Filtern
Dokumenttyp
Schlagworte
- Elastomer (8)
- Compression set (6)
- DSC (5)
- Dichtungen (5)
- Dynamic mechanical analysis (5)
- Elastomere (5)
- Druckverformungsrest (4)
- Glass transition (4)
- Low temperature behaviour (4)
- Sealing material (4)
Rubbers are widely used as sealing material in various applications. In many fieldsthefunction of seal materials at lowtemperatures is required. Therefore the understanding of faiiure mechanisms that lead to leakage at low temperatures is of high importance. Therefore the lower Operation temperature limit of rubber seals should be determined in dependence of the material properties.
The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the Standard tests a faster and more efficient technique was developed and applied. In addition the breakdown temperature of the sealing function of O-ring seals at lowtemperatures is measured in a component test Setup in dependence of the material and the degree of compression.
Rubber is widely used as sealing material in various applications. In many fields the sealing function at low temperatures is necessary. Therefore the understanding of failure mechanisms is of high importance. Rubbers are normally used above their glass-rubber transition region but the minimum working temperature limit is not defined precisely. Therefore the lower operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with the results of the standardized compression set according to ISO 815 respectively a modified test using the DMA equipment.
EVA is a widely used material for the encapsulation of photovoltaic modules. It melts at elevated temperatures, and seals the module before it is crosslinked at temperatures above 130 °C by a peroxide-initiated crosslinking reaction. EVA has good optical properties necessary for application in solar modules. For process optimization and quality management, a method for the quick and reliable characterization of EVA crosslinking behaviour is of great value. Here, the practicability of ultrasound for online crosslinking monitoring is demonstrated. A sound velocity increase of about 8 m/s during the crosslinking reaction is found. The ultrasound results are compared with rheometer measurements performed with a curemeter typically used for the investigation of rubber crosslinking.
Two types of commercially applied Ethylene/Vinyl Acetate Copolymers (EVA) for encapsulation of photovoltaic modules were investigated by the thermal analysis methods of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) in the temperature range from -150 °C to 200 °C. Glass transition, crystal melting and cross-linking were analyzed. The aims of the investigations were to gain more information for incoming goods control and to get information about the whole temperature dependent material properties in the investigated temperature range, starting at very low temperatures up to the crosslinking temperature region.
Rubbers are widely used as main sealing materials for containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste containers. According to appropriate guidelines and regulations safe enclosure of the radioactive container contents has to be guaranteed for long storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of seal behavior is of high importance.
In this paper we focus on the behavior of elastomer seals at low temperatures with regard to poten-tial decrease of leak-tightness. In addition, changes in material properties due to aging effects over long periods of time and their influence on the seal performance is investigated.
It is known that material properties of rubbers are strongly temperature dependent. At low tempera-tures this is caused by the rubber-glass transition (abbr. glass transition). During continuous cool-ing, the material changes from rubber-like entropy-elastic to stiff energy-elastic behavior, that al-lows nearly no strain or retraction due to the glass transition. Hence rubbers are normally used above their glass transition but the minimum working temperature limit is not defined precisely.
Aging of elastomer seals is important, as possible dynamic loads may have to be considered during the whole interim storage period (so far approved in Germany for up to 40 years) and for transporta-tion after storage.
For the investigations, fluorocarbon (FKM) and ethylene-propylene-diene (EPDM) rubbers were selected as they are often used in radioactive waste containers. Some materials were purchased from a commercial seal producer and some materials were compounded and cured at BAM. The elastom-ers where studied by several thermo-analytical methods and compression set to characterize the material behavior at low temperatures. Additionally component tests were performed to determine the breakdown temperature of the sealing function of complete elastomer O-rings.