Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (77)
- Zeitschriftenartikel (38)
- Beitrag zu einem Tagungsband (30)
- Posterpräsentation (6)
- Buchkapitel (3)
- Corrigendum (3)
- Forschungsbericht (2)
- Beitrag zu einem Sammelband (1)
- Dissertation (1)
Schlagworte
- Hydrogen (41)
- Welding (40)
- Wasserstoff (20)
- Diffusion (15)
- Creep-resistant steel (14)
- Schweißen (14)
- Hydrogen assisted cracking (11)
- Microstructure (11)
- Fügetechnik (10)
- High-entropy alloy (9)
Organisationseinheit der BAM
- 9 Komponentensicherheit (109)
- 9.0 Abteilungsleitung und andere (90)
- 9.4 Integrität von Schweißverbindungen (71)
- 9.2 Versuchsanlagen und Prüftechnik (32)
- 8 Zerstörungsfreie Prüfung (6)
- 8.4 Akustische und elektromagnetische Verfahren (4)
- 5 Werkstofftechnik (3)
- 5.1 Mikrostruktur Design und Degradation (3)
- 6 Materialchemie (2)
- 6.2 Material- und Oberflächentechnologien (2)
Paper des Monats
- ja (6)
This work explores the feasibility of producing bead-on-plate welds of a CrCoNi medium entropy alloy and a CrMnFeCoNi high entropy alloy using electron beam welding. The alloys were welded in two states: one in an as-cold-rolled condition and the other in an annealed condition. In addition, the materials are welded with two different parameters. The FCC microstructure of the welds is investigated using scanning electron microscopy assisted by energy-dispersive X-ray spectroscopy and electron-backscattered diffraction. The impact of the weld on the microstructure is discussed. The heat-affected zone is negligible for the annealed condition of both medium and high entropy alloys since there is no driving force for recrystallisation and the exposure time to high temperature is insufficient for grain coarsening. The texture formed in the fusion zone is also discussed and compared to the texture in the base metal and the heat-affected zone. Although the grain growth along the (100) crystallographic direction is preferential in all cases, the crystallographic texture type differs from each weld. Higher hardness values are measured in the medium entropy alloy’s base metal and fusion zone than in the high entropy alloy.
This work investigates the microstructure formed in friction stir welds of FCC alloys, focused on two multiprincipal alloys: a CoCrFeMnNi high-entropy alloy (HEA) and a CoCrNi medium-entropy alloy (MEA). A commercial stainless steel AISI 304 is used for comparison. The largest nugget was formed in the MEA, while the smallest was formed in the HEA. Grain refinement occurs in the stirred zone in all welds. Discontinuous dynamic recrystallisation is the predominant restoration mechanism during friction stir welding of the three investigated alloys. A sharp decrement in the Σ3 boundary fraction occurs in the stirred zone of the AISI 304 and HEA welds, while comparable values with the base metal are found for the MEA weld. The peak in the maximum index of crystallographic texture is observed on the advancing side of the stirred zone of the AISI 304 weld. A strong <001> θ-fibre texture is formed in the advancing side of the nugget in the AISI 304 from a well-established {123} <634> S-type texture in the base metal. Multiple crystallographic texture components without specific fibres are identified in most regions of the welds, indicating the complex shear path history during friction stir welding.
Das Kapitel beginnt mit einer kurzen Einführung über die Korrosion (Wechselwirkung zwischen einem Metall, einer korrosiven Umgebung und der der jeweiligen Konstruktion). Im zweiten Abschnitt werden die wichtigsten Formen der wässrigen elektrochemischen Korrosion (Flächenkorrosion, galvanische, selektive und interkristalline Korrosion sowie Loch- und Spaltkorrosion) betrachtet. Darüber hinaus wird die elektrochemische Korrosion unter mechanischer Belastung betrachtet (Spannungsrisskorrosion, wasserstoffunterstützte Rissbildung, Korrosionsermüdung), sowie Sonderformen der Korrosion (Erosion, Fretting und mikrobiologisch induzierte Korrosion). Der dritte Abschnitt befasst sich mit der chemischen und Hochtemperaturkorrosion (Oxidation, Aufkohlung, Hochtemperatur-Wasserstoffangriff, Aufschwefelung, Nitrierung, Halogenierung). Zusätzlich enthält das Kapitel Maßnahmen zur Vermeidung der Korrosion.
The chapter starts with a brief introduction about corrosion, which is defined as the interdependency between a metal, a corrosive environment, and the respective component design. The second section introduces the most important forms of aqueous electrochemical corrosion (uniform corrosion, galvanic corrosion, selective and intergranular corrosion, and finally pitting and crevice corrosion in the case of passive layer forming metals). In addition, electrochemical corrosion under applied mechanical load is introduced (stress corrosion cracking, hydrogen-assisted cracking, corrosion fatigue), as well as special forms of corrosion (erosion, fretting, and microbiologically induced corrosion). The third section of this chapter introduces (mostly dry) chemical corrosion and high-temperature corrosion (oxidation, carburization, high-temperature hydrogen attack, sulfurization, nitriding, halogenation). As in the case of electrochemical corrosion, chemical corrosion can also be superimposed by mechanical loads. Finally, general facts on the testing of corrosion are introduced.
Aircraft main landing gear (MLG) components are commonly manufactured from low-alloyed, martensitic, ultra-high strength steels (UHSS) that have to be coated for corrosion protection, representing an expensive and environmentally harmful production step. To avoid already partly banned corrosion protection plating, the new high-alloyed UHSS, Ferrium S53 (UNS S10500), has been designed to replace lowalloyed legacy materials and has been subjected to a limited field test over five years. As with the legacy alloys, UNS S10500 has a fully hardened martensitic microstructure known to be susceptible to hydrogen assisted cracking, per se. Containing about 10 wt% Cr, steels such as S10500 are at the lower limit for corrosion resistant alloys. Similar to super-martensitic stainless steels used in the oil and gas industry, a common failure sequence in marine environments represents pitting and subsequent hydrogen assisted stress corrosion cracking (HASCC). For addressing such phenomena quantitively, as required for respective lifetime assessments of MLG components and systems, the tolerance of such materials dependent on the absorbed hydrogen concentration must be evaluated quantitatively. However, there is a lack of such valuable materials data, as well as of the fractographic behavior dependent on the hydrogen concentration that might be absorbed during HASCC. To provide an improved understanding of the hydrogen dependent mechanical and fractographic behavior, samples of the legacy AISI 4340 and the new S10500 MLG steels have electrochemically been hydrogen-saturated and subjected to tensile testing. In contrast to a previous study, this contribution for the first time focuses on materials that have been salvaged from real service used landing gear components. In this study, it has been demonstrated that the service-applied S10500 steel has not only a higher strength, but also an improved ductility in comparison to the legacy AISI 4340 steel after similar service durations that provides a higher tolerance against hydrogen concentrations that might be absorbed during potential pitting and HASCC in marine environments. In addition, it has been found that the absorbed hydrogen concentration significantly affects the fracture behavior. Interestingly, hardening of the hydrogen charged low-alloyed AISI 4340 steel changes the fracture topography from trans- toward intergranular, while hardening of the S10500 steel turned the fracture topography from inter- to transgranular at respectively high hydrogen concentrations.
Creep-resistant steels such as the 13CrMoV9-10, used in the construction of thick-walled pressure vessels, are most commonly submerged arc welded (SAW). These steels can develop stress relief cracks (SRC) if the mandatory post weld heat treatment (PWHT) is performed improperly. Current PWHT parameters, such as heating rate and holding time at a specific holding temperature, are based on both empirical experience and conventional free shrinking welding experiments to characterize the SRC-susceptibility of the weld. These cannot adequately depict the higher residual stresses caused by the structurally induced stiffness of the surrounding construction. This study discusses the development of a repeatable, precise, and time-efficient methodology to study the effects of different stress levels and heating rates on the SRC susceptibility of the coarse grain heat-affected zone (CGHAZ). For that purpose, samples were thermically treated to simulate a coarse grain heat-affected zone (CGHAZ) and subsequently exposed to representative levels of stress during the heating phase of a PWHT. The recorded stress and heating rate–dependent strains were mathematically analyzed via curve tracing/calculus to identify interdependent effects. This procedure facilitates the measurement of material characteristics such as carbide growth on grain boundaries at the µm-scale via an integrated value over the entire sample volume. The first and second derivatives show a slight, precipitate-dependent, increase in hardness of the sample, depending on the heating rate and applied stress. This new methodology generates an improved assessment of the SRC susceptibility of SAW microstructures of creep-resistant CrMoV steels.
Multi-Principal-Element or High-Entropy Alloys (MPEAs/HEAs) have gained increasing interest in the past two decades largely due to their outstanding properties such as superior mechanical strength and corrosion resistance. However, research studies on their processability are still scarce. This work assesses the effect of different machining conditions on the machinability of these novel alloys, with the objective of advancing the introduction of MPEA systems into industrial applications. The present study focuses on the experimental analysis of finish-milling conditions and their effects on the milling process and resulting surface finish of CoCrFeNi, Al0.3CoCrFeNi and Al0.3CoCrFeNiMo0.2 alloys fabricated via Spark Plasma Sintering. Ball-nose-end milling experiments have been carried out various milling parameters such as cutting speed, feed per cutting edge, and ultrasonic assistance. In situ measurements of cutting forces and temperature on the tool edge were performed during the experiments, and surface finish and tool wear were analyzed afterwards. The results exhibited decreasing cutting forces by means of low feed per cutting edge and reduced process temperatures at low cutting speed, with the use of ultrasonic-assisted milling. It was shown that the machinability of these modern alloys through conventional, as well as modern machining methods such as ultrasonic-assisted milling, is viable, and common theories in machining can be transferred to these novel MPEAs.
Metals that are exposed to high pressure hydrogen gas may undergo detrimental failure by embrittlement. Understanding the mechanisms and driving forces of hydrogen absorption on the surface of metals is crucial for avoiding hydrogen embrittlement. In this study, the effect of stress-enhanced gaseous hydrogen uptake in bulk metals is investigated in detail. For that purpose, a generalized form of Sievert's law is derived from thermodynamic potentials considering the effect of microstructural trapping sites and multiaxial stresses. This new equation is parametrized and verified using experimental data for carbon steels, which were charged under gaseous hydrogen atmosphere at pressures up to 1000 bar. The role of microstructural trapping sites on the parameter identification is critically discussed.
Effect of Tensile Loading and Temperature on the Hydrogen Solubility of Steels at High Gas Pressure
(2023)
The hydrogen solubility in ferritic and martensitic steels is affected by hydrostatic stress, pressure, and temperature. In general, compressive stresses decrease but tensile stresses increase the hydrogen solubility. This important aspect must be considered when qualifying materials for high‐pressure hydrogen applications (e.g., for pipelines or tanks) by using autoclave systems. In this work, a pressure equivalent for compensating the effect of compressive stresses on the hydrogen solubility inside of closed autoclaves is proposed to achieve solubilities that are equivalent to those in pipelines and tanks subjected to tensile stresses. Moreover, it is shown that the temperature effect becomes critical at low temperatures (e.g., under cryogenic conditions for storing liquid hydrogen). Trapping of hydrogen in the microstructure can increase the hydrogen solubility with decreasing temperature, having a solubility minimum at about room temperature. To demonstrate this effect, the generalized law of the hydrogen solubility is parameterized for different steels using measured contents of gaseous hydrogen. The constant parameter sets are verified and critically discussed with respect to the high‐pressure hydrogen experiments.
Die Studie gibt einen kurzen Überblick über die jetzige Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Forschungsbedarfe für die Branche in den einzelnen Technologiefeldern Wasserstofferzeu-gung, -speicherung, -transport und -nutzung. Fügetechnologien haben dabei wesentliche Bedeutung für die er-folgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien. Die Schwerpunkte bzw. For-schungsbedarfe ergeben sich bspw. durch die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie durch Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstofferzeugung und -anwendung wird z.B. die Entwicklung effiziente Massenproduktionsmethoden von Elektrolyseuren und Brennstoff-zellen einen wichtigen Meilenstein bilden und laserbasierte Fügetechnologien sind hier zum Teil schon etabliert. Die additive Fertigung nimmt dabei eine Querschnittsposition ein und besitzt hohes Anwendungspotential für die Zukunft z.B. für die Fertigung von Komponenten in Gasturbinen. Aus den technischen Fragestellungen und For-schungsbedarfen ergeben sich zudem Herausforderungen für die notwendige Neu- und Weiterentwicklung von technischen Regelwerken und Normen und den Eingang in die Aus- und Weiterbildung von fügetechnischem Fachpersonal.
The article "Influence of welding stresses on relief cracking during heat treatment of a creep-resistant 13CrMoV steel: Part I - Effect of heat control on welding stresses and stress relief cracking" was originally published in the journal "Welding in the world" Online First without Open Access. After publication in volume 64, issue 5, page 807-817 the authors decided to opt for Open Choice and to make the article an Open Access publication. Therefore, the copyright of the article has been changed to The Author(s) 2020 and the article is forthwith distributed under the terms of the Creative Commons Attribution Attribution 4. 0 International License.
The article "Influence of welding stresses on relief cracking during heat treatment of a creep-resistant 13CrMoV steel: Part II - Mechanisms of stress relief cracking during post weld heat treatment" was originally published in the journal "Welding in the world" Online First without Open Access. After publication in volume 64, issue 5, page 819-829 the authors decided to opt for Open Choice and to make the article an Open Access publication. Therefore, the copyright of the article has been changed to The Author(s) 2020 and the article is forthwith distributed under the terms of the Creative Commons Attribution Attribution 4. 0 International License.
The avoidance of failures during the fabrication or operation of petrochemical reactors made of creep-resistant, low-alloy steels as 13CrMoV9-10 requires still research despite over 60 years of international investigations in the field of stress relief cracking. The quality of modern base materials and filler metals leads to the fact that previously known crack causes, such as impurities of S or P, recede into the background. Rather, the causes are increasingly to be found in the fabrication process. Investigations on the influence of heat control on the stresses in welded components and thus on the stress relief cracking sensitivity under realistic manufacturing conditions are not yet available. This work is subdivided in two parts. Part 1 of this study focused on the effect of heat control during submerged arc welding on the stresses. For this purpose, a testing facility was applied, which allows to observe the forces and moments accumulating during welding or heat treatment in a component-like specimen under shrinkage restraint. The stress acting in the specimen increases with higher preheat/interpass temperatures and higher heat input. During the heat treatment, the stresses are relieved. Nevertheless, cracks are formed already during heating. The total crack length correlates with the heat input.
Welding of 13CrMoV9-10 vanadium steel requires care due to an increased susceptibility to stress relief cracking during post weld heat treatment. Previous research into the crack formation in creep-resistant steels has focused on thermal and metallurgical factors; however, little knowledge has been gathered regarding the crack formation during post weld heat treatment considering real-life restraint conditions. This work is subdivided in two parts. Part I showed that an increasing heat input during submerged arc welding under restraint led to an increasing stress level in the joint prior to the post weld heat treatment. The magnitude of stress relief cracking observed in the heat-affected zone after the post weld heat treatment is affected by the heat input. In Part II of this work, the cracks and the associated microstructure which occurred under restraint were studied. The application of a Special acoustic emission analysis indicated that the cracks formed in a temperature range between 300 and 500 °C during the post weld heat treatment. The toughness in the heat-affected zone of the restrained welds was affected by the welding heat input.
Microstructural analyses of all specimens revealed accelerated aging due to precipitation of carbides during post weld heat treatment under restraint.
Residual stresses and distortions in welded I-girders for steel construction are relevant when evaluating the stability of steel beams and column members. The application of high strength steels allows smaller wall thicknesses compared to conventional steels. Therefore, the risk of buckling has to be considered carefully. Due to the lack of knowledge concerning the residual stresses present after welding in high strength steel components conservative assumptions of their level and distribution is typically applied. In this study I-girders made of steels showing strengths of 355 MPa and 690 MPa were welded with varying heat input. Due to the dimension of the I-girders and the complex geometry the accessibility for residual stress measurement using X-ray diffraction was limited. Therefore, saw cutting accompanied by strain gauge measurement has been used to produce smaller sections appropriate to apply X-ray diffraction. The stress relaxation measured by strain gauges has been added to residual stresses determined by X-ray diffraction to obtain the original stress level and distribution before sectioning. The combination of both techniques can produce robust residual stress values. From practical point of view afford for strain gauge application can be limited to a number of measuring positions solely to record the global amount of stress relaxation. X-ray diffraction can be applied after sectioning to determine the residual stresses with sufficient spatial resolution.
Measurement and numerical modeling of residual stresses in welded HSLA component-like I-girders
(2016)
The present contribution shows the residual stress results obtained from experiments with the sectioning method in comparison to global(structural) welding simulation models on component-like (i.e., large scale) I-girders made
of structural steel grades S355 and S690QL. Plates were welded by conventional gas metal arc welding using two different heat inputs. In addition, the base material was assumed to be stress-free. Based on these results, conclusions and recommendations for the design of welded I-girders are drawn.
The nonlinear analysis became a common tool to precisely assess the load-bearing behavior of steel beam and column members. The failure level is significantly influenced by different types of imperfections, among geometric also structural imperfections (residual stresses). Here are still gaps in the knowledge. Nowadays, 3-D welding simulation developed to a level where it could provide reliable estimation of weld-induced distortion and residual stresses. Nevertheless, modelling and computational effort are still in a less practicable range. In this study a simplified procedure to implement residual welding stresses in continuous large scale members is proposed and the influence on the ultimate limit state of slender members in compression is evaluated for two common structural steel grades. The results showed significant improvements in the utilization of load bearing capacity compared with simplified design methods. The comparatively general approach in this study offers
potential for future optimization.
This article presents the latest results of an ongoing national research project on improved models for the prediction of welding residual stresses of thick-plated welded I-girders. The experimental program is presented and the importance of different influencing factors on the residual stresses is discussed in detail. All results are compared for mild (S355J2+N) and high strength (S690QL) steel. Finally, conclusions for further works are drawn.
Welding is the most important joining technique and offers the advantage of customizable plate thicknesses. On the other hand, welding causes residual stresses and deformations influencing the load carrying capacity. Their consideration in the design requires simple and fast models. Though welding simulation has contributed to accurately access to these values nowadays, their application to large components remains still in a less practicable range. Nevertheless, many studies emphasized the need to make corrections in recently available simplified models. Especially the influence of residual stresses seems somewhat overestimated in many cases if comparing conventional structural steel S355 and high-strength steel S690. In the age of computer-aided design, an improved procedure to implement weld-inducted imperfections appears overdue. This will be presented in two parts. The first part illustrates the potential influence of post-welding imperfections exemplified for weak axis buckling in comparison with the general method in accordance with Eurocode 3. Residual stresses and initial crookedness were varied systematically in order to produce a scatter band of capacities. An approach to characterize the borders of these imperfections was untertaken before that. The excessive scattering of reduction factors for the load bearing capacity demonstrates the importance of these variables. Results were finally evaluated against advanced simulation models which will be further detailed in part two of this contribution.
In the field of modelling hydrogen assisted cracking (HAC) phenomenon, hydrogen diffusivity is an important input parameter for numerical simulation. In terms of hydrogen diffusion coefficients, they have great impact on realistic assessment of the evolution of possible crack critical hydrogen concentrations. In addition, the chemical compositions of steels can have a strong effect on hydrogen diffusion. Unfortunately, literature provides a wide range of available hydrogen diffusion coefficients even for similar microstructures and equal temperatures. The scattering of the data can lead to significant deviations in the results of simulating the evolving hydrogen concentrations due to hydrogen uptake (by fabrication or service). Thus, the application of such data to crack-models or for component life tie predictions can be realized up to the present only by considering envelope curves of such value, corresponding to a work or bench case scenario, respectively. For improved reliability of numerical simulaitons, it is necessary to minimize the mentioned deviation of these data. Hence, this work focuses on the validation of hydrogen diffusion coefficients obtained from permeation experiments at room temperature. Two baintic steels with different alloying concepts were investigated, the creep-resistant 7CrMoVTiB10-10 and the reactor pressure vessel grade 20MnMoNi4-5. A numerical model is presented for simulation of the corresponding hydrogen diffusion during permeation experiments using the finite element software ANSYS. Three different diffusion coefficients (obtained from different common calculation methods) are considered and compared to numerical results. The vases of thes calculation methods are permeation transients which are a direct measure for hydrogen. The results of the simulated hydrogen diffusion coefficients show that only one procedure for calculation of diffusion coefficitnes is suitable in comparision to the experimental values. Thus, it is suggested to use this method for analysis of experimental results in case of hydrogen diffusion during permeation experiments. Furthermore, this work supplies validated values for the hydrogen diffusion coefficients of both steel grades.
Offshore wind turbines are an important goal in national energy strategies worldwide. Foundation structures are manufactured from submerged arc welded (SAW) plates with thicknesses up to 200 mm. In that connection, high-strength steels like the S420G2+M are more and more applied offering the possibility for increased stability and load-bearing capacity of the foundations. These offshore steel grades can show a susceptibility for delayed hydrogen assisted cold cracking of the weld joints. For that purpose, a minimum waiting time (MWT) of up to 48 h (dependent on applied standards) is recommended before non-destructive testing is allowed and conducted. But this concept is based on older steel grades that have been used for three or more decades. Nowadays, the metallurgical improvements (clean steels, proper rolling, and heat treatment) of base materials and well as welding consumables must be anticipated. Hence, the MWT concept should be critically discussed as it is assumed to be very conservative. For that reason, the focus of this study was to investigate the diffusion behavior in S420G2+M steel and its multi-layer SAW joint. Electrochemical permeation experiments were carried at room temperature. Boundary conditions were anticipated in terms of using different sample thicknesses. From the experimental data, hydrogen diffusion coefficients and absorbed diffusible hydrogen concentrations had been calculated. It was shown that hydrogen diffusion in the base material is increased compared to the weld metal. In addition, the sample thickness had a significant on the calculated diffusion coefficients. The minimum and maximum diffusion coefficients had been used for numerical modelling of the hydrogen diffusion in the welding joint. It became clear that a MWT must be always regarded together with a critical initial diffusible hydrogen concentration for the evaluation of a possible delayed cracking as diffusion times were mostly > 48 h due to the thick plates.
This article provides an impression on potentials in applying nowadays welding simulation tools in construction design. This is carried out exemplary on plate girders from two structural steel grades. The calculated residual stresses are compared with measurements by sectioning method. It has been repeatedly stated that present Eurocode models fail to approximate the residual stresses. Especially for high strength steel (HSS) only limited information is available on realistic occurring residual stresses in typical I-girders. The investigations are aimed to give further guidance on these values. A few proposals on advanced models are discussed.
This article addresses the imperfections caused by the weld assembly in I-shape sections made of two structural steel grades. Load influencing imperfections are assumed as deviations from the ideal shape (e.g. bending distortion) and longitudinal residual stresses. The quality of a numerically aided design of components exposed to either compression and/or bending is significantly affected, depending on these parameters. The Eurocode (EC3) provides robust simplified models. As a result, the Ultimate Limit State (ULS) is approached on a conservative basis. The following investigations are aimed at providing further guidance on these values in component-like specimens. The long term goal is an improved understanding of the load-bearing capacity of such sections. As a first step in this process, the experimental and corresponding numerical studies are presented.
In vielen Bereichen des modernen Stahlbaus kommen geschweißte Vollwandträger, wie I-Träger zum Einsatz. Im Gegensatz zu Walzprofilen können die Bauhöhe, die Querschnittsform und die Blechdicken an die Beanspruchung angepasst werden, wodurch sich wirtschaftliche Vorteile erzielen lassen. Dabei werden heutzutage immer häufiger hochfeste Feinkornbaustähle mit (Mindest-) Fließgrenzen bis 690 MPa eingesetzt. Zur verbesserten Ausnutzung des Tragfähigkeitspotenzials geschweißter Profile aus diesen Stählen existieren keine geeigneten Modelle zur Erfassung der schweißfertigungsbedingten Eigenspannungen an realen Komponenten. Diese Daten werden durch konservative Annahmen angenähert. Die potentielle Tragfähigkeit geschweißter Konstruktionen wird daher in der Regel unterschätzt. Die Eigenspannungsannahmen in DIN EN 1993 basieren auf starken Vereinfachungen, bspw. im Rahmen sog. „Ersatzstabnachweise“. Diese setzen die Proportionalität der Eigenspannungsamplituden zur Fließgrenze voraus. Vergleichsrechnungen mit einem parametrisierten Eigenspannungsmodell zeigten mögliche Abweichungen in den berechneten Tragfähigkeiten über mehrere Knicklinien. Die Festlegungen hinsichtlich der anzuwendenden Knicklinie beeinflussen jedoch die Blechdicken und somit in erheblichem Maße auch die Fertigungskosten.
Als Optimierungsstrategie wurden in diesem Forschungsprojekt deswegen unterschiedliche anwendungsorientierte Modellansätze entwickelt, welche mithilfe nichtlinearer Traglastberechnungen, die höhere Ausnutzung von Tragfähigkeitsreserven ermöglichen sollen.
Forschungsziel war somit primär die Entwicklung und Bereitstellung entsprechender Berechnungsansätze. Experimentell wurde hierzu der Eigenspannungszustand von konventionell geschweißten Strukturen am Beispiel der im Stahlbau besonders häufig verwendeten I-Träger aus zwei gängigen Baustählen, einem unlegierten Baustahl S355J2+N und einem Feinkornbaustahl S690QL, erfasst und durch numerische Schweißstruktursimulationen ergänzt. Anschließend erfolgte die Ableitung eines vereinfachten Berechnungsmodells zur weiteren Berücksichtigung in nichtlinearen Tragfähigkeitsberechnungen. Die Erkenntnisse sollen in einen entsprechenden Anwenderleitfaden, herausgegeben durch das Technical Committee 8 der Europäischen Konvention für Stahlbau, einfließen und diesbezüglich als Orientierung einer möglichen zukünftigen Anpassung der Knicklinien in DIN EN 1993-1-1 dienen.
Im Projekt wurden die genannten Stähle in zwei typischen Dickenkombinationen von 25/15 mm und 20/10 mm (Gurt- und Stegbleche) zu Großprobekörpern „I-Träger“ unter industrienahen Fertigungsbedingungen mittels Metall-Aktivgasschweißen gefügt. Diese erzeugten die typischen Eigenspannungen, die in solchen Trägern nach der Fertigung vorliegen. Während des Schweißens wurden die Temperaturfelder durch Thermoelemente aufgezeichnet. Die Eigenspannungen wurden nach dem Schweißen experimentell durch eine Kombination aus mechanischem Zerlegen (Zerlegemethode) und anschließender mobiler Röntgendiffraktometrie (XRD) festgestellt. Der Einfluss der industriell üblichen Brennschnittkantenvorbereitung der Bleche auf die finalen
Eigenspannungszustände wurde experimentell zusätzlich an kleinmaßstäblichen Proben untersucht. Metallographische Analysen (Schliffbilder und Härtemessungen) komplettierten das experimentelle Programm der FE 2 (BAM, Berlin).
Die Ergebnisse zeigten, dass beim mechanischen Zerlegen bereits ein Großteil der Eigenspannungen herausgelöst wurde. Eine Aussage zu den nahtnahen Zugeigenspannungen war allerdings erst durch die Überlagerung mit der XRD möglich. Dabei zeigte der S690QL überwiegend ein besseres Verhalten als der S355J2+N, welches sich unter anderem in abgesenkten Zugeigenspannungen im Verhältnis zur jeweiligen Fließgrenze äußerte. Die maximalen Eigenspannungen wurden dabei zumeist in der Wärmeeinflusszone (WEZ) der Schweißnaht gemessen, unabhängig von der eingebrachten Streckenenergie oder der Festigkeit des Grundwerkstoffs. Die baupraktische Annahme, dass die maximalen Eigenspannungen in Höhe der Fließgrenze vorliegen können, wurde nur in Einzelfällen und nur für den S355J2+N bestätigt. Die experimentellen Ergebnisse zeigten für die Druckeigenspannungen ebenfalls reduzierte relative Eigenspannungswerte des S690QL. Dies zeigt die notwendige weitere Optimierung bei der Wahl der Bewertungsansätze für Eigenspannungen auf die Tragfähigkeit.
Die erzeugten Messwerte dienten im weiteren Verlauf als Eingangswerte für die Modellentwicklung und die numerischen Simulationen an I-Trägern durch die FE 1 (LSH, Cottbus). Die numerischen Schweißsimulationen erfolgten in Simufact.Welding® für die Simulationsmodelle mit „klassischem“ Schweißsimulationsansatz sowie in Ansys® für vereinfachte Simulationen und Näherungsansätze. Die Modelle lieferten insgesamt vergleichbare Ergebnisse für die Längseigenspannungen mit teils jedoch erheblichen Unterschieden in den Rechenzeiten. Durch eine angepasste Vernetzung konnte die Rechenzeit in allen Fällen deutlich reduziert werden. Aufgrund der verwendeten Bauteilgrößen ist die Anwendung der Modellierung mit Volumenelementen allerdings meistens nicht praktikabel. Für typische Trägerschweißungen bieten stattdessen Querschnittsmodelle mit der Annahme eines verallgemeinerten ebenen Verzerrungszustands eine mögliche Alternative. Der Abgleich der Ergebnisse mit den Experimenten lieferte zusammenfassend überwiegend gute bis befriedigende Übereinstimmungen. Die experimentell festgestellten Tendenzen wurden dabei in allen Fällen richtig vorhergesagt.
Eine umfassende Bewertung der erzielbaren Genauigkeiten war bisher nicht möglich. Dies lag einerseits daran, dass die Datendichte der mit der durch die Zerlegung gewonnen Ergebnisse gering war. Anderseits lieferten die überlagerten Ergebnisse mit der XRD in Teilen, insbesondere in den interessierenden Druckbereichen, widersprüchliche Aussagen zum Eigenspannungseinfluss, was bisher nicht abschließend geklärt werden konnte. Darüber hinaus entstanden etwaige Abweichungen in den Simulationen auch durch die zugrunde gelegten Materialdaten selbst. Diese entsprachen Standarddatensätzen aus Materialbibliotheken. Die Skalierung dieser erfolgte gleichmäßig über den gesamten Temperaturbereich. Insbesondere für den S690QL existierten zu wenige belastbare Materialkennwerte.
Entsprechende Versuche konnten im Rahmen dieses Vorhabens nicht mit durchgeführt werden.
Dennoch konnten hinsichtlich eines vereinfachten Berechnungsvorgehens zur Berücksichtigung der Schweißeigenspannungen in Tragfähigkeitsberechnungen einige wichtige Erkenntnisse gewonnen werden. Auf Basis der in den numerischen Schweißsimulationsmodellen ermittelten plastischen Dehnungsmuster, auch „Eigenspannungsquellen“, wurde eine vereinfachte Simulationsvorgehensweise vorgeschlagen und verifiziert. Die dabei eingeführten Vereinfachungen wurden im Hinblick auf die Berechnung ausschließlich der plastischen Längsdehnungen bzw. der Längseigenspannungen gewählt. Die Anwendbarkeit ist daher auf ausreichend lange Schweißträger mit Längsnähten beschränkt. Einige Modellmodifikationen zur weiteren Vereinfachung bzw. Modellimplementierung in die strukturmechanische Berechnung an großen Komponenten wurden vorgestellt. Abschließend erfolgt die Einstufung in eine mögliche Knicklinie auf Basis eines mittels GMNIA (geometrisch und materiell nichtlineare Analyse mit Imperfektionen) Berechnungen simulierten Streubands der Tragfähigkeiten mittels Abaqus® und Ansys®. Die anfängliche Hypothese einer günstigeren Knicklinie eines S690QL im Vergleich zum S355J2+N wurde dabei rechnerisch bestätigt. Der experimentelle Nachweis mittels entsprechender Trägerfähigkeitsversuche ist allerdings noch ausstehend.
With the introduction of a hydrogen-based energy and national economy, safety-relevant components for hydrogen technologies are becoming increasingly important. Characteristic of hydrogen technologies are, for example, harsh environmental conditions such as cryogenic or high-pressure storage, corrosion issues in fuel cells and electrolyzers, turbines, and many more. Additive manufacturing of components is becoming increasingly important and irreplaceable for the production of complex technical systems. Using the case studies of burners for gas turbines and electrodes and membranes for polymer (PEMFC) and solid oxide (SOFC) fuel cells, this article shows the potential of additive manufacturing of components. At the same time, however, the challenge of considering divergent mechanical properties depending on the direction of assembly in a "hydrogen-compatible" manner is also highlighted. Finally, the challenges posed by additive manufacturing and hydrogen for materials testing are highlighted under scenarios that are as realistic as possible.
Dieses Dokument fasst den Projekfortschritt des BAM-Projektes "Entwicklung von Wärmenachbehandlungsstrategien zur Vermeidung von Spannungsrelaxationsrissen" im Rahmen des Fachausschusses 1 "Schweißmetallurgie" des DVS e.V. für das Projektjahr 2021 zusammen und stellt die wichtigsten Ergebnisse in Kurzform vor.
Bewertungsmethode zur Interaktion von Metallurgie und Reaktionskräften beim PWHT warmfester Stähle
(2022)
Die Präsentation fasst die Entwicklung einer Ersatzprüfmethode für sogenannte Stress-Relief-Cracks (SRC) bei dickwandigen und kriechfesten geschweißten Stahlkomponenten zusammen. Über die Kombination von gezielter mechanischer Beanspruchung unter hoher Temperaturbeanspruchung werden die Effekte des Post Weld Heat Treatments auf SRC realistisch erstmal auf Laborskala nachgebildet.
Joining processes for components in hydrogen technologies: Current need and future importance
(2022)
This presentation gives an overview on the importance of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the three technological fields: hydrogen storage, transport and use (in terms of the emerging field of additive manufacturing). Finally, some remarks are given for necessary changes in the standardization.
Die Vortrag gibt einen Überblick, warum Kaltrissprüfung von geschweißten Stählen ständig weiterentwickelt werden muss. Am Beispiel des Implant- und Tekken-Tests werden die Einsatz- u. Anwendungsgrenzen bewertet. Zu berücksichtigen ist, dass beim Schweißen eine äußere mechan. Beanspruchung durch bauteilspezifische Steifigkeitsverhältnisse wirksam ist. Zusätzlich werden weiterführende Prüfverfahren zur Bestimmung der Wasserstoffkonzentration und -diffusion in Schweißnähten vorgestellt, wie die Trägergasheißextraktion (TGHE) für die Ermittlung der Wasserstoffkonzentration (ISO 3690) oder Hochtemperaturdiffusionskoeffizienten. Diese Werte sind für die schweißtechnische Praxis von großer Bedeutung, um Haltezeiten z.B. für das Wasserstoffarmglühen abzuleiten.
Martensitic 9 %-Cr steels like P91 and P92 show susceptibility to delayed hydrogen assisted cracking depending on their microstructure. In that connection, effective hydrogen diffusion coefficients are used to assess the possible time-delay. The small number of available diffusion coefficients varies already at room temperature by several orders of magnitude (mostly regarded as result of present microstructure). Especially P91 weld metal diffusion coefficients are rare so far. For that reason, electrochemical permeation experiments had been conducted using P92 base metal and P91 weld metal (in as-welded and heat-treated condition) with different thicknesses. The diffusion coefficients are calculated by two methods (time-lag and inflection point method) were performed. The results show that, despite of microstructural effects, the sample thickness must be considered as it influences the calculated diffusion coefficients. Finally, the comparison of calculated and measured hydrogen concentrations (determined by carrier gas hot extraction) enables the identification of realistic diffusion coefficients.
This presentation summarizes the latest results on the BAM-Themenfeld project SURDIA on processing of high-entropy alloys (HEAs) at BAM. At first, the influence of machining by ultrasonic-assisted milling on the surface integrity is presented. Second, the weld processing by Tungsten Inert Gas (TIG) welding is presented and the results of the Friction Stir Welding (FSW), which is conducted at BAM for the first time.
This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Finally, some remarks are given for necessary changes in the standardization and its challenges.
Martensitic 9 %-Cr steels like P91 and P92 show susceptibility to delayed hydrogen assisted cracking depending on their microstructure. In that connection, effective hydrogen diffusion coefficients are used to assess the possible time-delay. The small number of available diffusion coefficients varies already at room temperature by several orders of magnitude (mostly regarded as result of present microstructure). Especially P91 weld metal diffusion coefficients are rare so far. For that reason, electrochemical permeation experiments had been conducted using P92 base metal and P91 weld metal (in as-welded and heat-treated condition) with different thicknesses. The diffusion coefficients are calculated by two methods (time-lag and inflection point method) were performed. The results show that, despite of microstructural effects, the sample thickness must be considered as it influences the calculated diffusion coefficients. Finally, the comparison of calculated and measured hydrogen concentrations (determined by carrier gas hot extraction) enables the identification of realistic diffusion coefficients.
Wasserstoff erfüllt die zentrale Rolle für die Umwandlung der bisherigen fossil-basierten Energieerzeugung und -nutzung auf eine dekarbonisierte, nachhaltige Form. Dazu muss der Wasserstoff erzeugt, gespeichert, transportiert werden, bevor er wieder der Nutzung zugeführt wird. Hierzu sind entlang der gesamtem Prozesskette Wasserstofftechnologien notwendig, die einen sicheren Betrieb erfordern. Hierbei kommt dem schweißtechnischen Anlagen- und Behälterbau wesentliche Bedeutung zu, insbesondere (aber nicht ausschließlich) für Speicherung und Transport des Wasserstoffes. Der vorliegende Beitrag gibt einen kurzen Überblick, wo und wie die konventionelle Schweißtechnik hierzu wichtige Beiträge leistet. Die additive Fertigung, also das „Drucken“ von Bauteilen wird dabei zunehmend wichtiger, entlang der gesamtem Prozesskette der Wasserstofftechnologien. Gleichwohl darf nicht unterschätzt werden, dass auch wesentlicher Bedarf an der Erweiterung und teilweiser Neufassung von bestehenden Regel- und Normenwerken besteht.
Low-alloyed CrMoV steels, such as T24, are widely used for welded components in fossil power stations due to their excellent creep-strength. Spectacular failure cases in the recent years exhibited severe cracking in T24 welds. The results showed that hydrogen-assisted cracking (HAC) occurring up to 200 degree Celsius cannot be excluded. Hence, a basic understanding is necessary on how hydrogen affects the material properties of welded microstructures. In this regard, each weld microstructure (HAZ and weld metal) has influence on the HAC susceptibility and respective hydrogen diffusion. Thus, the present contribution summarizes different results obtained from experiments with grades T24 (CrMoV alloy) and T22 (CrMo) and thermally simulated HAZ. Tensile tests were conducted with hydrogen charged specimens and compared to hydrogen-assisted stress corrosion cracking results obtained from slow strain rate tests (SSRT) up to 200 degree Celsius. Electrochemical permeation and degassing experiments were performed to identify a particular weld microstructure influence on hydrogen diffusion and trapping (especially in the HAZ). The results showed that T24 base material has improved resistance to hydrogen-assisted degradation/cracking. In contrast, the as-welded HAZ had remarkably increased susceptibility (tesnile tests at hydrogen concentration of 1 to 2 ppm). SSRT experiments confirmed this at elevated temperatures for both the T24 and the T22. Hence, the evaluation of a particular degradation of the mechanical properties should be performed independently for each weld microstructure. In addition, the HAZ showed decreased diffusion coefficients (at room temperature) of approximately one magnitude compared to the base materials. Trapped hydrogen was determined in the T24 at temperatures up to 120 degree Celsius compared to 75 degree Celsius in the T22. This has to be considered in case of changing operational temperatures, e.g. in the case of start-up and shutdown processes of boiler components.
Adaption of Heat Control Concepts for Welding Stress Optimization in High-strength Steel Components
(2016)
High-strength structural steels from 690 MPa are increasingly applied at present. Major reasons are lightweight design trends and potential cost reductions. The structural design of welds and their manufacturing become more challenging with increasing material strength. By reasons of a higher yield ratio of these steels, the development of high residual stresses has to be avoided, since they are detrimental to the components safety and performance. Local restraint stresses and welding loads due to external shrinkage restraints occur. Frequently, this leads to critical tensile residual stresses in the weld and HAZ. In this study, influences of welding process parameters and restraint conditions on the residual stress state in welded components of high-strength steels were investigated. Multilayer GMAW tests under free shrinkage and experiments under well-defined restraints in special in-house developed testing facilities were accomplished. The tests permitted analyses of the resulting local residual stresses measured by means of X-ray diffraction and global reaction stress build-up while welding and cooling. Significant effects were found for heat control, seam configuration and restraint condition. Besides high restraints, elevated preheating and interpass temperatures lead to increased welding stresses. An adaption of welding parameters considering heat control, weld run sequence and seam configuration proved to be beneficial.