- nein (4)
Maintenance, Repair and Overhaul (MRO) is acquiring increasing commercial and socio-economic significance. For products and goods with high investment costs and a long lifespan, especially in the sectors of energy and transportation, a considerable portion of commercial profits are generated by after-sales services. In the field of research and development, not enough attention has been paid so far to tasks and approaches involving MRO. The field thus has a limited scientific background, despite a high potential in the business sector for technological and scientific optimization. The challenges and chances of MRO for sustainable enterprises will be explained with reference to the Fraunhofer Innovation Cluster Maintenance, Repair and Overhaul in Energy and Transport. The developments and project results of the four fields of innovation »Cleaning«, »Repair and Overhaul«, »Condition Monitoring and Diagnosis«, as well as »MRO Planning and Digital Assistance« will be explained.
The industrial demand for flexible and innovative manufacturing technologies is continuously increasing. These technologies have to be sustainable and resource-efficient, and have to allow the production of long-life capital goods. Consequently, the additive processes gain in importance as they offer an enormous potential of application, especially for the turbomachinery industry.
In order to use additive manufacturing technologies in industrial applications, it is necessary to consider the complete process chain, including all necessary pre- and postprocessing. Although additive manufacturing is increasingly covered in scientific research, the linking between this technology and conventional industrial processes is rarely described.
Laser remote welding is a dynamic and flexible joining technology which enables various new approaches in welding sequence and weld position planning. However, the challenge is to find the optimal set-up within this large parameter space. In this article, numerical welding simulation is used to deal with this challenge. For a car door, different welding sequences and weld positions were numerically analyzed and compared with respect to its welding distortion behavior.
Der Fokus des vorliegenden Beitrages liegt in der Anwendung der numerischen Schweißsimulation zur Berechnung des schweißbedingten Verzugs an industriellen Bauteilen. Anhand einiger Applikationsbeispiele werden die Möglichkeiten und Einschränkungen am Markt verfügbarer Softwareprodukte aufgezeigt. Hierbei liegt die Gewichtung in einer qualitativ korrekten Abbildung der zu analysierenden Phänomene. Diese stellt die Basis für nachfolgende Parameterstudien dar, welche signifikante Einflussgrößen auf die Verzugsausbildung detektieren. Der Vorteil derartiger simulationsgestützter Analysemethoden gegenüber rein experimentellen Ansätzen wird diskutiert. Aufgrund der heutigen Verfügbarkeit spezialisierter anwenderfreundlicher Schweißsimulationssoftware und günstiger Rechenressourcen macht die Industrie in den letzten Jahren immer mehr von den zahlreichen Vorteilen einer virtuellen Prozessauslegung mit Hilfe der Schweißsimulation Gebrauch. Komplexe Praxisanwendungen können heutzutage innerhalb von 1-2 Wochen unter Berücksichtigung aller Arbeitsschritte bearbeitet werden. Die Anforderungen an den Anwender seitens der Numerik und Materialmodellierung hat sich drastisch verringert, wohingegen ein gewisses Maß an Wissen und Erfahrung vom simulierten Prozess weiterhin entscheidend für den Erfolg der Simulation ist. Am Beispiel des Einspritzventils konnte das Potential einer virtuellen Prozessauslegung anschaulich aufgezeigt werden.
Understanding the influence of tool/pin shapes on the thermal and material flow behaviors in friction stir welding is of great significance for the optimal design of tool/pin based on a scientific principle. In this study, a numerical method based on computational fluid dynamics is employed to quantitatively analyze the thermo-physical phenomena in friction stir welding with two tools of different pin shapes (axisymmetrical conical tool and asymmetrical triflat tool). Through combining a steady state model with a transient state model, both the computation efficiency and accuracy are ensured. The boundary conditions of heat transfer and material flow are determined with considering a partial sticking/sliding contact condition at the toolworkpiece interface. The total heat generation, heat density and temperature distribution during the welding process with triflat tool are elucidated and compared with that of conical tool, and the material flow patterns and deformation regions of various pin orientations are illustrated in detail. It is found that the deformation zone caused by triflat tool is larger than that by conical tool, which is validated by the weld macrographs. The computed thermal cycles and peak temperature values at some locations are in good agreement with the experimentally measured ones.
Life Cycle Assessment (LCA) is applied in evaluating environmental impacts of state-of-the-art welding technologies. Manual Metal Arc Welding (MMAW), Laser Arc-Hybrid Welding (LAHW) and two Gas Metal Arc Welding (GMAW) variants are used to join a plate of 20 mm thick structural steel. The LCA results indicate that for 1 m weld seam, MMAW causes the highest environmental impacts in global warming potential (GWP), eutrophication potential (EP), acidification potential (AP), and photochemical ozone creation potential (POCP) among the selected processes, and the LAHW variant performances the least. Filler material and electricity consumptions generally dominate the impacts and reach shares of up to 80% and 61% in the respective impact categories. However, electrode coating consumption in MMAW remarkably contributes impacts on AP and EP, for instance 52% of AP and 76% of EP. Strategies for improvement of the applied welding technologies are discussed.
Partial penetration welding with a fiber laser at a 9-kW laser power was carried out on 20-mm-thick plates at different positions and analyzed by both experimental and numerical methods. Experiments were carried out for four different angular positions at 1.5 m/min welding speed. All four cases showed a tail-like structure of molten pool on the top surface. The in-depth mechanisms of the energy input characteristics in fiber laser position welding for eight different positions were studied by numerical simulation using the volume-of-fluid (VOF) method. Experimental and numerical results were compared for four cases and showed fair agreement. Observation of flow pattern and bead shape revealed that gravity had little influence on bead shape and flow structure, but changed the pore structure considerably. Flow structure showed a periodic behavior which probably nullified the effect of gravity in position welding. Most of the laser rays reached the bottom of the keyhole without interruption and then multiple reflections started within the keyhole. The first five reflections inside the keyhole delivered around 70 % of the total energy.
The presented apparatus enables laser beam welding of thick materials under local reduced pressure conditions, thus improving the quality of welds and reducing the laser beam power necessary for complete penetration welding. The vacuum cap presented in this article uses a local reduced ambient pressure environment in a tight zone around the welding area and, in contrast to a conventional vacuum chamber, it is movable in the welding direction. The mobile installation is very compact and reaches pressure values of around 200 mbar. The reduced pressure in the vacuum cap is sufficient to generate 50 % higher penetration depth in comparison to welding under ambient pressure conditions. The low pressure around the keyhole reduces the vapour-plasma plume and therefore prevents a defocusing and scattering of the laser radiation. This allows to raise the amount of laser beam power entering the keyhole as well as the effective power density.