Filtern
Dokumenttyp
- Vortrag (52)
- Zeitschriftenartikel (30)
- Beitrag zu einem Tagungsband (22)
- Buchkapitel (2)
- Forschungsbericht (2)
- Posterpräsentation (1)
Schlagworte
- Welding (33)
- Hydrogen (31)
- Wasserstoff (20)
- Schweißen (14)
- Diffusion (13)
- Creep-resistant steel (12)
- Fügetechnik (10)
- High-entropy alloy (9)
- Hydrogen assisted cracking (8)
- Mechanical properties (8)
Organisationseinheit der BAM
- 9 Komponentensicherheit (109) (entfernen)
Paper des Monats
- ja (6)
Influence of Surface Preparation on Cracking Phenomena in TIG-Welded High and Medium Entropy Alloys
(2022)
Multi-element systems with defined entropy (HEA—high entropy alloy or MEA—medium entropy alloy) are rather new material concepts that are becoming increasingly important in materials research and development. Some HEA systems show significantly improved properties or combinations of properties, e.g., the overcoming of the trade-off between high strength and ductility. Thus, the synthesis, the resulting microstructures, and properties of HEA have been primarily investigated so far. In addition, processing is crucial to achieve a transfer of potential HEA/MEA materials to real applications, e.g., highly stressed components. Since fusion welding is the most important joining process for metals, it is of vital importance to investigate the weldability of these materials. However, this has rarely been the subject of research to date. For that reason, in this work, the weldability depending on the surface preparation of a CoCrFeMnNi HEA and a CoCrNi MEA for TIG welding is investigated. The fusion welding of longer plates is described here for the first time for the CoCrNi alloy. The welds of both materials showed distinct formation of cracks in the heat affected Zone (HAZ). Optical and scanning electron microscopy analysis clearly confirmed an intergranular fracture topography. However, based on the results, the crack mechanism cannot be conclusively identified as either a liquid metal embrittlement (LME) or hot cracking-like liquid film separation.
Multiple principal element alloys encompass the well-known high entropy alloys (HEA). The alloy system represents a new class of materials consisting of at least three alloying elements, each containing 5 to 35 at.%. Thus, this alloying concept differs fundamentally from conventional materials such as steel or nickel alloys. For this purpose, the alloying elements are specifically selected, the microstructures are adjusted in a single-phase and, in some cases, multi-phase manner. In particular, conflicting goals, such as the trade-off between strength and ductility in conventional steels, are overcome. However, in the last 20 years, the focus has been on material synthesis. With the increase in available material quantities, the focus is now on processing issues such as joining and welding processes. The weldability of HEAs has received very little attention so far. The experience with dissimilar metal welds is completely lacking but is essential for the application of these materials in combination with conventional materials. The present study presents comprehensive experimental results on the weldability of an equimolar CoCrFeMnNi-HEA in cold-rolled and heat-treated condition, which was joined by tungsten inert gas welding to an austenitic steel AISI 304. The mechanical properties of the dissimilar metal welds were characterized by cross-weld tensile samples, whereas the local deformation in the weld of the different welding zones was measured by digital image correlation. In accordance with the respective initial HEA condition (cold-rolled vs. heat-treated), the local strain behavior was divergent and influenced the global mechanical properties of both DMW types. Nonetheless, the experiments provided proof in principle of the weldability for dissimilar joints of the CoCrFeMnNi-HEA welded to conventional materials like austenitic stainless steels ensuring a corresponding capability for mechanical loading. This allows further considerations on the application of these innovative materials.
The new multi-element alloying concept of systems with defined entropy (HEA — high-entropy alloy or MEA — medium-entropy alloy) is increasing in material research interest. Improved properties or combinations of properties are shown by several systems. Thus, the resulting microstructures and production of HEA/MEA as well as properties have been primarily investigated so far. Furthermore, processing is a key issue to transfer HEA/MEA systems to real components. Since welding is the most important joining process for metals, it is crucial to investigate the influence of welding to guarantee component integrity. Since most HEA are made of expensive alloying elements such as Co or Ni, they will not be used entirely as structural materials. Thus, it can be advantageous to weld conventional alloys such as austenitic stainless steels with the HEA and MEA to produce components that are both application-oriented and economically viable. Therefore, in this paper, first results of dissimilar metal welding, by tungsten inert gas (TIG) and friction stir welding (FSW), of a CoCrFeMnNi HEA as well as a CoCrNi MEA with a conventional AISI 304 austenitic stainless steel are presented. The focus is on the microstructure formation due to the two welding processes. The results of TIG welding show a dendritic microstructure, whereas in FSW both materials are stirred but still coexist.
With the introduction of a hydrogen-based energy and national economy, safety-relevant components for hydrogen technologies are becoming increasingly important. Characteristic of hydrogen technologies are, for example, harsh environmental conditions such as cryogenic or high-pressure storage, corrosion issues in fuel cells and electrolyzers, turbines, and many more. Additive manufacturing of components is becoming increasingly important and irreplaceable for the production of complex technical systems. Using the case studies of burners for gas turbines and electrodes and membranes for polymer (PEMFC) and solid oxide (SOFC) fuel cells, this article shows the potential of additive manufacturing of components. At the same time, however, the challenge of considering divergent mechanical properties depending on the direction of assembly in a "hydrogen-compatible" manner is also highlighted. Finally, the challenges posed by additive manufacturing and hydrogen for materials testing are highlighted under scenarios that are as realistic as possible.
Offshore wind turbines are an important goal in national energy strategies worldwide. Foundation structures are manufactured from submerged arc welded (SAW) plates with thicknesses up to 200 mm. In that connection, high-strength steels like the S420G2+M are more and more applied offering the possibility for increased stability and load-bearing capacity of the foundations. These offshore steel grades can show a susceptibility for delayed hydrogen assisted cold cracking of the weld joints. For that purpose, a minimum waiting time (MWT) of up to 48 h (dependent on applied standards) is recommended before non-destructive testing is allowed and conducted. But this concept is based on older steel grades that have been used for three or more decades. Nowadays, the metallurgical improvements (clean steels, proper rolling, and heat treatment) of base materials and well as welding consumables must be anticipated. Hence, the MWT concept should be critically discussed as it is assumed to be very conservative. For that reason, the focus of this study was to investigate the diffusion behavior in S420G2+M steel and its multi-layer SAW joint. Electrochemical permeation experiments were carried at room temperature. Boundary conditions were anticipated in terms of using different sample thicknesses. From the experimental data, hydrogen diffusion coefficients and absorbed diffusible hydrogen concentrations had been calculated. It was shown that hydrogen diffusion in the base material is increased compared to the weld metal. In addition, the sample thickness had a significant on the calculated diffusion coefficients. The minimum and maximum diffusion coefficients had been used for numerical modelling of the hydrogen diffusion in the welding joint. It became clear that a MWT must be always regarded together with a critical initial diffusible hydrogen concentration for the evaluation of a possible delayed cracking as diffusion times were mostly > 48 h due to the thick plates.
Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragverhaltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberechnungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Ausscheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Abkühlbedingungen geschaffen.
Martensitic 9% Cr steels like P91 and P92 can show an increased susceptibility to delayed hydrogen-assisted cracking. The focus of this study was the microstructure and heat treatment efect on the mechanical properties of P92 base material and P91 multi-layer weld metal in both as-welded and post weld heat treated (PWHT) condition. Tensile tests with hydrogen free reference samples and electrochemically hydrogen charged samples were carried out; the mechanical properties were assessed and supported by detailed fractographic analysis. Finally, a hydrogen and microstructure-dependent fracture criterion is established. All investigated microstructures showed a hydrogen-infuenced degradation of the mechanical properties compared to the hydrogen-free reference samples. The as-welded martensitic P91 weld metal had the highest degree of degradation in the presence of hydrogen. The P91 PWHT weld metal and the P92 base material had comparable properties. From that point of view, a signifcantly increased risk for hydrogen-assisted cold cracking during welding fabrication of P91 weld joints must be considered before any heat treatment is conducted.
High-entropy alloys (HEAs) are innovative high-performance materials that have attracted more and more research attention. HEAs are characterized by a solid solution of typically five equiatomic metallic elements. In addition, medium-entropy alloys (MEA, with three elements) are of interest and become more and more important. Depending on the alloy concept, HEAs and MEAs show exceptional mechanical properties, especially high-strength and ductility combinations at both cryogenic and elevated temperatures combined with excellent corrosion resistance. Future structural HEA/MEA components can be exposed to potential applications with hydrogen containing environments like high-temperature water in pressurized nuclear reactors or aerospace structures. Other potential applications could be in materials for vessel walls in the field of cryogenic and high-pressure hydrogen storage. So far, the susceptibility of HEAs/MEAs to hydrogen assisted cracking (if any) and the hydrogen diffusion is not investigated in detail yet and can limit or extend possible applications of HEA/MEA as structural materials. In our work, we focused on the hydrogen absorption, diffusion, and distribution in a HEA (CoCrFeMnNi the original Cantor-alloy) and a MEA (CoCrNi). Cathodic hydrogen charging was carried out for the hydrogen ingress, and thermal desorption analysis (TDA) revealed complex hydrogen trapping in both alloy types up to 300 °C. The absorbed total hydrogen concentrations were > 100 ppm for the HEA and > 40 ppm for MEA. In addition, the assessment of the peak deconvolution is not trivial and must consider both experimental and microstructure influences.
Multielement-Legierungen (MPEA – multiple pricipal element alloys) stellen eine neue Klasse von Werkstoffen dar, die aus mindestens drei äquiatomaren Legierungselementen mit jeweils einem Gehalt von 5–35 Atom-% bestehen. Somit unterscheidet sich das Legierungskonzept fundamental von konventionellen bspw. Stahl- oder Al-basierten Legierungen. In jüngster Zeit lag der Schwerpunkt auf dem Legierungs-Design der MPEA und der Überprüfung bzw. Erreichung der gewünschten Eigenschaften bzw. -kombinationen. Hierzu werden die egierungselemente gezielt ausgewählt und die Mikrostrukturen ein- und zum Teil auch mehrphasig eingestellt. Ziel sind hochinnovative MPEA mit angepassten Eigenschaften für die industrielle Anwendung. Dabei sollen insbesondere die bei konventionellen Legierungen wesentlichen Zielkonflikte, wie bspw. der Trade-off zwischen Festigkeit und Duktilität, überwunden werden. Darüber hinaus sind mechanische Eigenschaften bei sehr hohen sowie kryogenen Temperaturen bei gleichzeitig höchster Korrosionsbeständigkeit von hohem Interesse. Die Herstellung von Bauteilen erfordert dazu werkstoff- und beanspruchungsgerechte Füge- bzw. Schweißverfahren. Der Schweißeignung von MPEA wurde bis Ende 2021 nur äußert wenig Aufmerksamkeit zuteil. Die Auswirkungen durch Schweißprozesse auf die Metallurgie und die gewünschten Eigenschaften sind bisher kaum bekannt und limitieren die potenzielle Anwendbarkeit als Funktions- oder Konstruktionswerkstoffe.
In einem interdisziplinären BAM-Forschungsprojekt werden aktuell grundlegende Untersuchungen zur Schweißverarbeitung und resultierender Mikrostruktur-Anwendungseigenschafts-Beziehung verschiedener MPEA durchgeführt. Insbesondere Wärmeeinflusszone und Schweißgut sind geprägt durch eine Mikrostruktur, die aus Ungleichgewichtszuständen resultiert. Im Falle von MPEA wurde dies bisher nicht systematisch untersucht. Dazu erfolgte im Rahmen des Projektes eine umfassende Literaturauswertung zum Schweißen von MPEA und Zusammenfassung in einer umfassenden, systematischen Datenbasis. Aus diesem Grund sollen in der vorliegenden Studie die bisher bedeutsamsten Erkenntnisse zur Schweißbarkeit von MPEA systematisch nach MPEA-Typ und Schweißverfahren geordnet und mit eigenen aktuellen Forschungsergebnissen verglichen werden. Durch WIG- und Rührreibschweißversuche an den MPEA-Systemen CoCrNiFeMn bzw. CoCrNi konnten im Projektverlauf bereits wesentliche Fragestellungen beantwortet werden. Dazu zählen Auftreten bzw. Verhinderung intermetallischer Phasen/Seigerungen oder deren Auswirkung auf die Eigenschaften der Schweißverbindung (bspw. Festigkeit oder Korrosionsbeständigkeit).
Die Herausforderungen für die Fügetechnikbranche, die sich durch die neuen Wasserstoff-Technologiefelder „Erzeugung“, „Speicherung“, „Transport“ und „Nutzung“ ergeben, sind sehr vielfältig. Der DVS-Bericht 373 gibt dazu einen tieferen Einblick. Der hier vorliegende Kurzbericht stellt dazu ausgewählte Praxisbeispiele, zugehörige Herausforderungen und sich ergebende Chancen vor. Fügetechnologien haben dabei wesentliche Bedeutung für das erfolgreiche Umsetzen und Herstellen der benötigten technischen Komponenten, wie anhand der Themenkomplexe „Wasserstoff-Pipelines“ und „additive Fertigung“ betrachtet wird. Zudem ergeben sich Herausforderungen für die notwendigen Regelwerke und Normen, die nahezu vollständig angepasst oder geschaffen werden müssen.