff (Nr. G 202131).
Wasserstoff erfüllt die zentrale Rolle für die Umwandlung der bisherigen fossil-basierten Energieerzeugung und -nutzung auf eine dekarbonisierte, nachhaltige Form. Dazu muss der Wasserstoff erzeugt, gespeichert, transportiert werden, bevor er wieder der Nutzung zugeführt wird. Hierzu sind entlang der gesamtem Prozesskette Wasserstofftechnologien notwendig, die einen sicheren Betrieb erfordern. Hierbei kommt dem schweißtechnischen Anlagen- und Behälterbau wesentliche Bedeutung zu, insbesondere (aber nicht ausschließlich) für Speicherung und Transport des Wasserstoffes. Der vorliegende Beitrag gibt einen kurzen Überblick, wo und wie die konventionelle Schweißtechnik hierzu wichtige Beiträge leistet. Die additive Fertigung, also das „Drucken“ von Bauteilen wird dabei zunehmend wichtiger, entlang der gesamtem Prozesskette der Wasserstofftechnologien. Gleichwohl darf nicht unterschätzt werden, dass auch wesentlicher Bedarf an der Erweiterung und teilweiser Neufassung von bestehenden Regel- und Normenwerken besteht.
Der Vortrag gibt einen kurzen Überblick über die Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige FuE-Bereiche. Fügetechnologien haben dabei wesentliche Bedeutung für die Umsetzung von technischen Komponenten der Wasserstofftechnologien. Forschungsschwerpunkte ergeben sich insbesondere für die Erzeugung und den Transport des Wasserstoffs.
Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustäh-len mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragver-haltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberech-nungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Aus-scheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Ab-kühlbedingungen geschaffen.
The study provides an overview of the aspects of joining and its importance in manufacturing of components for the more and more important field of hydrogen as key factor for the energy transition to a decarburized future. To this end, the fundamentals of the technology fields of hydrogen production, storage, transport, and application are presented and the state of the art of manufacturing of components for hydrogen technologies by joining is summarized. Based on representative examples from practice, research and development, the importance of joining technology in hydrogen technologies is clearly highlighted and perspectives for the future are derived. From a macroeconomic perspective, the focal points, or trends of joining technologies here include: the erection of new infrastructure for hydrogen storage and transport, and the safe conversion of existing natural gas infrastructure and its challenges for welded materials. In addition, we show the problems that are anticipated with in-service repair welding of hydrogen pipelines. In hydrogen applications, the efficient mass production of fuel cells and electrolysers is becoming increasingly important. For that reason, the importance of additive manufacturing is highlighted. Finally, the challenges for technical regulations and standardization by using hydrogen are shown.
Multi-principal element alloys (MPEAs) are innovative materials that have attracted extensive research attention within the last decade. MPEAs are characterized by a solid solution of equiatomic metallic elements. Depending on the number of elements, they are also referred as high entropy alloys (HEAs with n ≥ 4 elements like CoCrFeMnNi) and medium-entropy alloys (MEA with n = 3 elements CoCrNi). Depending on the alloy concept, MPEAs show exceptional properties in terms of mechanical performance or corrosion resistance at extreme environments. In that connection, hydrogen and its challenges for the most metallic materials gets more and more important. MPEAs are candidate materials for the substitution of conventional materials like austenitic stainless steels e.g., at very high-pressure up to 1000 bar. Those pressures are typically reached in valves or compressors for refueling of tanks with operational pressure of 700 bar. So far, the susceptibility of HEA/MEAs to hydrogen assisted cracking (if any) and the especially the underlying hydrogen uptake and diffusion was not within the scientific scope and not investigated in detail yet. For that reason, we focused on the hydrogen absorption the characterization of the hydrogen diffusion and trapping at elevated temperatures in a CoCrFeMnNi-HEA (each element with 20 at.-%) and CoCrNi-MEA, each element with 33.3 at.-%). As reference grade, the commercially available austenitic stainless steel AISI 316L was investigated. High-pressure hydrogen charging was conducted at different pressures in autoclave environment with maximum value of 1,000 bar. Thermal desorption analysis (TDA) via carrier gas hot extraction with coupled mass spectrometry was used with a max. heating rate of 0.5 K/s up to 650 °C. The measured desorption spectra of the different samples were deconvoluted into a defined number of individual peaks. The individually calculated peak temperatures allowed the definition of activation energies for predominant trap sites in the respective materials as well as the percentage share of the totally absorbed hydrogen concentration. The results present for the first time the complex interaction of both MPEAs and high-pressure hydrogen charging. A deconvolution of four peaks was selected and a main desorption peak was identified the dominant hydrogen trap containing the biggest share of the absorbed hydrogen concentration. The chemical composition an austenitic phase of both MPEAs is responsible for delayed hydrogen diffusion and strong, but mostly reversible, trapping. The comparison with the 316L samples showed significantly higher activation energies in the MPEAs, whereas hydrogen was also trapped at very high extraction temperatures. The absorbed maximum hydrogen concentration at 1,000 bar was 130 ppm for the CoCrFeMnNi-HEA, 50 ppm for the CoCrNi-MEA and 80 ppm for the 316L. It is interesting that the CoCrFeMnNi-HEA has obviously a way higher trapping capability compared to the conventional austenitic 316L, which could be a major advantage in terms of resistance to hydrogen assisted cracking.