Filtern
Erscheinungsjahr
Dokumenttyp
- Beitrag zu einem Tagungsband (78)
- Zeitschriftenartikel (49)
- Beitrag zu einem Sammelband (37)
- Vortrag (22)
- Buchkapitel (8)
- Posterpräsentation (5)
- Sonstiges (2)
- Forschungsbericht (1)
Sprache
- Englisch (104)
- Deutsch (97)
- Mehrsprachig (1)
Schlagworte
- Beton (20)
- UHPC (14)
- Rheology (13)
- Concrete (12)
- Baustoffe (11)
- Zement (10)
- AKR (9)
- Durability (8)
- Self-compacting concrete (7)
- Alkali-Kieselsäure-Reaktion (6)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (38)
- 7.1 Baustoffe (38)
- 4 Material und Umwelt (5)
- 7.4 Baustofftechnologie (5)
- 4.4 Thermochemische Reststoffbehandlung und Wertstoffrückgewinnung (4)
- 7.7 Modellierung und Simulation (2)
- 4.0 Abteilungsleitung und andere (1)
- 7.0 Abteilungsleitung und andere (1)
- 7.2 Ingenieurbau (1)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (22)
Untersuchung des Einflusses der Gefügedichte von Betonen auf die AKR mit neuartiger Prüftechnik
(2011)
Trotz der zahlreichen Möglichkeiten zur Beeinflussung der Mörteleigenschaften durch Mischungsmodifikationen ist es nahezu unmöglich, einzelne Eigenschaften unabhängig von anderen zu verändern. Bei einer Mischungsoptimierung muss im Einzelfall immer entschieden werden, welcher der gewünschten Eigenschaften die höchste Priorität zukommt. Anhand von Parameterstudien wird im vorliegenden Artikel verdeutlicht, wie es für bestimmte Anwendungen sinnvoll sein kann, die Verschlechterung einzelner Eigenschaften zu akzeptieren, wenn dadurch eine für den speziellen Einsatzfall essenzielle Eigenschaft verbessert werden kann. Die komplexen Wechselwirkungen der einzelnen Bestandteile fuhren dazu, dass auch scheinbar widersprüchliche Kombinationen von Zusatzmitteln im Einzelfall erforderlich werden können. Zur Anpassung der meisten Mörteleigenschaften gibt es verschiedene Möglichkeiten der Zielerreichung mit jeweils unterschiedlichen Nebeneffekten. Frisch- und Festmörteleigenschaften sind dabei gleichermaßen zu beachten.
It has been shown in fire tests that polypropylene fibres reduce or avoid explosive spalling of high performance concrete. In the critical temperature ränge up to 300 °C the permeability of HPC increases by using polypropylene fibre. Due to this the water vapour, which is the main reason for explosive spalling, can escape. There exist different theories in the literature conceming the micro structural mechanisms, which cause an increase in the permeability. Within the framework of an internal research project at BAM an innovative methodology was developed for experimental verifying of existing theories and to get new insights into this problem The methodology used is unique and has been undertaken here for the first time. This consists of the combination of acoustic emission and ultrasonic measurement during temperature loading and the non-destructive micro structural analysis of cooled down samples with the aid of micro X-ray computed tomography. For the validation of the nondestructive test methods scanning electron microscopic images of prepared samples were undertaken. The results show that due to the thermal decomposition of the polypropylene fibres micro canals emerge. These are connected due to a simultaneous micro cack formation.
Whenever the preservation of original substance obtains priority in a restoration task, reprofiling techniques using repair mortars are a welcome solution. For ordinary concrete repair aesthetic aspects are of minor importance whereas for the restoration of natural stone elements they come to the fore. Especially for listed buildings and monuments, historico-cultural and aesthetical interests become the ruling Parameters for planning and execution of restoration tasks. Nevertheless the technical and constructive requirements have to be considered and deterioration processes have to be understood to ensure sustainability and durability of the repair task. Due o differences in the Chemical and mineralogical composition, natural stone provides a vast variety of texture and colour. Also the range of different mechanical and durability related properties is far wider than found with concrete for example. A research project dealing with the development of a modular repair mortar System for natural stone is currently set up at the BAM. To provide the conservator with the best possible options to match colour, texture and technical requirements, the System will be setup on a modular basis. Several different binder Systems on basis of cement, lime and sodium Silicate as well as polymer based Systems are planned, which can be combined with different aggregate compositions and different pigments. To evaluate the mortar performance, test procedures will be defined for tests on mortar samples and on composite specimens. In the paper the experimental Programme will be explained and first results will be presented and discussed.
Wärmebehandlung und Autoklavierung von UHPC - Neue Perspektiven für die Betonfertigteilindustrie
(2011)
Das Gefüge von UHPC ist durch eine dicht gepackte und fehlstellenarme Matrix gekennzeichnet. Eine zusätzliche Optimierung ist durch eine Wärmebehandlung bzw. hydrothermale Nachbehandlung (Autoklavierung) unter einem Wasserdampfsättigungsdruck möglich. Die Wärmebehandlung von Beton ist ein in der Betonfertigteilindustrie geläufiges Verfahren, um die Erstarrungszeit zu verkürzen und höhere Frühfestigkeiten zu erreichen.
This paper presents the results of an experimental study on the influence of polypropylene (PP) fibres on the thermal strain of high strength concrete (HSC) at temperatures up to 750°C. Concerning this topic only few results can be found in the literature and systematic investigations are missing. However, basic knowledge is necessary to understand the internal damage processes as well as for structural design.
To explain the differences in the thermal strain of HSC with and without addition of PP fibres the internal damage processes were investigated with acoustic emission (AE) analysis and ultrasound (US). Furthermore the weight loss was measured continuously during heating to monitor the drying of the specimen. This novel approach by combining these different methods with strain measurements at high temperatures allows the integral description of the internal damage processes. The results reveal significant differences in the thermal strain of HSC when PP fibres are added. Between 200°C and 250°C the thermal strain of HSC with PP fibres is superimposed by shrinkage caused by accelerated drying. Above 250°C it is lower than that of plain HSC without PP fibres. It is supposed that it is caused by a more homogeneous distribution of micro cracks whereby the fibre beds acting as defects in the concrete.
Hence this paper gives a contribution to the general understanding of the impact of PP fibres in HSC at high temperatures and points out the influence of the fibres on the thermal strain of HSC.